Search NASA⌕ Search

SEARCH · Search NASA

Results for “BOROSILICATE GLASS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Spherical gold nanoparticles and SiO{sub 2}/Au core/shell microparticles under intense femtosecond laser excitation: relaxation dynamics of gold nanoparticles and nanostructuring of borosilicate glass using SiO{sub 2}/Au microparticles

This paper reports surface nanostructuring of borosilicate glass covered with a water layer and the production of ∼150 nm diameter pits using SiO{sub 2}/Au core/shell microparticles under excitation with 50 fs pulses (λ = 780 nm) using the optical scheme of an inverted microscope with a 100{sup ×}, NA = 1.4 objective. We compare the thresholds for hole formation in glass with the use of SiO{sub 2}/Au and uncoated SiO{sub 2} microparticles. The threshold is 0.7 J cm{sup -2} for SiO{sub 2}/Au and 2.9 J cm{sup -2} for SiO{sub 2} microparticles, which coincides with the threshold for nanostructuring by a focused femtosecond pulse without microparticles: 3 J cm{sup -2}. Femtosecond pump – probe spectroscopy has been used to study the relaxation dynamics of laser pulse energy absorbed in a Au nanoparticle and the dynamics of energy dissipation to the ambient medium. The threshold for cavitation bubble formation in water with SiO{sub 2}/Au has been determined to be 0.06 mJ cm{sup -2}, which is a factor of 30 lower than the bubble formation threshold in the case of uncoated SiO{sub 2} microparticles. (nanostructures)

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Interaction of Embedded TRISO Particles with Melt of Alkaline Borosilicate Glass (ABG) - 12008

Spent tri-isotropic (TRISO) fuel particles are a high-level waste contained within a graphite compact/pebble, which is an intermediate-level waste. In this research, the particles were extracted from their graphite matrix with a use of aqueous HNO{sub 3}/H{sub 2}SO{sub 4} solution. The intercalation process produced three types of particles with different thickness of outer layers. The damage to the outer layers of TRISO particles can cause an undesirable release of fission products from the kernel of the particle. Alkaline borosilicate glass (ABG) was used as an encapsulating matrix in order to prevent the release of fission products from kernels. The aim of the research is to investigate an interaction of embedded TRISO particles with Melt of Alkaline Borosilicate Glass (ABG), and elucidate a chemical bonding and an interface formation between them. Particular emphasis was placed on the analysis of the intermediate chemical phase at the interface SiC/ABG as a function of the material impurity and thickness of the SiC layer. The findings revealed that there is a strong wetting angle between the SiC layer and the ABG and it can completely diminish the layer. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Deep-UV Raman spectroscopic analysis of structure and dissolution rates of silica-rich sodium borosilicate glasses

As part of ongoing studies to evaluate the relationships between structural variations in silicate glasses and rates of glass dissolution in aqueous media, molecular structures present in sodium borosilicate glasses of composition Na2O.xB2O3.(3-x)SiO2, with x 1 (Na2O/B2O3 ratio 1), were analyzed using deep-UV Raman spectroscopy. The results were quantified in terms of the fraction of SiO4 tetrahedra with one non-bridging oxygen (Q3) and then correlated with Na2O and B2O3 content. Increasing Na2O was found to raise the fraction of Q3 units in the glasses systematically, in agreement with studies on related glasses, and, as long as the value of x was not too high, contribute to higher rates of dissolution in single pass flow-through testing. The finding was obtained across more than one series of silica-rich glasses prepared for independent dissolution studies. In contrast, dissolution rates were less strongly determined by the Q3 fraction when the value of x was near unity and appeared to grow larger upon further reduction of the Q3 fraction. The results were interpreted to indicate the increasingly important role of network hydrolysis in the glass dissolution mechanism as the BO4 tetrahedron replaces the Q3 unit as the charge-compensating structure for Na+ ions. Finally, the use of deep-UV Raman spectroscopy was found to be advantageous in studying finely powdered glasses in cases where visible Raman spectroscopy suffered from weak Raman scattering and fluorescence interference.

