Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solids Formation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Glass formation and short-range order structures in the BaS + La 2 S 3 + GeS 2 system

Infrared (IR) optical materials have enabled a broad range of optical sensing and measurement applications in the mid-wave and long-wave IR. Many IR transmitting glasses are based on covalently-bonded selenides and tellurides, such as As 2 Se 3 and GeTe 2 , which typically have relatively low glass transition temperatures (T g ) on the order of 200 to 350 °C. Many applications have working temperatures above the T g of these materials, which compels the development of new IR materials. This work studies the underlying short-range order (SRO) structure and glass formability of a new family of ionically-bonded sulfide glasses, xBaS + yLa 2 S 3 + (1-x-y)GeS 2 , to develop high T g optical materials with a broad IR transmission range. These sulfide glasses were produced by melting sulfide materials inside evacuated and sealed carbon-coated silica ampoules at 1150 °C for 12 hours and quenching to room temperature to form glass. Glass samples were then characterized by IR and Raman spectroscopies and differential thermal analysis (DTA). It was found that by increasing the modifier concentration, the predominantly Ge 4 SRO units, the superscript defines the number of bridging sulfur (BS) ions in the tetrahedral network found in GeS 2 glasses, are ultimately converted to Ge 0 units at > 40 mol% network modifier content through the generation of non-bridging sulfur (NBS) ions. These molecular ionic units still form a glassy network, with some of the highest reported T g values to date for a pure sulfide glass. This suggests that this composition has strong ionic bonds between negatively-charged tetrahedral SRO units and the positively-charged modifier cations. While the glass network is depolymerized in the high modifier content glasses though the formation of a high concentration of molecular ionic Ge 0 SRO groups, they are, nevertheless, homogeneous glassy materials that exhibit the largest T g and ΔT (difference between crystallization temperature, T c , and T g ) values of glasses in this system, making them the optimal glasses for high T g IR optical components, including, potentially, refractory IR optical fibers.

non-crystalline solids, glass formation↗

Grid-assisted magnetron sputtering deposition of nitrogen graded TiN thin films

Titanium Nitride (TiN) films were obtained using the grid-assisted magnetron sputtering deposition technique on Al substrates in two conditions: under constant and variable nitrogen concentration along the thin solid film thickness. The formation of a film with variable N concentration (herein referred as graded film) was confirmed using energy filtered transmission electron microscopy, X-ray photoelectron spectroscopy and grazing incidence X-ray diffraction. The TiN thin films microstructures were also analysed using scanning and transmission electron microscopies (SEM and TEM). Finally, the viability of synthesizing TiN thin films with variable N concentration is herein proposed as an alternative method for tailoring the properties of such functional coating materials.

36 MATERIALS SCIENCE↗

Advanced strategies for the development of porous carbon as a Li host/current collector for lithium metal batteries

Lithium metal is considered a promising anode material for high-energy-density rechargeable batteries because of its high specific theoretical capacity (3860 mAh g -1 , low mass density (0.534 g cm -3 ), and low electrochemical redox potential (-3.04 V vs. the standard hydrogen electrode). However, the high reactivity of Li with the electrolyte leads to the formation of an unstable solid electrolyte interphase (SEI) and continuous side reactions. Also, the non-uniform lithium-ion flux and infinite volume expansion of Li metal cause the growth of Li dendrites. These pose significant safety challenges and cause rapid capacity fading of the lithium metal batteries (LiMBs). To resolve these issues, a low-cost, easily processed, lightweight, high-performance carbon-based porous matrix is considered promising to host Li metal deposition. The three-dimensional (3D) porous nano/microstructured carbon provides sufficient space for Li accommodation during Li plating, buffers the volume changes during Li plating/stripping, and lowers the effective current density contributing to dendrite-free Li deposition. Besides, the outstanding electrochemical and mechanical stability, flexibility and the high electronic conductivity enable the nano/microstructured carbon to serve as both Li host and current collector. The development of 3D carbon/Li composite by mechanical roll-press techniques not only eliminates the complex and risky procedure of making carbon/Li composite based on Li plating or molten Li infusion but also stabilizes the capacity at higher Li plating/stripping rates. Recently, there is an advancement in the lithiophilic decorations of 3D structure to introduce sufficient nucleation sites and the development of artificial SEI on top of the 3D matrix to suppress Li dendrite formation. Such 3D structural modifications create a uniform electric field, lower the Li nucleation overpotential, provide strong mechanical and chemical stability, and stabilize the interface thereby inhibiting the degradation of lithium and the electrolyte. Here we summarize the research progress on porous carbon/Li composites in terms of materials type, structure, fabrication technique, their electrochemical battery performance, and identify the critical challenges that need to be addressed for high-energy-density practical LiMBs.

