At least 649 records · Page 36

Microstructure and texture evolution of deformed Mg-Zn alloy during recrystallization

Highlights: • The texture intensity in the Mg-Zn alloy relied on the microstructure. • Fine DRXed grains showed a fiber texture distributing between <10.0> and <11.0>. • Coarse DRXed grains mainly exhibited <11.0> fiber texture. • The preferred growth of <11.0> oriented grains resulted in texture evolution. - Abstract: The microstructure and texture evolution of Mg-Zn alloy during recrystallization was investigated by EBSD in the present study. Deformed region, fine DRXed region and coarse DRXed region were obtained in Mg-Zn alloy during deformation. It was found that the texture intensity in DRXed region was weaker compared with the deformed region. The second phase at grain boundaries resulted in the formation of fine DRXed grains with weaker texture compared with the coarse DRXed region. Additionally, a remarkable grain-size driven textural transition from <10.0>–<11.0> texture to <11.0> texture were detected with the growth of DRXed grains. The recrystallized grains with small grain size showed a fiber texture distributing homogeneously between <10.0> and <11.0>, while <11.0> fiber texture was predominant for the large recrystallized grains. It is suggested that <11.0> oriented grains grew faster than other oriented grains, which was ascribed to larger misorientation between <11.0> oriented grains and their neighboring grains.

36 MATERIALS SCIENCE↗

High-Temperature Properties and Microstructural Stability of the AISI H13 Hot-Work Tool Steel Processed by Selective Laser Melting

The microstructural stabilities, softening resistance, and high-temperature tensile properties of the H13 hot-work tool steel by selective laser melting (SLM) were systematically studied. A series of tempering procedures were performed on the as-SLMed specimens. Afterwards, the mechanism of softening resistance behavior was discussed based on the XRD, SEM, EBSD observations, hardness measurements, and high-temperature tensile tests. It was found that the as-SLMed H13 consisted of α-iron and γ-iron. The carbide-stabilizing elements aggregated as the cell-like substructures for the rapid solidification of the SLM process. After the softening resistance treatment, the retained austenite transformed to ferrite and carbide mixtures. The cell-like substructures dissolved slowly into the matrix when the temperature was below 550 °C. These factors increased the hardness and retarded the softening of the material. When the temperature was 600 °C, the microstructural constituents transformed to soft ferrite and globular carbides, which lead to a considerable decrease of the hardness. Due to the grain refinement, solid solution strengthening, and residual stress, the as-SLMed H13 exhibited better mechanical properties than that of the wrought counterparts.

36 MATERIALS SCIENCE↗

Effects of LPSO/α-Mg interfaces on dynamic recrystallization behavior of Mg96.5Gd2.5Zn1 alloy

Highlights: • The effects of LPSO/α-Mg interfaces on the dynamic recrystallization (DRX) behavior of Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} (at.%) alloy during indirect extrusion at 350 °C were investigated. • The LPSO/α-Mg interfaces in Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} alloy appeared as two groups, including the basal and non-basal LPSO/α-Mg interfaces, which have various effects on the DRX behavior of Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} alloy. • Compared with the basal LPSO/α-Mg interfaces, DRX grains are preferentially nucleated near the non-basal LPSO/α-Mg interfaces where there is higher V{sub GROD} and lower required energy E{sub s} for the DRX nucleation. - Abstract: Mg-Gd-Zn alloy, which contains a long period stacking ordered (LPSO) structure, has the potential to become a high-strength Mg alloy within the automotive and aerospace industries. Two types of LPSO/α-Mg interfaces in Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} (at.%) alloy were characterized, namely, basal and non-basal LPSO/α-Mg interfaces. The effects of LPSO/α-Mg interfaces on the dynamic recrystallization (DRX) behavior during indirect extrusion at 350 °C were investigated. The grain reference orientation deviation (GROD) value (V{sub GROD}), derived from EBSD, could qualitatively characterize the dislocation density within a grain and determine the presence of DRX grain nucleation. The results suggested that the areas around non-basal LPSO/α-Mg interfaces always have higher V{sub GROD} than do basal LPSO/α-Mg interfaces. In addition, the stored energy (E{sub s}) required for DRX nucleation on the non-basal LPSO/α-Mg interface is lower than that on the basal LPSO/α-Mg interface. This is a result of the flat, sharp basal LPSO/α-Mg interface compared to the faceted non-basal LPSO/α-Mg interface. Regardless of whether the LPSO structure/α-Mg matrix interface is coherent or not, non-basal LPSO/α-Mg interfaces are favorable nucleation sites for DRX grains due to the higher V{sub GROD} and lower required energy E{sub s}.

