In-situ high-energy X-ray diffraction and crystal plasticity modeling to predict the evolution of te
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Here, in this study, we demonstrate that spatially resolved cooling curves derived from real-time infrared (IR) thermography during additive manufacturing (AM) can capture spatial variations in phase transformation temperatures through cooling curve analysis (CCA). Using this approach, we show that during laser hot-wire deposition of 410 stainless steel (410SS), the martensite start temperature (M s ) evolves dynamically throughout the build. The M s temperature is spatially nonuniform, ranging from 185 °C to 348 °C, with the lowest values toward the build center and higher values toward the upper region of the deposit. In the lower portion of the build, no M s inflection is detected via CCA, consistent with transformation occurring earlier during thermal cycling followed by tempering during subsequent thermal cycles. These trends in M s are corroborated by characterizing the microstructure by electron backscatter diffraction (EBSD). Traditionally, M s is assumed to be constant, and a single interpass temperature is applied during both deposition and residual stress modeling. Our results demonstrate that IR-derived cooling curves provide a route to spatially and temporally resolved transformation temperature tracking for dynamic interpass control and improved residual-stress modeling.
The project aimed to develop and characterize an optical pressure sensor capable of withstanding high temperatures, up to 1000 °C. Survivability in harsh environments was enabled using sapphire for both the substrate and the optical fibers, therefore mitigating thermal expansion mismatch. Such material cannot be machined through conventional microfabrication techniques, and unique additive and subtractive methods had to be studied and implemented. Subtractive methods included laser-machining the sapphire substrate using a picosecond laser machining tool. At first, the parameters of importance were theoretically and experimentally evaluated such that the fluence, the pulse spacing, and the number of passes were found to strongly influence the laser ablation process. A simulation tool was designed to predict the final pattern when inputting a set of parameters and a profile. This model was complemented with laser ablation material physics models and Bayesian uncertainty analysis for one dimensional and three dimensional ablation processes. An additive process called thermocompression bonding was studied in order to seal the diaphragm substrate to the back cavity. At first, bonding strength using this technique was examined using the chevron-notch method that allow to determine the fracture toughness of this bond. This parameter is independent of the geometry used and therefore can be extended to other geometries used in actual sensor bonding. A theoretical and experimental study of internal damage caused by the laser micromachining of the sapphire material was carried out. The research identified enhanced strength and fracture toughness along laser ablated surfaces. This was determined using bend bar specimens and Vicker’s microindentations. Softening of the plasticity behavior (as indicated by nanoindentation experiments) was also investigated using finite deformation plasticity modeling via a contact mechanics finite element simulation. Good correlations between experiments and the model were achieved to determine material parameters that can be used in future MEMS based sensor design and modeling to minimize sensor failure loads. The enhanced strength and fracture toughness was determined to be due to compressive residual stress near laser ablated surfaces. This was confirmed through x-ray spectra taken along different crystal structure planes in combination and Bayesian uncertainty analysis. The Bayesian analysis inferred the entire residual strain tensor (six components) and the residual stress tensor. The results illustrated compressive in-plane stress was the most likely cause of enhanced strength and toughness after laser machining. Due to major equipment failures, a parallel route for fabricating the sensor was taken, using commercially available sapphire removal method (subtractive) and ceramic adhesive bonding (additive). The fully-packaged sensor utilized laser micromachining for the sapphire substrate fabrication and was comprised only of high-temperature-compatible materials. Calibration tests of the sensor in both room-temperature and high-temperature plane-wave tubes showed good linearity and consistent frequency response, in the tested frequency range. The sensor also showed good thermal stability in tests up to 300 °C, proving the fiber-optic lever and its packaging process to be a promising approach for high-temperature measurements. The calibration from 23 °C to 300 °C gave a raw sensitivity of 3.9 × 10 -7 V/Pa and a normalized sensitivity of 9.8 × 10 -8 Pa -1 which were consistent within the temperature range. The sensor had a resonance at 16.3 kHz and a flat band (±3 dB) up to 10.3 kHz. The noise floor of the sensor at 1 kHz was 316 nV/Hz 1/2 , resulting in a MDP of 0.8 Pa. Previously, diaphragm delamination due to CTE mismatch was found at 500 °C, causing packaging failure. Unfortunately high temperature validation in hot jet environment could not be made in time. In the future, it is suggested that the two sapphire substrates be bonded by thermal compression bonding with an intermediate platinum layer instead of using an alumina-based adhesive, and therefore achieve higher temperature capacity up to 1000 °C.
