Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fuel cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Microstructural and chemical characterization of medium burnup fast reactor MOX using electron microscopy

A thorough post-irradiation examination campaign of medium burnup Sodium Fast Reactor (SFR) mixed oxide (MOX) fuel has been undertaken over the past two years to better understand the performance at intermediate burnup of this annular fuel design. Non-destructive examinations as well as destructive examinations of two pins have been recently published by the authors, providing data regarding the performance at macro-scale. The analyses of selected samples have continued to provide more details regarding the overall microstructure and, particularly, the fuel-cladding interaction.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

MONOLITHIC FUEL FABRICATION PROCESS DEVELOPMENT AT THE IDAHO NATIONAL LABORATORY

Within the Reduced Enrichment for Research and Test Reactors (RERTR) program directed by the US Department of Energy (DOE), UMo fuel-foils are being developed in an effort to realize high density monolithic fuel plates for use in high-flux research and test reactors. Namely, targeted are reactors that are not amenable to Low Enriched Uranium (LEU) fuel conversion via utilization of high density dispersion-based fuels, i.e. 8-9 gU/cc. LEU conversion of reactors having a need for >8-9 gU/cc fuel density will only be possible by way of monolithic fuel forms. The UMo fuel foils under development afford fuel meat density of ~16 gU/cc and thus have the potential to facilitate LEU conversions without any significant reactor-performance penalty. Two primary challenges have been established with respect to UMo monolithic fuel development; namely, fuel element fabrication and in-reactor fuel element performance. Both issues are being addressed concurrently at the Idaho National Laboratory. An overview is provided of the ongoing monolithic UMo fuel development effort at the Idaho National Laboratory (INL); including development of complex/graded fuel foils. Fabrication processes to be discussed include: UMo alloying and casting, foil fabrication via hot rolling, fuel-clad interlayer application via co-rolling and thermal spray processes, clad bonding via Hot Isostatic Pressing (HIP) and Friction Bonding (FB), and fuel plate finishing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of Aluminum-clad Spent Nuclear Fuel during Drying and Dry Storage

The DOE SNF Working Group ASNF Subgroup and the U.S. Nuclear Waste Technical Review Board have identified knowledge gaps regarding the management of aluminum-clad spent nuclear fuel (ASNF).[1, 2] The objectives of this research are to observe, sample and analyze the nature of aluminum surface corrosion and corrosion layer chemistry relevant to the ASNF performance over the duration of the dry storage segment of the fuel life cycle. The primary goal is to build an understanding of ASNF behavior, from reactor service and wet storage through drying and dry storage, with parallel testing of surrogate materials. The premise is that residual water affiliated with the aluminum oxide from corrosion during reactor service and wet storage, continues to influence ASNF performance during dry storage, and that even after successful drying the surface conditions of ASNF have yet to be satisfactorily characterized. The initial scope collected and analyzed specimens from irradiated non-fuel components of aluminum-clad Advanced Test Reactor (ATR) fuel elements that are routinely removed at the end of reactor service life. Techniques have been developed for remote material sampling from ATR elements from vented dry storage at the Irradiated Fuel Storage Facility (IFSF). These techniques involve 1) nipping off a small corner of the aluminum near where the end box had been removed and 2) scraping the exterior (non-fueled) plate surface to collect an oxide sample. This second effort targets ATR elements expected to have seen the longest residence in storage, both in the CPP-603 pool (with poor water quality) and in dry storage at IFSF, within the fuel handling scheduled to consolidate ATR at IFSF and receive the remaining inventory at CPP-666. Follow on work has been proposed to nip corners and collect scrapings immediately following ATR fuel drying, before placement in dry storage. Sample analysis will use multiple techniques to understand the chemical composition and morphology of the surface oxides. A simultaneous effort is progressing to develop surrogate materials to enable rigorous controlled experiments. Consistently produced, these surrogate materials can then be used to demonstrate limitations inherent to remote sampling and to validate performance models under relevant constraints. The combined efforts will substantiate ASNF performance and fuel management decisions regarding drying and packaging over a more complete range of life cycle conditions. [1] DOE Spent Nuclear Fuel Working Group, Aluminum-Clad Spent Nuclear Fuel: Technical Considerations and Challenges for Extended (>50 Years) Dry Storage, DOE/ID RPT#: 1575, prepared by Aluminum-Clad SNF Sub Working Group, June 2017. [2] U.S. Nuclear Waste Technical Review Board, Management and Disposal of U.S. Department of Energy Spent Nuclear Fuel, A Report to the United States Congress and the Secretary of Energy, December 2017, p. 143.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Severe accident modeling of a PWR core with different cladding materials

