Search NASA⌕ Search

SEARCH · Search NASA

Results for “Phase contrast microscopy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Comparative Dissolution of Iron-Bearing Minerals by Catecholate and Hydroxamate Siderophores under Oxic and Anoxic Conditions

Siderophores play a crucial role in biological iron (Fe) acquisition and mobilization by promoting Fe mineral and rock weathering. While the effects of the hydroxamate siderophore desferrioxamine B (DFOB) have been extensively studied, the role of catecholates in the dissolution of Fe mineral and rock under varying redox conditions remain limited. Moreover, despite Fe being one of the most redox-active metals, the siderophore-mediated redox transformations of solid-phase Fe and their impact on mineral dissolution are not well understood. Herein, this study systematically investigated dissolution behavior of both Fe(II) and Fe(III)-bearing minerals and rocks (Fe(II)- bearing basalt and olivine, and Fe(III)- bearing nontronite and goethite), by two structurally distinct biological siderophores, catecholate protochelin and hydroxamate DFOB, under both oxic and anoxic conditions. Batch experiments quantified Fe and transition metals (Mn, Ni, Zn, Mo) released from the tested minerals in the presence of siderophores. Throughout the dissolution experiments, siderophore concentrations and Fe-siderophore complexation in solutions were measured using UV-vis spectrometry. Fe redox changes under oxic and anoxic conditions by siderophores were determined, and mineral surface alterations following siderophore treatments were characterized through scanning electron microscopy (SEM) and time-of-flight secondary ion mass spectroscopy (ToF-SIMS). Results revealed distinct interplays of dissolution mechanisms, including ligand-exchange promoted dissolution and reductive dissolution, along with Fe(III) reduction and Fe(II) oxidation, contributing to the Fe(II)- and Fe(III)-rich mineral weathering under varying redox conditions. Under oxic conditions, both protochelin and DFOB enhanced Fe release from Fe(II)-rich basalt and olivine more effectively than from Fe(III)-rich minerals. DFOB induced greater Fe(II)-mineral dissolution than protochelin. This difference was attributed to a higher level of Fe(II) oxidation by DFOB in contrast to protochelin, as well as the protochelin oxidation with the loss of Fe binding groups (catechols). Under anoxic conditions, both siderophores significantly reduced Fe(III) in nontronite and goethite, with protochelin demonstrating substantially stronger Fe(III) reduction capacity than DFOB. However, Fe(III) reduction negatively impacted Fe release from Fe(III)-rich minerals. Instead, Fe release from Fe(II)-rich minerals was enhanced under anoxic conditions due to the absence of Fe(II) oxidation and labile Fe(II). Variations in siderophore adsorption also contributed to dissolution differences. Beyond iron, the release of transition metals from tested minerals was influenced by elemental contents, mineral compositions, and siderophore types, revealing distinct metal- and siderophore-dependent patterns. This systematic investigation highlights the roles of siderophores in Fe redox cycling and metal mobilization, enhancing our understanding of different siderophore behaviors in siderophore-mediated microbial metal acquisition within redox-dynamic environments, with implications for bioleaching industries and applications in agriculture and climate change mitigation.

Guo, Dongyi↗

Nanoscale morphology of Ni{sub 50}Ti{sub 45}Cu{sub 5} nanoglass

Nanoglasses are noncrystalline solids with a granular nano-/microstructure. In contrast to their nanocrystalline analogs, typically constituted of grains and grain boundaries, nanoglasses consist of glassy regions with a structure corresponding to melt-quenched glasses and amorphous interfaces characterized by a reduced density. Their unique properties can be controlled by modifying size and chemical composition of the granular and interfacial regions. Ni{sub 50}Ti{sub 45}Cu{sub 5} amorphous films were obtained by magnetron sputtering and analyzed to determine their nanoscale morphology and the formation mechanisms. The nanoglasses were noted to have a hierarchical nano-columnar structure with the smallest Ni-rich (Ni:Ti ratio of ca. 5:3) amorphous columns with diameters of about 8 nm and Ti-rich glassy interfacial regions with a substantially lower density. The results were obtained utilizing X-ray diffraction and different microscopic methods, e.g., atomic force microscopy and transmission electron microscopy. A detailed analysis indicates the complexity of the formation mechanisms of topologically and chemically distinguishable structural units with curvature driven surface diffusion, surface mobility, self-shadowing and internal stresses as the most important parameters. Common and simple synthesis method and the possibility for easy modification of the morphology and, consequently, the physical properties offer an opportunity for intensive studies of this new class of materials, opening the way towards possible applications. - Highlights: • Ni{sub 50}Ti{sub 45}Cu{sub 5} thin film nanoglasses were synthesized by magnetron sputtering. • Ti amorphous interfacial phase with reduced density is observed. • Stabilization of interfaces by specific local thermodynamic conditions.