36 MATERIALS SCIENCE↗

Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers

This paper investigates the microstructural characterization of the fracture propagation edge during laser beam welding of Ti6Al4V and 304 stainless steel using Cu, V, and Ni interlayers as a single Cu interlayer and composite interlayer structures with different Cu interlayer thicknesses. This study attempts to increase the Ti-SS joint strength through the use of the composite interlayers. X-ray diffraction characterization based on a 0.5-mm-thick Cu interlayer showed that the SS/Cu/Ti joint contained considerable brittle IMCs; however, the fracture surface of the SS/Cu-V/Ti composite interlayer sample did not contain any Fe-Ti IMCs or Cr{sub 2}Ti. EBSD observation indicated that the crack propagated transgranularly from solidified CuTi in the interdendritic regions of the FeTi compounds in the composite interlayer sample; however, the crack propagated intergranularly along Fe{sub 2}Ti grain boundaries in the single interlayer sample. The investigation based on a 1-mm-thick Cu interlayer showed that the SS/Ni-Cu1/Ti sample was stronger than the SS/Cu1/Ti sample due to a lack of CuTi at 3.5 kW. The tensile strength of the SS/Cu1-V/Ti joint was greater than that of the SS/Ni-Cu1/Ti joint due to the formation of ductile NiTi instead of brittle NiTi{sub 2}. The microstructures of the fracture edges after tensile testing illustrated that the eutectic CuTi + CuTi{sub 2} fractured at the SS/Cu1/Ti joint after tensile testing, while CuTi{sub 2} and eutectoid αTi + CuTi{sub 2} compounds fractured during the tensile experiment at the SS/Ni-Cu1/Ti and SS/Cu1-V/Ti joints, respectively. Investigations based on both the 0.5- and 1-mm-thick Cu interlayers showed that the tensile strength and elongation of the composite interlayer joints at a laser power of 3.5 kW were greater than those of the single interlayer joints.

36 MATERIALS SCIENCE↗

Austenitic Reversion of Cryo-rolled Ti-Stabilized Austenitic Stainless Steel: High-Resolution EBSD Investigation

In this study, AISI 321 austenitic stainless steel (ASS) was cryo-rolled and subsequently annealed at 650 and 800 °C to reverse BCC α′-martensite to FCC γ-austenite. The texture evolution associated with the reversion at the selected temperatures was investigated using high-resolution EBSD. After the reversion, TiC precipitates were observed to be more stable in 650 °C-annealed specimens than those reversed at 800 °C. {110} texture was mainly developed in specimens subjected to both annealing temperatures. However, specimens reversed at 650 °C have stronger texture than those annealed at 800 °C, even at the higher annealing time. The strong intensity of {110} texture component is attributed to the ability of AISI 321 ASS to memorize the crystallographic orientation of the deformed austenite, a phenomenon termed texture memory. The development of weaker texture in 800 °C-annealed specimens is attributed to the residual strain relief in grains, dissolution of grain boundary precipitates, and an increase in atomic migration along the grain boundaries. Based on the observed features of the reversed austenite grains and estimation from an existing model, it is suspected that the austenite reversion at 650 and 800 °C undergone diffusional and martensitic shear reversion, respectively.

