Search NASA⌕ Search

SEARCH · Search NASA

Results for “Sputtering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Suppression of near-edge optical absorption band in sputter deposited HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminates containing nonmonoclinic HfO{sub 2}

Nanolaminates of polycrystalline (tetragonal+orthorhombic) HfO{sub 2} and amorphous Al{sub 2}O{sub 3} are sputter deposited on unheated fused SiO{sub 2}, air annealed at 573-1273 K, and analyzed by x-ray diffraction and spectrophometry. Significant O 2p{yields}Hf 5d interband absorption occurs in all films at energy E{>=}6.2 eV. For E<6.2 eV, films annealed below 1273 K retain a featureless optical absorption edge despite further crystallization. A band with a 5.65 eV onset concurrently develops with m-HfO{sub 2} crystallization after a 1273 K anneal, indicating this phase and not nanocrystallinity per se is responsible for increased absorption.

36 MATERIALS SCIENCE↗

Effect of Post-deposition Annealing on the Physical Properties of DC Magnetron Sputtered Molybdenum Oxide Films

Molybdenum oxide films were deposited on glass and single crystal silicon substrates held at room temperature by sputtering of molybdenum target in an oxygen partial pressure of 2xl0{sup -4} mbar. The MoO{sub 3} films were annealed in oxygen atmosphere at various temperatures in the range 473-673 K. The effect of annealing temperature on the structure, chemical binding configuration, and optical properties of the MoO{sub 3} films was studied. The X-ray diffraction studies revealed that the as-deposited MoO{sub 3} films were amorphous. It crystallizes into a layered orthorhombic phase by the post-deposition annealing at a temperature of 673 K. The Fourier transform infrared spectrum of the MoO{sub 3} films annealed at 473 K exhibits the absorption bands at 560, 840 and 995 cm{sup -1} related to the active stretching modes of MoO{sub 6} octahedra. When the films annealed at 673 K the intensity of the absorption band observed at 560 cm{sup -1} diminished and the band of 995 cm{sup -1} split into two bands of 995 and 1010 cm{sup -1} which are related to the zig--zag rows of layered structure of MoO{sub 3}. The optical band gap of the as-deposited and annealed films was 3.07 and 3.20 eV respectively. The refractive index increased with increase of annealing temperature.

36 MATERIALS SCIENCE↗

Ultraviolet and blue photoluminescence from sputter deposited Ge nanocrystals embedded in SiO{sub 2} matrix

Ge nanocrystals (NCs) embedded in silicon dioxide (SiO{sub 2}) matrix are grown by radio-frequency magnetron sputtering and studied in order to understand the origin of ultraviolet (UV) and blue photoluminescence (PL) from the NC-SiO{sub 2} system. Ge NCs of diameter 7-8 nm are formed after postdeposition annealing, as confirmed by transmission electron microscopy and Raman scattering studies. Optical Raman studies indicate the presence of strain in the embedded Ge NCs. Polarization dependent low frequency Raman studies reveal surface symmetrical and surface quadrupolar acoustic phonon modes of Ge NCs. PL studies with 488 nm excitation shows a broad emission band peaked at {approx}545 nm, which is attributed to oxygen deficient defects in the SiO{sub 2} matrix. PL studies with 325 nm excitation show additional strong peaks in the 377-400 nm region. Time resolved PL studies in the UV-blue range show double exponential decay dynamics in the nanosecond time scale, irrespective of the NC size. Comparative studies of PL emission from SiO{sub 2} layers with no Ge content and with Ge content show that the {approx}400 nm PL emission is originated from a defective NC/SiO{sub 2} interface and the band is not unique to the presence of Ge. PL excitation spectroscopy measurements show large Stokes shift for the UV emission bands. We propose that the intense UV peaks at {approx}377 nm is originated from the twofold coordinated silicon defect at the interface between NC and SiO{sub 2} matrix and it is not necessarily specific to the presence of Ge in the oxide matrix. It is believed that due to the influence of strain on the NCs and interface states, PL from quantum confined carriers may be partially quenched for the embedded Ge NCs.

