Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 685 records · Page 38

Effect of Si impurities on microstructure and tensile properties of a cast Al-Mg-Fe alloy

Al-Mg alloys are attractive for structural castings owing to their superior strength and ductility in the as-cast state. However, given the tight tolerance for impurities, Al-Mg alloys produced from secondary sources still face multiple challenges. Here, we report the effect of increased Si impurity (0.05–1.6 wt%), which is commonly found in secondary Al sources, on microstructure and tensile properties of a cast Al-4.3Mg-1.6Fe (wt%) alloy, commercially referred to as Castaduct-42 alloy. Microstructural characterization revealed that Si addition increased the volume fraction, size, and aspect ratio of primary Al13Fe4 intermetallic particles as well as the volume fraction of other binary and ternary eutectic phases. Tensile testing results demonstrated that increasing Si impurities from 0.05 to 1.6 wt% reduced ductility from 14.3 ± 1.4 % to 2.2 ± 1.0 %. A particle cracking damage accumulation model coupled with failure analysis indicated primary Al13Fe4 intermetallic particles to be the major contributing factor to the deterioration in ductility with increasing Si content. Additionally, the stabilizing effect of Si on primary Al 13 Fe 4 was inconsistent with the CALPHAD calculation results based on existing CALPHAD databases which predict a slightly decreasing primary Al13Fe4 phase fraction with increasing Si concentration. This work provides new insights into the phase stability and mechanical behavior of the lesser studied Al-Mg-Fe-Si alloy system that will contribute to the development of sustainable cast Al-Mg based alloys.

36 MATERIALS SCIENCE↗

Application of Nano-Indentation Test in Estimating Constituent Phase Properties for Microstructure-Based Modeling of Multiphase Steels

For multiphase advanced high strength steels (AHSS), the constituent phase properties play a crucial role in determining the overall mechanical behaviors. Therefore, it is important to accurately measure/estimate the constituent phase properties in the research of AHSS. In this study, a new nanoindentation-based inverse method that we developed was adopted in estimating the phase properties of a low alloy Quenching and Partitioning (Q&P) steel. A microstructure-based Finite Element (FE) model was also generated based on the Electron BackScatter Diffraction (EBSD) and Scanning Electron Microscopy (SEM) images of the Q&P steel. The phase properties estimated from nanoindentation were first compared with those estimated from in-situ High Energy X-Ray Diffraction (HEXRD) test and, then, employed in the generated FE model to examine whether they can be appropriately used as the input properties for the model. The results show that the estimated phase properties from the inverse method are similar to those from HEXRD, and that the Ultimate Tensile Strength (UTS) and Uniform Elongation (UE) predicted from the FE model based on the estimated phase properties are also similar to those of tensile experiment of the Q&P steel. Based on the results in this study, the nanoindentation-based inverse method appears to be a viable way in determining the phase properties of complex multiphase steels with submicrometer grain sizes.

Cheng, Guang↗

DE-NE0000724 - Research Performance Final Report - Investigation of Thermal Aging Effects on the Evolution of Microstructure and Mechanical Properties of Cast Duplex Stainless Steels