25 ENERGY STORAGE↗

Microscopy X-ray imaging enriched with small angle X-ray scattering for few nanometer resolution reveals shock waves and compression in intense short pulse laser irradiation of solids

Understanding how laser pulses compress solids into high-energy-density states requires diagnostics that simultaneously resolve macroscopic geometry and nanometer-scale structure. Here we present a combined X-ray imaging (XRM) and small-angle X-ray scattering (SAXS) approach that bridges this diagnostic gap. Using the Matter in Extreme Conditions end station at LCLS, we irradiated 25 μm copper wires with 45 fs, 0.9 J, 800 nm pulses at 3.5 × 10 19 W/cm 2 while probing with 8.2 keV XFEL pulses. XRM visualizes the evolution of ablation, compression, and inward-propagating fronts with ∼ 200 nm resolution, while SAXS quantifies their nanometer-scale sharpness via the time-resolved evolution of scattering streaks. The joint analysis reveals that an initially smooth compression steepens into a nanometer-sharp shock front after t sh ≈ (18 ± 3) ps, consistent with an analytical steepening model and hydrodynamic simulations. The front reaches a velocity of c sh ≈ 25 k m / s and a lateral width of several tens of microns, demonstrating direct observation of shock formation and decay at solid density for the first time with few-nanometer precision. This integrated XRM–SAXS method establishes a quantitative, multi-scale diagnostic of laser-driven shocks in dense plasmas relevant to inertial confinement fusion, warm dense matter, and planetary physics.

Kluge, Thomas [Helmholtz-Zentrum Dresden-Rossendor↗

Lithium anode stable in air for low-cost fabrication of a dendrite-free lithium battery

Lithium metal, the ideal anode material for rechargeable batteries, suffers from the inherent limitations of sensitivity to the humid atmosphere and dendrite growth. Herein, low-cost fabrication of a metallic-lithium anode that is stable in air and plated dendrite-free from an organic-liquid electrolyte solves four key problems that have plagued the development of large-scale Li-ion batteries for storage of electric power. Replacing the low-capacity carbon anode with a safe, dendrite-free lithium anode provides a fast charge while reducing the cost of fabrication of a lithium battery, and increasing the cycle life of a rechargeable cell by eliminating the liquid-electrolyte ethylene-carbonate additive used to form a solid-electrolyte interphase passivation layer on the anode that is unstable during cycling. This solution is accomplished by formation of a hydrophobic solid-electrolyte interphase on a metallic-lithium anode that allows for handling of the treated lithium anode membrane in a standard dry room during cell fabrication.