The MAAP v.4 software has been used to model two severe accident scenarios in nuclear power reactors with three different materials as fuel cladding. The TMI-2 severe accident was modeled with Zircaloy-2 and SiC as clad material and a SBO accident in a Zion-like, 4-loop, Westinghouse PWR was modeled with Zircaloy-2, SiC, and 304 stainless steel as clad material. TMI-2 modeling results indicate that lower peak core temperatures, less H 2 (g) produced, and a smaller mass of molten material would result if SiC was substituted for Zircaloy-2 as cladding. SBO modeling results indicate that the calculated time to RCS rupture would increase by approximately 20 minutes if SiC was substituted for Zircaloy-2. Additionally, when an extended SBO accident (RCS creep rupture failure disabled) was modeled, significantly lower peak core temperatures, less H 2 (g) produced, and a smaller mass of molten material would be generated by substituting SiC for Zircaloy-2 or stainless steel cladding. Because the rate of SiC oxidation reaction with elevated temperature H{sub 2}O (g) was set to 0 for this work, these results should be considered preliminary. However, the benefits of SiC as a more accident tolerant clad material have been shown and additional investigation of SiC as an LWR core material are warranted, specifically investigations of the oxidation kinetics of SiC in H{sub 2}O (g) over the range of temperatures and pressures relevant to severe accidents in LWR 's. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

High-temperature secondary hydriding experiments with E110 and E110G claddings - 2016-0031

Secondary hydriding can take place during a loss-of-coolant accident event after the ballooning and burst of the zirconium alloy cladding. The oxidation and hydrogen uptake in the ballooned section can produce the weakest segment of the rod. This phenomenon was investigated in the past mainly for Zircaloy-4 cladding. We investigated the effect of secondary hydriding in VVER reactors with E110 and E110G alloys. A high-temperature facility was built to carry out high-temperature treatment of fuel cladding samples. The burst of tubes was reached with inner pressurization at 750 and 800 C. After burst the samples were oxidized in the same furnace for different periods and at different temperatures. The oxidized samples were tested in a tensile test machine with four-point bending tests. The microstructure of the samples was analyzed by optical and scanning electron microscopy. The hydrogen content of the cladding was measured by heat extraction, prompt gamma activation analyses, and neutron radiography methods. The experiments indicated that the ballooned section after oxidation became the weakest segment of the VVER fuel. According to the mechanical testing, the cladding samples were brittle even after a short oxidation time (200 s at 1,000 C) without any sign of ductile behavior. The comparison of E110 and E110G samples showed that the E110 tubes lost their load-bearing capability or even integrity much earlier than the E110G samples treated under similar conditions. (authors)

36 MATERIALS SCIENCE↗

FULL SIZE U-10MO MONOLITHIC FUEL FOIL AND FUEL PLATE FABRICATION-TECHNOLOGY DEVELOPMENT

Full-size U10Mo foils are being developed for use in high density LEU monolithic fuel plates. The application of a zirconium barrier layer too the foil is applied using a hot co-rolling process. Aluminum clad fuel plates are fabricated using Hot Isostatic Pressing (HIP) or a Friction Bonding (FB) process. An overview is provided of ongoing technology development activities, including: the co-rolling process, foil shearing/slitting and polishing, cladding bonding processes, plate forming, plate-assembly swaging, and fuel plate characterization. Characterization techniques being employed include, Ultrasonic Testing (UT), radiography, and microscopy.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A review of inherent safety characteristics of metal alloy sodium-cooled fast reactor fuel against postulated accidents