This report details the research activities carried out under DOE-NEUP award number DE-NE0000724 concerning the evolution of structural and mechanical properties during thermal aging of CF–3 and CF–8 cast duplex stainless steels (CDSS). The overall objective of this project was to use state-of-the-art characterization techniques to elucidate trends and phenomena in the mechanical and structural evolution of cast duplex stainless steels (CDSS) during thermal aging. These steels are commonly used as structural materials in commercial light water nuclear power plants, undergoing aging for decades in operation as cooling water pipes, pump casings, valve bodies, etc. During extended exposure to these conditions, CDSS are known to undergo a change in mechanical properties resulting in a loss of ductility, i.e. embrittlement. While it is generally accepted that structural changes within the ferrite phase, such as decomposition into iron (Fe)-rich and chromium (Cr)-rich domains, lead to the bulk embrittlement of the steels, many questions remain as to the mechanisms of embrittlement at multiple length scales. This work is intended to shed insight into the atomic level composition changes, associated kinetic mechanisms, and effects of changing phase structure on micro- and nano-scale deformation that lead to loss of impact toughness and tensile ductility in these steels. In general, this project provides a route to answer some of these major questions using techniques such as 3-dimensional (3-D) atom probe tomography (APT) and real-microstructure finite element method (FEM) modeling, which were not readily available when these steels were originally selected for service in light water reactors. Mechanical properties evaluated by Charpy V-notch impact testing (CVN), tensile testing, and microhardness and nanohardness measurements were obtained for each condition and compared with the initial baseline properties to view trends in deformation behavior during aging. Concurrent analysis of the microstructure and nanostructure by atom probe tomography (APT) and transmission electron microscopy (TEM) provide mechanistic insight into the kinetic and mechanical behavior occurring on the nano-scale. The presence and morphology of the ferrite, austenite, and carbide phases have been characterized, and formation of new phases during aging, including spinodal decomposition products (α- and α'-ferrite) and G-phase, have been observed. The mechanical and structural characterization have been used to create accurate FEM models based on the real micro- and nano-structures of the systems. These models provide new insight into the local deformation behavior of these steels and the effects of each individual phase (including ferrite, austenite, carbides, and spinodal decomposition products) on the evolving bulk mechanical behavior of the system. The project was divided into three major tasks: 1. Initial Microstructure and Mechanical Property Survey and Initiate Heat Treatment; 2. Microstructural Characterization and Mechanical Property Testing During Aging; and 3. Microstructure-based Finite Element Modeling. Each of these tasks was successfully executed, resulting in reliable data and analysis that add to the overall body of work on the CDSS materials. Baseline properties and aging trends in mechanical data confirm prior observations and add new insights into the mechanical behavior of the steels. Structural characterization on multiple length scales provides new information on phase changes occurring during aging and sheds light on the kinetic processes occurring at the atomic scale. Furthermore, a combination of mechanical testing and microstructural characterization techniques was utilized to design FEM models of local deformation behavior of the ferrite and austenite phases, providing valuable new information regarding the effects of each of the microstructural components on the hardening and embrittlement processes. The data and analysis presented in this report and the publication associated with this project (§V) increase the understanding of aging and deformation in CF–3 and CF–8 steels. These results provide valuable information that can be utilized to aid in making informed decisions regarding the ongoing use of these steels in commercial nuclear infrastructure.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Annealing Effects on Microstructure and Mechanical Properties of Ultrafine-Grained Al Composites Reinforced with Nano-Al{sub 2}O{sub 3} by Rotary Swaging

Microstructure evolution and variations in mechanical properties of Al-Al{sub 2}O{sub 3} nanocomposite produced by powder metallurgy were investigated and compared with commercially pure aluminum (Al-1050) after furnace annealing. Fine gas-atomized Al powder compacts were first sintered in flowing nitrogen, subsequently consolidated into wires by rotary swaging and eventually annealed at 300 and 500 °C for 24 h each. Scanning and transmission electron microscopy with energy-dispersive spectroscopy was utilized to document the microstructure evolution. Rotary swaging was proven to lead to a marked decrease in grain size. After heavy swaging to true deformation degree of φ = 6 and annealing at 500 °C, obvious recrystallization was observed at Al-1050’s existing grain boundaries and the crystals began to grow perpendicular to the flow direction. In the Al-Al{sub 2}O{sub 3} nanocomposite, fabricated from d{sub 50} = 6 μm Al powder, recrystallization partially occurred, while grains were still extremely fine. Due to the dual role of fine-grained Al{sub 2}O{sub 3} dispersion strengthening, the nanocomposite showed improved mechanical performance in terms of tensile strength, approximately twice higher than Al-1050 after annealing at 500 °C.