25 ENERGY STORAGE↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

ThO 2 and Th 1– x U x O 2 Nanoscale Materials and Thin Films for Nuclear Science Applications

This study investigates the dynamics and mechanisms of solution combustion synthesis (SCS) for the preparation of nanoscale ThO 2 and Th 1–x U x O 2 materials, utilizing metal nitrates (Th(NO 3 ) 4 and UO 2 (NO 3 ) 2 ) and acetylacetone (C 5 H 8 O 2 ) as reactants dissolved in a 2-methoxyethanol (C 3 H 8 O 2 ) solvent. By combining thermodynamic calculations, dynamic time–temperature profile measurements with differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA), this research reveals how variations in acetylacetone concentration and uranium content influence the structural parameters of the synthesized oxides. The time–temperature measurements show that the heating rate and maximum combustion temperatures are sensitive to acetylacetone concentration. DSC-TGA results indicate shifts in exothermic peak temperatures as the uranium content changes. The complexation between thorium and acetylacetone emerges as a critical factor, impacting combustion parameters and the structural characteristics of the final products. The uniform distribution of Th and U in the Th 1–x U x O 2 solid solution and the formation of nanoscale particles with strained crystallites are considered essential for the low-temperature densification of these materials for nuclear fuel pellet applications. Additionally, high-quality ThO 2 and Th 1–x U x O 2 thin (100–150 nm) films are successfully synthesized via electrospray deposition of combustible solutions followed by a brief period of heat treatment. Furthermore, these films exhibit excellent structural and morphological uniformity, making them ideal candidates for nuclear measurements, irradiation damage studies, and investigations into the physical properties of both pure and mixed oxides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Joining thick section aluminum to steel with suppressed FeAl intermetallic formation via friction stir dovetailing

A new solid-phase technique called friction stir dovetailing (FSD) has been developed for joining thick section aluminum to steel. In FSD, mechanical interlocks are formed at the aluminum-steel interface and are reinforced by metallurgical bonds where intermetallic growth has been uniquely suppressed. Lap shear testing shows superior strength and extension at failure compared to popular friction stir approaches where metallurgical bonding is the only joining mechanism. High resolution microscopy revealed the presence of a 40-70 nm interlayer having a composition of 76.4 at% Al, 18.4 at% Fe, and 5.2 at% Si, suggestive of limited FeAl3 intermetallic formation.

Friction stir dovetailing, Joining, Intermetallics↗

Effects of charged interfaces on electrolyte decomposition at the lithium metal anode

Lithium–Sulfur batteries are promising candidates to substitute conventional Li-ion batteries due to their higher energy density and reduced cost. However, several challenges related to the reactivity of the lithium metal anode have prevented this technology from becoming broadly commercialized. Lithium's high reactive nature leads to the continuous decomposition of the electrolyte and the formation of the solid-electrolyte interphase (SEI) layer. Thus, a comprehensive understanding of how the SEI film is formed is crucial to help elucidate improvements for this battery technology. In this work, we use density functional theory (DFT) based computational methods to investigate the effect of charged interfaces on the electrolyte degradation at the lithium anode. Here, several electrolyte mixtures were considered including 1,2-dimethoxyethane (DME) and 1,3-dioxolane (DOL) as solvents, and lithium bis(fluorosulfonyl)imide (LiFSI) and lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) as salts. It is found that the extent of salt decomposition is higher when the interface is charged. In addition, two types of solvent reduction mechanisms are identified: C–O bond cleavage and radical attacks. Charge transfer and evolution analysis are characterized in detail. Finally, solvent decomposition reactions are found to become more thermodynamically favorable and their activation barriers to be diminished under the effect of constant potentials and electric fields.

