At least 685 records · Page 38

Achieving a high-performance sodium-ion pouch cell by regulating intergrowth structures in a layered oxide cathode with anionic redox

In P2-type layered transition metal (TM) oxides, which are typical cathode materials for Na-ion batteries, the presence of Li within the TM layer could lead to the formation of specific Na–O–Li configurations that trigger additional oxygen redox at high charging voltages. However, the prismatic-type (P-type) to octahedral-type (O-type) phase transition and irreversible TM migration could be simultaneously aggravated in high state of charge, resulting in structural distortion. Here we demonstrate that excessive desodiation of P2-Na 0.67 Li 0.1 Fe 0.37 Mn 0.53 O 2 (NLFMO) induces the formation of neighbouring O-type stacking faults with an intergrowth structure (that is, interlacing of O- and P-type layers), which leads to out-of-lattice Li migration and irreversible oxygen loss. We show that, by controlling the depth of charge to tailor the intergrowth structure, a P-type stacking state can be uniformly interspersed between the O-type stacking state, thereby avoiding neighbouring O-type stacking faults. Adjusting the O/P intergrowth structure leads to both reversible migration of Li/TM ions and reversible anionic redox in the NLFMO cathode. In conclusion, we thereby achieve a high-performance pouch cell (with an energy density of 165 W h kg −1 based on the entire weight of the cell) with both cationic and anionic redox activities.

25 ENERGY STORAGE↗

Sr and Co Vapor-Phase Transport from LSCF Cathodes

A series of tests were performed to differentiate between surface diffusion and vapor-phase diffusion of chemical species from LSCF cathode material at typical sintering temperatures (up to 1100°C) in SOFC production. A GDC source substrate was printed with LSCF and separated by an air gap from a YSZ target substrate. Various geometries with long surface paths were employed to reduce the possibility of surface transport. Sr and Co were detected on the target substrates via energy dispersive spectroscopy (EDS) and x-ray photoelectron spectroscopy (XPS), including spatially resolved XPS. These results support a vapor-phase transport mechanism for Sr and Co. Sintering conditions and barrier layer requirements may need to be revisited to prevent the formation of undesired strontium zirconate at cathode/electrolyte interface due to vapor-phase transport.

vapor phase transport, SOFC cathode, Sr transport↗

Elucidating and Mitigating High-Voltage Degradation Cascades in Cobalt-Free LiNiO 2 Lithium-Ion Battery Cathodes

LiNiO 2 (LNO) is a promising cathode material for next-generation Li-ion batteries due to its exceptionally high capacity and cobalt-free composition that enables more sustainable and ethical large-scale manufacturing. However, its poor cycle life at high operating voltages over 4.1 V impedes its practical use, thus motivating efforts to elucidate and mitigate LiNiO 2 degradation mechanisms at high states of charge. Here, a multiscale exploration of high-voltage degradation cascades associated with oxygen stacking chemistry in cobalt-free LiNiO 2 , is presented. In this work, lattice oxygen loss is found to play a critical role in the local O3–O1 stacking transition at high states of charge, which subsequently leads to Ni-ion migration and irreversible stacking faults during cycling. This undesirable atomic-scale structural evolution accelerates microscale electrochemical creep, cracking, and even bending of layers, ultimately resulting in macroscopic mechanical degradation of LNO particles. By employing a graphene-based hermetic surface coating, oxygen loss is attenuated in LNO at high states of charge, which suppresses the initiation of the degradation cascade and thus substantially improves the high-voltage capacity retention of LNO. Overall, this study provides mechanistic insight into the high-voltage degradation of LNO, which will inform ongoing efforts to employ cobalt-free cathodes in Li-ion battery technology.