36 MATERIALS SCIENCE↗

Effects of transient thermal shock on the microstructures and corrosion properties of a reduced activation high-entropy alloy

The devices would subject transient thermal shocks (TTS) during operation under extremely harsh conditions of nuclear fusion reactors, which inevitably exert significant impact on the microstructure and performance of structural materials. Here, a reduced activation VCrFeTa 0.2 W 0.2 high-entropy alloy (HEA) was developed by vacuum arc melting. The effects of electron beam induced TTS on its microstructure, microhardness, and corrosion properties were investigated. The results indicate that the weight fraction of each phase changes after TTS, showing a significant decrease in the content of BCC1 phase and an increase in the content of BCC2 and Laves phases. The content of BCC1 phase continues to decrease slightly with increasing the power of TTS. Besides, the microhardness of the alloy increases from ~673 HV to ~714 HV after TTS treatments. In the reduced activation HEA, TTS results in a relatively low corrosion current density of ~0.472 μA/cm 2 in 3.5 wt% NaCl solution, around one-third of the current density observed in the as-cast sample. Furthermore, the VCrFeTa 0.2 W 0.2 HEA after TTS exhibits a pitting potential of ~1.165 V SCE , which is much higher than that of the as-cast sample. The refined composite multiscale entropy method is employed to analyze the influence of TTS on current fluctuation behavior during the corrosion process. The reduced activation VCrFeTa 0.2 W 0.2 HEA exhibits excellent properties in harsh environments after TTS, thereby showing advantageous property in the field of nuclear structural materials. Furthermore, TTS is an efficient and controllable strategy for the improvement of the HEAs’ microstructures and performances.

36 MATERIALS SCIENCE↗

Effect of deposition rate on microstructure and mechanical properties of 17-4 PH stainless steel fabricated by laser engineered net shaping

Laser engineered net shaping (LENS) is an additive manufacturing technique for fabricating and repairing metallic components. However, the relationships between its process parameters and the resulting mechanical properties of alloys such as 17-4 precipitation-hardening (PH) stainless steel require further investigation to enable reliable application. This study examines the specific effect of LENS deposition rate on the microstructure and mechanical properties of 17-4 PH stainless steel. Specimens were fabricated at two different deposition rates (8.47 and 9.31 mm s−1), subjected to subsequent solution and H900 aging treatment, and then evaluated via tensile testing, hardness measurements, and microscopy. A higher deposition rate results in a finer grain structure but increased porosity, leading to greater ultimate tensile strength (∼1294 MPa) yet lower ductility (strain at failure ∼5.8%) compared to the slower deposition rate (∼1266 MPa, ∼9.0% strain). Hardness follows the same trend as tensile strength. Tensile fracture surfaces for both conditions exhibited a mixed mode of ductile dimples and brittle quasi-cleavage regions, with chromium/silicon oxide particles identified within dimples. Complementary finite element modeling indicates that small void fractions primarily reduce ductility by enhancing localized plasticity, with only a marginal decrease in tensile strength. These integrated experimental and numerical results elucidate the mechanical properties linked to deposition rate, providing insight into tailoring LENS processes to achieve desired properties of 17-4 PH stainless steel.

17-4 PH stainlesssteel↗

Microstructure and mechanical properties of friction stir welded Haynes 282

Advanced ultrasupercritical (A-USC) steam plants are designed to operate at high temperatures and pressures due to the necessity for higher operational efficiency. The extreme operating conditions of A-USC requires the deployment of precipitation strengthened Ni-base alloys that exhibit elevated temperature strength and good fabricability. Fusion welding of precipitation strengthened nickel alloys lead to solidification cracking in fusion zone and/or liquation cracking in heat affected zone. Therefore, an alternative non-melting welding technique is a necessity to efficiently join nickel alloys. In the current study, friction stir welding, a solid state joining technique was implemented on a precipitation strengthened nickel-based superalloy, Haynes 282. Detailed microstructural and mechanical properties characterization was carried out. The processed region exhibited wrought, fine-grained microstructure, absence of weld defects such as voids and cracks and absence of elemental segregation. Both hardness and cross-weld tensile tests demonstrated that the weld region was stronger than the base material. And the cross-weld tensile samples failed in the base material. Based on joint efficiency analysis, friction stir welded Haynes 282 outperformed fusion welds.

