Quality Optimization of Commercial FeCrAl Tube Production

The objectives of this report are to summarize the various process parameters and conditions that trigger premature failures during the production steps for Generation II ATF FeCrAl seamless tubes in commercially available manufacturing processes, and to suggest optimized processing routes and parameters to improve the quality and the material yield of commercial tube production. The production process steps include (1) the heat production process, (2) the master bar production process, and (3) the tube reduction process. For heat production, not only chemical composition control but also elimination of solidification defects in the vacuum induction–melted ingot are key. A hot-isostatic press helped in reducing and eliminating the internal, preexisting cracks in the ingot, which could be a source of premature failure (e.g., crack initiation from oxide particles) in the latter part of the tube production process. The master bars were produced by a hot-extrusion process. The area reduction ratio and the extrusion temperature are key to controlling the quality of the master bars and the grain structure. Because of the limited deformation ability of FeCrAl alloys, especially at ambient temperatures, a controlled, uniform grain structure with relatively small grains (<100 µm) is required at the beginning of the tube reduction process. Furthermore, a relatively small amount of area reduction per pass, combined with controlled inter-pass annealing, is important to achieve a reduction in failure events, a highly uniform wall thickness, concentricity, and a high-quality surface finish. Based on the knowledge obtained regarding process conditions, FeCrAl tube production with optimized process parameters is currently in progress. A portion of the final tube inventory was delivered in late June 2017. Cross-sectional microstructural characterization was completed for screening the quality of as-received tubes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermodynamics of Bimetallic Joints between Titanium and Tantalum Produced by Laser Powder Bed Fusion

Laser powder bed fusion (LBPF) is currently the most mature metal additive manufacturing (AM) technology. While it does not have the same flexibility as directed energy deposition techniques to produce compositional gradients, LPBF can still be used to generate bimetallic parts by depositing one metal on a build plate made of another. Here, in this study, we print combinations of Ti-6Al-4V with Ta and characterize defects that occur at the interface. We use thermodynamic modeling to explain the formation of keyhole porosity and solidification cracks when Ta is built on a Ti baseplate, and the lack of defects when the materials are reversed. By understanding the mechanisms that lead to defect formation, the methodology demonstrated here can be applied to other material systems to efficiently design bimetallic LPBF processes.

36 MATERIALS SCIENCE↗

Texture evolution as a function of scan strategy and build height in electron beam melted Ti-6Al-4V

Metal additive manufacturing (AM) enables customizable, on-demand parts, allowing for new designs and improved engineering performance. Yet, the ability to control AM metal alloy microstructures (i.e., grain morphology, crystallographic texture, and phase content) is lacking. Furthermore, this work performs corroborative neutron diffraction and large-scale electron backscatter diffraction (EBSD) measurements to assess crystallographic texture in electron beam melted (EBM) Ti-6Al-4V as a function of scan strategy and build height. Texture components for one raster and two spot melt scan strategies were evaluated using a triclinic specimen symmetry to capture all possible texture components, which were found to be considerably different than previously reported values from studies employing orthotropic specimen symmetry. This finding highlights the importance of a standard method and best practice for assessing textures produced by AM.

36 MATERIALS SCIENCE↗

Effect of cooling rate and Mg addition on the structural evaluation of rapidly solidified Al-20wt%Cu-12wt%Fe alloy

The present work examines the effect of Mg contents and cooling rate on the morphology and mechanical properties of Al{sub 20}Cu{sub 12}Fe quasicrystalline alloy. The microstructure of the alloys was analyzed by scanning electron microscopy and the phase composition was identified by X-ray diffractometry. The melting characteristics were studied by differential thermal analysis under an Ar atmosphere. The mechanical features of the melt-spun and conventionally solidified alloys were tested by tensile-strength test and Vickers micro-hardness test. It was found that the final microstructure of the Al{sub 20}Cu{sub 12}Fe samples mainly depends on the cooling rate and Mg contents, which suggests that different cooling rates and Mg contents produce different microstructures and properties. The average grain sizes of the melt spun samples were about 100–300 nm at 35 m/s. The nanosize, dispersed, different shaped quasicrystal particles possessed a remarkable effect to the mechanical characteristics of the rapidly solidified ribbons. The microhardness values of the melt spun samples were approximately 18% higher than those of the conventionally counterparts. - Highlights: •Quasicrystal-creating materials have high potential for applications. •Different shaped nanosize quasicrystal particles were observed. •The addition of Mg has an important impact on the mechanical properties. •H{sub V} values of the MS0, MS3 and MS5 samples at 35 m/s were 8.56, 8.66 and 8.80 GPa. •The volume fraction of IQC increases with increasing cooling rates.

