At least 649 records · Page 36

Candidate Low-Temperature Glass Waste Forms for Technetium-99 Recovered from Hanford Effluent Management Facility Evaporator Concentrate

Alternative treatment and disposition options may exist for technetium-99 (99Tc) in secondary liquid waste from the Hanford Direct-Feed Low-Activity Waste (DFLAW) process. One approach includes development of an alternate glass waste form that is suitable for on-site disposition of technetium, including salts and other species recovered by ion exchange or precipitation from the EMF evaporator concentrate. By recovering the Tc content from the stream, and not recycling the treated concentrate, the DFLAW process can potentially be operated in a more efficient manner that lowers the cost to the Department of Energy. This report provides a survey of candidate glass formulations and glass-making processes that can potentially incorporate technetium at temperatures <700 °C to avoid volatilization. Three candidate technetium feed streams are considered: (1) dilute sodium pertechnetate loaded on a non-elutable ion exchange resin; (2) dilute sodium-bearing aqueous eluent from ion exchange recovery of pertechnetate, or (3) technetium(IV) oxide precipitate containing Sn and Cr solids in an aqueous slurry. From the technical literature, promising candidate glasses are identified based on their processing temperatures and chemical durability data. The suitability and technical risk of three low-temperature glass processing routes (vitrification, encapsulation by sintering into a glass composite material, and sol-gel chemical condensation) for the three waste streams was assessed, based on available low-temperature glass data. For a subset of candidate glasses, their long-term thermodynamic behavior with exposure to water and oxygen was modeled using Geochemist’s Workbench, with and without addition of reducing stannous ion. For further evaluation and development, encapsulation of precipitated TcO2/Sn/Cr in a glass composite material based on lead-free sealing glasses is recommended as a high priority. Vitrification of pertechnetate in aqueous anion exchange eluent solution using a high lead content borate glass, or other low melting glass is also recommended for further evaluation and development. Additional laboratory studies of phase behavior and chemical durability of low-temperature glasses is also recommended to provide risk mitigation if one of the primary development paths proves infeasible. This report is a deliverable for the task “Candidate Low-T Glass Waste Forms for EMF Bottoms On-Site Disposition Alternative Option.”

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Technetium incorporation in glass for the Hanford Tank Waste treatment and immobilization plant - 15066

A priority of the United States Department of Energy (U.S. DOE) is to dispose of nuclear wastes accumulated in 177 underground tanks at the Hanford Nuclear Reservation in eastern Washington State. These nuclear wastes date from the Manhattan Project of World War II and from plutonium production during the Cold War. The DOE plans to separate high-level radioactive wastes from low activity wastes and to treat each of the waste streams by vitrification (immobilization of the nuclides in glass) for disposal. The immobilized low-activity waste will be disposed of here at Hanford and the immobilized high-level waste at the national geologic repository. Included in the inventory of highly radioactive wastes is large volumes of {sup 99}Tc (∼9 x 10 E2 TBq or ∼2.5 x 10{sup 4} Ci or ∼1500 kg). A problem facing safe disposal of Tc-bearing wastes is the processing of waste feed into in a chemically durable waste form. Technetium incorporates poorly into silicate glass in traditional glass melting. It readily evaporates during melting of glass feeds and out of the molten glass, leading to a spectrum of high-to-low retention (ca. 20 to 80%) in the cooled glass product. DOE-ORP currently has a program at Pacific Northwest National Laboratory (PNNL), in the Department of Materials Science and Engineering at Rutgers University and in the School of Mechanical and Materials Engineering at Washington State University that seeks to understand aspects of Tc retention by means of studying Tc partitioning, molten salt formation, volatilization pathways, and cold cap chemistry. Another problem involves the stability of Tc in glass in both the national geologic repository and on-site disposal after it has been immobilized. The major environmental concern with {sup 99}Tc is its high mobility in addition to a long half-life (2.1 x 10{sup 5} yrs). The pertechnetate ion (TcO{sup 4-}) is highly soluble in water and does not adsorb well onto the surface of minerals and so migrates nearly at the same velocity as groundwater. Long-term corrosion of glass waste forms is an area of current interest to the DOE, but attention to the release of Tc from glass has been little explored. It is expected that the release of Tc from glass should be highly dependent on the local glass structure as well as the chemistry of the surrounding environment, including groundwater pH. Though the speciation of Tc in glass has been previously studied, and the Tc species present in waste glass have been previously reported, environmental Tc release mechanisms are poorly understood. The recent advances in Tc chemistry that have given rise to an understanding of incorporation in the glass giving rise to significantly higher single-pass retention during vitrification are presented. Additionally, possible changes to the baseline flowsheet that allow for relatively minor volumes of Tc reporting to secondary waste treatment will be discussed. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