36 MATERIALS SCIENCE↗

Property evaluation and microstructure characterization of the A3-3 matrix graphite - 18440

Spherical fuel elements with TRISO fuel will be used in the pebble-bed high temperature gas-cooled nuclear reactor. The fuel will be located within the center region of the elements, and will be suspended in, and surrounded by a shell of matrix graphite. The matrix graphite provides structural support to the fuel, prevents fuel damage, and allows for heat transfer from the fuel to the coolant. The raw materials for the matrix graphite, type A3-3, includes 64 wt% natural flake graphite, 16 wt% artificial graphite and 20 wt% phenol resin binder. After the final heat treatment, the resulting A3-3 matrix is composed of 71 wt% natural graphite, 18 wt% artificial graphite, and 11 wt% phenol resin-derived coke carbon. The microstructure of A3-3 matrix graphite has direct influences on the material properties, which are crucial to maintaining the integrity and safety of the fuel elements. This presentation will discuss microstructure features, such as lattice, and crystal parameters, porosity, pore size and distribution, and anisotropy. The multiple physical, mechanical and thermal properties of this material, including: elastic modulus, mechanical strength, and oxidation property will also be presented. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Integrated Predictive Tools for Customizing Microstructure and Material Properties of Additively Manufactured Aerospace Components

Additive Manufacturing (AM) refers to a process by which digital three-dimensional (3-D) design data is converted to build up a component by depositing material layer-by-layer. United Technologies Corporation (UTC) is currently involved in fabrication and certification of several AM aerospace structural components made from aerospace materials. This is accomplished by using optimized process parameters determined through numerous design-of-experiments (DOE)-based studies. Certification of these components is broadly recognized as a significant challenge, with long lead times, very expensive new product development cycles and very high energy consumption. Because of these challenges, United Technologies Research Center (UTRC), together with UTC business units have been developing and validating an advanced physics-based process model. The specific goal is to develop a physics-based framework of an AM process and reliably predict fatigue properties of built-up structures as based on detailed solidification microstructures. Microstructures are predicted using process control parameters including energy source power, scan velocity, deposition pattern, and powder properties. The multi-scale multi-physics model requires solution and coupling of governing physics that will allow prediction of the thermal field and enable solution at the microstructural scale. The state-of-the-art approach to solve these problems requires a huge computational framework and this kind of resource is only available within academia and national laboratories. The project utilized the parallel phase-fields codes at Oak Ridge National Laboratory (ORNL) and Lawrence Livermore National Laboratory (LLNL), along with the high-performance computing (HPC) capabilities existing at the two labs to demonstrate the simulation of multiple dendrite growth in threedimensions (3-D). The LLNL code AMPE was used to implement the UTRC phase field model that was previously developed for a model binary alloy, and the simulation results were compared against the UTRC simulation results, followed by extension of the UTRC model to simulate multiple dendrite growth in 3-D. The ORNL MEUMAPPS code was used to simulate dendritic growth in a model ternary alloy with the same equilibrium solidification range as the Ni-base alloy 718 using realistic model parameters, including thermodynamic integration with a Calphad based model for the ternary alloy. Implementation of the UTRC model in AMPE met with several numerical and parametric issues that were resolved and good comparison between the simulation results obtained by the two codes was demonstrated for two dimensional (2-D) dendrites. 3-D dendrite growth was then demonstrated with the AMPE code using nondimensional parameters obtained in 2-D simulations. Multiple dendrite growth in 2-D and 3-D were demonstrated using ORNL’s MEUMAPPS code using simple thermal boundary conditions. MEUMAPPS was then modified to incorporate the complex, time-dependent thermal boundary conditions obtained by UTRC’s thermal modeling of single track AM experiments to drive the phase field simulations. The results were in good agreement with UTRC’s experimental measurements.

