Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Corrosion Testing of Carbon Steel in Oxalic Acid that Contains Dissolved Iron

Radioactive liquid waste has been stored in underground carbon steel tanks for nearly 60 years at the Savannah River Site. The site is currently in the process of removing the waste from these tanks in order to place it into vitrified, stable state for longer term storage. The last stage in the removal sequence is a chemical cleaning step that breaks up and dissolves metal oxide solids that cannot be easily pumped out of the tank. Oxalic acid (OA) will be used to chemically clean the tanks after waste retrieval is completed. The waste tanks at SRS were constructed from carbon steel materials and thus are vulnerable to corrosion in acidic media. In addition to structural impacts, the impact of corrosion on the hydrogen generated during the process must be assessed. Electrochemical and coupon immersion tests were used to investigate the corrosion mechanism at anticipated process conditions. The testing showed that the corrosion rates were dependent upon the reduction of the iron species that had dissolved in solution. Initial corrosion rates were elevated due to the reduction of the ferric species to ferrous species. At later times, as the ferric species depleted, the corrosion rate decreased. On the other hand, the hydrogen evolution reaction became more dominant.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Oxy-Combustion Environmental Characterization: Fire- and Steam-Side Corrosion in Advanced Combustion

Steamside Oxidation: A first high pressure test was completed, 293 hr at 267 bar and 670°C; A parallel 1 bar test was done for comparison; Mass gains were higher for all alloys at 267 bar than at 1 bar. A comparison was made with longer-term literature data: Ferritic steels--no consistent pressure effect; Austenitic steels--fine grain alloys less able to maintain protective chromia scale as pressure increases; Ni-base alloys--more mass gains above 105 bar than below. Not based on many data points. Fireside Corrosion: 1. Conditions for most severe corrosion: Temperature: 700{degrees}C Deposit: Standard Corrosion Mix Duration: 160 hours Gas Atmosphere: O{sub 2} + 1000ppm SO{sub 2} Pt-catalyst placed in the hot zone next to the specimens 2. Possible SO{sub 2} threshold in gas atmosphere for corrosion; 3. Corrosion greater in steel alloys than Ni-based alloys; 4. Corrosion mechanism proposed for steel alloys and Ni-based alloys.

36 MATERIALS SCIENCE↗

CORROSION ISSUES ASSOCIATED WITH AUSTENITIC STAINLESS STEEL COMPONENTS USED IN NUCLEAR MATERIALS EXTRACTION AND SEPARATION PROCESSES

This paper illustrated the magnitude of the systems, structures and components used at the Savannah River Site for nuclear materials extraction and separation processes. Corrosion issues, including stress corrosion cracking, pitting, crevice corrosion and other corrosion induced degradation processes are discussed and corrosion mitigation strategies such as a chloride exclusion program and corrosion release testing are also discussed.

36 MATERIALS SCIENCE↗

Computer Modeling of Transport of Oxidizing Species in Grain Boundaries during Zirconium Corrosion

Zirconium (Zr) based alloys are widely used as the cladding materials in light-water reactors. The water-side corrosion of these alloys degrades their structural integrity and poses serious safety concerns. During the Zr corrosion process, a thin Zr oxide (ZrO2) layer forms on the alloy surface and serves as a barrier layer for further corrosion. The majority of the oxide has the monoclinic phase. At the transition region between the oxide and the metal, the oxide contains a thin layer of stabilized tetragonal phase. It is found that the texture of the tetragonal layer determines the protectiveness of the oxide for corrosion. The transport of oxidizing species, such as anion defects, cation defects, and electron through the tetragonal oxide layer could be the rate limiting step of the corrosion. The defect diffusion can be affected by the growing stresses and microstructures such as grain boundaries and dislocations. In this work molecular dynamics simulations are used to investigate the anion and cation diffusion in bulk and at grain boundaries in tetragonal ZrO2. The results show that defect diffusion at grain boundaries is complex and the behavior strongly depends on the grain boundary type. For most of the grain boundaries studied the defect diffusion are much slower than in the bulk, implying that grain boundaries may not be fast defect transport paths during corrosion. The connection between the modeling results and published experimental work will also be discussed. This work is funded by the Laboratory Directed Research and Development (LDRD) program at Idaho National Laboratory.