The thermal, mechanical, and neutronic performance of the metal alloy fast reactor fuel design complements the safety advantages of the liquid metal cooling and the pool-type primary system. Together, these features provide large safety margins in both normal operating modes and for a wide range of postulated accidents. In particular, they maximize the measures of safety associated with inherent reactor response to unprotected, double-fault accidents, and to minimize risk to the public and plant investment. High thermal conductivity and high gap conductance play the most significant role in safety advantages of the metallic fuel, resulting in a flatter radial temperature profile within the pin and much lower normal operation and transient temperatures in comparison to oxide fuel. Despite the big difference in melting point, both oxide and metal fuels have a relatively similar margin to melting during postulated accidents. When the metal fuel cladding fails, it typically occurs below the coolant boiling point and the damaged fuel pins remain cool-able. Metal fuel is compatible with sodium coolant, eliminating the potential of energetic fuel coolant reactions and flow blockages. All these, and the low retained heat leading to a longer grace period for operator action, are significant contributing factors to the inherently benign response of metallic fuel to postulated accidents. This paper summarizes the past analytical and experimental results obtained in past sodium-cooled fast reactor safety programs in the United States, and presents an overview of fuel safety performance as observed in laboratory and in-pile tests.

inherent safety↗

Results of NDE Technique Evaluation of Clad Hydrides

This report fulfills the M4 milestone, M4FT-14IN0805023, Results of NDE Technique Evaluation of Clad Hydrides, under Work Package Number FT-14IN080502. During service, zirconium alloy fuel cladding will degrade via corrosion/oxidation. Hydrogen, a byproduct of the oxidation process, will be absorbed into the cladding and eventually form hydrides due to low hydrogen solubility limits. The hydride phase is detrimental to the mechanical properties of the cladding and therefore it is important to be able to detect and characterize the presence of this constituent within the cladding. Presently, hydrides are evaluated using destructive examination. If nondestructive evaluation techniques can be used to detect and characterize the hydrides, the potential exists to significantly increase test sample coverage while reducing evaluation time and cost. To demonstrate the viability this approach, an initial evaluation of eddy current and ultrasonic techniques were performed to demonstrate the basic ability to these techniques to detect hydrides or their effects on the microstructure. Conventional continuous wave eddy current techniques were applied to zirconium based cladding test samples thermally processed with hydrogen gas to promote the absorption of hydrogen and subsequent formation of hydrides. The results of the evaluation demonstrate that eddy current inspection approaches have the potential to detect both the physical damage induced by hydrides, e.g. blisters and cracking, as well as the combined effects of absorbed hydrogen and hydride precipitates on the electrical properties of the zirconium alloy. Similarly, measurements of ultrasonic wave velocities indicate changes in the elastic properties resulting from the combined effects of absorbed hydrogen and hydride precipitates as well as changes in geometry in regions of severe degradation. However, for both approaches, the signal responses intended to make the desired measurement incorporate a number of contributing parameters. These contributing factors need to be recognized and a means to control them or separate their contributions will be required to obtain the desired information.

36 MATERIALS SCIENCE↗

Research Needs for Uranium-Zirconium- Based Metallic Fuels

The purpose of this report is to summarize the needs and present recommendations related to the future direction for U-Zr-based metallic fuel research (including binary U-Zr and ternary U-Pu-Zr alloys). These needs and recommendations were determined by subject matter experts from various institutions during a two-day workshop held at the University of Florida in November, 2019. During open-floor discussions, the highest priority gaps in our understanding of U-Zr-based fuels were down-selected, and near- and long-term needs that directly impact the implementation of these metallic fuels were identified. The identified near-term needs include investigation of the following phenomena: i) swelling and fission gas release, ii) fuel-cladding chemical interaction, iii) phase evolution/constituent redistribution, and iv) thermal properties of the fuels. The long-term needs are: i) investigation of fuel creep and plasticity and ii) fission product (lanthanide) transport. In addition, there was general agreement that all institutions and subject matter experts would benefit from an open-source metallic fuels database with thermophysical property and microstructural data, along with fuel operation/irradiation history, which should be regularly updated with vetted information from new experimental and computational investigations and used to advance metallic fuels research and development. Finally, we recommend that metallic fuel research should be ongoing and that fuel qualification and fuel optimization should be equally prioritized; research combining experiments with modeling and simulation has the largest potential impact.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Results of Oklo Diffusion Couple Experiments