DEVELOPMENT OF CRYSTAL-TOLERANT WASTE GLASSES

The loading of high-level waste in borosilicate glasses is limited by crystallinity constraints that cannot prevent crystal accumulation on the melter bottom and in the glass discharge riser of the melter. Pacific Northwest National Laboratory is studying variations in composition that are designed to constrain high-level waste glass compositions and develop the crystal-tolerant high-level waste glasses. These glasses will allow high waste loading without decreasing the lifetime of the melter by keeping the small spinel crystals suspended in the molten glass. Adding ~1 wt% of NiO to the baseline glass caused large spinel crystals to form up to 210 µm in size and resulted in the highest accumulation rate, ~ 227 mm/year, of all tested glasses. Noble metals that were added to high-Ni glass prevented large spinel crystals from forming and decreased the accumulation rate ~ 8.5 times. Adding ~5 wt% of Fe2O3 to the baseline glass resulted in a high number density of ~10-μm spinel crystals that remained suspended in the glass melt even after 17 days at 850°C. The accumulation rate of spinel crystals in high-chromia crucibles was only slightly higher compared with the accumulation rate in double crucibles. Only baseline glass exhibited about 2.6 times faster accumulation rate because of increased number of bigger crystals. These crystals were the result of glass enrichment with chromium that was leached out from the walls of high-chromia crucibles.

36 MATERIALS SCIENCE↗

The origin of the heterogeneous distribution of bismuth in aluminosilicate laser glasses

Abstract As one kind of novel and burgeoning laser materials, bismuth‐doped silicate glasses have aroused increasing attention for the super broadband near‐infrared (NIR) emission. However, the large optical scattering loss, resulting from optical heterogeneity in glass color and refractive index, limits their further applications in telecommunication system. Thus, it is urgent to uncover the essence of heterogeneity in Bi‐doped silicate glasses and subsequently improve glass optical performance. It will give us some hint to homogenize the glass component and Bi active centers so as to boost the development of Bi‐based glass materials. Here, taking 1 typical Bi‐doped calcium aluminosilicate glass as an example, we revealed the origin of the optical heterogeneities in glass color and refractive index through the NIR emission spectra, electron probe microanalyzer (EPMA) of elements and X‐ray photoelectron spectroscopy (XPS) of Bi 4f 5/2 , Bi 4f 7/2 , and Al 2p. The inhomogeneous distribution of Bi and aluminum components is responsible for the heterogeneity in this glass system. In addition, we found that tetrahedral coordinated aluminum favors the existence of Bi NIR centers, consequently resulting in enhanced Bi NIR emissions. Furthermore, based on our results and the role of Al 3+ in glass network, we demonstrate the homogenizing of glass component by finely tuning glass composition. This work will enrich the understanding of Bi‐doped laser glass and provide a guideline for the design of component‐derived Bi‐doped silicate glasses and fibers with efficient NIR emission and high optical quality.

Li, Xiaoman↗

Temperature-induced densification in compressed basaltic glass revealed by in-situ ultrasonic measurements

