Mesoscale model and X-ray computed micro-tomographic imaging of damage progression in ultra-high-performance concrete
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
In magnesium alloys, deformation twinning and its interactions with dislocation slip are responsible for a sigmoidal shape stress–strain behavior and an asymmetrical tension–compression yield strength in magnesium alloys. The sensitivity of twinning to the underlying microstructure renders the crystal plasticity method the most commonly adopted modeling approach for magnesium-twinning. This paper compares three state-of-the-art crystal plasticity-based twinning models from the literature, namely the elastic-viscoplastic self-consistent twinning-detwinning (EVPSC-TDT) model, crystal plasticity finite element model based on enhanced predominate twin reorientation approach (CPFE-ePTR), and the crystal plasticity finite element model based on “discrete twinning” approach (CPFE-DT). A polycrystalline microstructure is simulated with all three methods to compare the resulting stress–strain curves and lattice strains to those from the experimentally measured data. All three methods showed the capability of capturing the experimental results with different levels of accuracy. Additionally, the EVPSC-TDT method avoids solving the finite element matrices and showed the highest computational efficiency. The CPFE-ePTR model shows a higher accuracy in capturing the lattice strain. The CPFE-DT relies on high-resolution finite element mesh and is much slower than the other two methods, but it captured the local deformation concentration and stress reversal phenomena near the twin band, which was not possible with the other two methods. Based on the comparison, guidance for the selection of the appropriate model based on the specific modeling target is provided in this paper.
High-early-strength fiber-reinforced self-compacting concrete (FRSCC) is a practical material for the precast concrete industry to double its production capacity. In this study, we developed high-early-strength FRSCC mixtures that achieved a compressive and flexural strength of at least 24 MPa and 3.5 MPa, respectively, at 6 h, using commercially available components, typical mixing procedures, and air curing. A mix design process was developed based on the literature and experimental results. The effect of six different fiber reinforcements on the fresh and mechanical properties of concrete was analyzed. The cost limit was set at 523 USD/m 3 to make the concrete mix cost-effective.
Not Available
In this work, the sintering process of Portland cement was studied by combining thermomechanical analysis (TMA) and differential thermal analysis (DTA), together with X-ray diffraction (XRD) and scanning electron microscopy (SEM). Thermal analysis results employing both techniques indicted that phase transformations appeared at lower temperatures when CaF{sub 2} was incorporated in the raw materials. Besides, it was observed at high temperature that in some phase transformations TMA conducts to better resolution compared with the DTA measurements. Furthermore, mechanical properties and X-ray diffraction patterns corroborate the TMA and DTA results, corroborating that the final amount of alite (Ca{sub 3}SiO{sub 5}) is higher when a certain amount of CaF{sub 2} was present during the clinkerization process.
The deformation behavior was investigated in a consolidated Fe with a grain size ranging from submicrometer to tens of micrometer values under uniaxial compression and tension. In compression, shear banding occurred significantly at grain sizes >500 nm while only a single band was observed in samples with grain sizes of {approx} 100 nm. For the samples with grain sizes <{approx} 800 nm, the shear banding took place at angles of 48-51{sup o}. When the grain sizes were >{approx} 800 nm, the shear banding happened at an angle of 45{sup o} (in the maximum shear-stress plane). In tension, premature fracture happened in samples with grain sizes <1 {micro}m while shear banding was observed at grain sizes >1 {micro}m, and the shear banding angle was also close to 45{sup o}. For the samples with grain sizes > 2 {micro}m, homogeneous deformation took over in compression with a yield-point phenomenon being observed, but Lueders banding localization occurred in tension.
We have simultaneously measured the evolution of intermetallic volume, stress, and whisker density in Sn and Pb-Sn alloy layers on Cu to study the fundamental mechanisms controlling whisker formation. For pure Sn, the stress becomes increasingly compressive and then saturates, corresponding to a plastically deformed region spreading away from the growing intermetallic particles. Whisker nucleation begins after the stress saturates. Pb-Sn layers have similar intermetallic growth kinetics but the resulting stress and whisker density are much less. Measurements after sputtering demonstrate the important role of the surface oxide in inhibiting stress relaxation.
