Search NASA⌕ Search

SEARCH · Search NASA

Results for “ceramic processing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 685 records · Page 38

Effect of microwave-assisted sintering on dielectric properties of CaCu{sub 3}Ti{sub 4}O{sub 12} ceramic

In this present work, CaCu{sub 3}Ti{sub 4}O{sub 12} (CCTO) was synthesized by conventional solid-state reaction technique. The synthesis process was carried out in two phases; by conventional process (calcination and sintering at 1080°C for 10 hours) and phase II involves the micro assisted pre sintering of conventionally calcined CCTO for very short soaking time of 30 min at 1080°C in a microwave furnace followed by sintering at 1080°C for 10 hours in conventional furnace. X-ray diffraction (XRD) patterns confirmed the formation of single phase ceramic. Dielectric properties were studied over the frequency range from 50Hz -5MHz at temperatures (273K-343K). It was observed that pre- microwave sintering enhance the dielectric constant values from 10900 to 11893 and respectively reduces the dielectric loss values from 0.49 to 0.34 at room temperature(1 KHz). CCTO ceramics which are found desirable for many technological applications. The effect is more pronounced at low frequencies of applied electric field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Liquid Salt Heat Exchanger Technology for VHTR Based Applications

The objective of this research is to evaluate performance of liquid salt fluids for use as a heat carrier for transferring high-temperature process heat from the very high-temperature reactor (VHTR) to chemical process plants. Currently, helium is being considered as the heat transfer fluid; however, the tube size requirements and the power associated with pumping helium may not be economical. Recent work on liquid salts has shown tremendous potential to transport high-temperature heat efficiently at low pressures over long distances. This project has two broad objectives: To investigate the compatibility of Incoloy 617 and coated and uncoated SiC ceramic composite with MgCl 2 -KCl molten salt to determine component lifetimes and aid in the design of heat exchangers and piping; and, To conduct the necessary research on the development of metallic and ceramic heat exchangers, which are needed for both the helium-to-salt side and salt-to-process side, with the goal of making these heat exchangers technologically viable. The research will consist of three separate tasks. The first task deals with material compatibility issues with liquid salt and the development of techniques for on-line measurement of corrosion products, which can be used to measure material loss in heat exchangers. Researchers will examine static corrosion of candidate materials in specific high-temperature heat transfer salt systems and develop an in situ electrochemical probe to measure metallic species concentrations dissolved in the liquid salt. The second task deals with the design of both the intermediate and process side heat exchanger systems. Researchers will optimize heat exchanger design and study issues related to corrosion, fabrication, and thermal stresses using commercial and in-house codes. The third task focuses integral testing of flowing liquid salts in a heat transfer/materials loop to determine potential issues of using the salts and to capture realistic behavior of the salts in a small scale prototype system. This includes investigations of plugging issues, heat transfer, pressure drop, and the corrosion and erosion of materials in the flowing system.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Fast Pyrolysis Oil Stabilization: An Integrated Catalytic and Membrane Approach for Improved Bio-oils. Final Report