36 MATERIALS SCIENCE↗

Microstructural properties of phosphorus-doped p-type ZnO grown by radio-frequency magnetron sputtering

Phosphorus (P)-doped ZnO thin films were grown by radio-frequency magnetron sputtering to study the microstructural properties of p-type ZnO. As-grown P-doped ZnO, a semi-insulator, was converted to p-type ZnO after being annealed at 800 deg. C in an N{sub 2} ambient. X-ray diffraction, secondary-ion-mass spectrometry, and Hall effect measurements indicated that P{sub 2}O{sub 5} phases in as-grown P-doped ZnO disappeared after thermal annealing to form a substitutional P at an O lattice site, which acts as an acceptor in P-doped ZnO. Transmission electron microscopy showed that the formation of stacking faults was facilitated to release the strain in P-doped ZnO during post-thermal annealing.

36 MATERIALS SCIENCE↗

Thermal behavior of the microstructure and the electrical properties of magnetron-sputtered high-k titanium silicate thin films

We report on the high-temperature stability of high-dielectric-constant (high-k) titanium silicate (Ti{sub 0.5}Si{sub 0.5}O{sub 2}) thin films deposited by means of a magnetron sputtering process. We have investigated the effect of substrate deposition temperature T{sub d} (in the 20-600 deg. C range) and postdeposition annealing temperature T{sub a} (in the 200-800 deg. C range) on the electrical, microstructural, and optical properties of the films. The Ti-silicate films grown at room temperature were found to exhibit a combination of excellent electrical properties, including a k-value of 16.5, a leakage current as low as 3 nA at 1 MV/cm, and a dissipation factor tan({delta})<0.01. On the other hand, when the processing temperature (T{sub d} or T{sub a}) is {>=}300 deg. C, the leakage current of the films is found to degrade progressively. The x-ray diffraction, Raman spectroscopy, and transmission electron microscopy characterizations have shown that the Ti-silicate films exhibit an amorphous microstructure up to a temperature of about 600 deg. C. For higher temperatures, (i.e., T{sub d} of 600 deg. C or a T{sub a}{>=}700 deg. C) some anatase TiO{sub 2} nanocrystallites (in the 1.5-5 nm size range) formation is evidenced. This TiO{sub 2} nanocrystallite precipitation results from a thermally induced phase segregation of TiO{sub 2}-rich and SiO{sub 2}-rich environments, which is shown to be initiated at rather low processing temperatures. This progressive phase segregation, which leads to the precipitation of a low band gap and leaky TiO{sub 2}-rich phase in the films, is believed to be at the origin of the observed degradation of the leakage current of the Ti-silicate films with increasing temperatures (T{sub d} or T{sub a})

36 MATERIALS SCIENCE↗

Coercivity generation of surface Nd{sub 2}Fe{sub 14}B grains and mechanism of fcc-phase formation at the Nd/Nd{sub 2}Fe{sub 14}B interface in Nd-sputtered Nd-Fe-B sintered magnets

The coercivity of surface grains of a Nd-Fe-B sintered magnet can be measured unequivocally if the magnet is a thin slab with the orientation of its c-axis parallel to the largest surface. Due to the loss of part of the neodymium-rich grain boundary phase, the surface Nd{sub 2}Fe{sub 14}B grains have low coercivity after machining. When a Nd layer is sputter deposited on the surface and annealed in the temperature range from 500 to 675 deg. C, the surface coercivity recovers to its full value, which is identical to the coercivity of the bulk magnet from which the slab was cut. Transmission electron microscopy has indicated the formation of a fcc interfacial phase having a lattice constant a=0.548 nm between the surface grains and the Nd layer in the specimen whose surface coercivity was recovered. In addition to a double hexagonal closed packed phase (metallic Nd), A-type Nd{sub 2}O{sub 3} has been observed in the inner region of the Nd film away from the interface. A-type Nd{sub 2}O{sub 3} having a hexagonal structure with a=0.382 nm and c=0.598 nm is the most stable phase of the neodymium oxides with 2:3 stoichiometry. Since the fcc phase is derived from metastable C-type Nd{sub 2}O{sub 3} having a cubic structure with a=1.108 nm, the fcc phase is also a metastable phase. Therefore it is considered that the formation of the fcc phase results from the interfacial energy with the Nd{sub 2}Fe{sub 14}B grains.