Abstract Acoustic velocities of a model basalt glass (64 mol% CaMgSi2O6 + 36 mol% CaAl2Si2O8) were measured along different pressure-temperature (P-T) paths. One set of experiments involved isothermal compression-decompression cycles, performed at temperatures of 300, 641, 823, and 1006 K and pressures up to 12.2 GPa. The other set of experiments involved constant-load heating-cooling cycles at temperatures up to 823 K and pressures up to 7.5 GPa. Both sets of experiments were performed in a multi-anvil apparatus using a synchrotron-based ultrasonic technique. Our results show that the glass compressed isothermally at 300 K (cold-compression) displays anomalously decreasing compressional (VP) and shear (VS) wave velocities with increasing pressure until ~8 GPa. Beyond 8 GPa, both VP and VS start to increase sharply with pressure and irreversible densification of the glass occurred, producing large hysteresis loops of velocities upon decompression. However, for the glass compressed isothermally at increasingly higher temperatures (hot-compression), the velocity minima gradually shift to lower pressures. At temperature close to the glass transition temperature Tg, the velocity minima disappear completely, displaying a monotonic increase of velocities during compression and higher VP and VS during decompression. In addition, constant-load heating-cooling experiments show that velocities generally decrease slightly with increasing temperature, but start to increase once heated above a threshold temperature (~650 K). During cooling the velocities increase almost linearly with decreasing temperature, resulting in higher velocities (~1.5–2.5% higher) when returned to 300 K. This implies that a temperature-induced densification may have occurred in the glass at high pressures. Raman spectra on recovered samples show that the hot-compressed and high-P heated glasses contain distinctly densified and depolymerized structural signatures compared to the initial glass and the cold-compressed glass below the velocity transition pressure PT (~8 GPa). Such densification may be attributed to the breaking of bridging oxygen bonds and compaction in the intermediate-range structure. Our results demonstrate that temperature can facilitate glass densification at high pressures and point out the importance of P-T history in understanding the elastic properties of silicate glasses. Comparison with melt velocity suggests that hot-compressed glasses may better resemble the pressure dependence of velocity of silicate melts than cold-compressed glasses, but still show significantly higher velocities than melts. If the abnormal acoustic behaviors of cold-compressed glasses were used to constrain melt fractions in the mantle low-velocity regions, the melt fractions needed to explain a given velocity reduction would be significantly underestimated at high pressures.

Geochemistry & Geophysics↗

Comparison of Atomic and Electronic Structures of Silica and Sodium Silicate Glasses

Glass scintillators may hold great promise for low-cost, large-volume, shapeable radiation detectors. However, the light yield and energy resolution of glass scintillators to-date have been more than an order of magnitude worse than for crystalline scintillators and far from the theoretical limits. Glass scintillators are fabricated by dissolving rare-earth dopants into a glass matrix. Their operation relies on gamma ray absorption in the glass generating electrons and holes that must migrate to a rare-earth activator atom to emit light. The transport of carriers in the glass limits the performance, particularly in glasses where the solubility limit of activator is low, since carriers may recombine non-radiatively before reaching an activator atom. In this work, we aim to use atomistic simulations to discover the nature of electron transport in specific glass materials and how it may be enhanced by tuning the composition or forming process. The analysis proceeds in two steps: generation of a computational model of a given glass’s atomic structure, then extraction of the electronic structure to correlate electronic structure with carrier transport. Here we report results for two glasses: silica (SiO 2 ) and sodium silicate (Na 2 O:SiO 2 ). Multiple compositions of the latter are studied, namely Na 2 O:SiO 2 ratios of of 1:2, 1:3, and 3:7, with most results focused on the 3:7 composition. The overall goal is to establish a computational framework that can mimic a range of experimental glass structures by tuning computational parameters in the construction of the glass model, and enable studies of the correlation between atomic structure and electronic transport properties of the glass materials. These correlations would direct synthesis parameters for a given glass to optimize its transport properties.

36 MATERIALS SCIENCE↗

Enhanced Hanford Low-Activity Waste Glass Property Data Development: Phase 1

This report summarizes and analyzes data collected on a first test matrix of 36 low-activity waste (LAW) glass compositions intended to expand the LAW glass composition region over which glass property models are valid. The 36 LAW glass compositions were selected using statistical layered experimental design to explore a new glass composition region that overlaps and expands beyond the previously explored LAW glass composition region. The layered design of 36 LAW glasses consisted of 18 outer-layer glasses, 13 inner-layer glasses, a center glass (two replicates), and a glass previously tested at another laboratory (three replicates). The outer-layer glass compositions include extrema of the glass compositions that extend across and slightly beyond the compositions that are expected to be targeted for production. The analyses performed on these glasses include chemical composition (for target compositional verification), density, viscosity, electrical conductivity, crystal fraction, Canister Centerline Cooling with crystal identification, Product Consistency Test response, sulfur solubility, iron redox, and Vapor Hydration Test response. This report documents and discusses the results obtained from this testing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Oxidation States of Grim Glasses in EET79001 Based on Vanadium Valence