The U.S. DOE has designed four spent nuclear fuel (SNF) dry storage canisters for storing DOE standardized SNFs. The DOE standard canisters are cylindrical shells with a diameter of 24 inches (610 m) or 18 inches (457 m), a wall thickness of 0.5 inches (12.7 m) or 0.375 inches (9.53 m), and a length of 15 feet (4.57 m) or 10 feet (3.05 m). These DOE canister geometries are completely different from commercial canisters. The latter may experience chloride-induced stress cracking corrosion (CI-SCC) because they are stored near coastal regions. The former may not experience CI-SCC but face different challenges because they are stored in the SNF storage facilities. Because of large residual stresses, mechanical flaws may occur in the DOE canisters during long-distance transportation or lifting handling. To date, only limited structural integrity analyses were carried out through drop tests on the DOE canisters, but a more general flaw tolerance assessment has not been performed. Therefore, the failure assessment diagram (FAD)-based fracture mechanics method, as codified by the latest API 579-1/ASME FFS-1-2021 Edition, is adopted in this work to assess surface flaw tolerance for DOE canisters under operation loading and welding residual stresses (WRS), where the new code-recommended WRS distributions are used. To more adequately consider the transverse distribution of WRS, an equivalent WRS distribution is proposed to account for the WRS reduction with distance from the weld centerline. Moreover, the closed-form solutions of stress intensity factor K, which serves as the crack driving force during subcritical crack growth, are developed from the tabular data of the K factors provided in API 579-1/ASME FFS-1 and used to determine more accurate flaw sizes at flaw instability. Subsequently, the Level 2 assessment procedures with 12 assessment steps, as codified and detailed in API 579-1 and ASME FFS-1, are followed to assess the flaw tolerance for the surface flaws in the DOE standard canisters with consideration of normal or accident operation loads combined with WRS. The assessment results show that the four designs of DOE standard canisters can tolerate all surface flaws that meet the code permitted maximum sizes of a flaw length of 8 inches (i.e., 200 mm) and a flaw depth of 80% wall thickness. This demonstrates that all designs of DOE standard canisters are robust and reliable.
Several new results on the physics linking edge poloidal flows to turbulent momentum transport are reported. These are based on experiments on the HL-2A tokamak. Significant deviation from the neoclassical prediction for mean poloidal flow in Ohmic and electron cyclotron resonance heating (ECRH) heated L-mode discharges is derived from direct measurement of the turbulent Reynolds stress. The deviation increases prominently with ECRH power. The turbulent poloidal viscosity is synthesized from fluctuation data, and is found to be comparable to the turbulent particle diffusivity. The intrinsic poloidal torque characterized by the divergence of the non-diffusive residual stress is deduced from synthesis for the first time in a tokamak plasma. Experimental evidence which demonstrates the dynamics of spectral symmetry breaking in drift wave turbulence is in good agreement with the development of the poloidal torque. Finally, taken together, these results elucidate the connections between power injection, turbulence development, pressure gradient and residual stress from symmetry breaking.
Directed energy deposition (DED) based remanufacturing leverages the flexibility of additive manufacturing to add value to broken or worn components. DED offers the ability to repair cast iron, a material difficult to repair with traditional welding techniques. Despite this, development of appropriate DED process conditions for bimetallic cast iron structures lags low- and medium-carbon steel repair. Thermal stresses and porosity generated by high-temperature deposition on cast iron often lower mechanical properties and hinder the qualification process. In this report scanning speed, powder mass flow rate, and stepover width are studied in multiple-track structures deposited on gray cast iron. Dilution and residual stresses are found to be highly dependent on the selected process parameters. Samples with a higher volumetric energy input, e.g., slower scanning speeds and higher powder feed rates, showed improved density and lower residual stresses but suffered lower dilution into the substrate. The presented conditions further the development of additive manufacturing technologies for automotive repair.
