Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Exceptional strength and wear resistance in an AA7075/TiB 2 composite fabricated via friction consolidation

The friction consolidation method successfully reinforced aluminum 7075 alloy (AA7075) with high-volume fractions (12 and 24 vol%) of titanium diboride (TiB 2 ) by high pressure and severe plastic deformation at elevated temperatures. The consolidated AMCs have a uniform dispersion of submicron- and micron-sized TiB 2 particles in the AA7075 matrix, with significant refinement of the matrix grain size and the particles. The addition of TiB 2 significantly increases hardness by up to 50 %, Young’s modulus by up to 62 %, and ultimate tensile strength by up to 28 % to 672 MPa, while reducing ductility by 80 %. Wear resistance of 7075/24 vol% TiB 2 improves seven-fold compared to baseline, making it comparable to that of carburized steels. Microstructure-based finite element modeling provided a theoretical strength limit of ~730 MPa for the composites and indicated that high triaxiality in conjunction with severe equivalent plastic strain in a narrow area between the TiB 2 particles led to early fracture initiations, limiting the ductility.

36 MATERIALS SCIENCE↗

Dispersoid Distribution and Microstructure in Fe-Cr-Al Ferritic Oxide Dispersion-Strengthened Alloy Prepared by Friction Consolidation

INCOLOY® MA956 is a ferritic Oxide Dispersion Strengthened (ODS) alloy. Three different oxides, Y4Al2O9, YAlO3 and Y3Al5O12, have been observed in this alloy. The oxide particle sizes range from just a few up to hundreds of nm and these particles are responsible of the high temperature mechanical strength of this alloy. Mechanically alloyed MA956 powder was consolidated via Friction Consolidation using three different processing conditions. As a result, three small compacts of low porosity were produced. The compacts exhibited a refined equiaxed grain structure with grain sizes smaller than 10 µm and the desired oxide dispersion.YAlO3 and Y3Al5O12 were identified in the compacts by Scanning Electron Microscopy (SEM), Electron Dispersive Spectroscopy (EDS) and X-ray diffraction (XRD). The size distribution of precipitates above 50 nm showed a direct proportionality between average precipitate size and grain size. The total energy input during processing was correlated with the relative amount of each of the oxides in the disks: the higher the total processing energy input, the higher the relative amount of Y3Al5O12 precipitates. The elemental composition of the oxide precipitates was also probed individually by EDS showing an aluminum enrichment trend as precipitates grow in size.

Dispersoids↗

Microstructure Evolution and Mechanical Properties of the AZ91 Magnesium Alloy with Sr and Ti Additions in the As-Cast and As-Aged Conditions

Effect of different amounts of Sr and Ti additions with T6 heat treatment on microstructure and mechanical properties of the AZ91 alloy was investigated. The microstructure of the AZ91 alloy is consisted of the α-Mg phase surrounded by the semicontinuous network of β-Mg{sub 17}Al{sub 12} intermetallics. The average grain size and volume fraction of β phase decreased up to 1 wt.% Sr and 0.1 wt.% Ti additions. Exceeding Ti additions led to increase in both grain size and volume fraction. It was found that the grain refinement mechanism of AZ91 alloys with Sr additions was grain restriction factor. Also, 0.1 wt.% Ti addition could refine the grain structure of the AZ91 alloy by the formation of Al{sub 3}Ti particles that act as nucleation sites for the α-Mg phase. Furthermore, adding 1 wt.% Sr and 0.1 wt.% Ti enhanced the hardness values for both cast and aged AZ91 alloy. Moreover, ultimate tensile strength and tensile elongation values reached their maximum amounts with the 0.5 wt.% Sr and 0.1 wt.% Ti additions and more Sr and Ti additions deteriorated the mechanical properties of cast and aged AZ91 alloys. The fracture surface characterizations had good relations with the tensile properties. The fracture modes were cleavage and quasi-cleavage in the cast and aged AZ91 alloys. Furthermore, the optimum levels of Sr and Ti additions altered the fracture modes to more quasi-cleavage fractures.