36 MATERIALS SCIENCE↗

Second Annual Progress Report on Correlation Between Microstructure and Mechanical Properties of Neutron-Irradiated Ferritic-Martensitic and Austenitic Steels

Ferritic-martensitic steels G92-2b (an optimized Grade 92 heat), NF616 and T91, and austenitic stainless steel 800H and its Grain Boundary Engineering (GBE)-treated version 800H-TMP (ThermoMechanical Processing) were irradiated in the High Flux Isotope Reactor (HFIR) of Oak Ridge National Laboratory (ORNL) and the Advanced Test Reactor (ATR) of Idaho National Laboratory (INL). Selected G92-2b samples were irradiated up to 14.66 dpa in the HFIR at two temperature ranges: 400–496.7°C and 683.3– 720°C. NF616 and T91 were irradiated in the ATR up to 8.16 dpa with the irradiation temperatures ranged from 241°C to 447.5°C. Alloy 800H and 800H-TMP samples were irradiated in both the HFIR and the ATR. Selected 800H and 800H-TMP samples had HFIR irradiation to 1.28 dpa at 580°C and ATR irradiation up to 9.12 dpa at 359°C to 431°C. Vickers hardness measurements, fractography, and microstructural characterization were performed on the selected samples in the Low Activation Materials Design and Analysis (LAMDA) laboratory. Radiation-hardening of G92-2b was observed at the lower doses and lower irradiation temperatures (400- 496.7°C), with GB03 (0.52 dpa at 400°C) and GB04 (7.44 dpa at ~490°C) showing ~12% and ~8% hardening, respectively. Softening by ~14% was observed for GB05 (14.66 dpa at 496.7°C). Radiationsoftening of G92-2b was more prevalent at the higher irradiation temperatures (683.3-~720°C), with GB10 (0.46 dpa at 683.3°C), GB11 (7.44 dpa at ~720°C), and GB12 (14.63 dpa at ~720°C) showing ~8%, ~8%, and ~40% softening, respectively. Radiation-hardening of NF616 and T91 was observed with the hardness increased by ~37% to ~65% depending on the irradiation doses and irradiation temperatures. Within the studied irradiation conditions of NF616 and T91, samples with a higher dose had a larger hardness after irradiation. All the tested alloy 800H and 800H-TMP samples in this work showed radiation-hardening by ~96±7% to ~152±10%. Alloy 800H-TMP tended to have slightly smaller radiation-hardening than alloy 800H. The fractography results of G92-2b sample GB03, GB10, and GB11, together with the previously characterized fractography of GB04, GB05, and GB12, indicated that the ductility of G92-2b was maintained up to 14.66 dpa at the lower irradiation temperatures of 400-496.7°C, while some loss of ductility (less necking) was observed for higher doses at the higher irradiation temperatures of 683.3-720°C. This agrees with the previously reported tensile test results of G92-2b, where the elongation of G92-2b was reduced at higher doses at the higher irradiation temperatures. Dimple sizes increased at higher doses, which are more evident at the higher irradiation temperatures of 683.3-~720°C. The fractography of NF616 sample D2 (2.96 dpa at 291.5°C), D4 (5.91 dpa at 359°C), and D6 (8.16 dpa at 431°C) indicated loss of ductility with negligible necking for sample D2, while ductile failure for samples D4 and D6. Fractography of alloy 800H and 800H-TMP samples in various irradiation conditions showed ductile failure with obvious necking. Dimples were observed, with some of them containing large Ti-rich particles, in all the 800H/800H-TMP samples. Electron backscatter diffraction characterization of GB12 indicated the recovery of the lath structure, which was generally replaced by an equiaxed grain structure. Transmission electron microscopy (TEM) characterization showed the presence of frequent M 23 C 6 (M = primarily Cr), MX (M = primarily V), spherical Nb(C,N) precipitates, and occasional Laves phase precipitates in the G92-2b samples. MX precipitates with sizes of 20-30 nm were observed at boundaries of smaller grains, indicating the pinning effect of the V-rich precipitates. The lath structure recovery was more evident at the higher irradiation temperatures (683.3-~720°C), with decreased densities of line dislocations and M23C6 precipitates. The irradiated T91 (TA04) showed the growth of M23C6 precipitates to 101 ± 40 nm from the initial 68 ± 22 nm in the unirradiated condition. Dislocation loops of both {100} and {111} types were present in TA04. TEM characterization was also performed on the irradiated 800H (N4, N5, N6, and AR2) and 800H-TMP (P4, P5, P6, and HG1). Accumulation of M 23 C 6 precipitates at grain boundaries was observed in all the xii 800H/800H-TMP samples, and the presence of Ti(C,N) precipitates at grain boundaries and in the matrix was observed in the irradiated 800H-TMP. Some Ti(C,N) precipitates are embedded in the M 23 C 6 precipitates, maintaining specific orientation relationships between the precipitates and between the precipitate and matrix. In addition, nanoscale Si-rich clusters were observed in the matrix of all the 800H/800H-TMP samples, with EDS Si maps tending to have a lower contrast in 800H-TMP samples. Atom probe tomography was conducted on the same samples, supported by a Rapid Turnaround Examination project under Nuclear Science User Facilities. The results are being analyzed to be integrated with the TEM results for a confident description of the γ’ precipitates. Dislocation loops also formed in all the 800H/800H-TMP samples. The density and the average size of dislocation loops were quantified to be in the order of 10 22 – 10 23 m -3 and 11.7 – 15.9 nm, respectively, in the ATR-irradiated 800H/800H-TMP samples. The loop densities in irradiated 800H were higher than that in irradiated 800H-TMP under the same irradiation conditions. Further systematic data analyses, together with some complementary experiments, will be pursued for these samples to foster peer-reviewed journal article publications.