Gas-rich impact-melt (GRIM) glasses in SNC meteorites are very rich in Martian atmospheric noble gases and sulfur suggesting a possible occurrence of regolith-derived secondary mineral assemblages in these samples. Previously, we have studied two GRIM glasses, 506 and 507, from EET79001 Lith A and Lith B, respectively, for elemental abundances and spatial distribution of sulfur using EMPA (WDS) and FE-SEM (EDS) techniques and for sulfur-speciation using K-edge XANES techniques. These elemental and FE-SEM micro-graph data at several locations in the GRIM glasses from Shergotty (DBS), Zagami 994 and EET79001, Lith B showed that FeO and SO3 are positively correlated (SO3 represents a mixture of sulfide and sulfate). FE-SEM (EDS) study revealed that the sulfur-rich pockets in these glasses contain numerous micron-sized iron-sulfide (Fe-S) globules sequestered throughout the volume. However, in some areas (though less frequently), we detected significant Fe-S-O signals suggesting the occurrence of iron sulfate. These GRIM glasses were studied by K-edge microXANES techniques for sulfur speciation in association with iron in sulfur-rich areas. In both samples, we found the sulfur speciation dominated by sulfide with minor oxidized sulfur mixed in with various proportions. The abundance of oxidized sulfur was greater in 506 than in 507. Based on these results, we hypothesize that sulfur initially existed as sulfate in the glass precursor materials and, on shock-impact melting of the precursor materials producing these glasses, the oxidized sulfur was reduced to predominately sulfide. In order to further test this hypothesis, we have used microXANES to measure the valence states of vanadium in GRIM glasses from Lith A and Lith B to complement and compare with previous analogous measurements on Lith C (note: 506 and 507 contain the largest amounts of martian atmospheric gases but the gas-contents in Lith C measured by are unknown). Vanadium is ideal for addressing this re-dox issue because it has multiple valence states and is a well-studied element. Ferrous-dominated iron valences determined by microXANES on the Lith A and Lith B glasses provide little redox sensitivity. Vanadium valence measurements for impact glass in Lith C at three different locations yielded valence values of 3.1, 3.2 and 3.4 with inferred fO2 values of IW-0.7, IW-0.1 and IW+0.7, respectively. This range of oxygen-fugacity values is understandable because the glasses are shock-molten impact glasses which are heterogeneous in nature. Oxygen fugacity values obtained from the analysis of Fe-Ti oxides and Eu partitioning in pyroxenes from EET79001 Lith A and Lith B (host lithologies) were in the range of IW+0.3 to IW+1.9 suggesting that V in the Lith C impact glass was reduced in the impact process. Here, we examine whether the 506 from Lith A and 507 from Lith B GRIM glasses yield similar or different fO2 values from those of Lith C using the vanadium K-edge microXANES technique.

Sutton, S. R.↗

Technetium Incorporation in Glass for the Hanford Tank Waste Treatment and Immobilization Plant