36 MATERIALS SCIENCE↗

Fuel Matrix Degradation Model Development Update: Alloy Corrosion Rates and Hydrogen Generation

This work is being performed as part of the DOE NE Spent Fuel and Waste Science and Technology Campaign, Argillite and Crystalline Rock R&D work packages: SF-19AN01030101 and SF-19AN01030201. This document meets the milestone M4SF-19AN010301013 for Argillite R&D and the milestone M4SF-19AN010302013 for Crystalline R&D. The fuel matrix degradation (FMD) model calculates the degradation rate of spent UO2 fuel based on fundamental electrochemical theory and thermodynamics. The model provides the quantitative basis for radionuclide source term predictions in the generic disposal system analysis (GDSA) performance assessment (PA) model. The FMD model has been implemented in a manner that facilitates its integration with the GDSA-PA code and a preliminary, integrated FMD-GDSA model has been successfully tested (Jerden et al., 2017). The specific focus of on-going work is to accurately and quantitatively represent the generation of H2 in a breached waste package and its effect on the spent fuel degradation rate so that this key process can be accurately represented in PA models. It has been shown experimentally that millimolar concentrations of dissolved H2 in contact with spent fuel will inhibit oxidative dissolution and decrease the fuel degradation rates by as much as three orders of magnitude (e.g., Röllin et al., 2001, Ollila, 2008). This will lead to a significant decrease in the radionuclide source term values used in repository PA models. Sensitivity studies using the FMD model have shown that the dissolved H2 concentration is the dominant environmental variable affecting the UO2 spent fuel dissolution rate as long as a source of H2 persists in the breached waste package (Jerden et al., 2015). Therefore, on-going experimental and modeling efforts focus on H2 production, accumulation and interfacial reactions within a breached waste package. The anoxic corrosion of metallic engineering materials within a breached waste package will be the main source of H2 in crystalline and argillite rock repository systems. The most important H2-producing alloys present within a waste package include stainless steel, carbon steel, and aluminum alloys and the Zircaloy fuel cladding. A steel corrosion module was added to the FMD model to account for these H2 sources and couple the H2 generation rate with fuel degradation processes (Jerden et al., 2017). As discussed below, there is a need for experimental data from electrochemical corrosion tests to quantify the H2 generation rates due to the corrosion of these waste package alloys as a function of key environmental variables (Eh, pH, groundwater chemistry). This report presents results from series of electrochemical corrosion tests with materials present in waste packages that provide information needed to parameterize and validate the FMD model. The alloys tested include 316L stainless steel (316SS), AISI 4320 carbon steel (C-steel) and Zircaloy-4 fuel cladding (unirradiated). Potentiodynamic polarization and potentiostatic polarization tests were performed in buffer solutions at pH 4, 7 and 10 with NaCl concentrations of 0, 4 and 100 millimolar (mM). The potentiostatic tests were performed at voltages varying from 0.5 volts down to -0.66 volts, vs the standard hydrogen electrode (SHE), and all tests were performed at laboratory ambient temperatures (~22 °C). The corrosion rates measured during the electrochemical tests were used as direct input to a new FMD/in-package chemistry model that is being developed to provide accurate long-term spent fuel degradation rates as chemical conditions (Eh, pH, speciation) evolve within a breached waste package. This new model was developed by coupling the FMD model with the reactive transport code X1t, which is a module within the Geochemist’s Workbench (GWB) reaction path modeling code (Jerden et al., 2019). The reactive transport model consists of a 1D domain discretized with 21 reaction diffusion cells and includes a single waste packag

Jerden, James↗

Corrosion evaluation of metal foams in eutectic molten salts for high temperature latent heat energy storage application

