Effects of pore morphology on the cyclical oxidation/reduction of iron foams created via camphene-based freeze casting
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
Recent measurements at the Sandia National Laboratory of the x-ray transmission of iron plasma have inferred opacities much higher than predicted by theory, which casts doubt on modeling of iron x-ray radiative opacity at conditions close to the solar convective zone-radiative zone boundary. An increased radiative opacity of the solar mixture, in particular iron, is a possible explanation for the disagreement in the position of the solar convection zone-radiative zone boundary as measured by helioseismology and predicted by modeling using the most recent photosphere analysis of the elemental composition. In this report we present data from radiation burnthrough experiments, which do not support a large increase in the opacity of iron at conditions close to the base of the solar convection zone and provide a constraint on the possible values of both the mean opacity and the opacity in the x-ray range of the Sandia experiments. The data agree with opacity values from current state-of-the-art opacity modeling using the CASSANDRA opacity code.
Not provided.
High-temperature (800 ºC) steam-hydrogen redox cycling, relevant to grid-scale energy storage, is studied for iron-based freeze-cast lamellar foams. In contrast to previously studied Fe, Fe-Ni, and Fe-Co foams that rapidly degrade, Fe-25Mo foams feature a much-enhanced structural damage resistance. Utilizing in-situ x-ray diffraction, microscopy, and x-ray tomography, strong sintering inhibition is observed in Fe-Mo foams, creating a hierarchically porous lamellar structure. This leads to (i) wide channels between lamellae, enabling high macroscopic porosity (~78%) which can accommodate gas flow as well as volumetric expansion without lamellar contact, and (ii) microporosity within lamellae, providing additional free volume to accommodate expansion during oxidation, limiting both swelling of the lamellae and the formation of Kirkendall pores. Finally, these combined effects enable a near-complete reversibility of the microstructure during cycling, preventing damage produced via internal lamellar buckling, cracking, contacting and sintering, with a remarkably high porosity (65%) remaining after 50 consecutive redox cycles.
Slurry casting has been used to fabricate lithium-ion battery electrodes for decades, which involves toxic and expensive organic solvents followed by high-cost vacuum drying and electrode calendering. This work presents a new manufacturing method using a nonthermal plasma to create inter-particle binding without using any polymeric binding materials, enabling solvent-free manufacturing electrodes with any electrochemistry of choice. The cold-plasma-coating technique enables fabricating electrodes with thickness (>200 μm), high mass loading (>30 mg cm -2 ), high peel strength, and the ability to print lithium-ion batteries in an arbitrary geometry. This crosscutting, chemistry agnostic, platform technology would increase energy density, eliminate the use of solvents, vacuum drying, and calendering processes during production, and reduce manufacturing cost for current and future cell designs. Here, lithium iron phosphate and lithium cobalt oxide were used as examples to demonstrate the efficacy of the cold-plasma-coating technique. It is found that the mechanical peel strength of cold-plasma-coating-manufactured lithium iron phosphate is over an order of magnitude higher than that of slurry-casted lithium iron phosphate electrodes. Full cells assembled with a graphite anode and the cold-plasma-coating-lithium iron phosphate cathode offer highly reversible cycling performance with a capacity retention of 81.6% over 500 cycles. For the highly conductive cathode material lithium cobalt oxide, an areal capacity of 4.2 mAh cm -2 at 0.2 C is attained. We anticipate that this new, highly scalable manufacturing technique will redefine global lithium-ion battery manufacturing providing significantly reduced plant footprints and material costs.
An iron-rich high entropy alloy Al 0.65 CoCrFe 2 Ni comprising of both FCC and BCC phases was designed and fabricated using induction melting at a large industrial scale and suction casting at a small lab scale. Spinodally decomposed interdendritic regions were uniformly distributed in the industrially melted alloy, and a finer dendritic structure with smaller sized spinodal structures was observed in the alloy suction cast at lab scale. The suction cast alloy fabricated at the lab scale exhibited significantly higher compressive yield strength compared to the industrially cast alloy. The relative strengthening contributions in the alloys due to solid solution, grain boundary, dislocation interactions and interphase boundary were analyzed. Dislocation hardening was the major contributor responsible for the higher strength of the SC alloy. The deformation behavior in the alloys was examined with the help of orientation image mapping. Finally, intense slip band formation at large strains in the industrially melted alloy indicates that cold working can be an effective technique to enhance the strength of the dual-phase high entropy alloy processed at a large scale.
Disclosed are aluminum alloys with high iron content and methods of making and using.