This University of Massachusetts, Amherst project, "Fast Pyrolysis Oil Stabilization: An Integrated Catalytic and Membrane Approach for Improved Bio-oils" started on 1st February 2009 and finished on August 31st 2011. The project consisted following tasks: Task 1.0: Char Removal by Membrane Separation Technology The presence of char particles in the bio-oil causes problems in storage and end-use. Currently there is no well-established technology to remove char particles less than 10 micron in size. This study focused on the application of a liquid-phase microfiltration process to remove char particles from bio-oil down to slightly sub-micron levels. Tubular ceramic membranes of nominal pore sizes 0.5 and 0.8m were employed to carry out the microfiltration, which was conducted in the cross-flow mode at temperatures ranging from 38 to 45 C and at three different trans-membrane pressures varying from 1 to 3 bars. The results demonstrated the removal of the major quantity of char particles with a significant reduction in overall ash content of the bio-oil. The results clearly showed that the cake formation mechanism of fouling is predominant in this process. Task 2.0 Acid Removal by Membrane Separation Technology The feasibility of removing small organic acids from the aqueous fraction of fast pyrolysis bio-oils using nanofiltration (NF) and reverse osmosis (RO) membranes was studied. Experiments were carried out with a single solute solutions of acetic acid and glucose, binary solute solutions containing both acetic acid and glucose, and a model aqueous fraction of bio-oil (AFBO). Retention factors above 90% for glucose and below 0% for acetic acid were observed at feed pressures near 40 bar for single and binary solutions, so that their separation in the model AFBO was expected to be feasible. However, all of the membranes were irreversibly damaged when experiments were conducted with the model AFBO due to the presence of guaiacol in the feed solution. Experiments with model AFBO excluding guaiacol were also conducted. NF membranes showed retention factors of glucose greater than 80% and of acetic acid less than 15% when operated at transmembrane pressures near 60 bar. Task 3.0 Acid Removal by Catalytic Processing It was found that the TAN reduction in bio-oil was very difficult using low temperature hydrogenation in flow and batch reactors. Acetic acid is very resilient to hydrogenation and we could only achieve about 16% conversion for acetic acid. Although it was observed that acetic acid was not responsible for instability of aqueous fraction of bio-oil during ageing studies (described in task 5). The bimetallic catalyst PtRe/ceria-zirconia was found to be best catalyst because its ability to convert the acid functionality with low conversion to gas phase carbon. Hydrogenation of the whole bio-oil was carried out at 125°C, 1450 psi over Ru/C catalyst in a flow reactor. Again, negligible acetic acid conversion was obtained in low temperature hydrogenation. Hydrogenation experiments with whole bio-oil were difficult to perform because of difficulty to pumping the high viscosity oil and reactor clogging. Task 4.0 Acid Removal using Ion Exchange Resins DOWEX M43 resin was used to carry out the neutralization of bio-oil using a packed bed column. The pH of the bio-oil increased from 2.43 to 3.7. The GC analysis of the samples showed that acetic acid was removed from the bio-oil during the neutralization and recovered in the methanol washing. But it was concluded that process would not be economical at large scale as it is extremely difficult to regenerate the resin once the bio-oil is passed over it. Task 5.0 Characterization of Upgraded Bio-oils We investigated the viscosity, microstructure, and chemical composition of bio-oils prepared by a fast pyrolysis approach, upon aging these fuels at 90ºC for periods of several days. Our results suggest that the viscosity increase is not correlated with the acids or char present in the bio-oils. The viscosity increase is due to formation of high molecular weight polymeric species over time. Our work also suggests that hydrogenation of the samples is beneficial in eliminating the viscosity increase. Task 6.0 Commercialization Assessment Renewable Oil International LLC (ROI) was responsible for Task 6.0, Commercialization Assessment. As part of this effort ROI focused on methods to reduce char carryover in the vapor stream from the fast pyrolysis reactor and residence time of the vapor in the reactor. Changes were made in the bio-oil recovery methodology and a reactor sweep gas used to reduce vapor residence time. Cyclones were placed in the vapor stream to reduce char particulate carryover. Microfiltration of the bio-oil was also researched to remove char particulate from the bio-oil. The capital cost for these improvements would be less than 2% of the total plant capital cost.

09 BIOMASS FUELS↗

Ceramic/metal nanocomposites by lyophilization: Processing and HRTEM study

Highlights: Black-Right-Pointing-Pointer A cryogenic route has been used to obtain ceramic/metal nanostructured powders. Black-Right-Pointing-Pointer The powders present good homogeneity and dispersion of metal. Black-Right-Pointing-Pointer The metal nanoparticle size distributions are centred in 17-35 nm. Black-Right-Pointing-Pointer Both phases, ceramic and metal, present a high degree of crystallinity. Black-Right-Pointing-Pointer Good metal/ceramic interfaces due to epitaxial growth, studied by HRTEM. -- Abstract: This work describes a wet-processing route based on spray-freezing and subsequent lyophilization designed to obtain nanostructured ceramic/metal powders. Starting from the ceramic powder and the corresponding metal salt, a water-based suspension is sprayed on liquid nitrogen. The frozen powders are subsequently freeze-dried, calcined and reduced. The material was analyzed using X-ray diffraction analysis at all stages. High resolution transmission electron microscopy studies showed a uniform distribution of metal nanoparticles on the ceramic grain surfaces, good interfaces and high crystallinity, with an average metal particle size in the nanometric range.