High-temperature Thermal Energy Storage (TES) has drawn great attention as a technology that can increase the role and profitability of micro nuclear reactors in the decentralized clean energy market. Various research needs have been proposed by Idaho National Laboratory (INL) in "the Integrated Energy Systems: 2020 Roadmap" with the goal of utilizing the high temperature of 550 degrees or more generated in the 4th generation reactor to industrial purposes from the standpoint of integrated energy systems [1]. With the recent development of the 4th generation nuclear power plant, including micro nuclear reactor, there is a great deal of interest in researching how to efficiently couple a heat source to an industrial process through thermal processing. Texas A&M University (TAMU) and INL are currently collaborating to develop a novel latent heat storage design called HITB (Heat pipe-Integrated Thermal Battery). As part of the small-scale experimental demonstration research for HITB, a study for storage medium selection was conducted at TAMU. Eutectic salts have attracted interest as high-temperature heat storage medium for HITB. Especially, chloride molten salts and fluoride molten salts are considered promising candidates due to their high melting temperature, thermal stability, and high latent heat of fusion. Since eutectic salts have poor thermal conductivity in general, it is critical to distribute materials with high thermal conductivity evenly to facilitate the charging and discharging of heat. In this study, metal foam was considered in the HITB system to overcome the poor heat transfer characteristics of eutectic salts. In order to improve heat transfer, it is necessary to study materials with high thermal conductivity, corrosion resistant to molten salts, such as fins, extended surfaces, particles, microcapsulation, or foam structure. Porous structure of copper or aluminum can increase heat transfer area, form a thermal transfer network, and increase the effective thermal conductivity of thermal storage medium [2]. Since the melting temperature is required to be at least 450? in the current HITB design, various eutectic salts are being considered. FLiNaK and FLiBe, which are famous for fluoride salts, are good candidates, but due to the sharp rise in the price of LiF recently, they are excluded for economic reasons to be applied to large-capacity thermal energy storage. On the other hand, chloride salts are very cheap and easy to obtain, have a high melting temperature, and have a high latent heat of fusion, so they are recently in the spotlight as a phase change material. However, because of the hygroscopic nature of chloride salts, HCl gas due to impurity is easy to be released and is particularly vulnerable to corrosion. Chloride eutectic salts have been tested and suggested for metal alloys that are particularly resistant to corrosion, such as SS304, SS316, Hastelloy, Inconel 625, Incoloy 800H, which has low thermal conductivity, and is very expensive [3-6]. Porous materials with high thermal conductivity such as copper and aluminum have been tested for stability in fluids such as paraffin or water as metal foam or metal fin structures, but high temperature corrosion tests were not performed on various eutectic salts yet. Therefore, this study investigated the high temperature corrosion characteristics of metal alloys, such as C10100 foam, C10100 plate, 6101 alloy foam, and SS316 plate, while immersed in the candidate eutectic salts. A total of 20 tests for SS316 coupons and 10 tests for C10100 coupons were performed to ensure the repeatability of the present measurements. Since it is difficult to completely remove the salt inside metal foam due to the complex inner structure of the metal foam, only the surface condition was observed with a microscopy and scanning electron microscopy (SEM) image, except for measuring the corrosion rate and average mass loss.

25 ENERGY STORAGE↗

Effect of Minor Ce Additions on Corrosion Behavior of Experimental Pipeline Steel

Minor additions of rare earth elements (REEs) have been shown to improve various steel properties. In particular, Cerium (Ce), as a relatively abundant and inexpensive element, has received attention as a potentially beneficial minor alloying addition for a variety of steel applications, including pipelines materials. The objective of this work is to investigate the effect of Ce on corrosion performance of experimental high-strength pipeline steel. Electrochemical corrosion experiments were carried out on steel without and with 0.006, 0.018, and 0.03 wt.% of Ce in 3.5 wt.% NaCl saturated with CO2 at 20 oC. For comparison purposes, X100 carbon steel specimens machined from an experimental pipe with a yield strength of 731 MPa were tested under the same conditions. The electrochemical techniques employed included: potentiodynamic polarization (PDP), linear polarization resistance (LPR), and electrochemical impedance spectroscopy (EIS). In addition, post-corrosion surface characterization was performed using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS), while crystalline phases were determined by X-ray diffraction (XRD). The corrosion of base metal without Ce was lower (0.15 mm/y) compared to carbon steel X100 (0.9 mm/yr). The electrochemical results showed that adding Ce accelerates corrosion rates compared to base metal without Ce. No pitting corrosion of tested steel was detected.