36 MATERIALS SCIENCE↗

Reconstructing parent microstructures in martensitic and pearlitic Ti-Cu

Evaluating the microstructural evolution of parent phases has long been a challenge in metals with a partial or complete solid state transformation. Most parent microstructure evolution has to be inferred from the product microstructure, with some information permanently lost. Parent microstructure reconstructions relying on orientation relationships and EBSD data are a useful tool to overcome this challenge, though much background knowledge is required to do so. Here, this work introduces a reconstruction process for a eutectoid composition Ti-Cu binary alloy to evaluate the high temperature β-Ti phase from martensitic and pearlitic product microstructures. Martensitic microstructures were accurately reconstructed, enabling elucidation of β-Ti grain size and texture, and the employed script included for scientific reference. Pearlitic microstructures did not reconstruct effectively with the current process. However, new insight into the interfacial crystallographic orientations of pearlitic Ti-Cu microstructures was gleaned via this analysis, and future investigations of interest are discussed accordingly. Ultimately, these findings demonstrate tools widely implemented on conventional titanium and ferrous alloys can also be applied to understand parent microstructures in Ti-Cu and other alloys of emerging interest. This is especially of use as new manufacturing processes for such materials require understanding how parent phase microstructures respond to new, novel material processing such as AM.

36 MATERIALS SCIENCE↗

Investigation of deformation micro-mechanisms in nickel consolidated from a bimodal powder by spark plasma sintering

Bulk polycrystalline nickel compact was processed by spark plasma sintering from heterogeneous powder consisting of a mixture of nanometer and micrometer sized particles. The consolidated samples inherited the bimodal structure of the starting powder and was composed of ~ 55 vol.% coarse-grained (with the grain size larger than 1 μm) and ~ 45 vol.% ultrafine-grained (with an average grain size of ~ 550 nm) components. The deformation mechanisms were established by EBSD, X-ray line profile analysis and in-situ TEM observations. In the ultrafine-grained volume, the deformation occurred mainly through the activation of dislocation sources emitting full or partial dislocation either from grain interior or grain boundaries. Besides dislocation activity, rolling and sliding of nanograins were also observed during deformation by in-situ transmission electron microscopy, which have a considerable contribution to the observed high strain rate sensitivity of the bimodal microstructure. The cracks formed during deformation easily propagated in the nanograin regions due to the weaker particle bonding caused by the relatively high fraction of native oxide layer on the surface of the initial nanoparticles. - Highlights: • Bulk bimodal polycrystalline Ni was processed by SPS from a heterogeneous powder. • High SRS of the flow stress was observed which enhanced ductility and strength. • In-situ TEM revealed dislocation sources inside and at the boundaries of UFGs. • Twinning, partial dislocation and NG rolling were observed at crack tip vicinity. • The high SRS pertained to both dislocation activity in CG and NG rolling.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure characterization of LAE442 magnesium alloy processed by extrusion and ECAP

The magnesium alloy LAE442 was processed by extrusion and equal channel angular pressing (ECAP) to achieve ultrafine grained microstructure. Detailed characterization of the microstructure was performed by scanning electron microscope, electron back scattered diffraction (EBSD) and transmission electron microscope. The initial, as-cast, microstructure consisted of large grains of ~ 1 mm. The grain refinement due to the processing by severe plastic deformation led to a decrease of the average grain size to ~ 1.7 μm after the final step of ECAP. A detailed characterization of secondary phases showed the precipitation of Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. X-ray diffraction measurements proved that Li is dissolved within the magnesium matrix in the as-cast condition. Newly formed Al{sub 3}Li phase was observed after ECAP. The texture formation due to the extrusion and ECAP was different from that in the other magnesium alloys due to the activation of non-basal slip systems as a result of the decrease of the c/a ratio. - Highlights: • Combined extrusion and equal channel angular pressing results in significant grain refinement by factor 1000 approximately. • Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} secondary phases are present in the as-cast material while Li was dissolved in the Mg matrix. • Extrusion and ECAP have no effect on the composition of the secondary phases but they influence strongly their distribution. • Texture evolution is affected by decrease of c/a ratio due to the presence of Li and resulting activation of non-basal slip.