36 MATERIALS SCIENCE↗

Emergent chirality in a polar meron to skyrmion phase transition

Polar skyrmions are predicted to emerge from the interplay of elastic, electrostatic and gradient energies, in contrast to the key role of the anti-symmetric Dzyalozhinskii-Moriya interaction in magnetic skyrmions. Here, we explore the reversible transition from a skyrmion state (topological charge of –1) to a two-dimensional, tetratic lattice of merons (with topological charge of –1/2) upon varying the temperature and elastic boundary conditions in [(PbTiO 3 ) 16 /(SrTiO 3 ) 16 ] 8 membranes. This topological phase transition is accompanied by a change in chirality, from zero-net chirality (in meronic phase) to net-handedness (in skyrmionic phase). We show how scanning electron diffraction provides a robust measure of the local polarization simultaneously with the strain state at sub-nm resolution, while also directly mapping the chirality of each skyrmion. Using this, we demonstrate strain as a crucial order parameter to drive isotropic-to-anisotropic structural transitions of chiral polar skyrmions to non-chiral merons, validated with X-ray reciprocal space mapping and phase-field simulations.

42 ENGINEERING↗

Boosting the use of bauxite residue (red mud) in cement - Production of an Fe-rich calciumsulfoaluminate-ferrite clinker and characterisation of the hydration

Highlights: • Incorporation of 35 wt% of bauxite residue for production of CSAF clinker • Thermochemical calculations as suitable tool for predicting phase assemblage • Hydration of the cement was found to be accelerated in contrast to other CSA cements. • High early compressive strengths of 40 MPa In the present work, calciumsulfoaluminate-ferrite clinker was produced using 35 wt% of bauxite residue in combination with alumina, clay, limestone and gypsum. At a temperature of 1300 °C, the hydraulic phases ye'elimite, ferrite and C{sub 2}S were formed. Computed thermochemical predictions were a significantly better match for the real mineralogy than modified Bogue equations. Hydration of the clinker led to the formation of ettringite and monosulfate, resulting in compressive strengths of 17 MPa after 28d. Compressive strengths of 40 MPa after 2d, and 28d-strengths exceeding 50 MPa, were reached in blends with 10 wt% of anhydrite. The strength development was due to the rapid formation of ettringite, mainly originating from ye'elimite, which did not convert to AFm phases and led to a compact microstructure. Only when the ye'elimite dissolution decreased, did the ferrite phase react. In pastes with additional sulfates, ferrite hydration led to the formation of ettringite and to hydrogarnet. Cement nomenclature is used in this work.{sup 1}.

36 MATERIALS SCIENCE↗

Optical response of columnar TiO{sub 2}:Co on Si substrate

Vertically arranged columnar TiO{sub 2}:Co structure has been deposited on Si (100) substrate using the metal organic chemical vapor deposition (MOCVD) technique. SEM images confirm the columnar structure of the TiO{sub 2}:Co layer on Si (100). Concentration of the Co dopant has been defined by means of the energy dispersive x-ray (EDX) spectra. Co concentrations are varied at 0.18, 0.33, and 0.68 at. % using pure TiO{sub 2} as the reference. X-ray diffraction (XRD) spectra show that the TiO{sub 2}:Co layer have a rutile phase. Further analysis of this structure has been performed by using room temperature spectroscopic ellipsometry (SE) measurements in the energy range of 0.5 - 6.5 eV. This optical response shows the unique feature of significantly high density fringe especially below the band gap energy region (lower than 3.3 eV) in contrast to the conventional TiO{sub 2} thin film structure. This unique feature is interpreted as a dominant contribution of the vertical interfaces at columnar boundaries towards reflected light from the sample. The evolution of Ψ and Δ will be discussed as the function of Co concentration and some optical properties will be extracted after reasonably well data fitting by multilayer modelling. Furthermore, by comparing the SE data from different measurement orientations, it has been shown that TiO{sub 2}:Co tends to be anisotropic. This study enables us to further evaluate structural properties through optical responses given by SE measurement.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthetic approaches to borocarbonitrides, BC{sub x}N (x=1-2)

In order to synthesize borocarbonitrides of the general formula BC{sub x}N where x varies between 1 and 2, we have carried out high-temperature gas phase reaction of BBr{sub 3} with a mixture of ethylene and ammonia. The composition of the product was close to BC{sub 1.6}N as shown by x-ray photon spectroscopy (XPS) and electron energy loss spectroscopy (EELS). The products were further characterized by infra-red, Raman and other spectroscopic techniques. The borocarbonitrides obtained from the gas phase reaction have low surface areas, in contrast to those of similar compositions prepared by the urea method. First principles calculations show that the most stable structures of the compositions BCN and BC{sub 2}N contain BN-rich and carbon-rich domains where BN{sub 3} and NB{sub 3} units are present. - Graphical abstract: Vapor phase synthesis of BC{sub x}N (x=1-2) by the reaction of BBr{sub 3}, ethylene and ammonia leads to the formation of pan-like structure. Highlights: > We have carried out vapor phase reaction of BBr{sub 3}, ethylene and ammonia to synthesize BC{sub x}N (x=1-2). > HRTEM and AFM show the formation of pan-like structures with the central region formed of single layer of BC{sub x}N. > Borocarbonitrides formed by vapor phase synthesis show limited adsorption properties as compared to the urea route. > First principles calculations show that the most stable structure of the compositions BCN and BC{sub 2}N contain BN-rich and carbon-rich domains where BN{sub 3} and NB{sub 3} units are present.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultrafast infrared nano-imaging of far-from-equilibrium carrier and vibrational dynamics