36 MATERIALS SCIENCE↗

High temperature steam separation membrane

Ceramic proton-conducting oxide membranes are described herein, which are useful for separating steam from organic chemicals under process conditions. The membranes have a layered structure, with a dense film of the perovskite over a porous composite substrate comprising the perovskite material and a metallic material (e.g., Ni, Cu, or Pt). The perovskite comprises an ABO 3 -type structure, where “A” is Ba and “B” is a specified combination of Ce, Zr, and Y. The perovskite ceramic materials described herein have an empirical formula of Ba(Ce x Zr 1-x-n Y n )O 3-δ , wherein 0<x<0.8 (e.g., 0.1≤x≤0.7 or 0.2≤x≤0.5); and 0.05≤n≤0.2; and δ=n/2. In some embodiments n is about 0.2. In some other embodiments 0.6≤x≤0.8; and n is about 0.2, such as Ba(Ce 0.7 Zr 0.1 Y 0.2 )O 3-δ , also referred to herein as BCZY712.

Lee, Tae H.↗

In-Operando Study of Shape Retention and Microstructure Development in a Hydrolyzing Sol–Gel Ink during 3D-Printing

3D printing of amorphous and crystalline ceramics is of paramount importance for the fabrication of a wide range of devices with applications across different technology fields. Printed ceramics are remarkably enabled by the sol-gel synthesis method in conjunction with continuous filament direct ink writing. During printing, multiple processes contribute to the evolution of inks including shape retention, chemical conversion, solidification, and microstructure formation. Traditionally, depending on the ink composition and printing environment, several mechanisms have been associated with the shape retention and solidification of 3D printed structures: gelation, rapid solvent evaporation, energy-driven phase transformation, and chemical-driven phase transformation. Understanding the fundamental differences between these mechanisms becomes key since they strongly influence the spatiotemporal evolution of the materials, as the out-of-equilibrium processes inherent to the extrusion, relaxation, and solidification of printed materials have significant effects on the materials properties. Herein, we investigate the shape retention mechanism and the hydrolysis-induced material conversion and microstructure formation during the 3D printing of a water reactive sol-gel ink that transforms into titanium dioxide-based ceramic. This study aims at identifying characteristic mechanisms associated with the material transformation, establishing connections between the microstructure development and the timescales associated with solidification under operando 3D-printing conditions. The investigation of this material's out-of-equilibrium pathways under processing conditions is enabled by time-resolved coherent X-ray scattering, providing simultaneous access to temporospatially resolved microstructural and dynamics information. Furthermore, we explore X-ray speckle tracking as a tool to resolve deformations of the microstructure in a printed filament associated with the deposition of consecutive filaments. Through this work, we aim at providing a fundamental understanding of the relationships behind these transformative processes in 3D printing and their timescales as the basis for achieving unprecedented control over printed materials microstructure.

36 MATERIALS SCIENCE↗

Influence of poling on far-infrared response of lead zirconate titanate ceramics

The paper describes experiments revealing the anisotropy of the macroscopic dielectric response of poled lead zirconate titanate ceramics in the phonon frequency region. The results are discussed in terms of distinct polar phonon contributions and effective medium theory. The anisotropy probed in far-infrared experiments can be used to evaluate efficiency of the poling and/or depoling processes.