36 MATERIALS SCIENCE↗

Emerging hierarchical dislocation structures: Insights from scanning electron microscopy-electron backscatter diffraction in situ tensile testing and multifractal analysis

Understanding the evolution of dislocation structures during plastic deformation is critical for predicting the mechanical performance of metallic materials. In this work, we applied in situ scanning electron microscopy/electron backscatter diffraction tensile testing combined with multifractal (MF) analysis to assess deformation-induced dislocation structure evolution in solution-annealed 304 L stainless steel, both in its as-received and neutron-irradiated states (5.4 displacements per atom). The analysis of kernel average misorientation patterns revealed the formation of hierarchical dislocation arrangements that exhibit clear MF scaling behavior. Despite pronounced visual differences between nonirradiated and irradiated specimens—most notably, the appearance of dislocation channels after irradiation—the singularity spectra suggest that both conditions give rise to similar underlying hierarchical structures. MF analysis provides a quantitative measure of the spatial complexity and self-organization of dislocation patterns, highlighting the accelerated emergence and evolution of the dislocation structures in irradiated polycrystalline materials, as well as the limitation of their spatial extent. The findings indicate that irradiation not only modifies microstructure but also alters correlation-driven dislocation organization. More generally, they demonstrate that MF analysis is a powerful tool for probing mesoscale deformation mechanisms.

Dislocation structures↗

Wear characteristics of severely deformed aluminum sheets by accumulative roll bonding (ARB) process

Wear behavior of severely deformed aluminum sheets by accumulative roll bonding (ARB) process was characterized using a pin on disc wear machine at different conditions. The sheets were processed up to eight ARB cycles in order to induce a high strain ({approx} 6.4) to the samples. EBSD results showed that after eight cycles of ARB, sheets were found to contain ultrafine grains with high fraction of high angle grain boundaries. Wear experiments were conducted under different loading and operating conditions, including dry and immersion lubrication, and rotation speeds. Wear was continuously monitored by measuring the wear rates and morphologies of worn surfaces by scanning electron microscope (SEM). Contrary to expectation, the wear resistance of the ARBed Al sheets was less than the non-processed sheets. Wear rates of the ARBed Al sheets increased by increasing wear load and rotation speed, while, immersion lubrication decreased the wear rate significantly. Based on the observation and results, a model for the wear of the ARBed Al was proposed. - Research Highlights: {yields}The wear rate of the ARBed Al was higher than that of the non-processed alloy. {yields}This unexpected behavior was related to the low strain hardening capability and evolution of the ARB subsurface microstructure during the wear process. {yields}Sliding wear of the ARBed Al proceeded by surface deformation, and progressed by delamination of the deformed surface layer. {yields}The wear rate of ARBed Al increased by increasing applied load and sliding speed.

36 MATERIALS SCIENCE↗

Fractal analysis of Mo and Nb effects on grain boundary character and hot cracking behavior for Ni-Cr-Fe alloys

Highlights: • Cross section of the weld with lower RHGB fractal dimension exhibited higher DDC susceptibility than the surface section. • Mo and Nb addition induced tortuous GB character to increase fractal dimension and improve cracking resistance. • GROD maps indicated that the local strain increased within the grains close to RGBs till cracking. • At 1050 °C deformation recrystallized grains nucleated adjacent to DDC and blocked the crack propagation. - Abstract: In this paper, two filler metals of alloy 690 were evaluated on their hot cracking resistance based on the fractal analysis of random high-angle grain boundary (RHGB) morphologies. A grain reference orientation deviation (GROD) map based on EBSD technique was conducted to investigate the polycrystalline strain distribution on different RHGB network. It was found that for the 52M weld metal, specimen from the cross section with straight dendritic GBs exhibited lower fractal dimension, showing higher DDC susceptibility than the specimen from the surface section with higher fractal dimension due to equiaxed grains with tortuous GBs. With Mo and more Nb adding to the filler metal 52MSS, smaller grains nucleated and fractal dimension of the RHGB network increased, thus the cracking resistance was greatly improved. The GROD results revealed that local strain commonly concentrated around RHGB at high temperatures, especially near long and straight RHGB. The dense and tortuous RHGB network, resulting in the higher fractal dimension, could bear a more uniform strain distribution and balance the deformation between GB and grains, leading to better performance on cracking resistance. Moreover, dynamic recrystallized grains were observed beside GBs and their amount increases where there was cracking at 1050 °C, especially for the 52MSS. As a result, crack propagation path was blocked and fractal dimension increased as well.