36 MATERIALS SCIENCE↗

Effect of polycyclosilane microstructure on thermal properties

Thermal characterization of polysilanes has focused on the influence of organic side chains, whereas little is understood about the influence of silane backbone microstructure on thermal stability, phase properties, and pyrolysis. To address this knowledge gap, we prepared three distinct polycyclosilanes: linear polymers synthesized from the cyclosilane building blocks 1,4Si 6 and 1,3Si 6 , as well as a cyclic polymer of 1,3Si 6 . Thermal properties across the temperature range 25 to 600 °C were investigated using differential scanning calromietry (DSC) and thermogravimetric analysis (TGA). We found differences between linear and cyclic materials, including a phase transition unique to the cyclic polymer and lower rates of mass loss during pyrolysis. Density functional theory (DFT) calculations provided insight into microstructure-dependent pyrolysis.

36 MATERIALS SCIENCE↗

Effect of cooling conditions on microstructure and mechanical properties of friction stir welded 7055 aluminium alloy joints

Highlights: • Water cooling improves tensile properties of friction stir welded 7055 Al alloy. • Water cooling results in smaller grains and second phase in nugget zone. • Water cooling results in finer second phase in thermos-mechanically affected zone. • Water cooling results in finer second phase in heat affected zone. • Fracture surface is flat for air-cooled joint but zig-zag for water-cooled one. - Abstract: The microstructure and mechanical properties of friction stir welded 7055 aluminium alloy under air cooling and water cooling were investigated by means of hardness and tensile testing, optical microscopy and transmission electron microscopy. Water cooling results in reduced softening in the weld zone and therefore higher tensile strength compared to air cooling. Fracture generally occurs within the thermo-mechanically affected zone (TMAZ) and heat affected zone (HAZ) on the retreating side in joints welded under air cooling but shifts towards the TMAZ and nugget zone (NZ) in the joints welded under water cooling. The fracture surfaces are generally flat for the air-cooled joint, but exhibits a zig-zag feature for the water-cooled joint. The mechanical behaviour of the weld has been discussed in light of the change in grain structure and precipitation in the NZ, TMAZ and HAZ caused by cooling conditions.

36 MATERIALS SCIENCE↗

The Effect of SiC Addition on Microstructure and Mechanical Properties of Gas Tungsten Arc-Welded Ti-6Al-4V Alloy

In the present study, SiC powder was added in situ for bead-on-plate weldments and fusion butt joints to modify the microstructure and the corresponding mechanical properties. Cross sections of bead-on-plate welds demonstrated that the SiC addition resulted in significant changes of the titanium microstructure. Specifically, a fine lamellar structure of α-phase with a small amount of intergranular β-titanium within the fusion zone could be established. Moreover, the size of prior β-grains was significantly reduced. After welding, no intermetallic silicides were observed. In the fusion zone of the SiC-enhanced samples, a small increase in hardness resulted, and the samples showed an increase in tensile strength, yield strength and elongation.

36 MATERIALS SCIENCE↗

Interconnection of thermal parameters, microstructure and mechanical properties in directionally solidified Sn–Sb lead-free solder alloys

Considerable effort is being made to develop lead-free solders for assembling in environmental-conscious electronics, due to the inherent toxicity of Pb. The search for substitute alloys of Pb–Sn solders has increased in order to comply with different soldering purposes. The solder must not only meet the expected levels of electrical performance but may also have appropriate mechanical strength, with the absence of cracks in the solder joints. The Sn–Sb alloy system has a range of compositions that can be potentially included in the class of high temperature solders. This study aims to establish interrelations of solidification thermal parameters, microstructure and mechanical properties of Sn–Sb alloys (2 wt.%Sb and 5.5 wt.%Sb) samples, which were directionally solidified under cooling rates similar to those of reflow procedures in industrial practice. A complete high-cooling rate cellular growth is shown to be associated with the Sn–2.0 wt.%Sb alloy and a reverse dendrite-to-cell transition is observed for the Sn–5.5 wt.%Sb alloy. Strength and ductility of the Sn–2.0 wt.%Sb alloy are shown not to be affected by the cellular spacing. On the other hand, a considerable variation in these properties is associated with the cellular region of the Sn–5.5 wt.%Sb alloy casting. - Graphical abstract: Display Omitted - Highlights: • The microstructure of the Sn–2 wt.%Sb alloy is characterized by high-cooling rates cells. • Reverse dendrite > cell transition occurs for Sn–5.5 wt.%Sb alloy: cells prevail for cooling rates > 1.2 K/s. • Sn–5.5 wt.%Sb alloy: the dendritic region occurs for cooling rates < 0.9 K/s. • Sn–5.5 wt.%Sb alloy: tensile properties are improved with decreasing cellular spacing.