Chromium deposited by high-power impulse magnetron sputtering (HIPIMS) versus cathodic arc (CA) processes exhibits very different mechanical properties. Combining the two can result in a single-phase with superior performance that can be tailored for use in coating SiC for advanced nuclear fuel cladding. Coating morphology, residual stress, elemental depth profiles, and mechanical testing by scratch, pull-off adhesion, and microcantilevers are shown for HiPIMS, CA, and combined coatings. CA coatings were likely to spall and had lower adhesion strength due to tensile residual stresses but had desirable material properties. Additionally, by depositing an initial layer of Cr by HiPIMS followed by a layer of Cr by CA, a more adherent coating was achieved and some of the stress issues with CA morphology were resolved. Combined coatings withstood at least 80 MPa in pull-off adhesion tests and had maximum failure stress values of 5GPa in microcantilever tests. These results were better than either individual deposition method and point to a hybrid approach being a path forward for a more robust coating.
Tristructural isotropic (TRISO)–coated particle fuel is a proposed fuel for multiple advanced reactor concepts. The performance of the particle depends on whether the silicon carbide (SiC) layer remains intact to prevent the release of metallic and gaseous fission products. Mechanical fracture of the SiC layer is a potential failure mode under various fuel configurations and operating environments, including the potential transmission of matrix-originating cracks through TRISO particles. Furthermore, this study uses instrumented indentation techniques on cross-sectioned surrogate particles to examine the mechanical stability of the critical interface between SiC and the outer pyrolytic carbon (OPyC) layer. The observed behavior at the interface is rationalized by examining the radially dependent fracture behavior of the SiC layer and performing a numerical analysis to quantify the residual stresses that develop during the processing and cross-sectioning of the as-fabricated particle. Characterizing the SiC-OPyC interface of surrogate TRISO particles using nanoindentation provides unique insight into the interface's room-temperature residual stress and mechanical stability. The modeling efforts were used to investigate the experimental procedure further, and the results are presented herein to validate this fuel form's potential mechanical failure modes.
This is the dataset associated with the 2022 SRP Additive Manufacturing Prediction Challenge, originally hosted on Github at https://github.com/SRP-AM/SRP_AM_Prediction_Challenge. The benchmark was designed for validating prediction for the temperature history, residual stress, and distortion of an additively manufactured metal part with relatively simple geometry. A calibration problem with the same as-built geometry is provided with measured quantities of interest; including temperature histories at selective locations, post-build residual stress at selective locations, and overall distortion measurements. The challenge problem is presented with a different build sequence (i.e. thermal history). In this dataset, we include the actual recorded calibration and challenge measurements, as well as benchmark template files for testing predictions without incorporating the challenge data. Supplementary files around the materials and setup are available for transparency and reproducibility.
The potential for stress corrosion cracking (SCC) of welded stainless-steel interim storage containers for spent nuclear fuel (SNF) has been identified as a high priority data gap. This paper presents a fusion welding process that was developed for SNF canister repair. Submerged arc welding (SAW) was developed to weld 12.7 mm (0.5 in.) thick 304L stainless steel plates to simulate the initial welds on SNF canisters. The SAW procedure was qualified following ASME Boiler and Pressure Vessel Code requirements. During SAW, the welding temperature was recorded at various locations by using thermocouples. After SAW, weld microstructures were characterized, joint mechanical properties were tested, and the maximum tensile residual stress direction was identified. After SAW procedure qualification, artificial cracks were excavated perpendicular to the maximum tensile residual stress direction in the SAW heat affected zone. Machine cold-wire gas tungsten arc welding (CW-GTAW) was developed and used for repair welding at cracked locations.
