Search NASA⌕ Search

SEARCH · Search NASA

Results for “Cladding materials”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 685 records · Page 38

Report Summarizing Progress in Digital Image Correlation Analysis of Burst Phenomenon

This report is an update on the progress made towards utilizing in-situ methods to observe and quantify Zry-4 deformation behavior during burst testing. A heavily modified burst test was developed that allows both digital image correlation and infrared thermography to be utilized during testing to quantify strain and axial thermal gradient data during burst. A variety of tests ranging from 6.2-15.9 MPa internal pressure and utilizing both constant and transient pressure conditions were conducted and presently reported on. The test modifications, which are detailed extensively in a previous report, are effectively found to have no discernible impact on burst temperatures when compared to historical Zircaloy burst data. To support future modeling studies, the IR thermography data was used to approximate the thermal gradient down the axial length at burst for all the claddings. Then, DIC is first correlated to thermocouple temperature for a 10.3 MPa Transient pressure test, and then DIC correlated to IR thermal gradient data down the axial length of a 8.2 MPa Transient pressure test at several points.

36 MATERIALS SCIENCE↗

Effect of surface oxides on tritium entrance and permeation in FeCrAl alloys for nuclear fuel cladding: a review

Abstract Iron-chromium-aluminum (FeCrAl) alloys are being considered for the cladding of uranium dioxide fuel in light water reactors (LWRs). FeCrAl alloys have good mechanical properties at temperatures of 300 °C and higher, and have superlative resistance to attack by steam at temperatures of up to 1000 °C and higher. A concern has been raised that the use of FeCrAl for cladding would result in a higher content of tritium in the reactor coolant as compared with the current system where the cladding is a zirconium based alloy. This review shows that the flux of tritium from the fuel rod cavities to the coolant across the fuel cladding wall will be greatly reduced by the presence of oxides on the surface of the cladding. The review of current literature and permeation data show that (a) protective oxides are expected to be present on both sides of the FeCrAl cladding, and (b) depending on the characteristics of these oxide layers it is reasonable to expect about two–three orders of magnitude reduction in tritium permeation, relative to the permeation response in clean, unoxidized condition for FeCrAl steels of interest, around 277 °C–377 °C temperatures.

Electrochemistry↗

FY22 Progress Report on BISON Metallic Fuel Model Development and V&V Using EBR-II Legacy Data

In this report, the activities and achievements made by Argonne National Laboratory for the Nuclear Energy Advanced Modeling and Simulation (NEAMS) BISON code metallic fuel validation and verification project in FY2022 are summarized. The FIPD-BISON integration powered metallic fuel low-burnup swelling framework has been enhanced to cover both radial and axial swelling analyses. Axial-dependent as-fabricated fuel radius profiles have been used to improve the accuracy in evaluating radial swelling strain. The simulations of the IFR experiment X447, which was focused on FCCI/CCCI induced cladding degradation and failure, have been converted into a BISON metallic fuel assessment case with detailed documentation, which is also the first FIPD-BISON integration powered assessment case in BISON. A FIPD-BISON integration repository has been established to be an optional submodule of BISON to support FIPD-BISON integration powered assessment cases. Preliminary trials to simulate the in-cell out-of-pile transient experiment have been made after implementing some essential models such as cladding plasticity models and liquid phase penetration models. The initial results are promising and help identify gaps that need to be filled in FY2023 and beyond, to eventually achieve OPTD-BISON integration powered assessment cases.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Degradation and Failure Phenomena of Advanced Reactor Fuel Concepts: Sodium-Cooled Fast Reactor Metallic Fuel