36 MATERIALS SCIENCE↗

Spall damage of a Ta particle-reinforced metallic glass matrix composite under high strain rate loading

We investigate deformation and damage of a Zr-based bulk metallic glass (BMG) and its Ta particle-reinforced composite (MGMC) under impact loading, as well as quasi-static tension for comparison. Yield strength, spall strength, and damage accumulation rate are obtained from free-surface velocity histories, and MGMC appears to be more damage-resistant. Scanning electron microscopy, electron back scattering diffraction and x-ray computed tomography, are utilized for characterizing microstructures, which show features consistent with macroscopic measurements. Different damage and fracture modes are observed for BMG and MGMC. Multiple well-defined spall planes are observed in BMG, while isolated and scattered cracking around reinforced particles dominates fracture of MGMC. Particle–matrix interface serves as the source and barrier to crack nucleation and propagation under both quasi-static and impact loading. Finally, deformation twinning and grain refinement play a key role in plastic deformation during shock loading but not in quasi-static loading. In addition, 3D cup-cone structures are resolved in BMG, but not in MGMC due to its heterogeneous stress field.

36 MATERIALS SCIENCE↗

Heterogeneous in-situ nanostructure contributes to the thermoelectric performance of Zn{sub 4}Sb{sub 3}

Single-phase Zn{sub 4}Sb{sub 3} and ZnSb-containing samples were prepared by Plasma Activated Sintering. An abrupt decrease of thermal conductivity was found at about 400 K, which is attributed to the microstructure change of Zn{sub 4}Sb{sub 3}. Nanoscale inclusions and compositional inhomogeneities were found in Zn{sub 4}Sb{sub 3} sample at 473 K by high-resolution transmission electron microscopy. The phonon scattering is enhanced by increasing grain boundaries and chaotic structure, which reduces the thermal conductivity and increases the thermoelectric performance of Zn{sub 4}Sb{sub 3} at elevated temperature. The Rietveld refinement results show that large ZnSb grains in ZnSb-containing samples will accommodate excess Zn atoms, and then reduce thermoelectric performance.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Nano-Y{sub 2}O{sub 3} on Microstructure and Crack Formation in Laser Direct-Deposited In Situ Particle-Reinforced Fe-Based Coatings

In situ hard-particle-reinforced Fe-based composite coatings were prepared on Q235 steel substrates by direct laser deposition using Fe-based alloy powders containing 2 wt.% B, 3 wt.% Si and 1-3 wt.% nano-Y{sub 2}O{sub 3}. The microstructures, phase compositions, hardnesses and wear resistances of the deposited coatings with different nano-Y{sub 2}O{sub 3} contents were studied using metallographic microscopy, scanning electron microscopy, x-ray diffraction, transmission electron microscopy, microhardness tests and pin-on-disk abrasion tests (MMW-1A), respectively. The results showed that the appropriate addition of Y{sub 2}O{sub 3} played a role in grain refinement and in decreasing the number of brittle phases and impurity elements in the grain boundaries. Consequently, the number of cracks in the laser-deposited coating also decreased. The Fe-based composite coatings were mainly composed of α-Fe, γ-Fe and in situ-produced reinforced particle phases, such as Cr{sub 23}C{sub 6}, Cr{sub 7}C{sub 3}, (Cr, Fe){sub 7}C{sub 3}, Fe{sub 2}B, and CrFeB. When the content of nano-Y{sub 2}O{sub 3} was 2 wt.%, a Fe-based composite coating with a thickness of 4 mm that was free of cracks was obtained, and its surface hardness reached 650HV. Moreover, the wear resistance of the coating with 2 wt.% nano-Y{sub 2}O{sub 3} was the best among the samples studied. The presence of nano-Y{sub 2}O{sub 3} increased the solubility of Cr and Si in the solid solution, which eliminated the residual austenite region, and as a result, the phase transformation from γ-Fe to α-Fe was restrained and the transformation stress was also limited, thereby decreasing the probability of cracks in the coatings.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Developing ductile and isotropic Ti alloy with tailored composition for laser powder bed fusion