A priority of the United States Department of Energy (U.S. DOE) is to dispose of nuclear wastes accumulated in 177 underground tanks at the Hanford Nuclear Reservation in eastern Washington State. These nuclear wastes date from the Manhattan Project of World War II and from plutonium production during the Cold War. The DOE plans to separate high-level radioactive wastes from low activity wastes and to treat each of the waste streams by vitrification (immobilization of the nuclides in glass) for disposal. The immobilized low-activity waste will be disposed of here at Hanford and the immobilized high-level waste at the national geologic repository. Included in the inventory of highly radioactive wastes is large volumes of 99Tc (~9 × 10E2 TBq or ~2.5 × 104 Ci or ~1500 kg). A problem facing safe disposal of Tc-bearing wastes is the processing of waste feed into in a chemically durable waste form. Technetium incorporates poorly into silicate glass in traditional glass melting. It readily evaporates during melting of glass feeds and out of the molten glass, leading to a spectrum of high-to-low retention (ca. 20 to 80%) in the cooled glass product. DOE-ORP currently has a program at Pacific Northwest National Laboratory (PNNL), in the Department of Materials Science and Engineering at Rutgers University and in the School of Mechanical and Materials Engineering at Washington State University that seeks to understand aspects of Tc retention by means of studying Tc partitioning, molten salt formation, volatilization pathways, and cold cap chemistry. Another problem involves the stability of Tc in glass in both the national geologic repository and on-site disposal after it has been immobilized. The major environmental concern with 99Tc is its high mobility in addition to a long half-life (2.1×105 yrs). The pertechnetate ion (TcO4-) is highly soluble in water and does not adsorb well onto the surface of minerals and so migrates nearly at the same velocity as groundwater. Long-term corrosion of glass waste forms is an area of current interest to the DOE, but attention to the release of Tc from glass has been little explored. It is expected that the release of Tc from glass should be highly dependent on the local glass structure as well as the chemistry of the surrounding environment, including groundwater pH. Though the speciation of Tc in glass has been previously studied, and the Tc species present in waste glass have been previously reported, environmental Tc release mechanisms are poorly understood. The recent advances in Tc chemistry that have given rise to an understanding of incorporation in the glass giving rise to significantly higher single-pass retention during vitrification are presented. Additionally, possible changes to the baseline flowsheet that allow for relatively minor volumes of Tc reporting to secondary waste treatment will be discussed.

Kruger, Albert A.↗

Structural and thermal characterization of CaO-MgO-SiO2-P2O5-CaF2 glasses

The paper presents the influence of varying CaO/MgO ratio on the structure and thermal properties of CaO-MgO-SiO2-P2O5-CaF2 glasses. A series of eight glass compositions in the glass forming region of diopside (CaMgSi2O6) - fluorapatite [Ca5(PO4)3F] - wollastonite (CaSiO3) ternary system have been designed and synthesized by varying diopside/wollastonite ratio in glasses. The as prepared melt-quenched glasses have been characterized for their structure by infrared spectroscopy (FTIR) and magic angle spinning (MAS)-nuclear magnetic resonance (NMR) spectroscopy. Silicon is predominantly present as Q2 (Si) species, while phosphorus tends to coordinate in orthophosphate environment in all the investigated glasses. The change in CaO/MgO ratio had an insignificant affect on the structure of glasses. The thermal sintering and crystallization parameters for the studied glasses have been obtained from differential thermal analysis (DTA) while crystalline phase fractions in the sintered glass-ceramics have been analyzed by X-ray diffraction adjoined with Rietveld refinement. Diopside, fluorapatite, wollastonite and pseudowollastonite have crystallized as the main crystalline phases in all the glass-ceramics with their content varying with respect to variation in CaO/MgO ratio in glasses. Scanning electron microscopy (SEM) has been used to shed light on the microstructure of glass-ceramics. The possible implications of structure and sintering behaviour of glasses on their bioactivity have been discussed.