Belarbi, Zineb↗

Effectiveness of Vapor Corrosion Inhibitors Under Elevated Chloride Conditions for Aboveground Storage Tank Application

The sand quality used to construct the tank pad is an important contributing factor to the rate of corrosion that occurs on the soil-side of the aboveground storage tanks (ASTs) floor plates. Clean sand that meets specific criteria provides the first line of defense for mitigation of tank floor corrosion. However, it has been observed that the sand quality used for some existing tanks differ greatly from the specifications provided in the API 651 standard; this could be partially due to initial sand quality not meeting the specification, and partially due to the environmental effects over time. For example, rain-water intrusion could lead to higher than the specified contents of corrosive species such as chloride. Tank operators are increasingly using vapor corrosion inhibitors (VCIs) either as a stand alone or in combination with cathodic protection (CP) for ASTs to mitigate soil-side corrosion. VCIs are delivered either through-thefloor or injected through the ports in the ring wall. Experimental studies were conducted to evaluate VCIs’ performance at elevated chloride concentrations and to study the effectiveness of the delivery methods under extreme chloride conditions. The experimental work found that VCI performance is robust and not compromised due to high chloride levels, such as 300 ppm or more. The work also showed that the through-the-floor VCI delivery method is more beneficial compared to the through-the-sand-pad method when tank pad corrosivity is elevated.

Shukla, Pavan K.↗

Effectiveness of Vapor Corrosion Inhibitors Under Bacterial Activity for Aboveground Storage Tank Application

Bacterial activity is known to influence corrosion and can result in increasing soil-side corrosion of the aboveground storage tanks (ASTs) floor plates. Association for Materials Protection and Performance (AMPP) defines this phenomenon as Microbiologically Influenced Corrosion (MIC). It has been hypothesized that vapor corrosion inhibitors (VCIs) can not only function in presence of bacterial activity but can also function as biocides. Experiments were conducted to study the effect of bacterial activity on corrosion in the sand pad conditions and effect of VCIs in mitigating MIC. Various bacteria cultures were grown using commercially available culture media, and coupon exposure tests were performed with field sand mixed with the culture media. To this end, control and VCI-dosed electrolytes were prepared using the field sand plus bacteria cultures. Pre- and post-test bacteria concentration estimation and measurements, respectively, in the VCI-dosed electrolytes indicated that VCIs do not function as biocides, however, VCIs are highly effective for mitigating corrosion in presence of bacterial activity.

Shukla, Pavan K.↗

Fabrication of Superhydrophobic Calcium Phosphate Coating on Mg-Zn-Ca alloy and Its Corrosion Resistance

A novel superhydrophobic calcium phosphate coating was prepared on a magnesium alloy substrate by a highly effective chemical conversion process and subsequent chemical modification. Different methods were employed to characterize the surface morphology and chemical composition as well as measure the wettability of the coating. It was demonstrated that the as-prepared superhydrophobic calcium phosphate coating has a typical three-level hierarchical structure consisted of micro-protrusions, submicro-lumps and nano-grains, conferring excellent superhydrophobicity with a water contact angle of 159°. The electrochemical measurements and appropriate equivalent circuit revealed that the corrosion-resistant performance of the superhydrophobic calcium phosphate coating was significantly improved as compared with that of the substrate, the corrosion potential of the superhydrophobic coating increases from −1.56 to −1.36 V, and its corrosion current density decreases from 1.29 × 10{sup −4} to 1.3 × 10{sup −6} A/cm{sup 2}. The anti-corrosion mechanism of the superhydrophobic coating was also discussed. It can be indicated that the corrosion inhibitive properties of the coating are in accordance with its hydrophobicity, which is owing to the presence of a protective layer of air trapped in the grooves of the coating surface to isolate the underlying materials from the external environment.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Aqua-Blasted and Laser-Engraved Type 316L Stainless Steel

The effect of aqua blasting and laser engraving on surface microstructure development, residual stress and corrosion resistance of type 316L stainless steel has been investigated. Aqua blasting resulted in a deformed near-surface microstructure containing compressive residual stresses. Subsequent laser engraving produced a surface layer with tensile residual stresses reaching to a depth of 200 microns. Changes of surface roughness topography were accompanied by the development of a thick oxide/hydroxide film after laser engraving. The atmospheric corrosion behavior of all surfaces with MgCl{sub 2}-laden droplets was compared to their electrochemical response in 1M NaCl and 0.7 M HCl aqueous solutions. The measured total volume loss after atmospheric corrosion testing was similar for all investigated surface conditions. Laser-engraved surface exhibited the smallest number of corrosion sites, but the largest mean corrosion depth.