Through the Gateway for Accelerated Innovation in Nuclear (GAIN) initiative, the U.S. Department of Energy funded a GAIN Nuclear Energy Voucher to perform out-of-pile experiments related to the fuel design for Oklo Inc., headquartered in Santa Clara, CA. GAIN’s goal is to accelerate the innovation and application of advanced nuclear technologies, and voucher recipients do not receive direct financial awards but are provided access to national laboratory capabilities at no cost. This report documents the results of diffusion couple experiments performed as part of the GAIN-funded project for Oklo. This work addresses the specific problem of filling the gap in understanding of the fuel-cladding chemical interaction (FCCI) that result from the past focus on a particular fuel design. These knowledge and mechanistic modeling gaps make it difficult to extrapolate from prior fuel performance data to advance an economically competitive fuel design. Specifically, the current state-of-the-art fuel performance modeling cannot separate the entangled effects of temperature ranges, burnups, materials, and geometries.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Considerations for Defining G-Values for Aluminum-Clad Spent Nuclear Fuel

Sealed-canister dry storage of aluminum-clad spent nuclear fuel (ASNF) generated by research reactors is an alternative to current storage and disposition pathways as directed by the U.S. Department of Energy. The major challenge faced for this storage approach is radiolytic H 2 generation, including from the aluminum (oxy)hydroxide layers on the surface of ASNF. Experimental and modeling activities have been carried out to characterize the radiolytic yield as part of a DOE-sponsored research program to develop the technical basis for ASNF dry storage. The G-value is a commonly way to report results of radiolysis testing and is defined as the radiolytic yield of a species (e.g. molecular hydrogen) per unit radiation energy deposited into the material system. An independent technical review of the ASNF dry storage technical basis performed by Pacific Northwest National Laboratory raised questions about differences in G-value definitions used for experiments on ASNF surrogates consisting of aluminum samples with adherent (oxy)hydroxides compared to G-values reported in prior literature and how the magnitudes compared between different studies. Material systems resembling ASNF pose complications for measuring/defining G-values to predict the evolution of H 2 in a sealed canister, including i) accounting for radiolytic yields potentially arising from multiple sources, i.e., residual free (vapor), physisorbed, and chemisorbed/chemically bound waters; ii) deciding what portions of the multi-material system to include in the absorbed energy (radiation dose) calculation, considering possible energy exchange between materials as well as measurement limitations, and iii) capturing variations in G-value associated with non-linear yield vs. dose curves and/or dependence on the cover gas. This report summarizes previous literature information on radiolytic H 2 generation and associated G-values from mixed-material systems (generally oxides in contact with water or organic compounds) and from (oxy)hydroxides/hydrates to compare with the definitions and values for ASNF surrogate samples containing adherent aluminum (oxy)hydroxides.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanistic modeling of lifetime distribution of SiC/SiC composite claddings

Silicon carbide (SiC) fiber-reinforced SiC matrix (SiC/SiC) composites have emerged as a new material candidate for fuel claddings in light water reactors. Recent studies showed that the load capacity of SiC/SiC materials exhibits a considerable statistical variation. Therefore, reliability analysis plays a critical role in design of SiC/SiC composite claddings. Here, this paper presents a probabilistic model for the lifetime distribution of SiC/SiC composites. The model is anchored by a multiaxial stress-based failure criterion and subcritical damage accumulation mechanism. Based on the kinetics of subcritical damage growth, the lifetime distribution of a laboratory test specimen for any given loading history can be calculated. A finite weakest-link model is used to extrapolate the lifetime distribution of test specimens to full-length claddings. It is shown that the damage accumulation mechanism has a strong influence on the lifetime distribution of the cladding. This finding highlights the importance of understanding the static fatigue behavior of SiC/SiC composites. The present analysis also demonstrates an intricate length effect on the failure probability of the cladding, which is expected to play a crucial role in design extrapolation.

36 MATERIALS SCIENCE↗

High temperature steam oxidation of Cr-coated SiCf/SiC composite for LWR cladding applications

Chromium-coated silicon carbide fiber-reinforced ceramic matrix composites are potentially applicable to accident tolerant fuel cladding in light water reactors. Cr-coated silicon carbide composite, chemical vapor deposited silicon carbide, and pure Cr-metal were oxidized in 100% steam at atmospheric pressure for 4 hours using a thermogravimetric analyzer. Post-oxidation chemical analysis, phase identification and microstructural characterization indicates that the Cr coating layers did not adversely affect silicon carbide substrate under these conditions.