36 MATERIALS SCIENCE↗

Effects of He Ion Irradiation in Simple Borosilicate Glasses for HLW Immobilisation - 20324

High-level radioactive waste (HLW) consists of fission products and minor actinides. Borosilicate glass is the host material of choice in most countries to safely immobilize HLW, followed by eventual geological disposal. HLW glasses will experience both self-heating and self-irradiation effects due to the decay of fission products and minor actinides present therein. During the first 500 years of geological disposal, beta-gamma decay will be the main source of radiation due to short half-lives of fission products, as compared to very long-lived actinides which will be responsible for irradiation over much longer timescales. High-energy alpha particles and alpha recoil nuclei can potentially have significant impact (stored energy, volume change, accumulated dose, chemical durability) on the performance of the wasteform over longer timescales. Thus, to ensure safe and economic disposal over geological periods (10{sup 4} - 10{sup 6} years), the assessment of performance and properties in terms of radiation effects becomes indispensable. This work aims to simulate the effects of alpha decay in radioactive waste glasses. Two international glasses, namely UK 'MW' lithium-sodium borosilicate and Indian sodium-barium borosilicate, which are being used as HLW immobilization matrices by the UK and India respectively, were prepared by a melt-quench method and annealed below their glass transition temperatures. Both glasses were irradiated with 650 KeV He{sup 2+} ions with doses ranging from 10{sup 15} to 10{sup 17} ions/cm{sup 2}. Structural analysis was carried out using electron paramagnetic resonance (EPR) and Raman spectroscopies. First derivative continuous wave EPR spectra were recorded for all pristine and irradiated glass monoliths at room temperature using an X-band (frequency 9.6 GHz) EPR Bruker spectrometer. Results from EPR analyses showed the formation of irradiation induced paramagnetic centers at g ∼ 2.00 in all irradiated glasses. Raman spectra of pristine and irradiated samples were acquired, and showed notable changes in glass structure post-irradiation, with the emergence of a broad Raman band at 1560 cm{sup -1} upon irradiation with high fluences. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

EVALUATION OF IMPURITY EXTREMES IN A PLUTONIUM-LOADED BOROSILICATE GLASS

A vitrification technology utilizing a lanthanide borosilicate (LaBS) glass appears to be a viable option for the disposition of excess weapons-useable plutonium that is not suitable for processing into mixed oxide (MOX) fuel. A significant effort to develop a glass formulation and vitrification process to immobilize plutonium was completed in the mid-1990s. The LaBS glass formulation was found to be capable of immobilizing in excess of 10 wt % Pu and to be tolerant of a range of impurities. To confirm the results of previous testing with surrogate Pu feeds containing impurities, four glass compositions were selected for fabrication with actual plutonium oxide and impurities. The four compositions represented extremes in impurity type and concentration. The homogeneity and durability of these four compositions were measured. The homogeneity of the glasses was evaluated using x-ray diffraction (XRD) and scanning electron microscopy coupled with energy dispersive spectroscopy (SEM/EDS). The XRD results indicated that the glasses were amorphous with no evidence of crystalline species in the glass. The SEM/EDS analyses did show the presence of some undissolved PuO{sub 2} material. The EDS spectra indicated that some of the PuO{sub 2} crystals also contained hafnium oxide. The SEM/EDS analyses showed that there were no heterogeneities in the glass due to the feed impurities. The durability of the glasses was measured using the Product Consistency Test (PCT). The PCT results indicated that the durability of Pu impurity glasses was comparable with Pu glasses without impurities and significantly more durable than the Environmental Assessment (EA) glass used as the benchmark for repository disposition of high-level waste (HLW) glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of Impurity Extremes in a Plutonium-loaded Borosilicate Glass

A vitrification technology utilizing a lanthanide borosilicate (LaBS) glass appears to be a viable option for the disposition of excess weapons-usable plutonium that is not suitable for processing into mixed oxide (MOX) fuel. A significant effort to develop a glass formulation and vitrification process to immobilize plutonium was completed in the mid-1990's. The LaBS glass formulation was found to be capable of immobilizing in excess of 10 wt % Pu and to be tolerant of a range of impurities. To confirm the results of previous testing with surrogate Pu feeds containing impurities, four glass compositions were selected for fabrication with actual plutonium oxide and impurities. The four compositions represented extremes in impurity type and concentration. The homogeneity and durability of these four compositions were measured. The homogeneity of the glasses was evaluated using x-ray diffraction (XRD) and scanning electron microscopy coupled with energy dispersive spectroscopy (SEM/EDS). The XRD results indicated that the glasses were amorphous with no evidence of crystalline species in the glass. The SEM/EDS analyses did show the presence of some undissolved PuO{sub 2} material. The EDS spectra indicated that some of the PuO{sub 2} crystals also contained hafnium oxide. The SEM/EDS analyses showed that there were no heterogeneities in the glass due to the feed impurities. The durability of the glasses was measured using the Product Consistency Test (PCT). The PCT results indicated that the durability of Pu impurity glasses was comparable with Pu glasses without impurities and significantly more durable than the Environmental Assessment (EA) glass used as the benchmark for repository disposition of high-level waste (HLW) glasses. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Deformation mechanisms during nanoindentation of sodium borosilicate glasses of nuclear interest