Laser powder bed fusion (LPBF) is an advanced technology to create metallic components with complex geometry. Ti-6Al-4V (Ti64) is one of the most frequently used materials for LPBF. The intrinsic high cooling rates and ultra-high directional thermal gradient of melt, however, lead to a hierarchical structure composed of fine martensitic alpha' within columnar prior-beta grains in LPBF Ti64. This microstructure results in poor ductility and strong mechanical anisotropy in as-built Ti64 components, which largely limit their applications. Here, we report that the above shortcomings can be overcome by tailoring the alloy composition. Specifically, by reducing the aluminum content from 6 wt% to 4 wt%, the resultant LPBF Ti-4Al-4V (Ti44) alloy exhibits substantially improved ductility and mechanical isotropy. These improvements are attributed to grain refinement during solidification and the activation of multiple slip modes and twinning in the as-built material during deformation. This work offers a simple strategy to design new titanium alloys for LPBF with significantly improved ductility and isotropy.

36 MATERIALS SCIENCE↗

Development of nano-structured duplex and ferritic stainless steels by pulverisette planetary milling followed by pressureless sintering

Nano-structured duplex and ferritic stainless steel powders are prepared by planetary milling of elemental Fe, Cr and Ni powder for 40 h and then consolidated by conventional pressureless sintering. The progress of milling and the continuous refinement of stainless steel powders have been confirmed by means of X-ray diffraction and scanning electron microscopy. Activation energy for the formation of duplex and ferritic stainless steels is calculated by Kissinger method using differential scanning calorimetry and is found to be 159.24 and 90.17 KJ/mol respectively. Both duplex and ferritic stainless steel powders are consolidated at 1000, 1200 and 1400 °C in argon atmosphere to study microstructure, density and hardness. Maximum sintered density of 90% and Vickers microhardness of 550 HV are achieved for duplex stainless steel sintered at 1400 °C for 1 h. Similarly, 92% sintered density and 263 HV microhardness are achieved for ferritic stainless steel sintered at 1400 °C. - Highlights: • Synthesized duplex and ferritic stainless steels by pulverisette planetary milling • Calculated activation energy for the formation of duplex and ferritic stainless steels • Studied the effect of sintering temperature on density, hardness and microstructure • Duplex stainless steel exhibits 90% sintered density and microhardness of 550 HV. • Ferritic stainless steel shows 92% sintered density and 263 HV microhardness.

36 MATERIALS SCIENCE↗

3D Morphology of Bimodal Porous Copper with Nano-Sized and Micron-Sized Pores to Enhance Transport Properties for Functional Applications

Multiscale porous metals with multiscale porosity from nanometer to micrometer have a high specific surface area and high effective diffusivity for ion transport, thereby enhancing functionalities and extending the applications of porous metals. Herein, the Cu–Fe–Al ternary system was selected as the precursor alloy to construct multiscale, bimodal porous copper by the chemical dealloying method. The effect of the phase composition and initial microstructure of precursor alloys (Al x Fe 75– x Cu 25 , x = 10–60) on the three-dimensional (3D) morphology of multiscale porous metals was systematically investigated, with a goal to precisely control the multiscale porous structure. The four crystal structure phases (body-centered cubic (BCC), face-centered cubic (FCC), CsCl type (B2), and monoclinic) in precursor alloys were analyzed by synchrotron X-ray diffraction refinement. The 3D morphology, feature size distribution, and tortuosity of four representative porous Cu after dealloying Al x Fe 75– x Cu 25 ( x = 10, 30, 50, and 60) precursor alloys were directly visualized and quantified via advanced synchrotron X-ray nanotomography. The relationship between the phases/crystal structures of precursor alloys and their corresponding porous morphology was established: the micron-sized pores in bimodal porous Cu are formed by dissolving the CuFeAl phase with BCC and monoclinic crystal structures, and the nano-sized pores are formed by dealloying the CuFeAl phase with FCC and B2 crystal structures. The size of the nanoporous structure depends on the ratio between the more noble and more active components in the precursor alloy, while the size of the microporous structure depends on the corresponding phase size in the precursor alloy. The tortuosity results showed that the multiscale porous structure with both nanoporosity and microporosity exhibits lower tortuosity, which will enhance transport properties for functional applications.