36 MATERIALS SCIENCE↗

Mixed cation phases in sputter deposited HfO{sub 2}-TiO{sub 2} nanolaminates

Nanolaminate HfO{sub 2}-TiO{sub 2} films are grown by reactive sputter deposition on unheated fused SiO{sub 2}, sequentially annealed at 573 to 973 K, and studied by x-ray diffraction. A nanocrystalline structure of orthorhombic (o) HfTiO{sub 4} adjacent to an interface followed by monoclinic (m) Hf{sub 1-x}Ti{sub x}O{sub 2} is identified. m-Hf{sub 1-x}Ti{sub x}O{sub 2}, a metastable phase, is isomorphous with m-HfO{sub 2} and a high pressure phase, m-HfTiO{sub 4}. A Vegard's law analysis shows that the Ti atomic fraction in m-Hf{sub 1-x}Ti{sub x}O{sub 2} is much greater than Ti equilibrium solubility in m-HfO{sub 2}. A space group-subgroup argument proposes that m-Hf{sub 1-x}Ti{sub x}O{sub 2} arises from an o/m-HfTiO{sub 4} second order phase transition to accommodate the larger Hf atom.

36 MATERIALS SCIENCE↗

Stripe domains and spin reorientation transition in Fe{sub 78}B{sub 13}Si{sub 9} thin films produced by rf sputtering

Magnetic thin films have been obtained by rf sputtering from an amorphous Fe{sub 78}B{sub 13}Si{sub 9} target. The samples have been produced with thickness t ranging in the interval 25-1000 nm. Microstructural investigations indicate that the films have different microstructures varying from fully amorphous to partially nanocrystalline with increasing t. Magnetic hysteresis loops have been measured by means of high-sensitive magnetometry. A tailorable spin reorientation transition (SRT) from in-plane single-domain-like to out-of-plane multidomain state with increasing film thickness was observed. Magnetic force microscopy images have been obtained for all samples indicating that for t{<=}80 nm the magnetization lies in the film plane. For larger thickness, a stripe domain pattern has been observed, indicating the presence of a magnetic anisotropy axis perpendicular to the film plane. In this work, SRT and stripe domain structure have been studied as a function of thickness and sample microstructure.

36 MATERIALS SCIENCE↗

Growth and structural characterization of (0.2)Bi(Zn{sub 1/2}Ti{sub 1/2})O{sub 3}-(0.8)PbTiO{sub 3} epitaxial thin films by off-axis rf sputtering

We report the epitaxial growth of ferroelectric (0.2)Bi(Zn{sub 1/2}Ti{sub 1/2})O{sub 3}-(0.8)PbTiO{sub 3} thin films. Despite its high c/a ratio, the off-axis rf magnetron sputtering yields the epitaxial growth of high-quality thin films on (001) SrTiO{sub 3} substrates. The structural development of the film with increasing film thickness has been examined by using the synchrotron x-ray diffraction and x-ray reflectivity. The experimental results can be explained in terms of the strain relaxation process associated with the misfit dislocations between the thin film and the substrate.

36 MATERIALS SCIENCE↗

Epitaxial growth of aluminum nitride on AlGaN by reactive sputtering at low temperature

We report the synthesis of 1 {mu}m thick single crystalline aluminum nitride films by dc magnetron sputtering on AlGaN/GaN layer grown on sapphire substrate at low temperature (substrate temperature <250 deg. C). The microstructure of c-axis oriented AlN films deposited on Si (100) and AlGaN <0001> substrates was studied by x-ray diffraction, selected area electron diffraction, and transmission electron microscopy. The optimization of process parameters, involving low energetic ion bombardment on film surface (20-30 eV) during the growth, leads to an increase in the surface mobility and thus promotes AlN epitaxial growth on AlGaN substrate at 250 deg. C.