36 MATERIALS SCIENCE↗

Development of Crystal-Tolerant High-Level Waste Glasses

Twenty five glasses were formulated. They were batched from HLW AZ-101 simulant or raw chemicals and melted and tested with a series of tests to elucidate the effect of spinel-forming components (Ni, Fe, Cr, Mn, and Zn), Al, and noble metals (Rh2O3 and RuO2) on the accumulation rate of spinel crystals in the glass discharge riser of the high-level waste (HLW) melter. In addition, the processing properties of glasses, such as the viscosity and TL, were measured as a function of temperature and composition. Furthermore, the settling of spinel crystals in transparent low-viscosity fluids was studied at room temperature to access the shape factor and hindered settling coefficient of spinel crystals in the Stokes equation. The experimental results suggest that Ni is the most troublesome component of all the studied spinel-forming components producing settling layers of up to 10.5 mm in just 20 days in Ni-rich glasses if noble metals or a higher concentration of Fe was not introduced in the glass. The layer of this thickness can potentially plug the bottom of the riser, preventing glass from being discharged from the melter. The noble metals, Fe, and Al were the components that significantly slowed down or stopped the accumulation of spinel at the bottom. Particles of Rh2O3 and RuO2, hematite and nepheline, acted as nucleation sites significantly increasing the number of crystals and therefore decreasing the average crystal size. The settling rate of ≤10-μm crystal size around the settling velocity of crystals was too low to produce thick layers. The experimental data for the thickness of settled layers in the glasses prepared from AZ-101 simulant were used to build a linear empirical model that can predict crystal accumulation in the riser of the melter as a function of concentration of spinel-forming components in glass. The developed model predicts the thicknesses of accumulated layers quite well, R2 = 0.985, and can be become an efficient tool for the formulation of the crystal-tolerant HLW glasses for higher waste loading. A physical modeling effort revealed that the Stokes and Richardson-Zaki equations can be used to adequately predict the accumulation rate of spinel crystals of different sizes and concentrations in the glass discharge riser of HLW melters. The determined shape factor for the glass beads was only 0.73% lower than the theoretical shape factor for a perfect sphere. The shape factor for the spinel crystals matched the theoretically predicted value to within 10% and was smaller than that of the beads, given the larger drag force caused by the larger surface area-to-volume ratio of the octahedral crystals. In the hindered settling experiments, both the glass bead and spinel suspensions were found to follow the predictions of the Richardson-Zaki equation with the exponent n = 3.6 and 2.9 for glass beads and spinel crystals, respectively.

36 MATERIALS SCIENCE↗

EVALUATION OF IMPURITY EXTREMES IN A PLUTONIUM-LOADED BOROSILICATE GLASS

A vitrification technology utilizing a lanthanide borosilicate (LaBS) glass appears to be a viable option for the disposition of excess weapons-useable plutonium that is not suitable for processing into mixed oxide (MOX) fuel. A significant effort to develop a glass formulation and vitrification process to immobilize plutonium was completed in the mid-1990s. The LaBS glass formulation was found to be capable of immobilizing in excess of 10 wt % Pu and to be tolerant of a range of impurities. To confirm the results of previous testing with surrogate Pu feeds containing impurities, four glass compositions were selected for fabrication with actual plutonium oxide and impurities. The four compositions represented extremes in impurity type and concentration. The homogeneity and durability of these four compositions were measured. The homogeneity of the glasses was evaluated using x-ray diffraction (XRD) and scanning electron microscopy coupled with energy dispersive spectroscopy (SEM/EDS). The XRD results indicated that the glasses were amorphous with no evidence of crystalline species in the glass. The SEM/EDS analyses did show the presence of some undissolved PuO{sub 2} material. The EDS spectra indicated that some of the PuO{sub 2} crystals also contained hafnium oxide. The SEM/EDS analyses showed that there were no heterogeneities in the glass due to the feed impurities. The durability of the glasses was measured using the Product Consistency Test (PCT). The PCT results indicated that the durability of Pu impurity glasses was comparable with Pu glasses without impurities and significantly more durable than the Environmental Assessment (EA) glass used as the benchmark for repository disposition of high-level waste (HLW) glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Influence of strontium on structure, sintering and biodegradation behaviour of CaO-MgO-SrO-SiO2-P2O5-CaF2 glasses

The present study investigates the influence of SrO on structure, apatite forming ability, physico-chemical degradation and sintering behaviour of melt-quenched bioactive glasses with composition: mol.% (36.07 – x) CaO – x SrO - 19.24 MgO – 5.61 P2O5 – 38.49 SiO2 – 0.59 CaF2, where x varies between 0 – 10. The detailed structural analysis of glasses has been made by infra red spectroscopy (FTIR) and magic angle spinning-nuclear magnetic resonance spectroscopy (MAS-NMR). Silicon was predominantly present as Q2 (Si) species while phosphorus was found in orthophosphate type environment in all the investigated glasses. The apatite forming ability of glasses was investigated by immersion of glass powders in simulated body fluid (SBF) for time durations varying between 1 h – 7 days. While increasing Sr2+/Ca2+ ratio in glasses did not affect the structure of glasses significantly, their apatite forming ability was decreased considerably. Further, physico-chemical degradation of glasses has been studied in accordance with ISO 10993-14 “Biological evaluation of medical devices – Part 14: Identification and quantification of degradation products from ceramics” in Tris HCl and citric acid buffer and the possible implications of ion release profile from glasses in different solutions has been discussed. The addition of strontium in glasses led to a 7-fold decrease in chemical degradation of glasses in Tris-HCl. The sintering of glass powders rendered glass-ceramics (GCs) with varying degree of crystallinity and good flexural strength (98-131 MPa) where the mechanical properties depend on the nature and amount of crystalline phases present in GCs.