The U.S. Nuclear Regulatory Commission (NRC) is anticipating licensing applications and commercial use of new fuel types in advanced nuclear power reactors that would be designed and built in the United States. Pacific Northwest National Laboratory (PNNL) is providing technical assistance to the NRC related to the newly proposed nuclear fuel and cladding designs that would be deployed in these reactors. This report focuses specifically on the metallic fuel that is being considered for sodium-cooled fast reactors and specifically on mechanisms that would cause damage or failure to the fuel under reactor operating conditions and design basis accident conditions. There is historic experience with both metallic and oxide fuels in experimental sodium-cooled fast reactors, but this report will focus solely on metallic fuel. Currently two U.S.-based reactor designers are engaged with the NRC in the application or pre-application review and considering a sodium-cooled fast reactor. TerraPower is engaged with NRC in pre-application review of its Natrium reactor. The current design for this fuel uses a sodium-bonded uranium-10wt% zirconium (U10Zr) fuel clad in HT9 stainless steel. ARC Clean Technology is engaged with NRC in pre-application review of its ARC-100 reactor. The current design for this fuel uses a sodium-bonded uranium-10wt% zirconium (U10Zr) fuel with steel cladding. This report will focus on this fuel system specifically, with broader information given regarding other metallic fuel systems with other stainless steel alloy claddings. To support the NRC’s readiness efforts, this report will identify and discuss degradation and failure modes of metallic fuel concepts for sodium-cooled fast reactors, including fuel performance characteristics that may not be addressed within existing regulatory documents.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Amphiphilic Block Copolymers for Flocculation and Hydrophobization of Legacy Waste Suspensions in Flotation Driven Dewatering Operations - 20162

Flotation has been effectively demonstrated as a low footprint, high efficiency separation process when utilising simple anionic surface modifying agents such as sodium dodecyl sulphate (SDS). These agents increase hydrophobicity to remove suspended cationic surface charged particulates such as Mg(OH){sub 2} from waste suspensions similar to those at British nuclear fuel management sites- where corrosion processes have degraded fuel cladding. The technology is advantageous as it could effectively be retrofitted into existing waste management facilities at nuclear waste management sites such Sellafield and Hanford as the simplicity (no moving parts) and size of this technology coupled with low cost of construction could be rapidly deployed to aid in risk and hazard reduction decommissioning operations with minimum impact to secondary waste generation. Previously, sodium dodecyl sulphate has been deployed as a collector agent to increase the hydrophobicity of Mg(OH){sub 2} suspended particles, achieving a maximum particulate extraction percentage of 93%. To achieve further particulate extraction, flotation performance has been determined to be a function of the hydrodynamic limitations extracting fine material (>20 μm). Fine particulates have been shown in the minerals industry to have an inability to overcome slipstreams created from rising bubbles in flotation cells, likely due to the low mass and thus momentum of the colloidal material, preventing interaction between the hydrophobized particles and air-water interfaces (bubbles). To combat this mass transfer resistance poly(acrylic acid)-block-poly(n-butyl acrylate) amphiphilic diblock copolymers were synthesised via reversible addition-fragmentation chain-transfer (RAFT) polymerisation. The anticipated mode of action of these polymers involves the hydrophilic poly(acrylic acid) block polymer acting as a flocculation agent to increase the mass of the aggregates, and the hydrophobic poly(n-butyl acrylate) modifies the hydrophobicity of the resulting flocs. The concentration of this polymer (termed a macro-collector) was varied and the change in particle size distribution of the particulate suspension was analysed using static light scattering. The flotation performance was then characterised by several methods including percentage particulate recovery, volume reduction factor and residual bulk particulate concentration. This was then benchmarked against the traditional surfactant collector agent SDS. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Design of separate-effects In-Pile transient boiling experiments at the $\mathrm{TREAT}$ Facility

The cladding-to-coolant heat transfer during rapid power excursions, such as reactivity-initiated accidents, remains a crucial area of uncertainty in nuclear reactor safety. This uncertainty impacts the ability to accurately predict fuel performance behavior for these conditions. Improving our understanding of transient cladding-to-coolant heat transfer will enhance our ability to model design basis accidents and could increase design and improve safety margins for the current commercial fleet and advanced reactors. To address these issues, the Critical Heat Flux Static Environment Rodlet Transient Test Apparatus (CHF-SERTTA) experiment uses a novel approach with a borated stainless-steel heater rodlet that can replicate cladding temperatures experienced during a design-basis reactivity-initiated accident. The rodlet and experiment is instrumented to provide temperature and thermal-hydraulic conditions throughout the transient. The design of the rodlet allows for separate effect testing that eliminates complexities with a fuel and cladding specimen. We report the experiments have provided data that will be used to improve our understanding of boiling behavior, specifically critical heat flux, under transient conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanical Loads on Spent Nuclear Fuel in the General 30 cm Package Drop Scenario

