At least 649 records · Page 36

Effect of Tool Pin Eccentricity on the Microstructure and Mechanical Properties of Friction Stir Processed Al-6061 Alloy

Three different stir tools with the pin eccentricity of 0, 0.4 and 0.8 mm were applied to the friction stir processing (FSP) of Al-6061 alloy. Results show that the pin-affected zone (PAZ) enlarges and the grain size in the stir zone (SZ) decreases as the pin eccentricity increases. Moreover, the low peak FSP temperature induced by the pin eccentricity gives rise to the coarsening of strengthening precipitates in the SZ. Compared with the pin-eccentric FSP samples, the SZ produced without pin eccentricity exhibits the highest hardness and yield strength due to the high amount of fine precipitates. However, the application of pin eccentricity elevates the overall tensile properties of FSP samples through changing the failure location from heat-affected zone (HAZ) to SZ.

36 MATERIALS SCIENCE↗

Cooling Environment Effect on the Microstructure and Mechanical Properties of Friction Stir-Welded Joints

The heat input in friction stir welding (FSW) influences the localized properties in welded joint. The external cooling during FSW reduces the localized heating and post-weld cooling time by extracting heat comparatively at a faster rate. In the present study, we have investigated the effect of different cooling environments on the performance of friction stir-welded (FSWed) AA5052 strain-hardenable aluminum alloy. Welding was performed under three different cooling environments such as natural air, water and liquid nitrogen in order to understand their effects on grain structure, metallurgical changes and mechanical properties of the joints. It has been noted that the width of weld nugget zone, thermo-mechanically affected zone and heat-affected zone has been decreased with the respective change in cooling environments. Welding speed could also influence the width of different zones in weldment alike the cooling environments. Finer grain size has been noticed with water cooling against the liquid nitrogen cooling. Comparatively, water was observed to be more favorable cooling environment against liquid nitrogen because of its better weld quality (97%) compared with base metal. The favorable mechanical properties resulting from the different weldment regions for different cooling environments have been elaborated in the present study.

36 MATERIALS SCIENCE↗

High-Carbon Ferrochrome Effects on Microstructure and Mechanical Properties of Powder Metallurgy Titanium Alloys

In this paper, the powder metallurgy method was employed to prepare titanium alloys with high-carbon ferrochrome (HCFeCr). With the HCFeCr addition, the size of the β grains decreased and the lamellae of the α phase became thinner. The TiC strengthening phase precipitated at the grain boundaries, resulting in the inhibition of the β grain growth and hardness enhancement. In addition, Fe and Cr as β-stabilizing elements existed in the enriched β-Ti phase, which increased the β phase amount. The strength improvement was attributed to grain size optimization and strengthening phase formation. With the 9 wt.% HCFeCr addition, the corresponding Vickers hardness increased to 480 HV, which is 60% higher than the Ti6Al4V alloy. The tensile and yield strength was 1228 and 1140 MPa, respectively. The addition of HCFeCr can effectively enhance the strength and hardness while reducing the cost. This is a promising additive to obtain low-cost Ti alloys with high mechanical properties.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of B{sub 4}C-Blended M3:2 High-Speed Steel Powders Consolidated by Sintering and Heat Treatment

Water-atomized powders of M3:2 high-speed steel (HSS) were blended with B{sub 4}C and consolidated by cold press sintering. With the addition of B{sub 4}C (~ 0.2 vol.%), satisfactory mechanical properties were achieved for HSS by sintering at a temperature as low as 1190 °C [e.g., 53.2 ± 0.2 in the Rockwell hardness (HRC) and 3074 ± 56 MPa in bending strength]. High relative density (98.5%) and good strength were attributed to the mechanism described as follows: First, the atoms of boron and carbon escaped after the reaction between B{sub 4}C and iron matrix. Then, the sintered HSS was strengthened by boron atoms while they were distributed in M{sub 6}C or MC carbides and iron matrix. Second, a plenty of M{sub 6}C carbides were formed due to the release of carbon atoms. As a result, the value of solidus temperature was reduced. In addition, mechanical properties were greatly improved by heat treatment (quenching and tempering) (e.g., 61.2 ± 0.3 in HRC, 4356 ± 64 MPa in bending strength, and 42.3 ± 0.5 MPa m{sup 1/2} in fracture toughness, respectively).

36 MATERIALS SCIENCE↗

Effect of Rolling Temperature on the Microstructure and Mechanical Properties of AZ31 Alloy Sheet Processed through Variable-Plane Rolling

AZ31 magnesium alloy sheet was produced through variable-plane rolling (VPRing) under different temperatures, and a conventional rolled AZ31 alloy was investigated for comparison. A basal texture was formed during these two processes. The texture intensity was closely related to dynamic recrystallization and deformation mechanism. Four types of twins appeared, namely {10-12} extension twins, {10-13} and {10-11} contraction twins and {10-11}-{10-12} double twins. High rolling temperature and rolling plane alteration were beneficial for activating {10-11}-{10-12} double twins. The tensile strengths revealed a declining trend with elevated rolling temperatures. The AZ31 alloy rolled at 573 K showed advantageous combination with a high yield strength of 286 MPa and compromised elongation of 5%. The mechanical anisotropy of VPRed AZ31 sheet decreased with nearly similar yield strengths along the roll direction (RD), transverse direction and 45° away from the RD. The VPRing process improved the rollability and strength of Mg alloy and reduced its mechanical anisotropy.

36 MATERIALS SCIENCE↗

Effect of Delta Ferrite on Microstructure and Mechanical Properties of High-Chromium Martensitic Steel

The fusion zone of modified 9Cr-1Mo steel experiencing a peak temperature of 1450 °C and varying cooling rates between 1 and 40 °C/s from the peak temperature is simulated using Gleeble thermal simulator. Mechanical properties of the simulated samples are assessed by ball indentation and impression creep tests. The study evaluates the effect of cooling rate on volume fraction, morphology of retained delta ferrite in the simulated partially melted zone of an autogenous weld, and subsequently its effect on the mechanical properties of this zone. With varying cooling rate, volume fraction of delta ferrite does not change much; however, its morphology changes from polygonal island to grain boundary network in case of excessive slow cooling (1 °C/s). Morphological variation of delta ferrite affects the creep properties of this zone. Partially melted zone, which is cooled at 1 °C/s with delta ferrite present in the interdendritic regions, exhibits maximum creep strain and creep strain rate.

36 MATERIALS SCIENCE↗

The hydration, microstructure, and mechanical properties of vaterite calcined clay cement (VC 3 )

Limestone (calcite) calcined clay cement (LC 3 ) is a promising low-CO 2 binder, but the low activity of calcite cannot compensate the reduction in clinker factor, resulting in low one-day strength and limiting its broad applications. As recent carbon capture and utilization technologies allow scalable production of vaterite, a more reactive CaCO 3 polymorph, we overcome the challenge by introducing vaterite calcined clay cement (VC 3 ), inspired by the vaterite-calcite phase change. In the present study, VC 3 exhibits higher compressive strengths and faster hydration than LC 3 . Compared to hydrated LC 3 , hydrated VC 3 exhibits increased amount of hemi- and mono-carboaluminate formation and decreased amount of strätlingite formation. With gypsum adjustment, the 1-day strength of VC 3 is higher than that of pure cement reference. Finally, VC 3 , a low-CO 2 binder, presents great potential as a host of the metastable CaCO 3 for carbon storage and utilization and as an enabler of carbon capture at gigaton scales.

36 MATERIALS SCIENCE↗