58 GEOSCIENCES↗

Spectroscopic investigation of historical uranium glasses

Here, we present spectroscopic investigations of uranium in two historical glasses. A 1920's-1930's Art Deco (Bagley Carnival) green soda-lime-silica uranium glass bowl and a 1930's-1940's (Thomas Webb) yellow full lead crystal uranium glass vase were studied using optical absorption spectroscopy, XRF and SEM-EDX, X-band EPR and High- Energy Resolution Fluorescence-Detected (HERFD)-XANES. Uranium speciation may be different in the two glasses. Uranium occurs as uranyl groups (UO 2 2+ ) with minority reduced uranium species, mostly as U(V), more important in the Webb glass than in the Bagley glass. The differences between the two glasses arise from the fining procedure and result from the presence of other multivalent elements and differences in base glass composition. Electron Paramagnetic Resonance (EPR) spectra show the presence of an incipient signal close to g~2, partially annealed by heating to 550 °C, which we assign to a small concentration of radiation-induced defects caused by uranium decay. The presence of multivalent glass components in addition to U (As + Cu + Fe in the Bagley glass and Sb + Fe in the Webb glass) can trap the electron-hole pairs generated by the presence of uranium. This may explain the weakness of this signal in these glasses that anyway received a limited radiation dose since their fabrication. The low activity of these glasses, close to the background radiation, confirms that there is no danger to exhibiting them in museums.

36 MATERIALS SCIENCE↗

Effect of adjusting composition on the crystallization and luminescence properties in NaYF{sub 4}:Er{sup 3+} embedded glass ceramics

Highlights: • Intense 2.7 μm emission was achieved in transparent glass ceramics containing NaYF{sub 4}:Er{sup 3+} nanocrystals. • The crystallization and luminescence properties of the nanocrystals embedded glass ceramics are tuned by adjusting the Na{sub 2}O/NaF ratio. • Modifying the properties of glass ceramics through adjusting the glass composition is an effective route. - Abstract: Intense 2.7 μm emission was achieved in transparent glass ceramics containing NaYF{sub 4}:Er{sup 3+} nanocrystals. The effect of adjusting Na{sub 2}O/NaF ratio in glass composition on the crystallizing and luminescence behavior in the glass ceramics was investigated. The controllable crystallization property of NaYF{sub 4} nanocrystals was remained after modifying the glass composition and the crystallization temperature was largely reduced for the samples with high Na{sub 2}O content. The X-ray diffraction and transmission electron microscopy analysis evidenced the shrink of lattice parameter with increasing Na{sub 2}O content. High transparency was kept for these glass ceramic samples, and intense upconversion, near- and mid-infrared emissions were obtained in Er{sup 3+}-doped glass ceramics with an increase of red/green ratio and prominent Stark splits in the sample with high Na{sub 2}O content, indicating the change of crystal field around Er{sup 3+} in the host matrix. Our results indicate that the crystallization and luminescence properties of glass ceramics could be modified through adjusting the glass composition, and it is an effective route to develop glass ceramics with favorable properties.