The U.S. Department of Energy Office of Nuclear Energy (DOE-NE) Spent Fuel and Waste Science & Technology (SFWST) research program is guided by the high-level goal of closing prioritized knowledge gaps related to spent nuclear fuel (SNF) storage and transportation, which are summarized by Saltzstein et al. (2020). One of the high-priority knowledge gaps is the identification and quantification of mechanical loads that are expected to affect SNF during normal conditions of transportation and storage to inform the range of physical SNF test programs. This report uses modeling and analysis methods to estimate the mechanical loads on spent nuclear fuel (SNF) in the general 30 cm package drop scenario. The drop scenario assumes impact limiters are in place in the transportation configuration and the impact surface is perfectly rigid. The goal of this analysis is to consider the universe of potential mechanical loading conditions that can happen to SNF and present the results in a manner that is useful for materials testing, decision making, and regulatory rule making purposes. This study uses validated finite element models and methods to perform a broad parametric study of key variables that can affect the mechanical loads on SNF during a hypothetical package free drop scenario. Physical drop test data from a cask and fuel assembly drop test campaign is the basis for model validation. Additionally, the results of the parametric study are used to inform a damage model, which uses multiple nonlinear regression to estimate the relationships between input variables and output response. The parametric finite element analyses consider thousands of input variable combinations, while the damage model estimates millions of combinations. The breadth of this study provides confidence that the potential range of mechanical loads that SNF might experience during the general 30 cm package drop scenario are characterized well enough to consider this knowledge gap closed. While this report documents the overall peak values calculated in this study, the 95 th percentile values, the histograms, and the observed trends are equally important. This study covered a large range of SNF temperatures, room temperature to 300°C, and burnups, 10 GWd/MTU to 62 GWd/MTU. Each temperature and burnup combination has a different cladding yield strain, so it is more meaningful to summarize the calculated cladding strain response as its factor of safety, which is defined relative to the yield strain. The factor of safety is calculated as the yield strain divided by the peak cladding strain. A factor of safety greater than unity indicates that the cladding remains below yield, whereas a value less than unity is indicative of plastic deformation. In all cases of this study a safety factor over 1.0 was calculated, although in the most limiting case at 300°C the safety factor was only 1.01, which suggests that yielding could occur when additional loads like rod internal pressure are included. When the temperature is restricted to 200°C the limiting safety factor increases to 1.28, which has significant margin to accommodate internal pressure and potential local cladding defects that could cause a local stress concentration. An important trend in the calculated fuel rod mechanical loads is that the 2 nd highest loaded fuel rod in an assembly tends to be significantly lower than the highest loaded rod. The implication is that even if one rod in an assembly experiences a failure the loads would have to be significantly higher to cause two or more rods to fail.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fabrication of engineered dopant profiles in Er/Lu:YAG transparent laser ceramics via additive manufacturing

Transparent ceramic Er:YAG laser rods were fabricated via the direct ink write (DIW) method with engineered doping profiles featuring an Er-doped core with endcaps and core-clad structures. Laser rods up to 11 cm in length were produced which required development of a scalable process. To achieve this, multiple improvements were implemented, including printing the rods horizontally on a substrate, rather than vertically, eliminating the need for an external support structure and using a sacrificial drying layer to mitigate warping and defects. Highly transparent rods were achieved with optical scatter levels as low as 0.5%/cm (at 543 nm). A small refractive index difference of 5.7 ppm was measured at the interface between the Er-doped core and the Lu-doped endcaps and cladding. These results demonstrate DIW as a straightforward method for making good optical quality laser rods with engineered doping profiles to improve laser performance.