36 MATERIALS SCIENCE↗

Li Morphology Evolution during Initial Cycles in a Gel Composite Polymer Electrolyte

Understanding and controlling lithium morphology evolution and lithium dendrite formation and growth during cycling is one of the key challenges for high-energy lithium metal batteries. This challenge applies to liquid electrolyte batteries as well as solid-state and semi-solid-state batteries. Our current knowledge about the evolution of the Li morphology is mostly obtained from liquid electrolyte-based studies in a Li–Li symmetrical cell configuration. The knowledge obtained in such conditions may not readily transfer into solid-state or semi-solid-state batteries. In this work, Li morphology evolution during initial cycling in a full cell configuration with the LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC 622) cathode and a semi-solid-state gel composite electrolyte is monitored via post-mortem photographs and scanning electron microscopy at multiple length scales. The gel composite electrolyte contains a cross-linked poly(ethylene oxide)-based polymer electrolyte, ceramic fillers, and a liquid plasticizer. The results show that severe surface pitting occurs as early as the second stripping cycle. Pit formation and continuous dissolution during the stripping process are the main cause of the Li surface roughening and dendrite growth mechanism in the model gel composite electrolyte. Comparing Li dendrite growth mechanisms in liquid, polymer, and ceramic solid electrolytes, the dendrite growth mechanism observed in this model electrolyte resembles that of the liquid electrolyte the most. This study suggests that strategies to control Li morphology and prevent dendrite growth in a gel composite electrolyte should be similar to strategies applicable to liquid electrolytes.

25 ENERGY STORAGE↗

Transparent oxyfluoride glass ceramics co-doped with Er{sup 3+} and Yb{sup 3+} - Crystallization and upconversion spectroscopy

Transparent glass ceramics in the system SiO{sub 2}-B{sub 2}O{sub 3}-PbO-CdO-PbF{sub 2}-CdF{sub 2}-YbF{sub 3}-ErF{sub 3} showing infrared to visible anti-Stokes (upconversion) luminescence are studied in the present work. The glass compositions have been optimized in order to reduce the melting temperature and, hence, to obtain laboratory scale samples with good optical quality. Erbium-doped nanoscale Pb{sub 4}Yb{sub 3}F{sub 17} crystals are precipitated in the precursor glasses during annealing at temperatures 30-40 K above T{sub g}. A kinetically self-constrained growth explains the nano sizes of the crystals. Both the Stokes and anti-Stokes luminescence spectra of glasses could be explained with clustering of the Yb{sup 3+} and Er{sup 3+} ions in fluorine-rich regions. At the annealing temperature these regions act as nucleation precursors. The crystal growth further enhances the local concentration of these ions. Consequently, a series of energy transfer and energy cross relaxation processes occurs between adjacent rare earth ions leading to the observed luminescence spectra of the glass ceramics studied. -- Graphical abstract: A highly viscous shell (shown in the picture in dark blue) is build around the growing crystal (white circles). When the shell's T{sub g} approaches the annealing temperature, the crystal growth is fully suppressed for kinetic reasons. The upconversion luminescence, resulting from the simultaneous absorption of two and even three infrared photons, is depicted schematically in the right part of the figure. Display Omitted Highlights: {yields} New oxyfluoride glass compositions with reduced melting temperature are formulated. {yields} The phase Pb{sub 4}Yb{sub 3}F{sub 17} doped with Er{sup 3+} ions crystallizes in these glasses. {yields} A kinetically self-constrained growth explains the nano sizes of the crystals. {yields} Clustering of Yb{sup 3+}, Er{sup 3+} and Pb{sup 2+} ions into fluorine-rich glass regions is observed. {yields} The luminescence of glass-ceramics is consistent with its structure.

36 MATERIALS SCIENCE↗

Large-Scale Additive Manufacturing of Silicon Carbide with Process Monitoring

This report summarizes new capabilities in additive manufacturing (AM) of large-scale silicon carbide (SiC) components under the Advanced Materials and Manufacturing Technologies (AMMT) program. SiC is a promising material that is being considered for many advanced reactor designs due to its high temperature strength, radiation tolerance, minimal neutron absorption, and oxidation resistance [1-8]. One of the primary limitations to using SiC as an in-core structural material is the inability to fabricate large SiC components with complex geometries. While under the former Transformational Challenge Reactor (TCR) program, ceramic AM systems at the Oak Ridge National Laboratory (ORNL) were limited in the quantity and overall size achievable for producing ceramic AM components. To address this, ORNL has improved its infrastructure for binder jet and chemical vapor infiltration (CVI) processes with cutting-edge equipment coming online in a newly renovated laboratory space capable of producing larger components and higher throughput without compromise on part size. This report details the laboratory renovation progress, focusing specifically on the DesktopMetal (formerly ExOne) X25Pro binder jet, a large scale CVI furnace, and the added functionality of a software tool called Peregrine for quality assurance and control purposes.