36 MATERIALS SCIENCE↗

Ion-Exchange Interdiffusion Model with Potential Application to Long-Term Nuclear Waste Glass Performance

Ion exchange is an integral mechanism influencing the corrosion of glasses. Due to the formation of alteration layers in aqueous conditions, it is difficult to conclusively deconvolute the process of ion exchange from other processes, principally dissolution of the glass matrix. Therefore, we have developed a method to isolate alkali diffusion that involves contacting glass coupons with a solution of 6 LiCl dissolved in functionally inert dimethyl sulfoxide. Here, we employ the method at temperatures ranging from 25 to 150 °C with various glass formulations. Glass compositions include simulant nuclear waste glasses, such as SON68 and the international simple glass (ISG), glasses in which the nature of the alkali element was varied, and glasses that contained more than one alkali element. An interdiffusion model based on Fick’s second law was developed and applied to all experiments to extract diffusion coefficients. The model expands established models of interdiffusion to the case where multiple types of alkali sites are present in the glass. Activation energies for alkali ion exchange were calculated and the results are in agreement with those obtained in glass strengthening experiments but are nearly five times higher than values reported for diffusion-controlled processes in nuclear waste glass corrosion experiments. A discussion of the root causes for this apparent discrepancy is provided. The interdiffusion model derived from laboratory experiments is expected to be useful for modeling glass corrosion in a geological repository when the silicon concentration is high.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Distinct atomic structures of the Ni-Nb metallic glasses formed by ion beam mixing

Four Ni-Nb metallic glasses are obtained by ion beam mixing and their compositions are measured to be Ni{sub 77}Nb{sub 23}, Ni{sub 55}Nb{sub 45}, Ni{sub 31}Nb{sub 69}, and Ni{sub 15}Nb{sub 85}, respectively, suggesting that a composition range of 23-85 at. % of Nb is favored for metallic glass formation in the Ni-Nb system. Interestingly, diffraction analyses show that the structure of the Nb-based Ni{sub 31}Nb{sub 69} metallic glass is distinctly different from the structure of the Nb-based Ni{sub 15}Nb{sub 85} metallic glass, as the respective amorphous halos are located at 2{theta}{approx_equal}38 and 39 deg. To explore an atomic scale description of the Ni-Nb metallic glasses, an n-body Ni-Nb potential is first constructed with an aid of the ab initio calculations and then applied to perform the molecular dynamics simulation. Simulation results determine not only the intrinsic glass forming range of the Ni-Nb system to be within 20-85 at. % of Nb, but also the exact atomic positions in the Ni-Nb metallic glasses. Through a statistical analysis of the determined atomic positions, a new dominant local packing unit is found in the Ni{sub 15}Nb{sub 85} metallic glass, i.e., an icositetrahedron with a coordination number to be around 14, while in Ni{sub 31}Nb{sub 69} metallic glasses, the dominant local packing unit is an icosahedron with a coordination number to be around 12, which has been reported for the other metallic glasses. In fact, with increasing the irradiation dose, the Ni{sub 31}Nb{sub 69} metallic glasses are formed through an intermediate state of face-centered-cubic-solid solution, whereas the Ni{sub 15}Nb{sub 85} metallic glass is through an intermediate state of body-centered-cubic-solid solution, suggesting that the structures of the constituent metals play an important role in governing the structural characteristics of the resultant metallic glasses.

36 MATERIALS SCIENCE↗

Structure of rhenium-containing sodium borosilicate glass

A series of sodium borosilicate glasses were synthesized with increasing fractions of KReO4 or Re2O7, to 10000 ppm (1 mass%) target Re in glass, to assess the effects of large concentrations of rhenium on glass structure and to estimate the solubility of technetium, a radioactive component in typical low active waste nuclear waste glasses. Magic angle spinning nuclear magnetic resonance (MAS-NMR), Fourier transform infrared (FTIR) spectroscopy, and Raman spectroscopy were performed to characterize the glasses as a function of Re source additions. In general, silicon was found coordinated in a mixture of Q2 and Q3 structural units, while Al was 4-coordinated and B was largely 3-coordinate and partially 4-coordinated. The rhenium source did not appear to have significant effects on the glass structure. Thus, at the up to the concentrations that remain in dissolved in glass, ~3000 ppm Re by mass maximum. , the Re appeared to be neither a glass-former nor a strong glass modifier., Rhenium likely exists in isolated ReO4- anions in the interstices of the glass network, as evidenced by the polarized Raman spectrum of the Re glass in the absence of sulfate. Analogous to SO42-¬ in similar glasses, ReO4- is likely a network modifier and forms alkali salt phases on the surface and in the bulk glass above solubility.

borosilicate glass↗