36 MATERIALS SCIENCE↗

Sulphide Ga{sub x}Ge{sub 25-x}Sb{sub 10}S{sub 65(x=0,5)} sputtered films: Fabrication and optical characterizations of planar and rib optical waveguides

We report the fabrication and the physical and optical characterizations of sulphide Ga{sub x}Ge{sub 25-x}Sb{sub 10}S{sub 65(x=0,5)} rib waveguides. High quality films fabricated on SiO{sub 2}/Si wafer substrates were obtained using the sputtering magnetron rf deposition method. The slab waveguides obtained without annealing present propagation losses of about 0.6 dB/cm at 1550 nm. These optical losses are not important for implementation in optical devices based on silicon-on-insulator or polymer, for instance, atomic force microscopy measurements revealed low interface roughness between the different media (substrate/film and film/air). Reactive ion etching was used to pattern rib waveguides between 2 and 300 {mu}m wide. The parameters were optimized to obtain a dry etching process that had low surface roughness, vertical sidewalls, etch depth of more than 1 {mu}m, and reasonable etching rate. This technique was used to fabricate Y optical junctions for optical interconnections on chalcogenide amorphous films. Their optical transmission was demonstrated by optical near field of guided modes and optical losses were measured and discussed.

36 MATERIALS SCIENCE↗

Observation of Ti{sup 4+} ions in a high power impulse magnetron sputtering plasma

Multiply charged titanium ions including Ti{sup 4+} were observed in high power impulse magnetron sputtering discharges. Mass/charge spectrometry was used to identify metal ion species. Quadruply charged titanium ions were identified by isotope-induced broadening at mass/charge 12. Due to their high potential energy, Ti{sup 4+} ions give a high yield of secondary electrons, which in turn are likely to be responsible for the generation of multiply charged states.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Impact of magnetron configuration on plasma and film properties of sputtered aluminum nitride thin films

We have investigated the growth of the c-axis oriented aluminum nitride (AlN) thin films on (100) silicon by reactive dc magnetron sputtering at low temperature, considering the effect of the magnet configuration on plasma and film properties. It appears that a magnet modification can significantly modify both the plasma characteristics and the film properties. Electrical and optical characterizations of the plasma phase highlight that depending on the magnet configuration, two very different types of deposition process can be involved in the same deposition chamber. On the one hand, with a balanced magnetron (type 1), the deposition process enhances the production of AlN dimers in the plasma phase and enables to synthesize AlN films with different preferential orientations (100, 002, and even 101). On the other hand, a strongly unbalanced magnetron (type 2) provides a limited production of AlN species in the plasma phase and a strong increase in the ratio of ions to metal atom flux on the growing films. In the latter case, the ion energy provided by the ion flux to the growing film is typically in the 20-30 eV range. Thus, dense (002) oriented films with high crystalline quality are obtained without any substrate heating.

36 MATERIALS SCIENCE↗

Optical and electrical characterization of sputter-deposited FeSi{sub 2} and its evolution with annealing temperature

Optical and electrical properties of sputter-deposited FeSi{sub 2} thin films on p-Si(100) and SiO{sub 2}/p-Si(100) substrates as well as their evolution with rapid thermal annealing (RTA) temperature have been investigated. Optical absorption measurements were carried out to determine the absorption spectra of FeSi{sub 2} based on the proposed optical absorption model for the double-layer and triple-layer structures. A direct band gap behavior was concluded for both amorphous and polycrystalline semiconducting FeSi{sub 2}. An absorption coefficient in the order of 10{sup 5} cm{sup -1} at 1 eV and a band gap value of {approx}0.86 eV were obtained for the {beta}-FeSi{sub 2}. Hall effect measurements at room temperature indicate heavily doped and n-type conductivity for the FeSi{sub 2} films on p-Si, whose residual carrier concentration was found to be closely correlated with the observed subgap optical absorption via band tailing. The carrier mobility was shown to increase with decreasing residual carrier concentration when the RTA temperature was increased.