25 ENERGY STORAGE↗

Novel architectures for stabilization of Mn-rich cathodes: a high-valent approach to interfaces

Lithium- and manganese-rich (LMR) layered oxides continue to generate significant interest as promising, earth-abundant cathode materials for next-generation Li-ion batteries. In spite of their attractive capacity and cost advantages, a few long-standing challenges still hamper their widespread adoption, with manganese dissolution being one of the most persistent and vexing issues. In the present study, we explore the incorporation of Sb5+ as a high-valent cation and exploit its ability to form unique lithium-rich surface and grain-boundary structures that can integrate directly with the LMR lattice. When synthesized under appropriate conditions, Sb5+ orders strongly with Li+ to form localized Li+–Sb5+ motifs, which play a key role in restructuring the surface and grain-boundary regions. These restructured regions act as protective, stabilizing entities that substantially suppress electrolyte-driven side reactions, reduce impedance growth, limit manganese dissolution, and help retain cyclable lithium during long-term electrochemical cycling. Further improvements of the electrochemical performance of Sb-treated LMR were achieved using a well-known additive to mitigate Mn dissolution and highlight the synergistic effects of combined strategies. Overall, this work showcases how high-valent elements such as Sb5+ can help tailor the surface and intergranular regions and work in synergy with other modifiers (e.g. electrolyte additives), enhancing the cycle life and practical viability of LMR cathodes for use in graphite-based full cells.

Mallick, Subhadip [Argonne National Laboratory (AN↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Microstructural Insights into Performance Loss of High-Voltage Spinel Cathodes for Lithium-ion Batteries

Spinel-structured LiNi x Mn 2-x O 4 (LNMO), with low-cost earth-abundant constituents, is a promising high-voltage cathode material for lithium-ion batteries. Even though extensive electrochemical investigations have been conducted on these materials, few studies have explored correlations between their loss in performance and associated changes in microstructure. Here, down to the atomic scale, the structural evolution of these materials is investigated upon the progressive cycling of lithium-ion cells. Transgranular cracking is revealed to be a key feature during cycling; this cracking is initiated at the particle surface and leads to the penetration of electrolytes along the crack path, thereby increasing particle exposure to the electrolyte. The lattice structure on the crack surface shows spatial variances, featuring a top layer of rock-salt, a sublayer of a Mn 3 O 4 -like arrangement, and then a mixed-cation region adjacent to the bulk lattice. The transgranular cracking, along with the emergence of local lattice distortion, becomes more evident with extended cycling. Further, phase transformation at primary particle surfaces and void formation through vacancy condensation is found in the cycled samples. All these features collectively contribute to the performance degradation of the battery cells during electrochemical cycling.

25 ENERGY STORAGE↗

Regulating the Electron Distribution of Metal-Oxygen for Enhanced Oxygen Stability in Li-rich Layered Cathodes

Li-rich Mn-based layered oxides (LLO) hold great promise as cathode materials for lithium-ion batteries (LIBs) due to their unique oxygen redox (OR) chemistry, which enables additional capacity. However, the LLOs face challenges related to the instability of their OR process due to the weak transition metal (TM)-oxygen bond, leading to oxygen loss and irreversible phase transition that results in severe capacity and voltage decay. Herein, a synergistic electronic regulation strategy of surface and interior structures to enhance oxygen stability is proposed. In the interior of the materials, the local electrons around TM and O atoms may be delocalized by surrounding Mo atoms, facilitating the formation of stronger TM—O bonds at high voltages. Besides, on the surface, the highly reactive O atoms with lone pairs of electrons are passivated by additional TM atoms, which provides a more stable TM—O framework. Hence, this strategy stabilizes the oxygen and hinders TM migration, which enhances the reversibility in structural evolution, leading to increased capacity and voltage retention. This work presents an efficient approach to enhance the performance of LLOs through surface-to-interior electronic structure modulation, while also contributing to a deeper understanding of their redox reaction.

25 ENERGY STORAGE↗

Mitigation of rapid capacity decay in silicon-LiNi 0.6 Mn 0.2 Co 0.2 O 2 full batteries