We have investigated the effects of hydrogen implantation temperature on the ion-cut process of InP by examining the correlation between surface blistering and the ion induced damage, hydrogen distribution, and strain. Using Rutherford backscattering spectrometry, elastic recoil detection, and x-ray diffraction, it was found that both the point defects induced by the hydrogen implantation and the in-plane compressive stress were necessary for hydrogen trapping and H-platelet nucleation and growth. The control of implantation temperature is crucial for creating sufficient defects and strain to induce surface blistering or layer exfoliation.
In situ stress measurements during sputtering deposition of amorphous Fe{sub 80}B{sub 20} films are used to control their stress and magnetoelastic properties. The substrate curvature induced by the deposited film is measured optically during growth and quantitatively related to the deposition induced accumulated stress. The resulting magnetic properties are later correlated with the measured stress for a wide range of sputtering pressures [(2-25)x10{sup -3} mbar]. A significant tensile stress develops at the film-substrate interface during the early growth stages (initial 2-3 nm). At a critical thickness, a transition is observed from tensile to compressive stress, which is associated with amorphous island coalescence. By further increasing the thickness, a compressive stress follows, which is related to the local distortion induced by the ion peening effect. The Monte Carlo simulations of the sputtering process describe quantitatively the experimental results as a function of the Ar pressure and target bias voltage.
We report steady-state and time-resolved photoluminescence (TRPL) measurements on individual GaN nanowires (6-20 {mu}m in length, 30-940 nm in diameter) grown by a nitrogen-plasma-assisted, catalyst-free molecular-beam epitaxy on Si(111) and dispersed onto fused quartz substrates. Induced tensile strain for nanowires bonded to fused silica and compressive strain for nanowires coated with atomic-layer-deposition alumina led to redshifts and blueshifts of the dominant steady-state PL emission peak, respectively. Unperturbed nanowires exhibited spectra associated with high-quality, strain-free material. The TRPL lifetimes, which were similar for both relaxed and strained nanowires of similar size, ranged from 200 ps to over 2 ns, compared well with those of low-defect bulk GaN, and depended linearly on nanowire diameter. The diameter-dependent lifetimes yielded a room-temperature surface recombination velocity S of 9x10{sup 3} cm/s for our silicon-doped GaN nanowires.
Stress evolution during reactive magnetron sputtering of TiN, ZrN, and TiZrN layers was studied using real-time wafer curvature measurements. The presence of stress gradients is revealed, as the result of two kinetically competing stress generation mechanisms: atomic peening effect, inducing compressive stress, and void formation, leading to a tensile stress regime predominant at higher film thickness. No stress relaxation is detected during growth interrupt in both regimes. A change from compressive to tensile stress is evidenced with increasing film thickness, Ti content, sputtering pressure, and decreasing bias voltage.
Epitaxial growth of MgO barrier on Si is of technological importance due to the symmetry filtering effect of the MgO barrier in conjunction with bcc-ferromagnets. We study the epitaxial growth of MgO on (100)-Si by molecular beam epitaxy. MgO matches Si with 4:3 cell ratio, which renders Fe to be 45 deg. rotated relative to Si, in sharp contrast to the direct epitaxial growth of Fe on Si. The compressive strains from Si lead to the formation of small angle grain boundaries in MgO below 5 nm, and also affect the transport characteristics of Fe/MgO/Fe magnetic tunnel junctions formed on top.
Erbium-doped silicon-rich silicon oxide films deposited by plasma enhanced chemical vapor deposition suffer from compressive stress as deposited, which converts to a large tensile stress on annealing due to the release of hydrogen. Although the cracking that results from this stress can be avoided by patterning the films into ridges, significant stress remains along the ridge axis. Measurements of erbium photoluminescence sensitized by silicon nanoclusters in stressed and relaxed films suggest an important role for internal film stresses in promoting the phase separation of excess silicon into nanoclusters, which has previously been thought of as a thermally driven process.