Ultrafast infrared nano-imaging has demonstrated access to ultrafast carrier dynamics on the nanoscale in semiconductor, correlated-electron, or polaritonic materials. However, mostly limited to short-lived transient states, the contrast obtained has remained insufficient to probe important long-lived excitations, which arise from many-body interactions induced by strong perturbation among carriers, lattice phonons, or molecular vibrations. Here, we demonstrate ultrafast infrared nano-imaging based on excitation modulation and sideband detection to characterize electron and vibration dynamics with nano- to micro-second lifetimes. As an exemplary application to quantum materials, in phase-resolved ultrafast nano-imaging of the photoinduced insulator-to-metal transition in vanadium dioxide, a distinct transient nano-domain behavior is quantified. In another application to lead halide perovskites, transient vibrational nano-FTIR spatially resolves the excited-state polaron-cation coupling underlying the photovoltaic response. These examples show how heterodyne pump-probe nano-spectroscopy with low-repetition excitation extends ultrafast infrared nano-imaging to probe elementary processes in quantum and molecular materials in space and time.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Control of Surface Morphology during the Growth of (110)-Oriented GaAs by Hydride Vapor Phase Epitaxy

We present a study of the effect of hydride vapor phase epitaxy (HVPE) growth conditions on the morphology of GaAs grown on vicinal and nominally exact (110) GaAs substrates. We evaluate epilayer surfaces using a combination of Nomarski microscopy and atomic force microscopy. The surface morphology strongly depends on the growth conditions employed, as well as the substrate orientation. On substrates offcut 3° toward (111)A, faceting generally develops under conditions in which the growth is Ga-limited, although Ga-limited growth is not the only requirement for faceting. Low growth temperatures lead to a faceted morphology, while higher growth temperatures favor smooth growth and facet-free morphology. We show that the surface morphology is kinetically controlled and that the tendency to facet correlates with the growth rate. 3D growth occurs on nominally exact substrates, resulting in hillock formation, but reduction of the group V precursor partial pressure results in smooth morphology. Overall, our results are consistent with models for step-bunching-induced surface faceting that invoke a negative Ehrlich–Schwoebel step-edge barrier.

(110) oriented GaAs↗

Effect of Air Oxidation on Pore Structure Development and Mechanical Properties of Nuclear Graphite

This document reports on continuation of R&D activities at ORNL directed at investigating the effect of air oxidation of nuclear graphite on development and structure of porosity in the oxidized layer, and on the effect on mechanical properties of oxidized graphite. The material investigated was nuclear-grade graphite (purified PCEA graphite, from GrafTech International). Based on conclusions of previous work (ORNL/TM-2009/192), the method of analysis of the porosity in the oxidized layer based on optical microscopy coupled with automated image analysis was further improved and standardized. In addition, characterization of oxidized specimens by optical microscopy was complemented with measurements of mechanical properties (compressive strength) on a statistically significant number of specimens. A series of cylindrical shape specimens were machined and oxidized in air at two temperatures (600 and 700 o C) and at three levels of burn-off at each temperature (5-6 %; 10-12 % and 15-17%). The procedure used for specimen preparation and oxidation, and the oxidation equipment, were those recommended in ASTM D-7542-09. However, in order to comply with the aspect ratio requirements for specimens employed in compressive strength measurements (ASTM C-695-91) all specimens were machined with a length to diameter ratio of 2 (i.e. 25.4 mm height vs. 12.7 mm diameter) instead of 25.4 mm length and 25.4 mm diameter recommended by ASTM D-7542-09. After oxidation, mechanical properties (compressive strength) were measured on at least three samples obtained at equal oxidation conditions, while another specimen from the same lot was sectioned, mounted in resin and surface polished for optical microscopy analysis. In the latter procedure, mosaic pictures were collected of a rectangular stripe across the diameter of each specimen. These images were analyzed in order to derive the penetration depth and the pore structure in the oxidized layer as a function of oxidation temperature and weight loss level. Automated image analysis was performed using the commercial software Image Pro Plus. The results led to the conclusion that the depth of the oxidation layer is more dependent on the oxidation temperature than on the level of weight-loss. The penetration depth of the oxidized layer is about 6 mm at 600 o C and about 1.5 mm at 700 o C. Consequently, the 12.5 mm diameter specimens oxidized at 600 o C were completely penetrated by oxidation, while those oxidized at 700 o C had the oxidation layer restricted in a narrower band near the exposed surface. This difference was reflected by mechanical properties. A closer analysis of high magnification images in the oxidized layer revealed that oxidation attacks preferentially the binder phase in graphite, where development of fine new pores was observed. The density of new pores was higher near large pores pre-existing in graphite structure. Acute oxidation at low temperatures (e.g. 600 o C) causes more damage on mechanical strength than high temperature oxidation (700 o C). Although the latter is much faster, the oxidized layer is limited to a narrow zone next to the external surface, so that the core is not visibly affected. In contrast, oxidation at lower temperature, although slower, is more damaging because it penetrates deeply beyond the exposed surface.