36 MATERIALS SCIENCE↗

Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling

Highlights: • The Ti6Al4V/high Nb-TiAl metal-intermetallic (MIL) composite was fabricated. • The formation of γ and α{sub 2} phase at interface is diffusion controlled. • The formation of O phase at interface is due to the segregation of Nb atoms. • The Vickers hardness from Ti6Al4V to TiAl alloy shows a trend of a decrease then an increase and finally a decrease. - Abstract: Ti6Al4V (wt%)/Ti-44Al-8Nb-0.2W-0.2B-0.03Y (at.%) (high Nb-TiAl) metal–intermetallic laminate (MIL) composite with a defect-free interface was successfully prepared by hot-pack rolling and the interface microstructure was characterized by XRD, SEM, EBSD, and TEM techniques. The results showed that the interface was about 260 μm thick and consisted of four different microstructure regions. The thickness of each region was about 60–80 μm and the microstructure of the four regions consisted of acicular O, α{sub 2}, and β/B2 phases; acicular α{sub 2} phase; acicular α{sub 2} and β/B2 phases; and acicular γ, α{sub 2}, and β/B2 phases respectively. The resulting microstructure of the interface region was attributed to the interdiffusion of Ti atoms from the starting Ti6Al4V alloy layer to the high Nb-TiAl alloy layer and Al and Nb atoms from the high Nb-TiAl alloy layer to the Ti6Al4V alloy layer. The formation of acicular α{sub 2} and γ phases was diffusion-controlled and the Nb segregation at the interface caused the formation of O phase which had specific relationships with α{sub 2} and β/B2 phases. The detailed interface microstructural evolution of the Ti6Al4V/high Nb-TiAl MIL composite and the Vickers hardness of the composite are also discussed in this paper.

36 MATERIALS SCIENCE↗

High temperature oxidation behavior of Ni-based superalloy GH202

The isothermal oxidation kinetic and oxidation behavior of Ni-based superalloy GH202 were investigated at temperatures from 800 °C to 1100 °C. The microstructure of GH202 was characterized by scanning electron microscope (SEM) and electron back-scattered diffraction (EBSD). The composition and morphologies of oxide scales of the surface and cross-section samples were examined by X-ray diffraction (XRD), electron probe microanalysis (EPMA), and SEM combined with energy-dispersive spectroscopy (EDS). The results show that the growth of the oxide scales on GH202 obeyed a parabolic law with an activation energy of 247.8 KJ·mol{sup −1} from 800 °C to 1100 °C. The continuous and dense oxide scales that formed at 800 °C and 900 °C were composed of Cr{sub 2}O{sub 3}, NiCr{sub 2}O{sub 4} and a small amount of TiO{sub 2}. Beneath the oxide scales, aluminum-rich oxides formed along the grain boundaries due to internal oxidation. After treatment at 1000 °C for 150 h, the oxide scale was separated into two layers, the outer layer with sparse holes that was mainly composed of Cr{sub 2}O{sub 3} and TiO{sub 2} and an inner layer of dense Cr{sub 2}O{sub 3}. At 1100 °C for 100 h the outer layer was spalled, due to the looser oxide scale with large blocks of TiO{sub 2} and NiCr{sub 2}O{sub 4} which provided channels for oxygen diffusion. - Highlights: •Isothermal oxidation kinetic of GH202 obeys a parabolic law from 800 °C to 1100 °C. •The activation energy of GH202 is closed to the diffusion activation of Cr{sup 3+}. •The evolution process of oxide scales from 800 °C to 1100 °C is displayed by EPMA. •The oxidation behavior of GH202 is mainly controlled by Cr{sup 3+} and Ti{sup 4+}.