36 MATERIALS SCIENCE↗

Effect of Sm-Rich Phase on Corrosion Behavior of Hot-Extruded AZ31-1.5Sm Magnesium Alloy

The effects of Sm on the corrosion and microstructure behavior of hot-extruded AZ31 magnesium alloy were investigated by SEM, TEM, weight loss analysis, and electrochemical measurements. The results indicated that granular Al{sub 2}Sm phase ~ 4 μm in size in the hot-extruded AZ31 magnesium alloy modified with 1.5 wt.% Sm leads to significant grain refinement. The corrosion rate decreased from 15.98 × 10{sup −4} to 11.19 × 10{sup −4} g cm{sup −2} h{sup −1} in the transverse section and from 8.57 × 10{sup −4} to 6.20 × 10{sup −4} g cm{sup −2} h{sup −1} in the longitudinal section. Compared to the unmodified alloy, the corrosion potential of the Sm-modified alloy in the transverse and longitudinal sections increased by 98 and 62 mV, respectively, and the R{sub ct} value (charge transfer resistance) in the transverse and longitudinal sections of the modified alloy increased from 1764 and 1756 to 2928 and 2408 Ω cm{sup 2}, respectively. The results showed that the corrosion resistance of hot-extruded AZ31 magnesium alloy was significantly improved by Sm addition due to the grain refinement, the decreased dislocation density, and the suppression of micro-galvanic corrosion caused by Al-Sm-(Mn) intermetallic compounds.

36 MATERIALS SCIENCE↗

The Corrosion Behavior of Zn/Graphene Oxide Composite Coatings Fabricated by Direct Current Electrodeposition

The zinc (Zn) and Zn/graphene oxide (Zn/GO) composite coatings on the mild steel were fabricated by direct current electrodeposition from an acidic chloride bath without GO and that with four different concentrations (50, 100, 200 and 300 mg/L) of GO, respectively. The GO first is synthesized by using the typical Hummer method. Physical characterizations including the surface and cross-sectional morphology, chemical composition and crystal structure of the Zn and Zn/GO composite coatings were done by scanning electron microscope, energy-dispersive x-ray and x-ray diffraction. The crystalline size, texture coefficient, water contact angle and hardness of the Zn and Zn/GO composite coatings were measured. The corrosion behavior of the Zn and Zn/GO composite coatings was studied by the electrochemical corrosion tests including the potentiodynamic polarization test and the electrochemical impedance spectroscopy test and the immersion test. The result reveals that the corrosion resistance of the Zn coating is remarkably increased by the incorporation of GO. Furthermore, it does not show a linear increase with the increase in the amount of incorporated GO and an optimal corrosion resistance is provided by the Zn/GO composite coating attained from the electrolyte containing 100 mg/L GO. The influence of the incorporation of GO on the corrosion resistance of the Zn coating is explained in combination with their physical characterizations.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Role of Centrifugal Casting on Electrochemical Corrosion Behavior of A356-SiCp Composite in 3.5 wt.% NaCl

Role of graded microstructure in a centrifugally cast A356-SiC particle (SiCp) composite alloy disk on passivity and localized corrosion behavior in 3.5 wt.% NaCl environment has been investigated. The area fraction of SiCp has been found to decrease from the outer periphery to the core of the disk, while the apparent size and area fraction of the intermetallics and Mg-rich phase increase from the periphery to the core. As a consequence, the corrosion resistance of the as-cast disk varies with the distance from the periphery in the order 45 < 65 < 25 < 5 mm. The corrosion resistance of the centrifugally cast disk can be significantly improved through solution annealing at 540 °C for 2 h and solution annealing + aging at 175 °C for 2 h. However, between the two, the former has shown a better corrosion resistance and passivity than the latter. In the latter case, the aging treatment resulted in the precipitation of Mg{sub 2}Si phase which is prone to the corrosion attack.