36 MATERIALS SCIENCE↗

The Nanoscience Beamline (I06) at Diamond Light Source

The Nanoscience beamline (I06) is one of seven Diamond Phase-I beamlines which has been operational since January 2007 delivering polarised soft x-rays, for a PhotoEmission Electron Microscope (PEEM) and branchline, in the energy range 80-2100 eV. The beamline is based on a collimated plane grating monochromator with sagittal focusing elements, utilising two APPLE II helical undulator sources, and has been designed for high flux density at the PEEM sample position. A {approx}5 {mu}m ({sigma}) diameter beam is focussed onto the sample in the PEEM allowing a range of experiments using x-ray absorption spectroscopy (XAS), x-ray magnetic circular dichroism (XMCD) and x-ray magnetic linear dichroism (XMLD) as contrast mechanisms. The beamline is also equipped with a branchline housing a 6T superconducting magnet for XMCD and XMLD experiments. The magnet is designed to move on and off the branchline which allows a diverse range of experiments.

43 PARTICLE ACCELERATORS↗

A Transmission Electron Microscopy Study of a Refractory Metal Grain from a Calcium-Aluminum-Rich Inclusion in the Leoville CV3 Chondrite

Introduction: Calcium-aluminum-rich inclusions (CAIs) are an important component of chondritic meteorites. They can contain materials that are thermodynamically predicted and isotopically age dated to be among the first-formed solids in our solar system [1-5]. Observed in some CAIs are micron to sub-micron sized inclusions rich in Fe, Ni, and high-Z elements such as Pt, Os, Ir and W, in the form of refractory metal nuggets (RMNs), fremdlinges, and ‘nugget like objects’ (NLOs) [1,6]. Refractory siderophile elements such as Os, Ir and Ru are thermodynamically predicted to condense at temperatures well in excess of the major CAI phases such as melilite, perovskite, spinel and hibonite [2,7-9]. These refractory metal inclusions in CAIs can therefore serve as probes into the thermodynamic landscape of the early solar protoplanetary disk. Here we report on a refractory grain identified in a CAI of the Leoville CV3 chondrite. This work is part of an ongoing effort to gain insight into the thermochemistry of the early solar system through systematic analyses of the structure and chemistry of various components in CAIs [10-13]. Sample and Analytical Techniques: A fluffy type A CAI (Fig. 1A) was identified in a section of the Leoville, CV3 chondrite (Center for Meteorite Studies, Arizona State University collection, #821_C_3) using a JOEL-JXA 8530F electron microprobe at Arizona State University. Backscattered electron (BSE) imaging and energy-dispersive X-ray spectroscopy (EDS) were used to identify refractory metal grains in the CAI using a Thermo Fisher (formerly FEI) Helios NanoLab 660 G3 focused-ion-beam scanning-electron microscope (FIBSEM) located at the Kuiper Materials Imaging and Characterization Facility (KMICF) at the Lunar and Planetary Laboratory, University of Arizona. The FIB is equipped with an EDAX EDS system. We selected one of the larger (micron-sized) refractory metal grains, designated as ‘Spud’ (Fig. 1B) for further analysis. ‘Spud’ was extracted and thinned to electron transparency (<100 nm) using the FIB-SEM located in KMICF, following methods described by [14- 15]. The FIB section was analyzed using a 200 keV Hitachi HF5000 scanning transmission electron microscope (S/TEM) located at KMICF. The HF5000 is equipped with cold-field emission gun, 3rd-order spherical aberration corrector for STEM imaging, and an Oxford Instruments X-Max N 100 TLE energydispersive spectroscopy (EDS) system with dual 100 mm2 windowless silicon-drift detectors (Ω = 2.0 sr). Selected-area electron-diffraction (SAED) patterns were acquired to aid in determination of crystallinity and phase. Results: The mineralogy, texture, and morphology of the CAI are consistent with that of a fluffy type A (FTA) CAI [16]. BSE imaging at high magnifications revealed grains with high contrast, indicative of compositions rich in elements of higher atomic number relative to surrounding material. These high-Z grains have sizes that range from ∼250 nm to 4 µm. EDS analyses confirm that the bright grains are metal-rich inclusions. A minor fraction of the grains are composed of only Fe and Ni, but the majority (∼60%) of the identified inclusions also contained various refractory siderophiles including Os, Ru, Zr, Ir and Mo. EDS analysis on the FIB-SEM of Spud shows that it contains Fe, Ni, Mo and Ru. High-angle annular dark-field (HAAFD) imaging and EDS mapping in the TEM (Fig. 2) show that Spud occurs in melilite (Ca1.9Al1.99Si1.06O7). Spud contains a subhedral to anhedral morphology and is compositionally heterogenous (polyphasic, Fig. 2). Local spatial correlation occurs among Fe, Ni, and Pt, and also among Os, Ru, and Mo. SAED patterns show that the Fe-Ni-Pt, Fe-Os-Mo-Ru and Fe-Pt regions are crystalline. Discussion: CAIs can contain various types of inclusions rich in Fe, Ni and refractory siderophiles such as Os, Ru, W and Pt [1]. RMNs are micron-sized, single phase alloy grains and can contain Os, Ir, Ru and Rh [1,7,17]. NLOs are also micron-sized inclusions, but contain two phases, a refractory metal, and an oxide [6]. Fremdlinge are the largest of such inclusions (tens of microns in size) and are complex aggregates of Fe-Ni alloy, silicates, oxides, and sulfides [1,17]. While the size of Spud matches previous descriptions of RMNs and NLOs, Spud is neither a single-phase alloy like RMNs, nor does it contain one metal phase and one oxide like NLOs. Spud does not match the above described categories of refractory metal inclusions. The presence of refractory siderophiles such as Mo, Os, Ru, and Pt suggests a high-temperature origin. Thermodynamic modelling by [7] indicates condensation temperatures of 1917 K, 1693 K, 1613 K and 1415 K for Os, Mo, Ru and Pt respectively. These models also show that following the initial condensation of a refractory metal, alloying of solutes such as Fe, Ni and W, occurs in levels proportional to their partial pressures in the surrounding gas. Such alloying occurs at temperatures above the condensation temperatures of common CAI phases such as melilite (1529 K), perovskite (1441 K), spinel (197 K) and forsterite (1354 K) [2]. The polyphasic nature of Spud could be the result of such high-temperature alloying, possibly shortly after the condensation of Mo and Ru at 1693 K and 1613 K respectively. That Spud occurs as an inclusion is consistent with it having formed prior to and at temperature above that of its host melilite in this FTA CAI, which is qualitatively consistent with such prior thermodynamic modeling. Further, the polyphasic nature of Spud is similar to refractory grains from a FTA CAI in the Northwest Africa (NWA) 8323, CV3 chondrite [11-13]. These data suggest that such refractory metal grains could have been widespread in the inner and early solar protoplanetary disk and represent some of the earliest formed solids to have condensed. Acknowledgments: Research and instrumentation supported by NASA grants #NNX12AL47G, #NNX15AJ22G and #80NSSC19K0509, and NSF grants #1531243 and #0619599. Fig 2. STEM data on ‘Spud’. HAADF Image (Top) False-color EDS Maps (Bottom) References: [1] MacPherson G. J. (2014) T. of Geochem. Vol I: Met. And Cosmochem. Processes, 139-179. [2] Lodders K. (2003) ApJ, 591, 1220-1247. [3] Ebel D. S. (2006) Met. & the Early S. Sys. II., 253- 277. [4] Amelin Y. (2002) Science, 297, 1678-1683. [5] Connelly J.N. et.al. (2012) Science, 338, 651-655. [6] Schwander D. et al. (2015) GCA, 18, 70-87. [7] Palme H. and Wlotzka F. (1976) EPSL, 33, 45-60. [8] Berg T. et al. (2009) ApJ, 702, 172-176. [9] Liffman K. et al. (2021) Icarus, 221, 89-105. [10] Zega T.J. et al. (2021) PSJ, 2, 115. [11] Ramprasad T. et al. (2020) LPSC LI, Abstract #2472. [12] Ramprasad T. et al. (2021) Microscopy & Microanalysis, S1, 2792-2794. [13] Ramprasad T. et al. (2021) 84th MetSoc, Abstract #6123. [14] Zega T.J. et al. (2007) MAPS, 42, 1373-1386. [15] Ramprasad T. et al. (2022) MAPS, in revision. [16] Grossman L. (1975), GCA, 39, 433-454. [17] El Goresy A. et al. (1978) LPSC IX, Abstract#1100

T. Ramprasad↗

Electroless nickel – phosphorus coating on crab shell particles and its characterization

Being hydrophilic material, crab shell particles have only a limited number of applications. It is, therefore, necessary to modify the surface of the crab shell particles. To make them useful ever for the applications, the main theme we proposed in this article is to utilize crab shell particles (CSP) with the core coated with nickel phosphorus (NiP) as a shell using the electroless coating process. For dealing with serious environmental problems, utilization of waste bio-shells is always an important factor to be considered. Chelating ability of crab shell particles eliminates the surface activation in this work proceeding to the coating process. The functional group, phase structure, microstructure, chemical composition and thermal analysis of CSP and NiP/CSP were characterized using Fourier transform infra-red spectroscopy (FTIR), x-ray diffraction analyzer (XRD), scanning electron microscope (SEM), energy-dispersive x-ray spectroscopy (EDS), and thermogravimetric analysis (TGA). The combination of an amorphous and crystalline structure was exhibited by CSP and NiP/CSP. NiP/CSP has shown a better thermal stability when compared to uncoated CSP. Stability test, adsorption test, and conductivity test were conducted for the study of adsorption behavior and conductivity of the particles. CSP presented a hydrophilic property in contrast to hydrophobic NiP/CSP. NiP/CSP presented a conductivity of about 44% greater compared to the CSP without any fluctuations. - Highlights: • Utilization of crab shell waste is focused on. • NiP coating on crab shell particle is fabricated using electroless process. • Thermal analysis, stability test, adsorption test and conductivity test were done. • Organic matrix of crab shell particle favors the coating process. • Results demonstrate the characterization of CSP core – NiP shell structure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Extracting electron backscattering coefficients from backscattered electron micrographs