An intrinsic feature of disordered and out-of-equilibrium materials, such as glasses, is the dependence of their properties on their history. An important example is rheological memory, in which disordered solids obtain properties based on their deformation history. Here, in this study, we employ x-ray photon correlation spectroscopy with in situ rheometry to characterize memory formation in a nanocolloidal soft glass due to cyclic shear. During a cycle, particles undergo irreversible displacements composed of a combination of shear-induced diffusion and heterogeneous, residual strain fields. At lower shear amplitudes, the displacements resemble a random walk in which the directions in each cycle are independent of those in preceding cycles, while at high amplitude, the irreversible displacements in consecutive cycles become correlated. The magnitudes of the displacements decrease with each cycle before reaching a steady state where the microstructure has been trained to achieve enhanced reversibility even at shear amplitudes well above yielding and despite the presence of thermal fluctuations. At amplitudes below and near yielding, these decreases are monotonic, while well above yielding, they are nonmonotonic, suggesting evidence of shear banding. Accompanying this microstructural training are corresponding decreases in the dissipation during each cycle and the magnitude of the residual stress toward steady-state values. Memory of the training is revealed by measurements in which the amplitude of the shear is changed after steady state is reached. The magnitude of the particle displacements, as well as the dissipation and the change in residual stress, vary nonmonotonically with the new shear amplitude, having minima near the training amplitude, thereby revealing correlated microscopic and macroscopic signatures of memory.
A preliminary study on the microstructural characteristics and stress corrosion cracking susceptibility of a friction stir welded (FSW) 304L stainless steel plate was carried out. The weld examined was characterized by several typical microstructural features of friction stir welds including a gradient of dynamically recrystallized microstructure with distinct material flow patterns reflective of the complex distribution of thermomechanical histories. Evidence of process-induced microstructural sensitization was lacking Immersion testing of the friction stir welded plate in boiling magnesium chloride solution indicated the FSW region was more susceptible to SCC than the base 304L material, especially along the weld toes. The microstructural origins of this SCC susceptibility are not clear, but it is likely driven by residual stress imparted by the welding process. Future work will focus on direct examination of the SCC damaged microstructure and residual stress of the weld zone to further clarify the operative characteristics controlling SCC susceptibility.
Localized residual stress and elastic strain concentrations in microelectronic devices often affect the electronic performance, resistance to thermomechanical damage, and, likely, radiation tolerance. A primary challenge for the characterization of these concentrations is that they exist over sub-μm length-scales, precluding their characterization by more traditional residual stress measurement techniques. Here, in this study, we demonstrate the use of synchrotron x-ray-based differential aperture x-ray microscopy (DAXM) as a viable, non-destructive means to characterize these stress and strain concentrations in a depth-resolved manner. DAXM is used to map two-dimensional strain fields between the source and the drain in a gallium nitride (GaN) layer within high electron mobility transistors (HEMTs) with sub-μm spatial resolution. Strain fields at various positions in both pristine and irradiated HEMT specimens are presented in addition to a preliminary stress analysis to estimate the distribution of various stress components within the GaN layer. γ-irradiation is found to significantly reduce the lattice plane spacing in the GaN along the sample normal direction, which is attributed to radiation damage in transistor components bonded to the GaN during irradiation.
The original purpose of this project was to develop a probabilistic model for SCC-induced failure of spent fuel storage canisters, exposed to a salt-air environment in the temperature range 30-70°C for periods up to and exceeding 100 years. The nature of this degradation process, which involves multiple degradation mechanisms, combined with variable and uncertain environmental conditions dictates a probabilistic approach to life prediction. A final report for the original portion of the project was submitted earlier. However, residual stress measurements for as-welded and repair welds could not be performed within the original time of the project. As a result of this, a no-cost extension was granted in order to complete these tests. In this report, we report on the results of residual stress measurements.