In this paper we analyze results of Molecular Dynamics simulations of Vickers nanoindentation, performed for sodium borosilicate glasses of interest in the nuclear industry. Three glasses have been studied in their pristine form, as well as a disordered one that is analogous to the real irradiated glass. We focused in the behavior of the glass during the nanoindentation in order to reveal the mechanisms of deformation and how they are affected by microstructural characteristics. Results have shown a strong dependence on the SiO{sub 2} content of the glass, which promotes densification due to the open structure of SiO{sub 4} tetrahedra and also due to the strength of Si-O bonds. Densification for the glasses is primarily expressed by the relative decrease of the Si-O-Si and Si-O-B angles, indicating rotation of the structural units and decrease of free volume. The increase of alkali content on the other hand results to higher plasticity of the matrix and increased shear flow. The most important effect on the deformation mechanism of the disordered glasses is that of the highly depolymerized network that will also induce shear flow and, in combination with the increased free volume, will result in the decreased hardness of these glasses, as has been previously observed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atom Probe Tomography Investigation of Clustering in Model P 2 O 5 -Doped Borosilicate Glasses for Nuclear Waste Vitrification

Atom probe tomography (APT) has been utilized to investigate the microstructure of two model borosilicate glasses designed to understand the solubility limits of phosphorous pentoxide (P 2 O 5 ). This component is found in certain high-level radioactive defence wastes destined for vitrification, where phase separation can potentially lead to a number of issues relating to the processing of the glass and its long-term chemical and structural stability. The development of suitable focused ion beam (FIB)-preparation routes and APT analysis conditions were initially determined for the model glasses, before examining their detailed microstructures. In a 3.0 mol% P 2 O 5 -doped glass, both visual inspection and sensitive statistical analysis of the APT data show homogeneous microstructures, while raising the content to 4.0 mol% initiates the formation of phosphorus-enriched nanoscale precipitates. This study confirms the expected inhomogeneities and phase separation of these glasses and offers routes to characterizing these at near-atomic scale resolution using APT.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of the iron content and redox state on the structure of sodium borosilicate glasses: A Raman, Moessbauer and boron K-edge XANES spectroscopy study

The structure of iron-bearing sodium borosilicate glasses with up to 10 mol% FeO has been investigated in the range 0.15 ≤ Fe{sup 3+}/SFe ≤ 0.95. According to Moessbauer spectroscopy, Fe{sup 3+} and Fe{sup 2+} are mainly in tetrahedral and octahedral coordination, respectively, although other coordination states exist for both cations. From XANES experiments, we conclude that increasing Fe content and varying redox states have only a minor effect on the relative proportions of BO{sub 3} and BO{sub 4} units. In Raman spectra, a decrease of the proportion of BO{sub 4} species present in danburite-like units (Na{sub 2}O.B{sub 2}O{sub 3}.2SiO{sub 2}) is found upon increasing iron content and oxidizing state. Whereas the insensitivity of the overall boron speciation to iron content and redox state points to weak interactions between boron and iron, the changes affecting BO{sub 4} species do indicate a more subtle interplay between Fe{sup 3+} and the other tetrahedrally coordinated cations (Si,B) because of the competition between tetrahedral Fe{sup 3+} and B{sup 3+} for charge compensation by Na{sup +}. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

X-ray irradiation-induced ionization of CdS{sub 1-x}Se{sub x} nanocrystals embedded in borosilicate glass

Optical absorption spectra of x-ray irradiated CdS{sub 1-x}Se{sub x} nanocrystals embedded in a borosilicate glass matrix are studied. The observed transformation of the confinement-related features in the spectra is related to the x-ray-induced negative ionization of the nanocrystals with charge transfer across the nanocrystal/matrix interface. The radiation-induced changes and their relaxation upon postirradiation storage as a function of nanocrystal size and composition are discussed.