25 ENERGY STORAGE↗

Characterization of Preliminary Powder Production and Consolidation for Advanced LEU Fuel Concepts

A set of novel uranium-based alloys has been proposed for use in advanced LEU fuel systems that utilize powder metallurgical methods for fabrication of the fuel forms. This study seeks to evaluate the effectiveness of current fabrication methods to produce powder of each of the candidate alloys and consolidate composite systems. Powder samples were produced via atomization and analyzed for particle size, shape, and microstructure utilizing sieving methods and scanning electron microscopy (SEM). Preliminary pellet consolidation tests were conducted with the atomized powder using a press and sinter method. The resulting pellets were analyzed via SEM to evaluate the morphology of the composite system. These preliminary tests demonstrate the ability to produce powder but did not yield the desired quality of powder and impacted the ability to fabricate a fully dense pellet. A refined process is under development to produce a higher yield of small (<250 µm) spherical powder.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

UPDATE ON THE STATUS OF ODS ALLOYS FOR FOSSIL ENERGY APPLICATIONS

The goal of this effort is to generate data that demonstrate and quantify the improvements made earlier in this project in joining, microstructural modifications to minimize isotropy effects, and environmental lifetime modeling, in terms that can be readily assessed by potential users of oxide dispersion-strengthened (ODS) alloys. A report has been prepared compiling results from literature reports of ODS alloy joining trials to provide a comprehensive documentation of the methods, procedures, and resulting microstructures and mechanical properties of joining methods available for use with ODS alloys. This report will be updated as continuing evaluations of joining techniques are completed and the results reported. Some further results from joining using pulsed plasma-assisted diffusion bonding, and transient liquid phase bonding are reported here. Long-term environmental exposures of representative ODS FeCrAl alloys in air have been completed, and data required for refinement of an oxidation-limited life-prediction model developed earlier are being generated from post-test analyses. Continuing exposures in a CO2-steam mixture (at 1100 C in 500h cycles) have exceeded 3kh, and results so far indicate a greater degree of scale spallation than observed in air (in 100 h cycles), starting at 1 to 2kh for ODS alloys MA956 and PM2000, whereas much less scale spallation was observed for a non-ODS (weaker) model FeCrAlY alloy.

36 MATERIALS SCIENCE↗

UPDATE ON THE STATUS OF ODS ALLOYS FOR FOSSIL ENERGY APPLICATIONS

The goal of this effort is to generate data that demonstrate and quantify the improvements made earlier in this project in joining, microstructural modifications to minimize isotropy effects, and environmental lifetime modeling, in terms that can be readily assessed by potential users of oxide dispersion-strengthened (ODS) alloys. A report has been prepared compiling results from literature reports of ODS alloy joining trials to provide a comprehensive documentation of the methods, procedures, and resulting microstructures and mechanical properties of joining methods available for use with ODS alloys. This report will be updated as continuing evaluations of joining techniques are completed and the results reported. Some further results from joining using pulsed plasma-assisted diffusion bonding, and transient liquid phase bonding are reported here. Long-term environmental exposures of representative ODS FeCrAl alloys in air have been completed, and data required for refinement of an oxidation-limited life-prediction model developed earlier are being generated from post-test analyses. Continuing exposures in a CO2-steam mixture (at 1100 C in 500h cycles) have exceeded 3kh, and results so far indicate a greater degree of scale spallation than observed in air (in 100 h cycles), starting at 1 to 2kh for ODS alloys MA956 and PM2000, whereas much less scale spallation was observed for a non-ODS (weaker) model FeCrAlY alloy.