36 MATERIALS SCIENCE↗

TEV-3349 "ATF-2 2A Loop Pin Cladding Requirements"

Industry partners, including Westinghouse, Framatome, General Electric, General Atomics, Toshiba, etc. require requirements for fuel pins they insert in the reactor for testing. This document contains those requirements. These requirements represent an agreement between ATR and NS&T, and include the requirements for pins fabricated at the INL. These include inspections such as radiography, helium leak check, etc.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Postirradiation characterization of palladium as an additive for fuel cladding chemical interaction mitigation in metallic fuel

This work describes the microstructural and elemental characterization of irradiated metallic fuels containing palladium as an additive. The use of additives has been proposed to control Fuel-Cladding Chemical Interaction (FCCI) and thus to promote higher fuel utilization (i.e., higher burnup). In this work, Pd has been investigated as a potential additive to metallic fuel to bind lanthanides, impeding their migration and attack on the cladding. The influence of Pd on the microstructure, chemistry and performance of metallic fuel has been characterized via scanning electron microscopy for two metallic fuel designs—namely, annular and solid fuel. Pd was observed to play an important role in the chemistry of the fuel. Indeed, the addition of Pd leads to the formation of new phases. Pd was detected to combine not only with the lanthanides, as intended, but also with Zr, a main element of the fuel matrix. While Pd proved to be effective in preventing lanthanide migration and their attack on the cladding, the Pd-Zr compound may potentially lead to other unexpected fuel-performance issues, such as the formation of low-melting point phases and increased unalloyed U available for FCCI interaction with Fe in the cladding. Even the increase of Zr to 13wt%. did not completely mitigate this adverse phenomenon generated by the Pd-Zr interaction. Furthermore, the efficacy of using this additive needs further investigation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Particulate plutonium released from the Fukushima Daiichi meltdowns

Traces of Pu have been detected in material released from the Fukushima Daiichi Nuclear Power Plant (FDNPP) in March of 2011; however, to date the physical and chemical form of the Pu have remained unknown. Here we report the discovery of particulate Pu associated with cesium-rich microparticles (CsMPs) that formed in and were released from the reactors during the FDNPP meltdowns. The Cs-pollucite-based CsMP contained discrete U(IV)O 2 nanoparticles, <~10 nm, one of which is enriched in Pu adjacent to fragments of Zr-cladding. The isotope ratios, 235 U/ 238 U, 240 Pu/ 239 Pu, and 242 Pu/ 239 Pu, of the CsMPs were determined to be ~0.0193, ~0.347, and ~0.065, respectively, which are consistent with the calculated isotopic ratios of irradiated-fuel fragments. Thus, considering the regional distribution of CsMPs, the long-distance dispersion of Pu from FNDPP is attributed to the transport by CsMPs that have incorporated nanoscale fuel fragments prior to their dispersion up to 230 km away from the Fukushima Daiichi reactor site.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

First-Principles Studies of Tritium Species Diffusivity Across the Interfaces of Ni-NiZr Alloy-Zircaloy-4

A tritium producing assembly, also known as tritium producing burnable absorber rods (TPBARs), consists of a metal getter tube located between the cladding and γ-LiAlO2 pellets. The metal getter tube is composed of a nickel (Ni) layer coated on Zircaloy-4. The getter assembly is used to capture tritium (3H) species (mainly 3H2 and 3H2O) generated from γ-LiAlO2 pellets during irradiation. Exploring 3H species (3H2, 3H2O) dissociation on the Ni surface and diffusion in the Ni layer and across the interface of Ni-plated Zircaloy-4 getters can provide insights on tritium transport and retention in the pellets and the getter materials. . In FY25, based on the ideal interface model of Ni-Zircaloy-4 generated in FY24, we will further explore the diffusion pathways of 3H across such Ni-ZrNi-alloy layer-Zircalory-4 interfaces under different conditions, including with oxide/hydroxide clusters on the Ni layer, and impurities located in ZrNi-alloy and Zircalory-4 layers. Due to the size limitation of DFT simulation, we will separate the 3-layer system into 3 sub-systems: Ni-ZrNi interface, ZrNi alloy layer, ZrNi-alloy-Zircaloy-4 interface, and simulate the diffusion barriers for tritium.