36 MATERIALS SCIENCE↗

Engineering Graphene-Ceramic 3D Composite Foams by Freeze Drying

A 3D graphene foam produced by the chemical vapor deposition (CVD) technique is recognized as an effective nanofiller material, as it does not agglomerate in the matrix. Though CVD facilitates pristine graphene foam production, the method poses limitations in developing large-scale 3D graphene composite foams as advanced engineering materials. In this paper, a freeze-drying (FD) process is used to produce a composite 3D foam, which is a mixture of graphene nanoplatelet (GNP) and a low-temperature co-fired ceramic (LTCC). The freeze-dried GNP-LTCC reticulated 3D composite foam has an average pore size ranging from 70 to 100 μm. Pore size is varied by regulating the heat transfer rate during the freezing process using a thermally conductive aluminum (Al) mold and a thermally insulating acrylonitrile butadiene styrene (ABS) mold. Computational thermal modeling is used to visualize the heat transfer and its effect on foam pore size. Subsequently, a freeze-dried GNP-LTCC composite foam is embedded into the LTCC matrix to form a hierarchical assembly by a spark plasma technique without compromising the 3D structure of the FD foam. This study established that a simple, eco-friendly, and scalable processing methodology can produce advanced graphene-based 3D composite foams as the future tailorable nanofillers for designing multimatrix materials.

36 MATERIALS SCIENCE↗

Green emission from Eu{sup 2+}/Dy{sup 3+} codoped SrO-Al{sub 2}O{sub 3}-B{sub 2}O{sub 3} glass-ceramic by ultraviolet light and femtosecond laser irradiation

A spectroscopic investigation of Eu{sup 2+}/Dy{sup 3+} codoped SrO-Al{sub 2}O{sub 3}-B{sub 2}O{sub 3} glass-ceramic is presented. The sample exhibits green emission excited by ultraviolet (UV) light and near-IR femtosecond (fs) laser. The emission profile obtained by near-IR fs laser irradiation is similar to that by UV excitation, indicating that both of the emissions come from 5d {yields} 4f transition of the Eu{sup 2+} ions. The relationship between the upconversion luminescence (UCL) intensity and pump power reveals a two-photon process in the conversion of near-IR radiation to the green emission. The possible mechanism of UCL from such glass-ceramic is proposed.

36 MATERIALS SCIENCE↗

RADIOACTIVE DEMONSTRATIONS OF FLUIDIZED BED STEAM REFORMING WITH ACUTAL HANFORD LOW ACTIVITY WASTES VERIFYING FBSR AS A SUPPLEMENTARY TREATMENT

The U.S. Department of Energy's Office of River Protection is responsible for the retrieval, treatment, immobilization, and disposal of Hanford's tank waste. Currently there are approximately 56 million gallons of highly radioactive mixed wastes awaiting treatment. A key aspect of the River Protection Project cleanup mission is to construct and operate the Waste Treatment and Immobilization Plant (WTP). The WTP will separate the tank waste into high-level waste (HLW) and low-activity waste (LAW) fractions, both of which will subsequently be vitrified. The projected throughput capacity of the WTP LAW Vitrification Facility is insufficient to complete the cleanup mission in the time frame required by the Hanford Federal Facility Agreement and Consent Order, also known as the Tri-Party Agreement (TPA). Therefore, Supplemental Treatment is required both to meet the TPA treatment requirements as well as to more cost effectively complete the tank waste treatment mission. Fluidized Bed Steam Reforming (FBSR) is one of the supplementary treatments being considered. FBSR offers a moderate temperature (700-750 C) continuous method by which LAW and other secondary wastes can be processed irrespective of whether they contain organics, nitrates/nitrites, sulfates/sulfides, chlorides, fluorides, and/or radio-nuclides like I-129 and Tc-99. Radioactive testing of Savannah River LAW (Tank 50) shimmed to resemble Hanford LAW and actual Hanford LAW (SX-105 and AN-103) have produced a ceramic (mineral) waste form which is the same as the non-radioactive waste simulants tested at the engineering scale. The radioactive testing demonstrated that the FBSR process can retain the volatile radioactive components that cannot be contained at vitrification temperatures. The radioactive and nonradioactive mineral waste forms that were produced by co-processing waste with kaolin clay in an FBSR process are shown to be as durable as LAW glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Melt Infiltrated Ceramic Matrix Composites for Shrouds and Combustor Liners of Advanced Industrial Gas Turbines