25 ENERGY STORAGE↗

Chemistry of Electrolyte Reduction on Lithium Silicide

Silicon anodes are promising for next-generation lithium-ion batteries due to high theoretical capacity. However, their performance and lifetime are currently limited by continuous electrolyte reduction and solid-electrolyte interphase (SEI) formation. Thus, SEI studies are important but often complicated due to the rough morphology of samples, buried interfaces, and the presence of binders. Here, we demonstrate the chemical origin of SEI formation by electrolyte reduction on lithium silicide thin films, synthesized by diffusion of pure evaporated lithium into smooth sputtered silicon. These model samples allowed for accurate estimation of irreversible capacity loss due to electrolyte reduction and for precise characterization of the resulting SEI by vibrational and photoelectron spectroscopies. Spectroscopic characterizations showed clear evidence that lithium silicide reduced electrolyte directly upon contact. Negligible first-cycle irreversible capacity loss was observed for the lithium silicide compared to silicon, indicating that the decomposition product of electrolyte on lithium silicide is able to stop further electrolyte reduction to a large extent. Fluoro-ethylene carbonate was shown to significantly affect the chemistry of electrolyte reduction on lithium silicide and subsequent cycling performance. The results of this basic study reveal the chemistry occurring at the interface of the lithium silicide and electrolyte and help in understanding the limited calendar lifetime of Li-ion batteries with Si anodes.

25 ENERGY STORAGE↗

Towards underwater additive manufacturing via additive friction stir deposition

Given the challenges in feed material supply and quality control, metal additive manufacturing has rarely been implemented in austere environments, especially underwater. This paper explores the underwater operation potential of an emerging solid-state additive technology: additive friction stir deposition, wherein material feeding and bonding are enabled by mechanical forces with minimal influences from water. It is demonstrated that additive friction stir deposition of 304 stainless steel can be successfully performed with the print head and substrate immersed in water. High temperature is reached in the deposition zone (>60% melting temperature); the material deposition behavior is similar to that in typical open-air operation. The as-deposited material is fully-dense, having fewer annealing twins and a substantially smaller grain size than the feed material (4.98 μm vs. 31.44 μm ). Such microstructural changes stem from dynamic recrystallization caused by the large strain and high temperature introduced during deposition. In addition to grain refinement, small equiaxed dispersoids (~2–3 μm or less) are formed and evenly distributed in the austenite steel matrix. Rich in Cr, Mn, and O, these particles likely result from the reaction between the elements in stainless steel and water at elevated temperatures.

16 TIDAL AND WAVE POWER↗

High Current-Density-Charging Lithium Metal Batteries Enabled by Double-Layer Protected Lithium Metal Anode

The practical application of lithium (Li) metal anode (LMA) is still hindered by non-uniformity of solid electrolyte interphase (SEI), formation of "dead" Li, and continuous consumption of electrolyte although LMA has an ultrahigh theoretical specific capacity and a very low electrochemical redox potential. Herein, we report a facile protection strategy for LMA using a double layer (DL) coating that consists of a polyethylene oxide (PEO)-based bottom layer which is highly stable with LMA and promotes uniform ion flux, and a cross-linked polymer-based top layer which prevents solvation of PEO layer in electrolytes. Li deposited on DL-coated Li (DL@Li) exhibits a smoother surface and much larger size than that deposited on bare Li. The LiF/Li 2 O enriched SEI layer generated by the salt decomposition on top of DL@Li further suppresses the side reactions between Li and electrolyte. Driven by the abovementioned advantageous features, the DL@Li||LiNi 0.6 Mn 0.2 Co 0.2 O 2 cells demonstrate capacity retention of 92.4% after 220 cycles at a current density of 2.1 mA cm -2 (C/2 rate) and stability at a high charging current density of 6.9 mA cm -2 (1.5C rate). These results indicate that the DL protection is promising to overcome the rate limitation of LMAs and high energy-density Li metal batteries.

25 ENERGY STORAGE↗

Flexible Aqueous Li‐Ion Battery with High Energy and Power Densities

Abstract A flexible and wearable aqueous symmetrical lithium‐ion battery is developed using a single LiVPO 4 F material as both cathode and anode in a “water‐in‐salt” gel polymer electrolyte. The symmetric lithium‐ion chemistry exhibits high energy and power density and long cycle life, due to the formation of a robust solid electrolyte interphase consisting of Li 2 CO 3 ‐LiF, which enables fast Li‐ion transport. Energy densities of 141 Wh kg −1 , power densities of 20 600 W kg −1 , and output voltage of 2.4 V can be delivered during >4000 cycles, which is far superior to reported aqueous energy storage devices at the same power level. Moreover, the full cell shows unprecedented tolerance to mechanical stress such as bending and cutting, where it not only does not catastrophically fail, as most nonaqueous cells would, but also maintains cell performance and continues to operate in ambient environment, a unique feature apparently derived from the high stability of the “water‐in‐salt” gel polymer electrolyte.