36 MATERIALS SCIENCE↗

Incorporation and distribution of rhenium in a borosilicate glass melt heat treated in a sealed ampoule

We investigated a mass balance of rhenium (used as a surrogate for technetium-99) in a borosilicate glass that was mixed with excess Re source (KReO4) beyond its solubility and heat treated in a vacuum-sealed fused silica ampoule. Distribution of Re in the bulk of the glass, in a salt phase formed on the melt surface, and in condensate material deposited on the ampoule wall was evaluated to understand the Re migration into different phases during the reaction between the molten glass and KReO4. The information gained from this study will contribute to an effort to understand the mechanism of technetium retention in or escape from glass melt during early stages of glass batch melting, which is a goal of the present series of studies.

borosilicate glass↗

NM in HLW Borosilicate Glass: Focus on the High Performances of the IHMM Operated at La Hague Plant - 19019

Ruthenium, palladium and rhodium, which belong to Platinum-Group Metals (PGM), are part of fission products resulting from nuclear fuel reprocessing. All High Level Waste (HLW) vitrification facilities have experienced operational issues that can be related to the presence of Noble Metals (NM) in the melter. These metals have low solubility and modify glass properties such as viscosity or electrical and thermal conductivity. These dense metals also tend to settle to the bottom of the melter. Whatever the vitrification process operated, the specific properties and behavior of NM have a propensity to impact the production capacity by decreasing the glass throughput and increasing downtimes. Orano and the CEA have studied the behavior of NM in borosilicate glass for many years. It has led to several technological improvements and process operation optimizations on the Induction Heated Metallic Melter (IHMM) currently operated at La Hague plant. These enhancements, implemented since active commissioning, have headed to a high efficiency in terms glass production and NM incorporation (more than 21000 canisters produced with up to 3 % of Noble Metals in the glass). This paper sets out the continuous improvement program implemented on the La Hague vitrification lines that has led to outstanding records of operation in terms of production capacity and NM incorporation. The benefits of the close collaboration between R and D, engineering, and operation teams is particularly emphasized. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Process Parameter Effects on Material Removal in Magnetorheological Finishing of Borosilicate Glass

We investigate the effects of processing parameters on material removal for borosilicate glass. Data are collected on a magnetorheological finishing (MRF) spot taking machine (STM) with a standard aqueous magnetorheological (MR) fluid. Normal and shear forces are measured simultaneously, in situ, with a dynamic dual load cell. Shear stress is found to be independent of nanodiamond concentration, penetration depth, magnetic field strength, and the relative velocity between the part and the rotating MR fluid ribbon. Shear stress, determined primarily by the material mechanical properties, dominates removal in MRF. The addition of nanodiamond abrasives greatly enhances the material removal efficiency, with the removal rate saturating at a high abrasive concentration. The volumetric removal rate (VRR) increases with penetration depth but is insensitive to magnetic field strength. The VRR is strongly correlated with the relative velocity between the ribbon and the part, as expected by the Preston equation. A modified removal rate model for MRF offers a better estimation of MRF removal capability by including nanodiamond concentration and penetration depth.

Miao, C↗

Third-order nonlinear optical properties of Bi{sub 2}S{sub 3} nanocrystals doped in sodium borosilicate glass studied with Z-scan technique

Research highlights: {yields} Sol-gel method to realize the synthesis of Bi{sub 2}S{sub 3} nanocrystals doped in the glass. {yields} High dispersion and narrow distribution of Bi{sub 2}S{sub 3} nanocrystals in the glass. {yields}Z-scan technique employed for nonlinear optical properties of the glass. {yields} Observation that an obvious third-order optical nonlinear properties in the glass. -- Abstract: The third-order nonlinear optical properties of Bi{sub 2}S{sub 3} nanocrystals doped in sodium borosilicate glass are measured by Z-scan technique. The microstructures of the glass are characterized by means of X-ray diffraction, transmission electron microscopy, scanning transmission electron microscopy, energy dispersion X-ray spectra, and high-resolution transmission electron microscopy. The results show that the Bi{sub 2}S{sub 3} nanocrystals ranging from 10 to 30 nm are determined to be of the orthorhombic crystalline phase, and the third-order optical nonlinear refractive index {gamma}, absorption coefficient {beta}, and susceptibility {chi}{sup (3)} of the glass are determined to be 2.56 x 10{sup -16} m{sup 2} W{sup -1}, 4.13 x 10{sup -10} mW{sup -1}, and 1.43 x 10{sup -10} esu, respectively.