36 MATERIALS SCIENCE↗

Plastic homogeneity in nanoscale heterostructured binary and multicomponent metallic eutectics: An overview

Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.

36 MATERIALS SCIENCE↗

Advances and Achievements in In Situ Analysis of Corrosion and Structure–Property Relationship in Mg Alloys

Every year, TMS Magnesium Committee carefully selects a special topic in magnesium (Mg) related research and development not only having the hottest subject from both academic and industrial perspectives but also demonstrating major achievements within this subject. Following last year’s topic on Mg microallying [1], this year’s focus is on in-situ methods and associated techniques in their broad definition spanning from laboratory- to large- scale facilities to process monitoring. The applications of in-situ techniques have a wide spectrum from the analysis of melts and liquid-solid transitions to solid-state phenomena during thermo-mechanical processing and heat treatments to surface interactions with various environments. Therefore, such works are of significant interest to scientists working in the area of Mg alloy development as well as to a much broader audience from both academia and industry. This interest is primarily caused by challenges in the analysis of structure-property relationship in Mg alloys, and even cursory glance of literature reveals sharp increase of publications relevant to this topic recently. For instance, very high reactivity of Mg as well as its well-known propensity to substantially alter structure upon unloading in mechanical testing makes it difficult to understand and thus to simulate correlation between microstructures observed in post-mortem analysis and physical processes during testing or fabrication. However, recent advances in in-situ analysis based on large-scale research facilities such as neutron scattering and synchrotron radiation sources as well as microscopy-based, acoustic emission, and other more traditional techniques allowed significant achievements. Apart from apparent development of relevant experimental techniques, a significant part of this success should also be attributed to increasing accessibility of the facilities and simplification of their use from a user perspective. The selection of articles in this special topic is quite far from comprehensive review covering all aspects of in-situ methods available for metallic materials development. However, this was not the purpose in any case. Instead, this selection is intended to present several studies on Mg alloys and Mg-based composites with the use of in-situ techniques. In addition, it overviews two techniques, ‘Acoustic Emission’ (AE) and ‘Ambient-Pressure X-ray Photoelectron Spectroscopy’ (AP-XPS), that are rather novel to the Mg community. These studies are supposed to give readers representative examples of such techniques potential and to help in navigating the spectrum of modern state-of-the-art analytical methods facilitating the development of Mg alloys. These articles are organized in the order corresponding to typical Mg alloy lifecycle from material preparation and solidification to thermo-mechanical processing and product fabrication to degradation.

36 MATERIALS SCIENCE↗

The role of ternary alloying elements in eutectoid transformation of U10Mo alloy part I. Microstructure evolution during arc melting and subsequent homogenization annealing in U9.8Mo0.2 X alloy ( X = Cr, Ni, Co)

This paper describes the microstructural evolution in an alloy of uranium with 10 wt.% molybdenum (U10Mo), with minor addition of a third alloying element, namely, Cr, Ni, or Co, at 0.2 wt.%. The microstructures of arc-melted buttons in the as-cast condition show significant Mo segregation. The segregation behavior of Cr, Ni, and Co was investigated through detailed scanning electron microscope imaging. A homogenization heat treatment at 900°C for 48 h results in uniform Mo distribution and associated grain growth in all of the four alloys that were fabricated. Further, formation of multiple phases was noted in U-9.8 wt.% Mo-0.2 wt.% Ni and U-9.8 wt.% Mo-0.2 wt.% Co alloys after the homogenization annealing step. The greatest grain-boundary-initiated eutectoid transformation as measured by % volume fraction was observed when the homogenized U-9.8 wt.% Mo-0.2 wt.% Ni alloy was aged at 500°C for 20 h. The least eutectoid transformation occurred in U10Mo.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Shape memory properties and microstructural evolution of rapidly solidified CuAlBe alloys