Silicon (Si)-based materials have been considered as the most promising anode materials for high-energy-density lithium-ion batteries because of their higher storage capacity and similar operating voltage, as compared to the commercial graphite (Gr) anode. But the use of Si anodes including silicon-graphite (Si-Gr) blended anodes often leads to rapid capacity decay in Si-Gr/LiNixMnyCo z O 2 (x+y+z=1) full cells, which has been attributed to surface instability of the Si component. In addition to stabilizing the surface, this work investigates the potential of the Si-Gr blended anodes in a full-cell configuration and its impact on the capacity contribution from active components. Using dQ/dV plots of the full cells, a powerful but simple-to-implement differential potential approach is developed to decouple the capacity contribution and degradation from the graphite and silicon components. Data collected from three-electrode cells confirm the results from the differential potential approach, which suggests a voltage slippage to a higher voltage at the blended anode side. Additionally, the voltage slippage causes a reduced utilization of the Gr component and exacerbates side reactions between the Si-Gr anode and carbonate electrolytes. Furthermore, based on these failure mechanisms, we adopted a mitigation strategy to tune the open circuit voltage of the prelithiated anode while stabilizing the surface. As a result, the full cells with the modified Si-Gr anodes (mass loading, 2.5 mAh/cm 2 ) offer a highly reversible full-cell energy density of 390 Wh/kg (based on the mass of both anode and cathode materials in a full cell) with a cycling CE of 99.9% over 200 cycles.

25 ENERGY STORAGE↗

Evaluation of Chemical and Structural Homogeneity in Single Particles of Li 1-x Ni 0.33 Mn 0.33 Co 0.33 0 2

Identifying irreversible phenomena at single particles of battery cathode materials is an important step to understanding degradation pathways upon cycling. LiNi 0.33 Mn 0.33 Co 0.33 O 2 (LiNMC(111)) single particles of size 200 x 300 nm were studied before and after cycling using Scanning X-ray Diffraction Microscopy (SXDM) and ptychographic microscopy. Here, with resolutions of 30 and 5 nm, respectively, it was possible to map the (003) reflection and nickel oxidation state changes in single particles at different states of charge. While the compositions measured by the c lattice parameter from SXDM were found to be homogeneous, mapping at higher resolution using ptychography revealed that Ni oxidation states decrease sharply 0-25 nm from the edge, then trail into a steady oxidation state toward the interior of the particle. Within the 30 nm length scale, we conclude that LiNi 0.33 Mn 0.33 Co 0.33 O 2 single particles are highly structurally reversible.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comprehensive Characterization of Multi-Phase Sulfurized Polyacrylonitrile Cathodes for Lithium-Sulfur Batteries

Sulfurized polyacrylonitrile (SPAN) is considered one of the most promising cathode materials to overcome the operational challenges that plague lithium-sulfur (Li-S) batteries. However, material properties and electrochemical performance implications of SPAN prepared under different synthesis conditions are not yet fully investigated. In this study, we show the impacts of different synthesis conditions on the formation of sulfur to PAN bonds and redox reaction mechanisms of multi-phase SPAN via comprehensive material and electrochemical characterizations. In-situ Raman analysis was first applied to study the multi-phase SPAN-based Li-S cells. We found that both elemental sulfur and chemically bonded sulfur are present under the synthesis condition of 300 degree C/3 h along with unreacted PAN. The incompletely sulfurized, multi-phase SPAN exhibited an unusually rapid capacity degradation in the resultant Li-S cells, which is attributed to polysulfide formation and continuously growing interfacial impedance in the Li-S cells. On the other hand, SPAN samples prepared under the synthesis condition of 350 degree C/3 h are found completely sulfurized with chemically bonded sulfur to the PAN backbone without the presence of free elemental sulfur. Complete sulfurization of SPAN led to exceptionally stable cycle performance due to excellent reversible redox processes of chemically bonded sulfur with Li+ in the Li-S cells.

DIRECT ENERGY CONVERSION,ENERGY STORAGE↗

Research advances on cobalt-free cathodes for Li-ion batteries - The high voltage LiMn 1.5 Ni 0.5 O 4 as an example

LiMn 1.5 Ni 0.5 O 4 is one of the most promising cathode materials for use in either next generation lithium-ion batteries or all solid-state batteries. However, despite the significant Research and Development (R&D) carried out throughout the last two decades the material has not made serious inroads into market. One of the major reasons is the lack of consistency in the reported intrinsic properties and electrochemical performance owing to major controversies in synthesis, crystal structure and bulk and interfacial properties of LiMn 1.5 Ni 0.5 O 4 , notably in contact with electrolytes. This paper is a compelling review providing an assessment on the mainstream R&D dealing with the various crystal structures of LiMn 1.5 Ni 0.5 O 4 and their evolutions observed during synthesis and cycling in correlation with their electrochemical performance. Influence of electrolytes and additives along with modifications through doping and surface treatments are interrelated, and the electronic and ionic transport properties of the ordered and disordered LiMn 1.5 Ni 0.5 O 4 phases are discussed. Overall, this review provides a detailed assessment on LiMn1.5Ni0.5O4 and the underlying mechanisms governing its electrochemical performance broadly providing a focused framework for further advancement towards commercialization.