Wright, Ian G↗

High-pressure synthesis, crystal structure and magnetic property of ilmenite-type FeGeO{sub 3}

We synthesized well-crystallized ilmenite-type FeGeO{sub 3} to investigate its structural and magnetic properties. Ilmenite-type FeGeO{sub 3} were synthesized by high-pressure synthesis technique using a Kawai-type multi-anvil apparatus. Their structural and magnetic properties were examined by XRD analysis with Rietveld refinement, transmission electron microscopy, Moessbauer spectroscopy and SQUID-magnetization measurements. The subsequent annealing after the high-pressure synthesis was effective to improve the crystallinity of the ilmenite-type FeGeO{sub 3}. The primary particle size of ilmenite-type FeGeO{sub 3} was {approx}15 nm. Some particles seemed to be covered with non- or poorly crystalline phase even after the annealing, and others showed a lamellar microstructure parallel to the (0 0 1) plane. Theilmenite-type FeGeO{sub 3} showed typical antiferromagnetic behavior with the Neel temperature of 79 K. - Graphical abstract: Crystal structure, transmission electron micrograph and temperature dependent susceptibility of ilmenite-type FeGeO{sub 3}. Highlights: Black-Right-Pointing-Pointer Ilmenite-type FeGeO{sub 3}, a novel polymorphism of FeGeO{sub 3} was successfully synthesized. Black-Right-Pointing-Pointer It was synthesized by using high pressure technique at 23.5 GPa at 500 Degree-Sign C. Black-Right-Pointing-Pointer Subsequent annealing in vacuum was effective to improve the crystallinity. Black-Right-Pointing-Pointer Its primary particle size was {approx}15 nm, and some grains had lamellar microstructure. Black-Right-Pointing-Pointer It showed typical antiferromagnetic behavior with the Neel temperature of 79 K.

36 MATERIALS SCIENCE↗

Microstructural and basic mechanical characteristics of ZA27 alloy-based nanocomposites synthesized by mechanical milling and compocasting

Particulate nanocomposites with the base of ZA27 alloy were synthesized using an innovative route, which includes mechanical milling and compocasting. Scrap from the matrix alloy and ceramic nanoreinforcements were mechanically milled using the ball-milling technique, which led to the formation of composite microparticles. The use of these particles in the compocasting process provided better wettability of ceramic nanoreinforcements in the semi-solid metal matrix, which resulted in a relatively good dispersion of the nanoreinforcements in nanocomposite castings. The presence of nanoreinforcements led to the grain refinement in the matrix of nanocomposites. The mechanical properties of the synthesized nanocomposites are improved and compared with the properties of the metal matrix. The observed increase in the hardness of nanocomposites with Al2O3 nanoreinforcements (20–30 nm) was 6.5% to 10.8%, while the yield strength of these nanocomposites has increased by 12.2% to 23.2%. The hardness and compressive yield strength of the nanocomposites with Al2O3 nanoparticles (100 nm) increased by 1.7% to 8.0% and 2.3% to 8.3%, respectively. The increase in hardness of the nanocomposites with SiC nanoparticles (50 nm) was 11.5% to 20.6%, while the increase in the yield strength was 15.6% to 24.5%. The greatest contribution to the overall strengthening in the synthesized nanocomposites is the result of increased dislocation density due to the difference in coefficients of thermal expansion for the matrix alloy and nanoreinforcements. © The Author(s) 2018.

60 APPLIED LIFE SCIENCES↗

Microstructure characterization of the stir zone of submerged friction stir processed aluminum alloy 2219

Aluminum alloy 2219-T6 was friction stir processed using a novel submerged processing technique to facilitate cooling. Processing was conducted at a constant tool traverse speed of 200 mm/min and spindle rotation speeds in the range from 600 to 800 rpm. The microstructural characteristics of the base metal and processed zone, including grain structure and precipitation behavior, were studied using optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Microhardness maps were constructed on polished cross sections of as-processed samples. The effect of tool rotation speed on the microstructure and hardness of the stir zone was investigated. The average grain size of the stir zone was much smaller than that of the base metal, but the hardness was also lower due to the formation of equilibrium θ precipitates from the base metal θ′ precipitates. Stir zone hardness was found to decrease with increasing rotation speed (heat input). The effect of processing conditions on strength (hardness) was rationalized based on the competition between grain refinement strengthening and softening due to precipitate overaging. - Highlights: • SZ grain size (∼ 1 μm) is reduced by over one order of magnitude relative to the BM. • Hardness in the SZ is lower than that of the precipitation strengthened BM. • Metastable θ′ in the base metal transforms to equilibrium θ in the stir zone. • Softening in the SZ results from a decrease of precipitation strengthening.