Lee, Yoonjo↗

Aluminum Clad Spent Nuclear Fuel Long Term Dry Storage Technical Issues Action Plan - Technical and Engineering Activities

The DOE Spent Nuclear Fuel Working Group (SNFWG)’s report on technical considerations and challenges for extended dry storage of aluminum-clad spent nuclear fuel (ASNF) entitled, Aluminum-Clad Spent Nuclear Fuel: Technical Consideration and Challenges for Extended (>50 Years) Dry Storage, DOE/ID RPT-1575, June 2017 identified five knowledge gaps and technical data needs. This DOE SNFWG report also made several recommendations including one to develop an action plan to identify needed technical and engineering activities and analyses to address the identified knowledge gaps and technical data needs. A team composed of twenty SNF management experts and appropriate subject matter experts from the Idaho National Laboratory and Savannah River National Laboratory was assembled to develop this action plan. The action plan identifies and recommends six technical and engineering tasks and estimated cost and schedule for task completion. It is estimated that $5M and 18 months will be required to execute the recommended tasks.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Improved Accident Tolerance of Austenitic Stainless Steel Cladding through Colossal Supersaturation with Interstitial Solutes

We proposed a program-supporting research project in the area of fuel-cycle R&D, specifically on the topic of advanced fuels. Our goal was to investigate whether SECIS (surface engineering by concentrated interstitial solute – carbon, nitrogen) can improve the properties of austenitic stainless steels and related structural alloys such that they can be used for nuclear fuel cladding in LWRs (light-water reactors) and significantly excel currently used alloys with regard to performance, safety, service life, and accident tolerance. We intended to demonstrate that SECIS can be adapted for post-processing of clad tubing to significantly enhance mechanical properties (hardness, wear resistance, and fatigue life), corrosion resistance, resistance to stress–corrosion cracking (hydrogen-induced embrittlement), and – potentially – radiation resistance (against electron-, neutron-, or ion-radiation damage). To test this hypothesis, we measured various relevant properties of the surface-engineered alloys and compared them with corresponding properties of the non–treated, as-received alloys. In particular, we studied the impact of heat exposure corresponding to BWR (boiling-water reactor) working and accident (loss-of-coolant) conditions and the effect of ion irradiation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Dissolution Flowsheet for Skull Oxide Generated during U-Mo Alloy Casting for High Performance Research Reactor Fuel

The Savannah River National Laboratory was requested to develop dissolution flowsheets for high assay low enriched U scrap generated during the fabrication of high performance research reactor fuel. The scrap streams include U-10Mo and U-10Mo-Zr foils, rejected Al-clad fuel plates, and skull oxide from casting molds. Flowsheets for the dissolution of the U-10Mo-Zr foils and Al-clad U-10Mo-Zr mini-plates received from BWX Technologies, Inc were developed and demonstrated in the first phase of this project. In the second phase (this work), the skull oxide from a U-10Mo casting mold was obtained from the Y-12 National Security Complex (Y-12) and small-scale experiments were performed to demonstrate dissolution flowsheets.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Transition from Irradiation-Induced Amorphization to Crystallization in Nanocrystalline Silicon Carbide

Response to irradiation of nanocrystalline 3C-SiC is studied using 2 MeV Au+ ions near the critical temperature for amorphization and is compared to the behavior of its monocrystalline counterpart under the identical irradiation conditions. The irradiated samples have been characterized using in-situ ion channeling, ex-situ x-ray diffraction, and helium ion microscopy. Compared to monocrystalline 3C-SiC, a faster amorphization process in the nanocrystalline material (average grain size = 3.3 nm) is observed at 500 K. However, the nanograin grows with increasing ion fluence at 550 K and the grain size tends to saturate at high fluences. The striking contrast demonstrates a sharp transition from irradiation-induced interface-driven amorphization at 500 K to crystallization at 550 K. The results could show potential impacts of nanocrystalline SiC on nuclear fuel cladding and structural components of next-generation nuclear energy systems.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