diffusion barrier↗

An influence of manufacturing tolerances on Pin-Cell k-infinity of MOX fuel using data from the FUBILA experiment program

An influence of manufacturing tolerances (MTs) was evaluated on the pin-cell k-infinity of MOX fuel through the random sampling of CASMO5 calculations. The data from the FUBILA experiment program was used as the manufacturing parameters. For the uncertainties of element/isotope mass fractions, their covariance matrices were calculated by the generalized least square method. The total k-infinity uncertainty was 120-250 pcm (percent mille). From the breakdown of k-infinity uncertainty per materials, the MTs of fuel pellet had a dominant influence. The individual influences were also evaluated for element/isotope mass fractions, an inner/outer diameter, and a density. Those of element/isotope mass fractions were less than a few dozen pcm. Since the perturbations of fuel pellet diameter and density caused large variations to the total amount of heavy metals and effect of spatial self-shielding, they had a negative correlation with the k-infinity perturbation. On the AG3 (Al-Mg alloy) over-cladding, the inner/outer diameter perturbations had both negative and positive correlations. The negative one was due to decrease in amount of light water and the positive one was due to increase in amount of AG3. Since the effect of neutron slowing-down by light water had a dominant influence, the influence of the former negative correlation was larger than that of the latter positive correlation. It is, therefore, concluded that the consideration of the MTs that had a large influence on the effect of neutron slowing-down is important for precise quantification of the pin-cell k-infinity uncertainty of MOX fuel. (author)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Tantalum Experiments in Fully-Reflected Water-Moderated Triangular-Pitched U(6.90)O 2 Fuel Rod Lattices (1.02 cm Pitch)

The United States (US) Department of Energy (DOE) Nuclear Energy Research Initiative funded the design and construction of the Seven Percent Critical Experiment (7uPCX) at Sandia National Laboratories (SNL). The start-up of the experiment facility and the execution of the experiments described here were funded by the DOE Nuclear Criticality Safety Program. The 7uPCX is designed to investigate critical systems with fuel for light water reactors in the enrichment range above 5 % 235 U. The 7uPCX assembly is a water moderated and — reflected array of aluminum-clad U(6.90 %)O 2 fuel rods. Other critical experiments performed in the 7uPCX assembly are documented in LEU-COMP-THERM-078, LEU-COMP-THERM-080, LEU-COMP-THERM 096, LEU- COMP-THERM-097, LEU-COMP-THERM-101, LEU-COMP-THERM-102, and LEU-COMP-THERM-111. Applied interests in neutron-absorbing elements at epithermal and intermediate neutron energy ranges at DOE’s Hanford Site and Savannah River Site were identified through DOE Office of Environmental Management (EM) workshops and needs surveys performed in conjunction with the National Nuclear Security Administration/Nuclear Criticality Safety Program. In response, a team lead by Oak Ridge National Laboratory (ORNL) performed a study evaluating the use of 7uPCX for testing the epithermal cross sections of materials at SNL. This marked the inception of the set of experiments described here. The purpose of these experiments was to measure the effects of tantalum in nearly-critical systems. The tantalum was introduced into the fuel arrays as experiment rods within a central test region. The central test region was designed to target the epithermal neutron energy range by providing a dry cylindrical cavity constructed of aluminum and lined with 0.04 in (0.1016 cm) thick cadmium sheet. The central test region has an outer diameter of 3.75 in (9.525 cm) length of 31 in (78.74 cm) and can hold 85 tantalum rods nominally 0.25 in (0.635 cm) outside diameter and 31.25 in (79.375 cm) long. The critical experiments were done using a set of triangular-pitched grid plates fabricated for these experiments. The grid plate set accommodated a fuel array of a total of 2016 fuel rod positions on a pitch of 0.4 in (1.016 cm) in a series of 21 hexagonal rings positioned around the central test region. The fuel used in these experiments was fabricated using unirradiated 6.90 % enriched UO 2 fuel pellets from fuel elements designed to be used in the internal nuclear superheater section of the Pathfinder boiling water reactor operated in South Dakota by the Northern States Power Company in the 1960s. The fuel elements were obtained from The Pennsylvania State University where they had been stored for many years. The fuel pellets in those fuel elements were removed from the original Incoloy cladding and reclad in 3003 aluminum tubes and end caps for use in the experiments reported here. The eight cases in this experiment series were performed in 2024 in the Sandia Critical Experiments (SCX) at the Sandia Pulsed Reactor Facility by varying the number of fuel rods in the critical assembly. The personnel involved in conducting these experiments included David Ames, Elijah Lutz, Beth Hanson, Patrick Ward, Jason Soares, and Augie Chapa from SNL, as well as Mathieu Dupont and B.J. Marshall from ORNL. Case 1 had no tantalum experiment rods. Case 2 had seven tantalum rods in the center of the central test region. Case 3 had 18 tantalum rods in the third hexagonal ring of the central test region. Case 4 had 19 tantalum rods in the center of the central test region. Case 5 had 30 tantalum rods in the outer most positions of the central test region. Case 6 had 37 tantalum rods in the center of the central test region. Case 7 had 61 tantalum rods in the center of the central test region. Case 8 had 85 tantalum rods filling all positions in the central test region. All eight critical experiments are judged to be acceptable as benchmark experiments.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Thermal Modelling of Advanced Test Reactor Fuel in a Generalized Dry Storage System