36 MATERIALS SCIENCE↗

Microstructure and hydrogenation properties of a melt-spun non-stoichiometric Zr-based Laves phase alloy

Alloy with composition of Zr{sub 0.9}Ti{sub 0.1}V{sub 1.7} off normal stoichiometric proportion is selected to investigate the effect of defects introduced by non-stoichiometry on hydrogenation kinetics of Zr–Ti–V Laves phase alloys. Microstructure and phase constituent of melt-spun ribbons have been investigated in this work. The activation process, hydrogenation kinetics, thermodynamics characteristics and hydride phase constituent of as-cast alloy and melt-spun ribbons are also compared. Comparing with the as-cast alloy, the dominant Laves phase ZrV{sub 2} is preserved, V-BCC phase is reduced and α-Zr phase is replaced by a small amount of Zr{sub 3}V{sub 3}O phase in melt-spun ribbons. Melt-spun ribbons exhibit easy activation and fast initial hydrogen absorption on account of the increased specific surface area. However, the decrease in unit cell volume of the dominant phase leads to the decrease in hydrogen absorption capacity. Melt-spinning technique raises the equilibrium pressure and decreases the stability of hydride due to the decrease of unit cell volume and the elimination of α-Zr phase, respectively. Melt-spun ribbons with fine grains show improved hydrogen absorption kinetics comparing with that of the as-cast alloy. Meanwhile, the prevalent micro twins observed within melt-spun ribbons are believed to account for the improved hydrogen absorption kinetics. - Highlights: • Role of defects on hydrogenation kinetics of Zr-based alloys is proposed. • Microstructure and hydrogenation properties of as-cast/melt-spun alloy are compared. • Melt-spinning technique improves the hydrogenation kinetics of Zr{sub 0.9}Ti{sub 0.1}V{sub 1.7} alloy. • Refined grains and twin defects account for improved hydrogen absorption kinetics.

36 MATERIALS SCIENCE↗

The Effects of Low Frequency on the Microstructure and Mechanical Properties of High-Strength Al-Mg Aluminum Alloys by Wire and Double-Pulsed Arc Additive Manufacturing

An innovative and high deposition efficiency process, the double-pulsed arc additive manufacturing process, is used to produce high-strength Al-Mg wall components. This dissertation investigates the electrical parameter acquisition, bead appearance, porosity morphology, microstructure and mechanical properties of additively manufactured high-strength Al-Mg wall components and how these are affected by the low frequency of the double-pulsed arc additive manufacturing process. Then, using this process at different low frequencies of 0, 1, 3, 5, 7 and 9 Hz, multilayer deposition experiments were performed. It can be observed that the deposit porosity is obviously eliminated compared with cold metal transfer (CMT) process. The bead appearance of the deposited aluminum wall varies clearly with low frequencies, and at a low frequency of 3 Hz, its appearance is the best of all. The optical observation of microstructure proves that the average grain size varies significantly with low frequency, and at a low frequency of 1 Hz, it is the smallest. In addition, the deposited wall showed maximum mean microhardness and maximum ultimate tensile strength at a low frequency of 3 Hz. Considering the deposited porosity and mechanical priorities, double-pulsed arc additive manufacturing with a frequency of 3 Hz is more suitable for making high-strength Al-Mg wall components than at other low frequencies.

