Intrinsic Stress in Aerosol Deposited TiO2 Films Measured by Substrate Bending.
Abstract not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
SPIE DCS, Virtual, April 3-4, 2022
Abstract not provided.
This report demonstrates a chemical functionalization method for controlling atomic layer deposition (ALD) of TiO{sub 2} in low-density nanoporous materials. Functionalization of silica aerogel with trimethylsilane is shown to strongly suppress TiO{sub 2} growth via ALD. Subsequent modification of the functionalization through selective removal of the hydrocarbon groups reactivates the aerogel towards TiO{sub 2} deposition. These results demonstrate the potential use of ALD as a selective tool for creating novel nanoporous materials. Nanoporous materials present significant technological advantage for a wide range of applications, including catalysis, energy storage and conversion, nanoelectronics to name just a few (1-4). Hence, there is considerable interest in developing synthetic pathways for the fabrication of nanoporous materials with tailored properties. Aerogels (AGs) are unique low-density, open-cell porous materials consisting of submicrometer pores and ligaments that can be used as a robust material platform for designing novel nanoporous materials. In recent years, a synthetic approach based on ALD on AG templates has emerged as a promising method for the directed growth of nanoporous materials (5-11, 18). This approach has been used successfully to prepare millimeter-sized high aspect ratio aerogels coated uniformly with zinc oxide (ZnO), tungsten (W) and alumina (Al{sub 2}O{sub 3}) (10, 11). The ALD process utilizes two sequential, self-limiting surface reactions resulting in a layer-by-layer growth mode. The self limiting nature of the surface reactions makes ALD a particularly suitable technique for uniform deposition onto high aspect ratio porous substrates. Additionally, chemical specificity of the surface reactions in ALD enables one to control the deposition process through selective functionalization of the substrate surface. In fact the functionalization of planar substrates such as silicon wafers with organosilane groups (R{sub n}SiX{sub 4-n} (n = 1-3)) has been shown to deactivate the substrate towards ZrO{sub 2}, HfO{sub 2}, ZnO, and TiO{sub 2} ALD processes (12-16). A possible mechanism for the deactivation effect is the blocking of surface functional groups, such as hydroxyl (OH) moieties, which serve as chemisorption sites for the ALD precursors and hence are essential for nucleating the deposition process. Henceforth, we shall refer to these surface functional groups as nucleation sites for the ALD process.
We report on one-step in situ codoped TiO2 thin films synthesized by cosputtering. The purpose of this acceptor-donor passivated codoping approach is to overcome the optoelectronic limitations that arise for monodoped TiO2 in photocatalytic applications. To evaluate these added benefits, the TiO2:WN thin films were characterized by different techniques. X-ray diffraction patterns and X-ray photoelectron spectral analysis revealed that both N and W dopants are mostly present in the desired substitutional locations. Additionally, the codoping approach was found to reduce the internal strain and defect density of the TiO2:WN films as compared to their monodoped TiO2:N counterparts. This defect reduction is confirmed via photocharge lifetime variation obtained using visible light flash photolysis time-resolved microwave conductivity measurements (FP-TRMC). Photocharge lifetime analysis indicated the presence of three distinct decay processes: charge trapping, recombination, and surface reactions. These characteristic lifetimes of the codoped TiO2:WN films (i.e., 0.08, 0.75, and 11.5 us, respectively) were found to be about double those of their nitrogen monodoped TiO2:N counterparts (i.e., 0.03, 0.35, and 6.8 us), quantitatively confirming the effective passivating outcome of the tungsten-nitrogen codoping approach developed here. The practicality of this method was confirmed by integrating the TiO2:WN films as photoanodes for the electro-photocatalytic, solar light driven degradation of a real pollutant (i.e., atrazine). A significant increase in the degradation kinetics, leading to a 4-fold increase in the pseudo-first-order degradation constant for the optimally doped TiO2:WN photoanodes (0.106 min-1) from the undoped TiO2-x ones (0.026 min-1), is a direct consequence of the increased photocharge lifetimes in tandem with visible light photosensitivity.