In this work, the effects of Be addition on the microstructure and phase transformation temperatures of Cu–12Al–xBe (x = 0.4, 0.5 and 0.6 wt.%) shape memory alloys fabricated by using the arc-melting and melt-spinning techniques have been investigated. X-ray diffraction analysis revealed that the arc-melted alloys consisted of austenitic β{sub 1}, martensitic β{sub 1}′ and γ{sub 2} precipitate phases, whereas melt-spun ribbons were composed of a fully martensitic phase. The average grain size of martensitic phases in melt-spun ribbons was determined by electron microscopy images, showing a decrease with increasing Beryllium (Be) amount. Moreover, it was found that the Be addition in the arc-melted alloys had a distinct effect on the morphology of the γ{sub 2} precipitate phase. Transmission electron microscopy analysis showed that the thickness of martensitic plates in the melt-spun ribbons reduced with increasing Be addition. In a differential scanning calorimeter analysis, no martensitic transformation (M{sub s}) peak was observed in arc-melted alloys, but it was clearly detected in melt-spun ribbons, in which M{sub s} decreased dramatically with increasing Be addition. The improvement in the shape memory ability of melt-spun ribbons was explained in terms of the refinement in grain size and martensitic plates. - Highlights: • The CuAlBe SMAs were produced by means of arc-melter and melt-spinner techniques. • MT was directly obtained in melt-spuns without any intermediate process. • The transformation temperatures decreased with increasing Be amount. • The thickness of martensitic plates in the ribbons reduced with increasing Be. • SMP of CuAl was improved by the addition of Be together with rapid solidification.

36 MATERIALS SCIENCE↗

Solidification texture, variant selection, and phase fraction in a spot-melt electron-beam powder bed fusion processed Ti-6Al-4V

The effect of a spot melt strategy on the solidification texture, variant selection, phase fraction, and their variations along the build height was investigated in comparison to a conventional linear melt strategy. Ti-6Al-4V alloy samples were manufactured by an electron-beam powder bed fusion process using two different melt strategies and characterized using high-energy synchrotron x-ray diffraction. The linear and spot melt cases resulted in β<100> cube and fiber textures, respectively, with the cube/fiber axis nearly parallel to the build direction. The α phase exhibited Burgers orientation relationship (BOR) with the parent β phase for both melt strategies. Although all of the key texture components and the BOR between the α and β phases were consistently observed in both cases along the build height, there were several measurable differences between the two. At the top of the build height, the β<100> build texture intensity was stronger in the linear case. However, the texture intensity in the linear case decreased gradually from the top to near the substrate, whereas the spot melt case did not show this trend. Moreover, the BOR was examined along the build height and the results showed that there is a distinct variant selection in the spot melt case, unlike the linear case. Specifically, the planar variants sharing ($\bar101$) β || (0002) α with [$\bar2\bar2\bar2$]β and [$2\bar22$]β were the most prominent in the spot melt, but no preference was identified in the directional variants. The β phase fraction was slightly lower in the spot melt case compared to the linear case. In both the cases, the β phase fraction decreased moving towards the substrate but remained significantly higher than that of the powder feedstock. Overall, the novel spot melt strategy produced a more homogeneous microstructure in terms of both the phase fraction and texture across the build height.

36 MATERIALS SCIENCE↗

Additively-manufactured Al-0.3Zr-0.2Ce-0.2Cu alloy with high creep resistance and electrical conductivity

Here, a new, solute-lean Al-0.3Zr-0.2Ce-0.2Cu (wt.%) alloy is developed for additive manufacturing that overcomes the classical tradeoff between conductivity and creep resistance. The rapid-cooling-enabled supersaturation of Zr, and its uniform distribution in α-Al matrix, along with formation of submicron (Ce,Cu)-rich intermetallic particles on solidification lead to unusually high creep resistance at 200 °C. Near-zero secondary creep rates are achieved up to the alloy yield stress (YS) of 65 MPa at 200 °C in as-fabricated state. The Zr-solute-induced dislocation-climb suppression mechanism underlying this improvement also restricts dynamic recovery above YS, as noted from appreciable primary creep and its transitioning to near-zero secondary creep rates. A combination of relatively coarse, epitaxially-grown α-Al grains, low Zr concentration in α-Al, and the impurity-scavenging effect of Ce to purify α-Al matrix produces high electrical conductivity of ∼48 %IACS. Aging precipitation of L1 2 -Al 3 Zr nanoprecipitates doubles the YS (to ∼150 MPa) at room temperature and increases alloy conductivity to ∼58 %IACS, but loss of solid-solution Zr out of α-Al matrix leads to activation of dislocation climb, degrading the creep properties as compared to the supersaturated Al-Zr solid solution in the as-fabricated state. Compared to L1 2 -Al 3 Zr nanoprecipitates, submicron (Ce,Cu)-rich particles formed on solidification are more effective at impeding dislocation climb, producing a threshold stress for dislocation creep of ∼ 50 MPa at 200 °C. The new alloy design concepts, especially solute-induced dislocation-climb suppression for creep resistance, explored here may pave way for the design of new metallic alloys for thermal/electrical conductors and other high-temperature applications.