25 ENERGY STORAGE↗

Application of electron backscatter diffraction techniques to quantify effects of aging on sub-grain and spatial heterogeneity in NMC cathodes

Identification and evaluation of structural heterogeneity in spent cathode materials is crucial to developing appropriate remediation strategies for novel recycling processes. Native heterogeneities may be exacerbated during the cell's operational lifetime, as sub-particle-scale variations induce anisotropic expansion and contraction upon cycling. Structural transformations resulting from repeated cycling and calendar aging predominantly occur at the secondary particle surface and at the grain boundaries (GBs) between primary particles. However, the diffusion and stress build up around and across GBs are poorly understood. In this study, electron backscatter diffraction (EBSD) is employed to track sub-grain lattice structure across a statistically relevant number of Li(Ni0.33Mn0.33Co0.33)O2 (NMC-111) particles. Specifically, differences in lattice misorientation – measured as the deviation from the grain's average orientation – are tracked as a function of position within the electrode (near current collector, middle, and near separator) and as a function of electrochemical cycling. Further, a novel method of structural analysis is developed, offering insight into sub-grain diffusion behavior by comparing lattice misorientation near the grain boundary versus in the grain bulk. The present results suggest that electrode-scale spatial heterogeneity in lattice structure is induced by initial manufacturing conditions, and that radial gradients in lattice misorientation evolve at the primary particle scale with repeated electrochemical cycling.

25 ENERGY STORAGE↗

In Situ Diffraction and Ex Situ Transmission X‐Ray Microscopy Studies of Solid‐State Upcycling for NMC Cathodes

Upcycling of recycled LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) cathodes offers an economical route to produce cathode materials with increased energy density (i.e., LiNi 0.8 Mn 0.1 Co 0.1 O 2 , NMC811) that meet the performance needs of present-day electric vehicles. In this work, solid-state upcycling of NMC622 via calcination with Ni(OH) 2 and LiOH was monitored using in situ synchrotron powder X-ray diffraction measurements. Sequential Rietveld refinements indicate that the calcination proceeds by initially converting Ni(OH) 2 to a rocksalt NiO phase followed by lithiation of NiO to form LiNiO 2 (LNO), with both NMC and LNO phases present in nearly equal proportions at the calcination endpoint. Variable-energy transmission X-ray microscopy tomograms of upcycled samples reveal that the NMC and LNO domains are intermixed at sub-micron length scales. Depth-dependent analysis of multi-elemental fitting maps matches the expected NMC811 composition at the secondary particle level and indicates that transition metal diffusion is not limited by the secondary particle size.

cathode upcycling↗

First-principles study of the structures and redox mechanisms of Ni-rich lithium nickel manganese cobalt oxides

To reduce the cobalt (Co) content in lithium-ion batteries, Ni-rich (high-Ni) lithium nickel manganese cobalt oxides (NMC) are pursued as one of the next-generation cathode materials. However, there is still debate on the crystal and electronic structures of the baseline, LiNiO 2 . Density Functional Theory (DFT) calculations were performed to provide a theoretical understanding of Ni-rich NMC. First, it was found that the commonly used $R\bar{3}m$ structure for LiNiO 2 is metallic, contrary to the experimentally reported mix-conducting behavior. Among the four different space groups, $R\bar{3}m$, C2/m, P2 1 /c, and P2/c, P2/c with charge disproportionation of Ni 2+ and Ni 4+ is the most energetically stable and semiconducting structure of LiNiO 2 . Therefore, the atomic structures of representative Ni-rich NMC were built by partially replacing Ni with Co or Mn in the P2/c LiNiO 2 to form Li x Ni y Mn z Co 1-y-z O 2 . In the fully lithiated (x=1.0) high Ni content NMC (y>0.5), the oxidation state of all Mn ions becomes 4+, while Co ions still maintain 3+, and part of the Ni ions become 3+ to compensate for the charge. Upon delithiation, the local environment shows more variation of the charge states on the transition metal (TM) ions. The average oxidation on each TM follows a sequence of losing electrons that starts from Ni 2+ to Ni 3+ , then oxidizing Ni 3+ and Co 3+ , while Mn 4+ remains electrochemically inactive till x=0. Finally, a general relationship for the oxidation state change in each TM as a function of x is derived and shows agreement with both modeling and experimental data.