This report covers work performed under the Advanced Materials for Advanced Industrial Gas Turbines (AMAIGT) program by GE Global Research and its collaborators from 2000 through 2010. A first stage shroud for a 7FA-class gas turbine engine utilizing HiPerComp{reg_sign}* ceramic matrix composite (CMC) material was developed. The design, fabrication, rig testing and engine testing of this shroud system are described. Through two field engine tests, the latter of which is still in progress at a Jacksonville Electric Authority generating station, the robustness of the CMC material and the shroud system in general were demonstrated, with shrouds having accumulated nearly 7,000 hours of field engine testing at the conclusion of the program. During the latter test the engine performance benefits from utilizing CMC shrouds were verified. Similar development of a CMC combustor liner design for a 7FA-class engine is also described. The feasibility of using the HiPerComp{reg_sign} CMC material for combustor liner applications was demonstrated in a Solar Turbines Ceramic Stationary Gas Turbine (CSGT) engine test where the liner performed without incident for 12,822 hours. The deposition processes for applying environmental barrier coatings to the CMC components were also developed, and the performance of the coatings in the rig and engine tests is described.

33 ADVANCED PROPULSION SYSTEMS↗

Development of a silicon carbide ceramic based counter-flow heat exchanger by binder jetting and liquid silicon infiltration for concentrating solar power

A silicon carbide ceramic counter-flow heat exchanger with integrated headers was printed by binder jetting additive manufacturing process. Multiple phenolic binder infiltration cycles (3 or 5) followed by pyrolysis were conducted to increase the net carbon content of the printed SiC specimens. Subsequently, to attain full densification, silicon melt infiltration was used. The microstructure and mechanical properties were comprehensively characterized on the densified material. The chemical compositions and visual distribution of the various regions in the specimens were determined via scanning electron microscopy, while X-ray diffraction and synchrotron µ-computed tomography were used to provide a quantitative assessment of the volume fractions of the identified phase regions. Microhardness measurements showed dependence on the local microstructure. The fracture strength of the material was correlated with the specimen density and agreed with the reported values in the literature. High-temperature exposure at 750 °C for up to 200h did not degrade the strength for the specimens with three phenolic-binder infiltrations; however, the strengths degraded for ones with five phenolic-binder infiltrations. The associated fracture toughnesses of the specimens were ~3.4 MPam 1/2 at room temperature and 750°C, and the thermal conductivities varied from >150 W/mK at room temperature to ~45 W/mK at 750°C. Hence, this study validated the use of the binder-jetting printed SiC ceramic materials for high-temperature heat exchanges. Lastly, we also present in this work the first successful fabrication of a binder-jetting printed one-piece dense SiC ceramic heat exchanger body with unblocked channels that can be used for the flow of heat transfer fluids.

36 MATERIALS SCIENCE↗

On electrolyte wetting through lithium-ion battery separators

The wettability by electrolyte is a critical characteristic of lithium-ion battery separators since electrolyte absorption is essential for ionic transport. Most importantly, fast absorption of electrolyte facilitates the electrolyte filling and wetting processes during the battery assembly. However, theoretical or experimental investigation of separator wettability has rarely been reported, and thus very little quantitative data can be found in the existing literature. Here, innovative experimental techniques and associated analytical models have been developed to fully characterize the electrolyte wetting behavior through battery separators. Both in-plane and through-plane imbibition processes are investigated. The results show that, electrolyte needs significantly longer time to wet separators than it does for commercial electrodes. The wetting rate depends significantly on the pore size, porosity, and micro-structure of the separators. Electrolyte in-plane wetting is only observed in the separators manufactured by the wet process. Increasing separator porosity and pore size is shown to be substantially increasing through-plane wetting rate. In addition, ceramic coating is shown to increase in-plane wetting but retard through-plane wetting.