Star-CCM+, a computational fluid dynamics (CFD) software was used to conduct modeling and simulation of the thermal performance of a dry storage configuration consisting of Department of Energy Standardized Canisters (DOESCs) loaded with aluminum-clad spent nuclear fuel (ASNF.) The configuration includes nine DOESCs loaded with Advanced Test Reactor ASNF contained within a stainless steel overcanister centered in a ventilated, concrete overpack. The simulations were used to estimate the maximum temperatures reached by backfill gases inside the overcanister and DOESCs.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Reactor and fuel cycle performance of light water reactor fuel with 235 U enrichments above 5%

Recent advances in nuclear fuel materials research, particularly on the topic of accident-tolerant fuels, have brought up potential opportunities for expanding the operating envelope of existing light water reactors. As many of the performance improvements offered by these technologies may be most fully realized by increasing fuel enrichment beyond the standard 5% limit, this paper examines the potential reactor performance and fuel cycle performance of low-enriched uranium oxide fueled light water reactors by generically considering pressurized water reactors with 235 U enrichment from 5 to 7%. Advanced cladding, including accident-tolerant cladding, has the potential to increase fuel burnup limits related to hydrogen in the cladding that coincide with those limits associated with end-of-life reactivity. Therefore, higher enrichment will be necessary in order to realize the higher fuel burnups. This work includes evaluation of the fuel cycle length, discharge burnup, reactivity coefficients, and fuel cycle performance, including radioactive waste and environmental impact metrics per unit energy generated. The analysis was performed using the evaluation metrics from the US Department of Energy Office of Nuclear Energy Fuel Cycle Evaluation and Screening Study. The reactor performance and safety analysis show that enrichments between 5 and 7% would have similar fuel temperature and moderator temperature coefficients. However, the soluble boron coefficient would decrease in magnitude, requiring more corrosive boric acid in the coolant or other methods of reactivity control during the fuel cycle. At these higher enrichments the maximum burnup at the rim of the fuel pellet would increase by almost a factor of two, which is expected to impact the formation of high-burnup structure in the fuel and the corresponding thermo-mechanical fuel properties. The fuel cycle performance assessment shows that increasing enrichment reduces the quantity of high-level waste disposed per unit energy generated, but it increases the natural resource requirements normalized to a gigawatt-electricity-per-year basis. Another impact is the slightly higher discharge burnup, resulting in somewhat different activity levels of the spent nuclear fuel and high-level waste radioactivity at 100 and 100,000 years after fuel discharge. The environmental impacts—including land use, water use, carbon emission, and radiological exposure—are of the same magnitude per unit energy generated. Finally, however, the impacts are distributed differently. Less than 5% enrichment has marginally more impact on the back-end of the fuel cycle, and greater than 5% enrichment has marginally more impact on the front-end of the fuel cycle. Ultimately, no neutronic or reactor safety hindrances to employing light water reactor fuel with enrichments greater than 5% are identified; given the achievable reactor performance benefits with advanced fuels, further practical exploration of increased enrichment fuel is recommended.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Demonstration of new fracture criteria based on micro-structure and compare to empirical model and measurements