36 MATERIALS SCIENCE↗

Room temperature photoluminescence of CdTe nanocrystals embedded in a SiO{sub 2} matrix deposited on silicon by reactive rf sputtering

CdTe nanocrystals embedded in a SiO{sub 2} matrix were fabricated by radio frequency sputtering employing the texture of a SiO{sub 2} layer as template. The SiO{sub 2} film texture was controlled through the O{sub 2} partial pressure (OPP) in the working atmosphere. The CdTe crystallinity was better for the samples synthesized on rougher SiO{sub 2} films. For these samples, the room temperature photoluminescence spectra showed a signal at 1.74 eV, related to the CdTe nanoparticles. Additional photoluminescence signals at 1.65 and 1.68 eV have been associated to recombination processes at the nanoparticle/matrix interfaces. The results indicate that the employed methodology produces, in a single step, CdTe nanoparticles with light emission at room temperature. After thermal annealing all the samples presented emission due to quantum confinement effects. The photoluminescence emission may be varied from 1.69 to 2.15 eV by appropriate control of the OPP.

36 MATERIALS SCIENCE↗

Dust Growth by RF Sputtering

The effect of the dust particle growth by RF sputtering on glow discharge has been investigated. It has been found that the growth of dust particles modifies the electrical characteristics of the discharge. In particularly, the absolute value of the self-bias voltage decreases during the particle growth due to the electron losses on the dust particles. To find the correlation between the dust growth and the self bias evolution, dust particles have been collected at different times. The dust particle growth rate is found to be linear.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Combined Thermochromic And Plasmonic: Optical Responses In Novel Nanocomposite Au-VO{sub 2} Films Prepared By RF Inverted Cylindrical Magnetron Sputtering

We prepared gold/Vanadium dioxide nanocomposites thin films by the rf reactive inverted cylindrical magnetron sputtering (ICMS) for the first time and report their enhanced surface plasmon resonance (SPR) tunable shift reversibility. ICMS has been attracting much attention for its ability for uniform coating of three-dimensional objects and high-rate deposition of dielectric materials. To investigate the optical properties of gold nanoparticles embedded in an active matrix (VO{sub 2}) composite film was synthesized on corning glass substrates for several substrate temperatures ranging from 400 deg. C to 600 deg. C. The X-ray diffraction results demonstrated that the Au and VO{sub 2} were well crystallized. The optical transmission properties were measured from 300nm to 1100nm and the absorption peak due to the surface plasmon resonance (SPR) of Au nanoparticles were observed. Under external temperature stimuli, the tunable reversibility of the SPR shift was observed when the nanocomposites temperature varies from 20 deg. C to 100 deg. C. The enhancement of this shift of SPR was observed as the substrate temperature increases and it was found that the shift of SPR increased rapidly with increasing substrate temperature but then remained constant at {approx}57 nm for substrate temperature higher than 500 deg. C.

36 MATERIALS SCIENCE↗

Structural Study And Optical Properties Of TiO{sub 2} Thin Films Elaborated By Thermal Oxidation Of RF Magnetron Sputtered Ti Films

We report on the effect of thickness on the structural and optical properties of TiO{sub 2} thin films obtained by direct exposure of Ti metal film to thermal oxidation. Ti thin films with thicknesses ranging from 87 nm to 484 nm were deposited onto glass substrate by RF magnetron sputtering. Thereafter, the as-deposited Ti films were annealed in air at temperature equal to 520 deg. C. The structural evolution and optical properties of obtained TiO{sub 2} films were studied by means of Rutherford backscattering spectrometry (RBS), grazing incidence X-ray diffraction (GIXRD), scanning electron microscopy (SEM) and UV-Visible spectroscopy. The films thicknesses were extracted from RBS spectra. From X-ray diffraction spectra, we can see that all the films present three TiO{sub 2} phases (anatase, rutile and Brookite). The anatase and rutile phases exhibit a strong preferred orientation along (004) and (210) planes respectively. The grain sizes, D (nm), did not change much with increasing thickness. The average value of <D>(nm) was equal to 29 nm for anatase and 26 nm for rutile. The micrographs taken from SEM experiments indicate that the films present a dense micro structure with very small grains. Transmittance spectra show that all the films present a good transparency in the visible region. The dependence of transmittance, optical band gap and refractive index on the thickness of the films was also studied.

36 MATERIALS SCIENCE↗