This project developed self-cleaning photocatalytic coatings that remove contamination without human intervention. The coatings chemically remove organic contaminants and leave no residue. The photocatalyst will not negatively affect other coating properties, especially corrosion resistance. Titanium dioxide, TiO2, is an extremely popular photocatalyst because of its chemical stability, nontoxicity, and low cost. TiO2 is commonly used in the photocatalytic oxidation of organic matter or pollutants in the gas and liquid phases. However, TiO2 does have some drawbacks. It has limited light absorption because of its large band-gap and suffers from a photonic efficiency of less than 10 percent for organic degradation. Dopants can lower the band-gap and improve efficiency. Since the photocatalytically active form of TiO2 is a nanocrystalline powder, it can be difficult to make a robust coating with enough catalyst loading to be effective. Photocatalysts become active when certain light energy is absorbed. When photons with an energy greater than the band-gap, Eg, (wavelengths shorter than 400 nm) impinge upon the surface of the TiO2, an electron-hole pair is formed. The electron-hole pair oxidizes adsorbed substances either directly or via reactive intermediates that form on the surface, such as hydroxyl radicals (OH) or superoxide ions (O2-). Several factors can influence the band-gap energy of TiO2, two of which are crystal structure and impurities. TiO2 exists as three crystal structures brookite, anatase, and rutile that can be controlled via heat treatment. Anatase is the most photocatalytically active crystal form of TiO2. Doping TiO2 with impurities can alter its band-gap energy, as well as its effectiveness as a catalyst. Depending on their size, dopant atoms can occupy either the substitutional or interstitial lattice positions. Atoms that are relatively large will assume the interstitial positions and create a much greater energy disturbance in the crystal than will smaller atoms that take on the substitutional positions. This energy disturbance narrows the band-gap and thus allows photons with longer wavelengths and smaller energies (such as those in the visible-light spectrum) to create electron-hole pairs. Raman spectroscopy was performed for the purpose of determining the crystal structure and the degree of crystallinity of the TiO2 particles. Reflectance measurements indicated the wavelengths of light absorbed by the different catalysts.
Nanosecond laser flash photolysis and photocurrent measurements have been used to investigate use of [(Ru(bpy)2(4,4'-(PO3H2)2bpy)]2+ attached to TiO2 nanoparticle films, TiO2-RuII, in a dye-sensitized photoelectrosynthesis cell (DSPEC) configuration for H2 production. In these experiments, laser flash excitation of TiO2-RuII and rapid injection lead to TiO2(e-)-RuIII with subsequent TiO2(e-)-RuIII → TiO2-RuII back electron transfer monitored on the nsec time scale with and without added triethanolamine (TEOA) and deprotonated ethylenediaminetetraacetic tetra-anion (EDTA4-) as irreversible electron transfer donors. With added TEOA or EDTA4-, a competition exists between back electron transfer and scavenger oxidation with the latter leading to H2 production in the photoelectrosynthesis cell. Reduction of TiO2(e-)-RuIII by both TEOA and EDTA4- occurs with kD ~ 106 M-1 s-1. EDTA4- is a more efficient scavenger by a factor of ~3 because of a more favorable partition equilibrium between the film and the external solution. Its increased scavenger efficiency appears in incident photon-to-current conversion efficiency (IPCE) measurements, in electron collection efficiencies (ηcoll), and in photocurrent measurements with H2 production. Evaluation of electron collection efficiencies by transient current measurements gave ηcoll ~ 24% for TEOA and ~ 70% for EDTA4-. The dynamics of back electron transfer are minimized, and collection efficiencies, photocurrents, and hydrogen production are maximized by application of a positive applied bias consistent with the results of I-V measurements. A pH dependent plateau is reached at ~0 V at pH = 4.5 (EDTA4-) and at ~ -0.4 V at pH 6.7 (TEOA). The difference is qualitatively consistent with the influence of pH on electron population in trap states below the conduction band and the role they play in back electron transfer. The excitation dependence of IPCE measurements matches the spectrum of TiO2-RuII with IPCE values ~3 times higher for EDTA4- than for TEOA as noted above. Absorbed photon-to-current efficiency (APCE) values are light-intensity dependent because of the effect of multiple injection events and the influence of increasing trap site electron densities on back electron transfer. The key to efficient H2 production is minimizing back electron transfer. Application of a sufficiently positive potential relative to ECB for TiO2 accelerates loss of electrons from the film in competition with back electron transfer allowing for H2 production with efficiencies approaching 14.7% under steady-state irradiation.
Carbothermal reduction of semiconducting TiO2 into highly conductive titanium oxycarbide (TiOxCy) was investigated. The thermally produced uniform carbon layer on TiO2 (Degussa P25) protects the TiO2 nanoparticles from sintering and, at the same time, supplies the carbon source for doping TiO2 with carbon. At low temperatures (e. g., 700 degrees C), carbon only substitutes part of the oxide and distorts the TiO2 lattice to form TiO2-xCx with only substitutional carbon. When the carbon-doped TiO2 is annealed at a higher temperature (1100 degrees C), x-ray diffraction and x-ray photoelectron spectroscopy results showed that TiOxCy, a solid solution of TiO and TiC, was formed, which displays different diffraction peaks and binding energies. It was shown that TiOxCy has much better oxygen revolution reaction activity than TiO2 or TiO2-xCx. Further studies showed that the TiOxCy obtained can be used as a support for metal electrocatalyst, leading to a bifunctional catalyst effective for both oxygen reduction and evolution reactions.