The US nuclear industry is currently exploring extending the peak rod average burnup limits above the current regulatory limit of 62 GWd/tU. A potential concern for fuel exceeding the burnup limit is the fragmentation during a temperature transient such as a loss-of-coolant accident (LOCA). In the event of cladding failure, the fragmented fuel could relocate and disperse within the reactor. The potential impact of fuel fragmentation, relocation and dispersal (FFRD) on licensing assumptions for burnup extension has focused a great amount of efforts and research on this topic.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal Model for Horizontal In-Water and In-Air Mini-Plate Experiments in the Advanced Test Reactor

Mini-Plate (MP) irradiation tests are a fueled experiment designed for irradiation in multiple test locations in the Advanced Test Reactor (ATR) at the Idaho National Laboratory (INL). MP experiments are considered a non-instrumented drop-in test where small aluminum-clad fuel plate samples are cooled directly by the ATR Primary Coolant System (PCS) water. These fueled experiments contain aluminum-clad fuel mini plates consisting of monolithic U-10Mo. Previous thermal analyses have been documented concerning oxide growth[1] and thermal safety margin[2] for the MP-2 experiment. A thermal analysis has been performed on the MP-2 experiment using a new technique for calculating the necessary time after the experiment has been irradiated and reactor shutdown necessary to not exceed the 95% lower bound blister threshold temperature for the fuel in a horizontal in air configuration. A horizontal in water model has also been analyzed and will be discussed. After the experiment is irradiated in the ATR, it is necessary to calculate the fuel meat temperatures at 12 hours after shutdown. This is done to assure that at the 12 hour mark, if this experiment is removed from the reactor and accidentally dropped onto the working tray and is in the most severe geometrical configuration of horizontal (minimum heat transfer) that fission products will not be released. The blister threshold temperature is considered this safety limit. The horizontal in air analysis is also performed considering that the experiment is horizontal in a drained canal and filled with air and natural convection heat transfer with air on the outside. The initial mini-plate testing campaign known as MP-1 [3] has been irradiated and its purpose was to form the base fuel specimens fabricated by various processes so that a single process can be down-selected for qualification. MP-2 will then serve to populate a comprehensive fuel performance data set for the down-selected fabrication process. The MP-2 experiment will be irradiated in several locations of the ATR as shown in Figure 1. The fuel plate thickness and geometry is identical to the MP-1 experiment [3], with the only variable being the fuel meat thickness. This model of the B-12 position is treated as encompassing the I-21, I-24, and B-9 positions since it has more fuel and higher total heat than the other positions. Since the blister threshold temperature is a function of fission density, a series of fission densities is calculated for the B-12 position to cover the other three positions. The B 12 position specifically uses fuel meat that is 0.016 in thick by 3.25 in long and 0.75 in tall. The total plate thickness is 0.050 in. Aluminum cladding forms the barrier between the PCS and the fuel meat. The purpose of this paper is to demonstrate this new technique developed to calculate the necessary decay time after shutdown for a series of fission densities using the ABAQUS [4] finite element and heat transfer code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