36 MATERIALS SCIENCE↗

Effect of Laser Shock Peening on Residual Stress, Microstructure and Hot Corrosion Behavior of Damage-Tolerant TC21 Titanium Alloy

The effect of laser shock peening (LSP) on the residual stress, microstructure and hot corrosion behavior of damage-tolerant TC21 alloy was investigated. The equilateral scanning pattern was adopted to obtain a large overlapping area for LSP. The hot corrosion experiments in a salt mixture composed of 75 wt.% Na{sub 2}SO{sub 4} + 25 wt.% NaCl at 700 and 800 °C for a total exposure of 25 h were conducted. The results demonstrated that LSP caused a high compressive residual stress with a significant increase in micro-hardness and microstructural changes in the form of crystal defects, i.e., high density dislocations. The crystal defects promoted the outward diffusion of Al, Cr and Ti to form protective mixed oxides (Al, Cr, Ti)O{sub 2}. These oxides improved the adhesion of outer oxide layer and hindered the inward diffusion of O, S and Cl, which was beneficial to improve hot corrosion resistance. The mass gains of LSP-treated specimens after hot corrosion at 700 and 800 °C were, respectively, 3.72 and 4.78 mg/cm{sup 2}, which were much lower than those of untreated specimens (5.65 and 6.81 mg/cm{sup 2}). Therefore, LSP leads to an improvement in resistance to hot corrosion of TC21 alloy.

36 MATERIALS SCIENCE↗

Electrochemical Corrosion Behavior of Plasma-Sprayed FeCrNiMoCBSi Amorphous/Nanocrystalline Coatings in Simulated Seawater Medium

A novel FeCrNiMoCBSi coating was fabricated on F22 marine steel by plasma spraying. The coating microstructure and composition were characterized by scanning electron microscope, transmission electron microscope, x-ray diffraction, differential scanning calorimetry, and x-ray photoelectron spectroscopy. The results showed that the coating consisted of amorphous and nanocrystalline phases. Additionally, the corrosion resistance in simulated seawater was evaluated by electrochemical corrosion methods. It was found that the coating exhibited an excellent resistance to pitting corrosion. For long-time immersion tests, the corrosion resistance was gradually decreased with the increasing through-porosity due to the permeation of the corrosive solution into the coating. The coating lost its efficacy through three stages, namely the protection stage, the permeation stage, and the failure stage.

36 MATERIALS SCIENCE↗

Modeling of concrete cracking due to corrosion process of reinforcement bars

The reinforcement corrosion in Reinforced Concrete (RC) is a major reason of degradation for structures and infrastructures throughout the world leading to their premature deterioration before design life was attained. The effects of corrosion of reinforcement are: (i) the reduction of the cross section of the bars, and (ii) the development of corrosion products leading to the appearance of cracks in the concrete cover and subsequent cover spalling. Due to their intrinsic complex nature, these issues require an interdisciplinary approach involving both material science and structural design knowledge also in terms on International and National codes that implemented the concept of durability and service life of structures. In this paper preliminary FEM analyses were performed in order to simulate pitting corrosion or general corrosion aimed to demonstrate the possibility to extend the results obtained for a cylindrical specimen, reinforced by a single bar, to more complex RC members in terms of geometry and reinforcement. Furthermore, a mechanical analytical model to evaluate the stresses in the concrete surrounding the reinforcement bars is proposed. In addition, a sophisticated model is presented to evaluate the non-linear development of stresses inside concrete and crack propagation when reinforcement bars start to corrode. The relationships between the cracking development (mechanical) and the reduction of the steel section (electrochemical) are provided. Finally, numerical findings reported in this paper were compared to experimental results available in the literature and satisfactory agreement was found.

36 MATERIALS SCIENCE↗

Polishing-assisted galvanic corrosion in the dissimilar friction stir welded joint of AZ31 magnesium alloy to 2024 aluminum alloy

Galvanic corrosion of a dissimilar friction stir welded 2024-T3 Al/AZ31B-H24 Mg joint prepared using a water-based and a non-water-based polishing solution was characterized. Microstructure and the distribution of chemical elements were analyzed using optical microscopy, scanning electron microscopy and energy dispersive X-ray spectroscopy. The stir zone polished using water-based solution was observed to be much more susceptible to galvanic corrosion attack than that obtained using non-water-based polishing solution. The location of corrosion attack was observed in the narrow regions of AZ31 Mg alloy adjacent to Al2024 regions in the stir zone. The occurrence of galvanic corrosion was due to the formation of Mg/Al galvanic couples with a small ratio of anode-to-cathode surface area. The corrosion product was primarily the porous magnesium hydroxide with characteristic microcracks and exhibited a low microhardness value.

36 MATERIALS SCIENCE↗