25 ENERGY STORAGE↗

Feasibility of Prelithiation in LiFePO 4

Lithium iron phosphate (LiFePO 4 ) is widely applied as the cathode material for the energy storage Li-ion batteries due to its low cost and high cycling stability. However, the low theoretical specific capacity of LiFePO 4 makes its initial capacity loss more concerning. Therefore, lithium compensation by way of prelithiation and applications of sacrificial Li-rich additives in LiFePO 4 is imminent in elevating the energy density and/or prolonging the lifetime of the LiFePO 4 -based Li-ion batteries (LIBs). Prelithiation in LiFePO 4 is herein carried out by electrochemical and chemical methods and its feasibility is proved on the basis of the electrochemical evaluations such as the initial charge capacity and the cycling stability. In addition, the site of the pre-intercalated Li-ions is found via comprehensive physical characterizations and the density functional theory (DFT) calculations. Furthermore, these findings open a new avenue for elevating the energy density and/or prolonging the lifetime of the high-energy-density batteries.

36 MATERIALS SCIENCE↗

Investigation of Key Electronic States in Layered Mixed Chalcogenides With a d 0 Transition Metal as Li-Ion Cathodes

Lithium-rich transition metal chalcogenides are witnessing a revival as candidates for Li-ion cathode materials, spurred by the boost in their capacities from transcending conventional redox processes based on cationic states and tapping into additional chalcogenide states. A particularly striking case is Li 2 TiS 3-y Se y , which features a d 0 metal. While the end members are expectedly inactive, substantial capacities are measured when both Se and S are present. Using X-ray absorption spectroscopy, it is shown that the electronic structure of Li 2 TiS 3-y Se y is not a simple combination of the end members. The data confirm previous hypotheses that, in Li 2 TiS 2.4 Se 0.6 , this behavior is underpinned by concurrent and reversible redox of only S and Se, and identify key electronic states. Moreover, wavelet transforms of the extended X-ray absorption fine structure provide direct evidence of the formation of short Se–Se units upon charging. The study uncovers the underpinnings of this intriguing reactivity and highlights the richness of redox chemistry in complex solids.

25 ENERGY STORAGE↗

Mechanically Reinforced Pseudosolid Polyelectrolyte Membranes via Layer-by-Layer Assembly for High-Performing Lithium-Metal Batteries

Ionogels are emerging as high-potential pseudosolid electrolytes for lithium-metal batteries (LMBs), leveraging their intrinsic high ionic conductivity from entrapped ionic liquid (IL) electrolytes. However, their practical application is hindered by poor mechanical strength stemming from the confinement of ILs within a polymer matrix. To address this challenge, the formation of conformal polyion coatings with functional groups is reported to be relevant to LMBs’ application on ionogels, utilizing a layer-by-layer (LbL) assembly strategy. Here, this approach significantly enhances the mechanical strength (Young's modulus and tensile strength) and electrochemical performance of ionogels, owing to the tailored interface modifications introduced by functional groups’ specific conformal polyion coatings. The core of this methodology leverages the inherent ionic structure of ionogels to enable facile interface modification through Coulombic interactions between polyanions and polycations. These conformally coated interface functionalized membranes show improved electrochemical performance when integrated with cathode materials such as LiFePO 4 (LFP) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) in an LMB configuration, underscoring their potential for robust, high-conductivity, pseudosolid membranes for LMB applications. These innovative pseudosolid membranes offer improved mechanical and electrochemical properties, leading to higher battery efficiency and safety, making them promising candidates for next-generation LMB technology.

25 ENERGY STORAGE↗