25 ENERGY STORAGE↗

Effect of a micro-scale dislocation pileup on the atomic-scale multi-variant phase transformation and twinning

In this paper, we perform concurrent atomistic–continuum (CAC) simulations to assess the contribution of the internal stress induced by the microscale dislocation pileup at an atomically structured interface to the atomic-scale phase transformations (PTs), reverse PTs, and twinning. The main novelty of this work is to unify the atomistic description of the interface and the coarse-grained (CG) description of the lagging dislocations away from the interface within one single framework. Our major findings are: (a) the interface dynamically responds to a pileup by forming steps/ledges, the height of which is proportional to the number of dislocations arriving at the interface; (b) the pileup-induced internal stress concentration profile follows neither the classical Eshelby model nor the super-dislocation model alone, but a combination of them; (c) when the pre-sheared sample is compressed, a direct square-to-hexagonal PT occurs ahead of the pileup tip and eventually grows into a wedge shape. The two variants of the hexagonal phases form a twin with respect to each other; (d) upon a further increase of the loading, part of the newly formed hexagonal phase transforms back to the square phase. The square product phase resulting from this reverse PT forms a twin with respect to the initial square phase. All phase boundaries (PBs) and twin boundaries (TBs) are stationary and correspond to zero thermodynamic Eshelby driving forces; and (e) the microscale dislocation pileup-induced internal shear stress and the structural change at the atomic-scale interface reduces the stress required for initiating a PT by a factor of 5.5, comparing with that in the sample containing no dislocations. This work is the first characterization of the behavior of PTs/twinning resulting from the reaction between a microscale dislocation slip and an atomically structured interface. In conclusion, the gained knowledge will advance our understanding of how the multi-phase material behaves in many complex physical processes, such as the synthesis of multi-phase high-entropy alloys or superhard ceramics under high-pressure torsion, deep mantle earthquakes in geophysics, and so on, which all involve dislocation slip, PTs, twinning, and their interactions across from the atomistic to the microscale and beyond.

36 MATERIALS SCIENCE↗

Structure, Chemistry, and Charge Transfer Resistance of the Interface between Li 7 La 3 Zr 2 O 12 Electrolyte and LiCoO 2 Cathode

All-solid-state batteries promise significant safety and energy density advantages over liquid-electrolyte batteries. The interface between the cathode and the solid electrolyte is an important contributor to charge transfer resistance. Strong bonding of solid oxide electrolytes and cathodes requires sintering at elevated temperatures. Knowledge of the temperature dependence of the composition and charge transfer properties of this interface is important for determining the ideal sintering conditions. To understand the interfacial decomposition processes and their onset temperatures, model systems of LiCoO 2 (LCO) thin films deposited on cubic Al-doped Li 7 La 3 Zr 2 O 12 (LLZO) pellets were studied as a function of temperature using interface-sensitive techniques. X-ray photoelectron spectroscopy, secondary ion mass spectroscopy, and energy-dispersive X-ray spectroscopy data indicated significant cation interdiffusion and structural changes starting at temperatures as low as 300 °C. La 2 Zr 2 O 7 and Li 2 CO 3 were identified as decomposition products after annealing at 500 °C by synchrotron X-ray diffraction. X-ray absorption spectroscopy results indicate the presence of also LaCoO 3 in addition to La 2 Zr 2 O 7 and Li 2 CO 3 . On the basis of electrochemical impedance spectroscopy and depth profiling of the Li distribution upon potentiostatic hold experiments on symmetric LCO|LLZO|LCO cells, the interfaces exhibited significantly increased impedance, up to 8 times that of the as-deposited samples after annealing at 500 °C. Here, our results indicate that lower-temperature processing conditions, shorter annealing time scales, and CO 2 -free environments are desirable for obtaining ceramic cathode|electrolyte interfaces that enable fast Li transfer and high capacity.

25 ENERGY STORAGE↗