Yang, Chongyin↗

In Operando XRD and TXM Study on the Metastable Structure Change of NaNi 1/3 Fe 1/3 Mn 1/3 O 2 under Electrochemical Sodium-Ion Intercalation

In operando XRD and TXM-XANES approaches demonstrate that structure evolution in NaNi 1/3 Fe 1/3 Mn 1/3 O 2 during cycling follows a continuous change, and the formation of a nonequilibrium solid solution phase in the existence of two phases. Here, an O3' and P3' monoclinic phase occur, and redox couples of Ni 3+ /Ni 4+ and Fe 3+ /Fe 4+ are mainly responsible in the charge voltage range from 4.0 to 4.3 V.

36 MATERIALS SCIENCE↗

An Interconnected Channel-Like Framework as Host for Lithium Metal Composite Anodes

Lithium (Li) metal anodes have long been counted on to meet the increasing demand for high energy, high–power rechargeable battery systems but they have been plagued by uncontrollable plating, unstable solid electrolyte interphase (SEI) formation, and the resulting low Coulombic efficiency. These problems are even aggravated under commercial levels of current density and areal capacity testing conditions. In this work, the channel–like structure of a carbonized eggplant (EP) as a stable “host” for Li metal melt infusion, is utilized. With further interphase modification of lithium fluoride (LiF), the as–formed EP–LiF composite anode maintains ≈90% Li metal theoretical capacity and can successfully suppress dendrite growth and volume fluctuation during cycling. EP–LiF offers much improved symmetric cell and full–cell cycling performance with lower and more stable overpotential under various areal capacity and elevated rate capability. Furthermore, carbonized EP serves as a light–weight high–performance current collector, achieving an average Coulombic efficiency ≈99.1% in ether–based electrolytes with 2.2 mAh cm –2 cycling areal capacity. Furthermore, the natural structure of carbonized EP will inspire further artificial designs of electrode frameworks for both Li anode and sulfur cathodes, enabling promising candidates for next–generation high–energy density batteries.

25 ENERGY STORAGE↗

Modulating Li + and Polysulfide Solvation with Low-Density Moderately Solvating Electrolytes for Lithium–Sulfur Batteries

Lithium–sulfur (Li–S) batteries show great promise as the next-generation rechargeable batteries, yet they still suffer from polysulfide shuttling and interphasial instability. Electrolyte, as the medium for ion transport and sulfur conversion, plays a crucial role in overcoming these challenges. Here, we introduce a moderately solvating electrolyte (MSE) based on low-density, low-viscosity, and nonfluorinated ether co-solvents that balances polysulfide suppression, Li metal stabilization, and redox kinetics. Through multiple solvent–solvent and solvent-ion interactions, the optimized MSE weakens Li + -solvent pairing while strengthening cation–anion interactions, thereby lowering the desolvation barrier and promoting the formation of a favorable solid–electrolyte interphase (SEI). Meanwhile, MSE limits the polysulfide dissolution but improves the accessibility of active material through better wettability and tailored solvation environment, leading to an altered sulfur deposition mechanism with β – α conversion. This approach enables a stable cycling of high-mass loading Li–S cells (> 3.5 mg cm -2 ) at both room temperature and 45 °C (where shuttling and side reactions are severer), and demonstrates a pouch cell with lean electrolyte content (4.5 µL mg s -1 ). This work highlights a practical route to develop high-performance electrolyte for Li–S cells and provides mechanistic insights into their operation.

25 ENERGY STORAGE↗