36 MATERIALS SCIENCE↗

In-situ EBSD study of deformation behavior of retained austenite in a low-carbon quenching and partitioning steel via uniaxial tensile tests

Through using in-situ electron back-scattered diffraction and uniaxial tensile tests, this work mainly focuses on the deformation behavior of retained austenite (RA) in a low-carbon quenching and partitioning (Q&P) steel. In this paper, three different types of RA can be distinguished from different locations, respectively, RA grains at the triple edges, twinned austenite and RA grains positioned between martensite. The results have shown that grains at the triple edges and twinned austenite could transform easily with increasing strain, i.e. are less stable when compared with RA grains distributed between martensite that could resist a larger plastic deformation. Meanwhile, the strain leads to rotations of RA grains distributed at the triple edges and between martensite. Moreover, RA grains with a similar orientation undergone similar rotations with the same true strain. These RA grains rotated along a specific slip plane and slip direction and the grain rotation is taken as a significant factor to improve the ductility of steel. In addition, grain sizes of RA decreased gradually with an increase of true strain and smaller (0–0.2 μm) grains were more capable of resisting the deformation. According to kernel average misorientation (KAM) analysis, it can be found that strain distribution is preferentially localized near martensite–austenite phase boundaries and in the interior of martensite. The average KAM values increased continuously with increasing true strain. - Highlights: •The in-situ and ex-situ tensile specimens differ to some extent in mechanical properties. •Retained austenite grains at the triple edges and twinned austenite transformed easily at the early stage of true strain. •Film-like retained austenite grains only rotated prior to the transformation during straining. •Retained austenite grains having with a similar orientation experienced similar rotations during the same true strain.

36 MATERIALS SCIENCE↗

Analyzing the microstructural evolution and hardening response of an Al-Si-Mg casting alloy with Cr addition

Highlights: • The formation of β-Al{sub 5}FeSi intermetallics was suppressed since impurity Fe has been consumed by Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics; • A large number of Al{sub 13}Cr{sub 4}Si{sub 4} dispersoids were observed in Al dendrites in the as-quenched and aged alloy; • The precipitation of Cr-bearing dispersoids harden the as-quenched alloy by over 10HV; • The current thermodynamic database underestimate the solubility of Fe in Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics during solidification simulation. - Abstract: Chromium is added to Al-Si based casting alloys for the mitigation of die soldering. In the present work, EBSD, EDS and TEM characterizations are combined with thermodynamic simulations to study the microstructural evolution and hardening response of an Al-Si-Mg-Cr casting alloy during heat treatments. It is shown that the Fe-containing intermetallic compounds formed in the inter-dendritic region were acicular π-Al{sub 8}(Fe, Cr)Mg{sub 3}Si{sub 6} phase and polyhedral Al-(Cr, Fe)-Si phase which is structurally similar to face-centered cubic Al{sub 13}Cr{sub 4}Si{sub 4}. The polyhedral Al-(Cr, Fe)-Si intermetallics that crystallized prior to β-Al{sub 5}FeSi consumed impurity Fe, suppressing the formation of β phase during gravity die casting process. Also, Cr-addition enables the precipitation of nano-scale Cr-bearing dispersoids in Al dendrite during solution treatment at 813 K. Hardness increment of over 10 HV can be induced by the Cr-bearing dispersoids for as-quenched alloy. Though the dispersoids have a moderate hardening effect on the as-quenched alloy, they may impair the ageing hardening response by acting as heterogeneous nucleation sites for coarse Mg-Si rods and Si particles when quenching into water at 338 K.