36 MATERIALS SCIENCE↗

Behavior of sodium borosilicate glasses under compression using molecular dynamics

We have performed classical molecular dynamics simulations in order to study the changes under compression in the local and medium range structural properties of three sodium borosilicate glasses with varying sodium content. These glasses have been isostatically compressed up to 20 GPa and then decompressed in order to analyze the different mechanisms that affect densification, alongside with the permanent modifications of the structure after a full compression/decompression cycle. The results show that the atomic packing is the prominent characteristic that governs the amount of densification in the glass, as well as the setup of the permanent densification. During compression, the bulk modulus increases linearly up to approximately 15 GPa and more rapidly for higher pressures, a behavior which is reflected on the rate of increase of the average coordination for B and Na. Radial distribution functions at different pressures during the cycle help to quantify the amount of distortions in the elementary structural units, with a pronounced shortening of the Na–Na and Na–O bond lengths during compression. A subsequent decomposition of the glassy matrix into elementary Voronoi volumes verifies the high compressibility of Na-rich regions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Impact of Na—H+ Exchange on Long-Term Borosilicate Glass Corrosion: Experiments and Field Observations

New insights from laboratory experiments coupled with field observations indicate that pore water solutions that eventually breach containment materials in disposal systems will interact with sodium-excess borosilicate waste glass in an unexpected way. Because many glass waste forms are relatively sodium-rich, they are especially vulnerable to Na+—H+ exchange (ion exchange or simply, IEX). Although the kinetics of this process has been previously investigated for early-stage glass reactions, the implications of IEX for long-term dissolution resistance have not yet been realized. Non-radioactive glass with major- and minor-element chemical compositions similar to Hanford high-Na waste glass were subjected to dissolution experiments to quantify the rates of matrix dissolution and IEX rates. Single-Pass Flow-Through (SPFT) tests quantified the IEX rate at 40°C pH = 8 and silica saturation and showed a dependence upon the fraction of excess sodium in the glass. The equation for the rate (in moles of sodium released per meter squared per second) dependence on excess sodium is: log10rate[mol/(m2∙s)] = 0.63R + (-11.0); r2 = 0.86 where R = molar Na+/(M3+). Further, rates of Na release are slower by ≥30% in D2O-based solutions compared to those in H2O. These results are the hallmark of IEX reactions. Our results are compared against those from a lysimeter field experiment consisting of glasses buried in Hanford sand and to dissolution experiments conducted with a Pressurized Unsaturated Flow (PUF) apparatus. These longer-term tests indicate an initial decrease in dissolution rate by a factor of 10×, and then a constant steady-state rate thereafter. Thus, these data show that IEX reactions are important at near-saturation conditions and effectively prevent dissolution rates from falling below a minimum value. In sum, IEX modifies the long-term behavior of glass dissolution and models cannot assume that dissolution of Na-rich borosilicate glass will decrease by a factor of 100× to 1000×, as argued for minerals and less sodic glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Failure and penetration response of borosilicate glass during short-rod impact

The failure characterization of brittle materials like glass is of fundamental importance in describing the penetration resistance against projectiles. A critical question is whether this failure front remains 'steady' after the driving stress is removed. A test series with short gold rods (D = 1 mm, L/D{approx_equal}5-11) impacting borosilicate glass at {approx}1 to 2 km/s was carried out to investigate this question. The reverse ballistic method was used for the experiments, and the impact and penetration process was observed simultaneously with five flash X-rays and a 16-frame high-speed optical camera. Very high measurement accuracy was established to ensure reliable results. Results show that the failure front induced by rod impact and penetration does arrest (ceases to propagate) after the rod is totally eroded inside the glass. The impact of a second rod after a short time delay reinitiates the failure front at about the same speed.

36 MATERIALS SCIENCE↗