Titanium dioxide nanoparticles (TiO{sub 2} NPs) studies have been performed using relatively high NPs concentration under acute exposure and limited studies have compared shape effects. We hypothesized that midterm exposure to low TiO{sub 2} NPs concentration in lung epithelial cells induces carcinogenic characteristics modulated partially by NPs shape. To test our hypothesis we synthesized NPs shaped as belts (TiO{sub 2}-B) using TiO{sub 2} spheres (TiO{sub 2}-SP) purchased from Sigma Aldrich Co. Then, lung epithelial A549 cells were low-exposed (10 µg/cm{sup 2}) to both shapes during 7 days and internalization, cytokine release and invasive potential were determined. Results showed greater TiO{sub 2}-B effect on agglomerates size, cell size and granularity than TiO{sub 2}-SP. Agglomerates size in cell culture medium was 310 nm and 454 nm for TiO{sub 2}-SP and TiO{sub 2}-B, respectively; TiO{sub 2}-SP and TiO{sub 2}-B induced 23% and 70% cell size decrease, respectively, whilst TiO{sub 2}-SP and TiO{sub 2}-B induced 7 and 14-fold of granularity increase. NO{sub x} production was down-regulated (31%) by TiO{sub 2}-SP and up-regulated (70%) by TiO{sub 2}-B. Both NPs induced a transient cytokine release (IL-2, IL-6, IL-8, IL-4, IFN-γ, and TNF-α) after 4 days, but cytokines returned to basal levels in TiO{sub 2}-SP exposed cells while TiO{sub 2}-B induced a down-regulation after 7 days. Midterm exposure to both shapes of NPs induced capability to degrade cellular extracellular matrix components from chorioallantoic membrane and Ki-67 marker showed that TiO{sub 2}-B had higher proliferative potential than TiO{sub 2}-SP. We conclude that midterm exposure to low NPs concentration of NPs has an impact in the acquisition of new characteristics of exposed cells and NPs shape influences cellular outcome. - Graphical abstract: (A) Lung epithelial cells were low exposed (below 10 µg/cm{sup 2}) to titanium dioxide nanoparticles (TiO{sub 2}-NPs) shaped as spheres (TiO{sub 2}-SP) and belts (TiO{sub 2}-B) for midterm (7 continuous days) separately. (B) Then, cells from each cell culture were harvested and seeded on the top of the chorioallantoic membrane (CAM) for 5 days and (C) invasion and proliferation of cells were analyzed in CAM sections. - Highlights: • Hydrodynamic size of TiO2- SP was smaller than TiO2-B in cell culture media • TiO2- SP induced higher decrease in cell size than TiO2-B • TiO2-SP induced a transient cytokine release and TiO2-B a downregulation • TiO2-B caused higher proliferative capability than TiO2-SP.
Lunar ilmenite (FeTiO3) is a potential resource capable of providing oxygen for life support and spacecraft propellant for future lunar bases. Estimates of TiO2 content in mature mare soils can be made using an empirical relation between the 400/500 nm reflectance ratio and TiO2 wt percent. A TiO2 abundance map was constructed for the entire near-side lunar maria accurate to + or - 2 wt percent TiO2 using CCD images obtained at the Tumamoc Hill 0.5 m telescope in Tucson, employing bandpass filters centered at 400 and 560 nm. Highest TiO2 regions in the maria are located in western Mare Tranquillitatis. Greater contrast differences between regions on the lunar surface can be obtained using 400/730 nm ratio images. The relation might well be refined to accommodate this possibly more sensitive indicator of TiO2 content. Another potential lunar resource is solar wind-implanted He-3 which may be used as a fuel for fusion reactors. Relative soil maturity, as determined by agglutinate content, can be estimated from 950/560 nm ration images. Immature soils appear darker in this ratio since such soils contain abundant pyroxene grains which cause strong absorption centered near 950 nm due Fe(2+) crystal field transitions. A positive correlation exists between the amount of He-3 and TiO2 content in lunar soils, suggesting that regions high in TiO2 should also be high in He-3. Reflectance spectrophotometry in the region 320 to 870 nm was also obtained for several regions. Below about 340 nm, these spectra show variations in relative reflectance that are caused by as yet unassigned near-UV absorptions due to compositional differences.
Titania (TiO2) nanofibers were fabricated by electrospinning three representative spin dopes made of titanium (IV) n-butoxide (TNBT) and polyvinylpyrrolidone (PVP) with the TNBT/PVP mass ratio being 1/2 in three solvent systems including N,N-dimethylformamide (DMF), isopropanol, and DMF/isopropanol (1/1 mass ratio) mixture, followed by pyrolysis at 500 C. The detailed morphological and structural properties of both the as-electrospun precursor nanofibers and the resulting final TiO2 nanofibers were characterized by SEM, TEM, and XRD. The results indicated that the precursor nanofibers and the final TiO2 nanofibers made from the spin dopes containing DMF alone or DMF/isopropanol mixture as the solvent had the common cylindrical morphology with diameters ranging from tens to hundreds of nanometers, while those made from the spin dope containing isopropanol alone as the solvent had an abnormal concave morphology with sizes/widths ranging from sub-microns to microns. Despite the morphological discrepancies, all precursor nanofibers were structurally amorphous without distinguishable phase separation, while all final TiO2 nanofibers consisted of anatase-phased TiO2 single-crystalline grains with sizes of approximately 10 nm. The electrospun TiO2 nanofiber mat is expected to significantly outperform other forms (such as powder and film) of TiO2 for the solar cell (particularly dye-sensitized solar cell) and photo-catalysis applications.