36 MATERIALS SCIENCE↗

Alloying Effects on Creep and Oxidation Resistance of Austenitic Stainless Steel Alloys Employing Intermetallic Precipitates

Microstructure evolution during creep testing at 750 C and 100 MPa of Fe-20Cr-30Ni-2Nb (at.%) alloys with and without 0.4 Si, 0.2 Zr or 5.0 Al additions has been studied, in order to explore the viability of Fe-rich austenitic stainless alloys strengthened by intermetallic phases. Fine Fe{sub 2}Nb Laves phase dispersions with the size of less than 1 {micro}m within the {gamma}-Fe matrix were obtained in the base and Si-modified alloys after aging at 800 C. The addition of Si helped to refine and stabilize the size of particles, resulting in finer and denser Fe{sub 2}Nb dispersion than that in the base alloy. The alloys with only solution heat-treatment exhibited superior creep resistance to the aged ones, which is due to dynamic precipitation of the Fe{sub 2}Nb Laves phase during creep testing with a size of 300-400 nm, resulting in more effective pinning of dislocations. The base alloy also showed the meta-stable {gamma}*-Ni{sub 3}Nb phase with a size of 50 nm during the transient state of the creep testing. The Zr-modified alloy achieved significant improvement of creep properties. This is hypothesized to be due to the stabilization of {delta}-Ni{sub 3}Nb phase relative to Fe{sub 2}Nb, resulting in the formation of multiple fine dispersions of stable intermetallic compounds of {delta} and Fe{sub 2}Nb within the {gamma}-Fe matrix. A small amount of a (Ni, Zr and Nb)-enriched unidentified phase was also observed. The addition of Al significantly improved the oxidation resistance because of the formation of protective alumina scales on the surface. The alloy also showed superior creep resistance to that of the base alloy due to the formation of a dense dispersion of spherical Ni{sub 3}Al, typically 30 nm in diameter. Collectively, these findings provide the alloy design basis for creep and oxidation-resistant austenitic stainless steel alloys via intermetallic precipitates.

36 MATERIALS SCIENCE↗

Fundamental Relationship of Microstructure and Ionic Conductivity of Amorphous LLTO as Solid Electrolyte Material

All-solid-state Li-ion batteries (ASSLiB) attracted lots of attention mainly due to their higher safety compared with commercial Li-ion batteries. The research of solid electrolyte is critical for the development of ASSLiB, and among all the candidates of solid electrolyte materials, amorphous Lithium Lanthanum Titanate Oxide (LLTO) is promising because of its outstanding electrochemical stability up to 12V. However, the fundamental relationship among the ionic conductivity, microstructure, and mechanism of Li ion transport is still unrevealed. In this study, both amorphous LLTO thin film and LLTO powder were successfully prepared by sol-gel process. In order to determine the relationship between microstructure and ionic conductivity, various annealing time at 500°C were applied. This work shows that the ionic conductivity increases from 2.32 × 10 -8 S/cm to 9.01 × 10 -6 S/cm with the annealing time before LLTO starts to crystallize and decreases back to ~1.6 × 10 -9 S/cm after the formation of crystal phase. The absolute value of difference is close to 3 orders of magnitude. Furthermore, the morphology of the thin film changes accordingly, solvent evaporation, surface refinement and crystallization phases would occur sequentially, and this indicates that there is an optimal synthesis condition for the LLTO film. However, the changes of structure, morphology and ionic conductivity does not affect activation energy. This will help researchers to find optimized synthesis condition of amorphous LLTO and potentially search for and design other solid electrolyte materials.

25 ENERGY STORAGE↗