The objective of this project, which includes close collaboration with scientists from INL and ANL, is to investigate and demonstrate the use of advanced mechanical surface treatments like laser shock peening (LSP) and ultrasonic nanocrystal surface modification (UNSM) and establish baseline parameters for enhancing the fatigue properties and SCC resistance of nuclear materials like nickel-based alloy 600 and 304 stainless steel. The research program includes the following key elements/tasks: 1) Procurement of Alloy 600 and 304 SS, heat treatment studies; 2) LSP and UNSM processing of base metal and welds/HAZ of alloys 600 and 304; (3) measurement and mapping of surface and sub-surface residual strains/stresses and microstructural changes as a function of process parameters using novel methods; (4) determination of thermal relaxation of residual stresses (macro and micro) and microstructure evolution with time at high temperatures typical of service conditions and modeling of the kinetics of relaxation; (5) evaluation of the effects of residual stress, near surface microstructure and temperature on SCC and fatigue resistance and associated microstructural mechanisms; and (6) studies of the effects of bulk and surface grain boundary engineering on improvements in the SCC resistance and associated microstructural and cracking mechanisms
Unraveling the effects of continuous dislocation interactions with interfaces, particularly at the nanometer length scales, is key to a broader understanding of plasticity, to material design and to material certification. To this end, this work proposes a novel discrete dislocation dynamics-based model for dislocation interface interactions tracking the fate of residual dislocation on interfaces. This new approach is used to predict the impact of dislocation/interface reactions on the overall mechanical behavior of accumulative roll bonded nanometallic laminates. The framework considers the dynamic evolution of the interface concurrent with a large network of dislocations, thus, accounting for the local short and long range effects of the dislocations under the external boundary conditions. Specifically, this study focuses on two-phase Fe/Cu nanometallic laminates, and investigates the role of the underlying elastic and plastic contrast of the Fe and the Cu layers on the composite response of the material. Moreover, the role of initial microstructures, resulting from processing is also investigated. Subsequently, the model is used to examine the effect of layer thickness and interface orientation relationship on the residual stresses of the relaxed microstructure. The associated mechanical response of these laminates are compared when loaded under normal direction compression, as well as shear compression. Finally, this work predicts a dominant effect of the layer thickness, as compared to the interface orientation relationship, on the macroscopic response and on the residual stresses of these nanolaminates, while the local dislocation transmission propensity through the interface is significantly influenced by the corresponding orientation relationship.
Two types of physical vapor deposition Cr coatings were deposited on chemical vapor deposited SiC coupons using conventional direct current magnetron sputtering (DCMS) and high-power impulse magnetron sputtering (HiPIMS) to mitigate the corrosion of SiC, an advanced fuel and structural material in light water nuclear reactor cores. Coating microstructure was characterized using scanning electron microscopy and scanning transmission election microscopy. X-ray diffraction analysis was conducted for phase identification and qualitative analysis of residual stresses. The mechanical integrity of the coatings was evaluated using scratch testing, micro-indentation, and nano-indentation tests. Additionally, the microstructure of the DCMS coating consisted of fine columnar grains with nanoscale intercolumnar channels, while the HiPIMS microstructure was denser and free of any columnar defects. The DCMS coating showed a small tensile residual stress, while the HiPIMS coating was under compressive stress. Both types of coatings showed good mechanical integrity in terms of ductility and adhesion to the substrate. Corrosion performance of the coatings was assessed with a 30-day high temperature water autoclave test. Both types of coatings formed a protective Cr 2 O 3 surface layer 20-30 nm thick during the autoclave test. In the DCMS coating, the columnar defects provided permeation pathways for water penetration resulting in oxide formation in the intercolumnar regions in the interior of the coating. Overall, both types of Cr coatings offer promise for the mitigation of hydrothermal corrosion of SiC in light water reactor operating environments.
Stress corrosion cracking (SCC) had occurred in early-generation high-level nuclear waste tanks constructed by welding carbon steel. This paper describes an ultrasonic inspection system and its fundamental ability to detect and quantify the length of SCC on thick welded steel plates. The finite element method (FEM) was applied to simulate the welding process to estimate the welding residual stress field. Growth of stress corrosion cracks is driven by crack stress intensities exceeding the subcritical cracking threshold intensity. The subject plate was experimentally inspected with ultrasonic nondestructive evaluation (NDE) techniques to characterize the extent of SCC. The NDE system uses a piezoelectric transducer to generate guided waves in the thick steel plate, and a scanning laser Doppler vibrometer (SLDV) to measure multidimensional time–space wavefield data over a user-defined scanning area in the plate surface. The measured wavefield data can show wave interactions in a localized area in the plate due to the presence of the discontinuities of the SCC. To generate an inspection image that can precisely show the crack’s location and/or the dimension, the wavefield data are further processed to generate inspection image that maps the entire sample plate so the crack can be clearly identified in the plate while its length can be readily estimated. In conclusion, the ultrasonic test results for crack length agree well with the visually estimated length and are close to that predicted by the FEM for cracks in the weld residual stress field.