Electron backscattering micrographs possess the so-called Z-contrast, carrying information about the chemical compositions of phases present in microstructures. The intensity at a particular point in the backscattered electron micrograph is proportional to the signal detected at a corresponding point in the scan raster, which is, in turn, proportional to the electron backscattering coefficient of a phase at that point. This article introduces a simple method for extracting the electron backscattering coefficients of phases present in the microstructure, from the backscattered electron micrographs. This method is able to convert the micrograph's greyscale to the backscattering-coefficient-scale. The prerequisite involves the known backscattering coefficients for two phases in the micrograph. In this way, backscattering coefficients of other phases can be determined. The method is unable to determine the chemical compositions of phases or the presence of an element only from analysing the backscattered electron micrograph. Nevertheless, this method was found to be very powerful when combined with energy dispersive spectroscopy, and the calculations of backscattering coefficients. - Research Highlights: {yields}A simple method for extracting the electron backscattering coefficients {yields}The prerequisite is known backscattering coefficients for two phases {yields}The information is complementary to the EDS-results. {yields}This method is especially useful when a phase contains a light element (H, Li, Be, and B)

36 MATERIALS SCIENCE↗

Modulation periodicity dependent structure, stress, and hardness in NbN/W{sub 2}N nanostructured multilayer films

NbN/W{sub 2}N nano-multilayer films with a modulation periodicity, {Lambda}, ranging from 5.1 to 157.4 nm have been deposited on a Si(100) substrate by reactive magnetron sputtering in Ar/N{sub 2} mixtures. The {Lambda} dependent structural and mechanical properties for the resulting NbN/W{sub 2}N multilayers have been evaluated by means of low-angle x-ray reflectivity, x-ray diffraction, high-resolution transmission electron microscope, and nanoindentation measurements. The finding is that for films with {Lambda}{<=} 10.6 nm, fcc NbN layers are coherent with cubic W{sub 2}N layers, resulting in NbN layers and W{sub 2}N layers that are in the compressive and tensile states, respectively. In contrast, as {Lambda} is larger than 10.6 nm, a phase transition from W{sub 2}N to W occurs in the W{sub 2}N layer, which is a result of the coherent interface strain relaxation. For this case, all layers are in the compressive state, and the coherent interface disappears. The intrinsic compressive stress evolution with {Lambda} can be interpreted in terms of interface stress. The formation of coherent interface at small {Lambda} ({<=}10.6 nm) is helpful for releasing point defects in layers, leading to a low compressive stress ({<=}1.1 GPa). The hardness for the obtained multilayer film increases with decreasing {Lambda}, and approaches a maximum value of 43.7 GPa when {Lambda} is 7.4 nm. The maximum strengthen at lower {Lambda} is mainly attributed to coherent interface stresses and the modulus difference between the NbN and W{sub 2}N layers. The increase in hardness with a decrease in {Lambda} is interpreted by the Lehoczky model.

36 MATERIALS SCIENCE↗

Ultrafast optical pump-probe spectroscopy is used to reveal the coexistence of coupled antiferromagnetic (AFM)/ferroelectric (FE) and ferromagnetic (FM) orders in multiferroic TbMnO3 films, which can guide researchers in creating new kinds of multiferroic materials.

Multiferroic materials have attracted much interest in the past decade, due not only to their novel device applications, but also their manifestations of coupling and interactions between different order parameters (particularly electric polarization and magnetic order). Recently, much attention has been focused on perovskite manganites, RMnO{sub 3} (R = rare earth ions), due to the discovery of a large magnetoelectric effect in these materials. The first member of this family to be discovered was TbMnO{sub 3} (TMO), which is now well established as a typical magnetoelectric multiferroic. Extensive experimental and theoretical studies have already been done on single crystal TMO (SC-TMO). In brief, SC-TMO, with a distorted orthorhombic perovskite structure, has an antiferromagnetic (AFM) phase transition at T{sub N} {approx}40 K with sinusoidally ordered Mn moments. Below T{sub FE} {approx} 28 K, ferroelectric (FE) order develops owing to the appearance of cycloidal spiral spin structure. In contrast, there are relatively few reports describing the properties of TMO thin films (typically grown on SrTiO{sub 3} (STO) substrates). In general, thin films can enable new functionality in materials, as their physical parameters can be changed by modifying their structure via strain imposed by the substrate. Strain in particular has the potential to directly couple FE and FM orders, which is very rare. This could benefit electronic device applications by providing low power consumption, high speed operation, and greater electric/magnetic field controllability. Previous investigations of magnetic properties in TMO films revealed an unexpected ferromagnetic (FM) order, in contrast to SC-TMO. However, several important questions regarding these films are still unanswered for instance: (1) What mechanism induces FM order? (2) Can FM, sinusoidal AFM and spiral AFM (or FE) orders coexist? (3) Can FM order be coupled to FE order? To fully understand these unique materials, experimental techniques capable of dynamically unraveling the interplay between these degrees of freedom on an ultrafast timescale are needed. Here, we use ultrafast optical pump-probe spectroscopy to reveal coexisting coupled magnetic orders in epitaxial TMO thin films grown on (001)-STO, which were not observed in previous work. Our temperature (T)-dependent transient differential reflectivity ({Delta}R/R) measurements show clear signatures of sinusoidal AFM, spiral AFM (FE) and FM phases developing as the film thickness changes. We carry out first-principle density functional theory (DFT) calculations to explain the coupling between AFM/FE and FM orders. These results reveal that the coupling between different magnetic orders observed in our multiferroic TMO thin films may offer greater control of functionality as compared to bulk single crystal multiferroics.