Additive Manufacturing↗

Investigation on microstructure characterization and property of rapidly solidified Mg-Zn-Ca-Ce-La alloys

Rapidly solidified (RS) Mg-Zn-Ca-Ce-La (wt.%) alloys have been produced via atomizing the alloy melt and subsequent splat-quenching on the water-cooled copper twin-rollers in the form of flakes. Microstructure characterization, phase compositions and thermal stability of the alloys have been systematically investigated. The results showed that with addition of RE (Ce and La) to the Mg-6Zn-5Ca alloy, the stable intermetallic compounds i.e. the Mg{sub x}Zn{sub y}RE{sub z} phase with a few Ca (about 3 at.%), shortened as the T Prime phase, were formed at the expense of the binary Mg-Zn and Ca{sub 2}Mg{sub 6}Zn{sub 3} phases, which was possibly beneficial to the enhanced thermal stability of the alloy. In the Mg-6Zn-5Ca-3Ce-0.5La alloy, the composition of the T Prime phase in the grain interior was different from that at the grain boundaries, in which the segregation of the La elements was found, and the atomic percentage ratio of Zn to Ce in the T Prime phase within the grains was close to 2. Moreover, the stable Mg{sub 2}Ca phases were detected around the T Prime phases at the grain boundaries in the alloy. - Research Highlights: Black-Right-Pointing-Pointer The phase constitution of RS Mg-6Zn-5Ca alloy can be improved by RE additions. Black-Right-Pointing-Pointer In the Mg-Zn-Ca-Ce-La alloys, the Mg{sub x}Zn{sub y}RE{sub z} phase with a few Ca (T Prime phase) is formed. Black-Right-Pointing-Pointer The formation of the T Prime phase leads to the loss of the Mg-Zn and Ca{sub 2}Mg{sub 6}Zn{sub 3} phases. Black-Right-Pointing-Pointer The composition of the T Prime phase differs from the grain interior to the grain boundary.

36 MATERIALS SCIENCE↗

Investigation of structural and magnetic properties of rapidly-solidified iron-silicon alloys at ambient and elevated temperatures

In this work, we investigated the ambient temperature structural properties (~300 K) and the ambient and high temperature (up to 900 K) direct current (DC) magnetic properties of melt-spun Fe-x wt.% Si (x = 3, 5, & 8) alloys. The wheel surface speeds selected for the study were 30 m/s and 40 m/s. The thickness, width, lattice parameter, saturation magnetization (MS), and intrinsic coercivity (HCI) of the melt spun ribbons are presented and compared with data in the literature. The ribbons produced at the lower wheel surface speed (30 m/s) were continuous having relatively uniform edges compared to the ribbons produced at the higher wheel surface speed. The thickness and the width of the melt-spun ribbons ranged between ~15-60 μm and 500-800 μm, respectively. The x-ray diffraction spectra of the melt-spun ribbons indicated the presence of disordered α-phase, irrespective of the composition, and the wheel-surface speed. The lattice parameter decreased gradually as a function of increasing silicon content from ~0.2862 nm (Fe-3 wt.% Si) to ~0.2847 nm (Fe-8 wt.% Si). Wheel surface speed was not shown to have a significant effect on the magnetization, but primarily impacted the ribbon structure. A decreasing trend in the saturation magnetization was observed as a function of increased silicon content. The intrinsic coercivity of the melt-spun alloys ranged between ~50 to 200 A/m. Elevated temperature evaluation of the magnetization in the case of Fe-3 & 5 wt.% Si alloy ribbons was distinctly different from the Fe-8 wt.% Si alloy ribbons. The curves of the as-prepared Fe-3 wt.% Si and Fe-5 wt.% Si alloy ribbons were irreversible while that of Fe-8 wt.% Si was reversible. The MS for any of the combinations of wheel surface speed and composition decreased monotonically with the increase in temperature (from 300 – 900 K). The percentage decrease in MS from 300 K to 900 K for the Fe-3 wt.% Si and Fe-5 wt.% Si alloys was ~19-22 %, while the percentage decrease in the same temperature range for Fe-8 wt.% Si alloy was ~26-30 %. It appears that Fe-3 wt.% Si and Fe-5 wt.% Si alloys ribbons are primarily comprised of the α phase (disordered phase) with any minor constituents being beyond the detection limits of the studies performed, while the Fe-8 wt.% Si alloy ribbons are comprised of disordered and regions of short-range ordering.

Elevated Temperature↗