36 MATERIALS SCIENCE↗

Effect of filling materials on the microstructure and properties of hybrid laser welded Al-Mg-Si alloys joints

Highlights: • A serious comparison was made on the hybrid laser welded AA6061-T6 joint with different filling materials. • The microstructure of the welded joint was characterized using EBSD and SEM. • A strength model was successfully built to predict the strength of the hybrid laser welded AA6061-t6 joint. • The study shed new insights on how to select appropriate filling materials when using hybrid laser welding. - Abstract: A serious investigation was conducted to examine the influence of filling materials on the microstructure and properties of hybrid laser welded AA6061-T6 joints. The results of the tensile tests showed that the welded joint with ER4043 filling materials had higher tensile strength than that with ER5356 filling material. Based on the results obtained a strength model was built to predict and explain the enhancement of the yield strength of the hybrid laser welded AA6061-T6 joint with different welding wires. In contrast to the tensile strength, the ER4043 joint showed lower fatigue strength than that of the ER5356 joint due to extensive presence of micropores in fusion zone. Further, the corrosion experiment illustrated that the ER4043 joint had poorer resistance to the corrosive attack under 3.5% NaCl solution. A summary was made on the performance of both welded joints to shed new insights on selecting appropriate filling materials when welding AA6061-T6 by hybrid laser welding method.

36 MATERIALS SCIENCE↗

Effect of microstructures on hot compression behavior of a Ti-43Al-2Si alloy fabricated by cold crucible continuous casting

Highlights: • TiAl alloys with different lamellar colonies were fabricated by cold crucible continuous casting. • EBSD was used to investigate the evolution of lamellae during the hot compression. • Lamellar colony boundaries promote the dynamic recrystallization process. - Abstract: To investigate the influence of lamellar orientation and colony boundary on deformation behavior, fully lamellar Ti-43Al-2Si alloys were prepared by cold crucible continuous casting and isothermal compression tests were conducted at different temperatures in the range 1373–1523 K with a strain rate of 0.01 s{sup −1}. The as-cast microstructures were elongated colony with lamellae oriented at nearly 45° to the compression direction and equiaxed colony with various lamellae orientations, respectively. The results revealed that serious cracking or sliding traces appeared on the surface of deformed specimens with elongated colony original microstructure and that their peak stresses were lower compared to those of specimens with equiaxed colony original microstructure. The relationship between deformation behaviors and as-cast microstructure was analyzed in detail. It was found that the recrystallization/globularization level is significantly lower than that in specimens with equiaxed colony original microstructure during hot deformation owing to the preferred nucleation sites in colony boundaries. Finally, the lamellae conversion process was characterized to reveal the softening mechanisms of full lamellar TiAl-based alloy during hot compression.

36 MATERIALS SCIENCE↗

Formation of intermetallic structures at the interface of steel-to-aluminium explosive welds

Highlights: • The interface of Fe-Al explosive welds was characterised by SEM/EDS and EBSD. • The intermetallics formed at the weld interface are rich in Al (Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}). • The presence of intermetallic phases on the interface deeply affects the weldability. • Al-rich intermetallics increase the solidification time of the weld interface. - Abstract: The formation of intermetallic structures at the interface of carbon steel to 6082 aluminium alloy explosive welds and their influence on the weldability of these two materials were studied. The morphology, the microstructure, the chemical and phase compositions of the welds were characterised by several types of microscopy techniques. The interface characterisation proved that explosive mixtures with a lower detonation velocity were revealed as being more suitable for achieving consistent welds since jet entrapment was prevented and continuous molten layers were not formed at the weld interface. It was also found that the physical properties of the intermetallic phases generated at the weld interface have a strong influence on the weldability of steel-to-aluminium explosive welds. Specifically, it was shown that the formation of aluminium-rich intermetallic phases at the weld interface increases the solidification time of the interfacial molten material, decreasing the weldability of these two materials. The formation of these intermetallic compounds should be avoided by reducing the interaction between the flyer and the baseplate as well as by avoiding excessive molten layers.

36 MATERIALS SCIENCE↗