36 MATERIALS SCIENCE↗

Modulation of microstructure and optical properties of Mo-doped ZnO thin films by substrate temperature

Highlights: • Mo-doped ZnO films are obtained by sputtering at various substrate temperatures. • High-quality MZO thin films with good crystalline have been obtained at 200 °C. • Deposition temperature affects the amount of defects in the crystalline structure - Abstract: Mo-doped ZnO(MZO) films were deposited on Si (1 1 1) substrates by radio frequency sputtering at different substrate temperatures of 200, 300 and 400 °C. The effect of the substrate temperature on the structural and optical properties of the MZO films has been investigated. X-ray diffraction results reveal that all the films are polycrystalline with a hexagonal wurtzite structure with a preferential orientation according to the direction (0 0 2) plane. The crystallinity and surface morphologies of the films are strongly dependent on the growth temperature, which in turn exerts a great effect on microstructural and optical properties of the MZO films. The optical absorption measurements show high ultraviolet (UV) absorbance property of MZO with sharp and intense absorption band in this region and the optical band gap (E{sub g}) are 3.18, 3.22, 3.25 and 3.21 eV for the films deposited at room temperature, 200, 300 and 400 °C. The photoluminescence (PL) intensity of a strong broad violet–blue emission from MZO nanostructures with increasing deposited temperature was also observed. X-ray photoelectron spectroscopy (XPS) was employed to investigate the surface chemical composition of growth products.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of diffusion bonded W/steel joint using V/Ni composite interlayer

Diffusion bonding between W and steel using V/Ni composite interlayer was carried out in vacuum at 1050 °C and 10 MPa for 1 h. The microstructural examination and mechanical property evaluation of the joints show that the bonding of W to steel was successful. No intermetallic compound was observed at the steel/Ni and V/W interfaces for the joints bonded. The electron probe microanalysis and X-ray diffraction analysis revealed that Ni{sub 3}V, Ni{sub 2}V, Ni{sub 2}V{sub 3} and NiV{sub 3} were formed at the Ni/V interface. The tensile strength of about 362 MPa was obtained for as-bonded W/steel joint and the failure occurred at W near the V/W interface. The nano-indentation test across the joining interfaces demonstrated the effect of solid solution strengthening and intermetallic compound formation in the diffusion zone. - Highlights: • Diffusion bonding of W to steel was realized using V/Ni composite interlayer. • The interfacial microstructure of the joint was clarified. • Several V–Ni intermetallic compounds were formed in the interface region. • The application of V/Ni composite interlayer improved the joining quality.

36 MATERIALS SCIENCE↗

Effects of Bi-Sb Addition and Solution Treatment on Microstructures and Mechanical Properties of Al-20 wt.% Mg{sub 2}Si Composites

In this study, the effects of compound modification with Bi and Sb and solution treatment on the microstructures evolution and the mechanical properties of Al-20 wt.% Mg{sub 2}Si composites were investigated. The specimens were observed by optical microscope, scanning electron microscope equipped with an energy-dispersive spectrometer and x-ray diffraction. The characterization results showed that 2.0 wt.% Sb and 0.2 wt.% Bi addition refined the primary Mg{sub 2}Si from 95 to 10 μm, accompanied by a change in morphology from coarse dendrites to dispersive fine polygons. After solution treatment at 540 °C for 15 h, the sharp polygonal primary Mg{sub 2}Si particles were blunted and the flake-like eutectic Mg{sub 2}Si phases were changed to small spherical particles, resulting in the increase in the Brinell hardness of the composites from HB 94.53 to 134.67. Mechanical tests revealed that both tensile strength and hardness of the composite were improved by compound modification with Bi and Sb, and the ultimate tensile strength (UTS) was increased from 216 MPa unmodified to 257 MPa with optimum modification of 2 wt.% Sb and 0.2 wt.% Bi. A propounded change in hardness from HB 94.53 to 130.67 was also investigated.

36 MATERIALS SCIENCE↗