36 MATERIALS SCIENCE↗

Atomic-Scale Structural Mapping of Active Sites in Monolayer PGM-Free Catalysts by Low-Voltage 4D-STEM

Two-dimensional (2D) materials have attracted a large amount of attention in both basic and applied fields, and scanning transmission electron microscopy (STEM) is often uniquely well-suited for characterizing the atomic-scale structure of these materials [1-4]. As a result, STEM is poised to significantly impact progress on platinum group metal (PGM)-free catalysts, which are currently under intense development to enable low-cost, commercially viable hydrogen fuel cells [5]. While recent advancements have resulted in fuel cell performance comparable to Pt catalysts by some measures [6], cell durability remains a significant challenge, limiting practical applications [7]. Catalytically active sites in PGM-free materials are proposed to be FeN4 complexes embedded in a graphene lattice (Fig. 1b) within layered or other larger materials, but this is still under debate largely due to the range of potential actives sites predicted by computational methods and lack of methods for directly validating these models [5]. Fundamental insights into the atomic structure and resulting degradation pathways of proposed active sites are therefore needed to fully understand and control cell performance and durability [6].2D materials typically make ideal samples for STEM, but those within PGM-free catalysts present additional challenges since these materials are often defect-rich, with a high density of edges, dopant atoms, etc., which significantly increase susceptibility to beam damage at standard operating voltages. This makes analysis of potential FeN4 active sites particularly challenging, since a large proportion of Fe exists at edge sites where beam-induced atomic displacements can prohibit high-resolution structural characterization [6]. Conventional dark-field imaging compounds this problem by producing less signal for a given dose and being less sensitive to light elements than dose-efficient phase contrast imaging techniques such as those enabled by four-dimensional (4D)-STEM [8-10] (Fig. 1a). Consequently, active site structural analysis is often left to methods such as low-resolution imaging combined with quantum chemical calculations [6], which hinders accurate determination of reaction and degradation mechanisms.Here, we demonstrate direct atomic-scale structural mapping of FeN4 sites by performing low-voltage 4D-STEM on a model PGM-free catalyst system with many exposed monolayer regions. To accomplish this, we pair a 30 keV aberration-corrected probe with a fast pixelated detector that has optimal performance at low beam voltages [11]. This enables us to simultaneously image light and heavy elements with high signal-to-noise by center-of-mass analysis (Fig. 1c) while minimizing beam-induced atomic displacements at sensitive sites. The monolayer nature of these materials additionally allows for experimental validation by direct comparison with multislice simulations [12] of model structures (Fig. 1d-e). This work demonstrates how low-voltage 4D-STEM will provide new insights into the atomic-scale structure and degradation mechanisms of active sites in PGM-free catalysts, facilitating the development of low-cost hydrogen fuel cells and other energy conversion technologies in the future [13].

Zachman, Michael↗

Magnéli phases Ti{sub 4}O{sub 7} and Ti{sub 8}O{sub 15} and their carbon nanocomposites via the thermal decomposition-precursor route

A new synthetic approach for producing nano-powders of the Magnéli phases Ti{sub 4}O{sub 7}, Ti{sub 8}O{sub 15} and their carbon nanocomposites by thermal decomposition-precursor route is proposed. The formation mechanism of the single-phase carbon nanocomposites (Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C) from metal–organic precursors is studied using FT-IR, elemental analysis, TG, STA-MS and others. The synthesis parameters and conditions were optimized to prepare the target oxides with the desired microstructure and physical properties. The electrical and transport properties of Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C are investigated. These nano-materials are n-type semiconductors with relatively low thermal conductivity in contrast to the bulk species. The nanostructured carbon nanocomposites of Magnéli phases achieve a low thermal conductivity close to 1 W/m K at RT. The maximum ZT{sub 570} {sub °C} values are 0.04 for Ti{sub 4}O{sub 7}/C powder nanocomposite and 0.01 for Ti{sub 8}O{sub 15}/C bulk nanocomposite. - Graphical abstract: From the precursor to the produced titanium oxide pellet and its microstructure (SEM, TEM micrographs) as well as results of phase and thermoelectric analyses. - Highlights: • Magnéli phases Ti{sub 4}O{sub 7}/Ti{sub 8}O{sub 15} via thermal decomposition-precursor route is proposed. • The formation mechanism of the nanocomposites Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C are investigated. • Microstructure of Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C are examined. • The electrical and transport properties of Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C are investigated. • The maximum figure of mertit ZT{sub 570} {sub °C} of Ti{sub 4}O{sub 7}/C and Ti{sub 8}O{sub 15}/C are 0.01 and 0.04.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