Surface roughness development of photoresist (PR) films during low pressure plasma etching has been studied using real-time laser light scattering from photoresist materials along with ellipsometric and atomic force microscopy (AFM) characterization. We show that evolution of the intensity of light scattered from a film surface can be used to study the development of surface roughness for a wide range of roughness starting from subnanometer to few hundred nanometers. Laser light scattering in combination with ellipsometry and AFM is also used to study the reticulation mechanism of 193 and 248 nm PRs during argon plasma processing. We employ a three-layer model (modified layer, rough layer, and bulk film) of the modified PR surface (193 and 248 nm PRs) to simulate and understand the behavior of ellipsometric {psi}-{delta} trajectories. Bruggeman's effective medium approximation is employed to study the roughness that develops on the surface after reticulation. When the glass transition temperature of the organic materials is reached during Ar plasma processing, the PR films reticulate and roughness develops rapidly. Roughness development is more pronounced for 248 nm PR than for 193 nm PR. Simulation of {psi}-{delta} shows that the growth of roughness is accompanied by strong expansion in the materials, which is stronger for 248 nm PR than 193 nm PR. The leading factors responsible for reticulation are found to be compressive stress that develops in the modified surface layer as it is created along with strong molecular chain motion and expansion of the material when the temperature is increased past the glass transition temperature. Reticulation leads to a significantly different surface morphology for 248 nm PR as compared to 193 nm PR and can be related to differences in molecular structure and composition leading to different responses when a modified surface layer is formed by ion bombardment accompanying plasma etching.
Droplet quartz crystal microbalance has been demonstrated to be a promising tool for accessing material properties of fluids as well as the diverse solid-fluid interface phenomena. However, a microliter droplet localized on the surface of the electrodes of finite lateral size may cause a nonuniform distribution of the plane velocity, which may lead to surface normal fluid flow and generate the compressional waves above the crystal surface. In the present article, we report systematical investigation on both resonance frequency and dissipation measurements with reference to the small droplets of silicone oils spreading on the surface of the quartz crystal microbalance. Significant cyclical variations in the resonant frequency and resistance of the crystal have been observed as the characteristic sizes of the silicone oil droplets are close to specific values known to favor compressional wave generation. The experimental results have been compared with the theoretical values predicted by the finite element computation associated with a simple hydrodynamic model. Good agreement between theory and experiment has been obtained. The finding indicates that the small droplets on the crystal surface can act as resonant cavities for the compressional wave generation and that the greatest propensity to exhibit periodical resonance behavior in the frequency and dissipation measurements is at droplet height of lambda{sub c}/2 above the crystal surface.
Laser shock compression experiments on precompressed samples offer the possibility to explore extreme material states unreachable by static or single-shock compression techniques alone. We have found significant increases in static compression pressure in a wide-opening and thin diamond precompression cell. This suggests that the precompression target is adaptable to advanced coupling techniques with laser-driven dynamic compression methods. The novel coupling techniques proposed give the potential to access outstanding material states required in planetary and condensed-matter physics.
The in-plane roll-bending process is a special wedge rolling with a configuration of two conical rolls which can form strips into open ring products. The spread of a ring is usually not considered in previous radius predicting models by Yang et al. and Xian et al. However, the spread increases to 10% for a ring with average reduction of 56%, and there is a discrepancy between the predicted radius and the experiment. Spread analysis/calculation has become an urgent problem in radius prediction and precision control of unequal deformation in this process. A finite element (FE) model considering spread effect is established and evaluated by experiments. A comparison between the predicted results with/without considering spread by FE analysis and experiments is carried out. The result shows that the predicted results considering spread are much closer to the experiments than those without considering spread effect. Based on the FE simulation, the spread characteristics of the ring with two types of cross section (including partly and entirely compressed cross section) are investigated. It is found that, there exist three spread regions, including outer positive region, middle negative region and inner positive region for the partly compressed ring; and there are outer positive region and inner negative region for the entirely compressed ring. The spread mostly happens at the outer positive region for both types of ring. The effects of process parameters, such as wedge angle, bite location, friction coefficient and rotational speed of roll, on spread for three aluminum alloys, 3A21O, 5A02O and 2A12T4, are investigated. The results indicate that the spread decreases with an increase in wedge angle, whereas increases with the growth of bite location; the spread remains stable with increasing friction coefficient and fluctuates within 3%-8% with a rise in rotational speed of roll. The spread of the partly compressed ring is less than 6%; large spread (larger than 6%) occurs when the ring is entirely compressed; the spread may reach a maximum value of 18.8% for material 5A02O.
We report on the fabrication and characterization of ultrathin (down to 50 nm) tensile strained SiGe films on mesoporous Si substrates. Low temperature oxidation of the porous substrate relaxes the compressive strain in the as grown monocrystalline (mc) SiGe. Applying this method to a 50 nm thick mc-Si{sub 0.72}Ge{sub 0.28} film, a tensile strain >0.78% can be achieved without compromising crystalline quality and up to 1.45 % without the appearance of cracks.