The major difference between the secondary and primary Al alloys is the amount of Fe in the alloys - recycling of Al alloys gradually leads to an increase in their Fe content. Thus, many secondary alloys allow up to 0.60% Fe as compared to the primary alloys that use between 0.10% and 0.20% Fe. Unfortunately, in Al alloys with higher iron content, iron-intermetallic phases form that are detrimental to the tensile properties and elongation of the Al castings. For example, in A356 alloys with iron at 0.10%, the ductility achieved is typically 8% whereas for secondary 356 alloys with iron around 0.6%, the ductility achieved is 3% or less. These intermetallic phases cannot be effectively modified with standard casting practices or standard heat treatment. Thus, new techniques need to be developed that can help secondary Al alloys overcome the mechanical property and cost barriers and are the focus of this project. We propose to lower the cost penalty and address mechanical properties issues in Al castings by a two-pronged approach: 1. Use an ultrasonics-based technique to modify the size and distribution of the deleterious intermetallics in the castings during the solidification process; and 2. Use PNNL-developed novel heat-treatment technique to lower the temperature and/or shorten the heat-treatment duration post-solidification processing.
Conservation of critical materials is an increasing area of focus in the Unites States. In 2023, aluminum was added to the US Department of Energy Final Critical Materials List which has spurred public and private research into sustainable management of these resources. Additionally, efficiency in manufacturing and conservation of natural resources are growing concerns with targets to lower global carbon emissions, as primary aluminum alloy production is energy intensive, requiring 14 MWh of electricity plus 0.4 tonnes of CO2 per tonne of Al. Due to these factors, is essential that more sustainable manufacturing methods for aluminum alloys are developed going forward. To this end, much research is ongoing on the topic of more efficient utilization and recovery. However, most of this research still requires primary aluminum in the production process. Here, it will be attempted to bypass the use of primary aluminum and produce useful material recycled from 100% post-consumer scrap. Even considering recent developments in recycling of Al scrap, there is still a large amount of post-consumer scrap that is underutilized due to high impurity content, and that amount will increase significantly as more and more aluminum alloys are utilized in vehicles. This “scrap wave” is expected to cover 80% of the demand for automotive aluminum alloys by 2050 . A challenge to be addressed before the coming scrap wave can be fully utilized is that the tolerance of manufacturing techniques to impurities or off-spec alloy compositions must be increased. Particularly, in 5000-and 6000-series alloys (the most common wrought alloys in durable products), excess iron, copper, and silicon create brittle intermetallics during casting that remain in the extruded microstructure which limit the formability, ductility, and corrosion resistance of the alloy. Concerningly, many of the highest-volume post-consumer aluminum scrap streams such as automotive shredder scrap contain a mix of alloys including both wrought and cast alloys. Their compositions can vary widely depending on geography and the time of year. Because they are mixed, they often contain high content of multiple alloying elements such as Si and Cu in higher concentrations than are found in typical wrought alloys. They may also be contaminated with non-Al alloys from fasteners that get mixed in and often have high content of unwanted elements such as Fe. As a method for utilizing these underused scrap streams that are high in tramp elements, an emerging extrusion technology is being developed at the Pacific Northwest National Laboratory (PNNL) that aims to upcycle 100% post-consumer aluminum scrap directly into extruded components without the addition of primary aluminum . This new technology, called Shear Assisted Processing and Extrusion (ShAPE), is enabling a shift away from today’s recycling paradigm by reaching deeper into lower-value scrap streams, using shredder scrap as the extrusion billet material. Sometimes referred to as Twitch or Tweak, these scrap streams result from shredding and sorting of automobiles, building materials, appliances, and consumer goods. ShAPE combines the linear axis of conventional extrusion with a rotating extrusion die. This rotating die applies large strain to the material during extrusion, which breaks up large impurity-containing intermetallic particles, reducing their deleterious effects. This has been demonstrated for 6063 machining scrap spiked with excess Fe, and Twitch scrap high in Fe, Si and Cu where strength and ductility were retained for both feedstock compositions. Additionally, the extreme plastic deformation during ShAPE enables extrusion of billets with high Si that are too brittle for processing by conventional extrusion. By using 100% post-consumer shedder scrap as feedstock, ShAPE has the potential to slash embodied energy and carbon in extruded components by >80% compared to conventional extrusion of primary aluminum alloys.
Alloy developers worldwide have struggled to create creep-resistant alumina-forming, iron-based austenitic stainless steels for use as high-temperature structural alloys, but with limited success in balancing alloy cost, oxidation, and creep resistance. Here, this article describes the research and development of a novel cast alumina-forming austenitic stainless steel. This work won the prestigious Engineering Materials Achievement Award presented at IMAT 2023 in Detroit.
A high fatigue strength aluminum alloy comprises in weight percent copper 3.0-3.5%, iron 0-1.3%, magnesium 0.24-0.35%, manganese 0-0.8%, silicon 6.5-12.0%, strontium 0-0.025%, titanium 0.05-0.2%, vanadium 0.20-0.35%, zinc 0-3.0%, zirconium 0.2-0.4%, a maximum of 0.5% other elements and balance aluminum plus impurities. The alloy defines a microstructure having an aluminum matrix with the Zr and the V in solid solution after solidification. The matrix has solid solution Zr of at least 0.16% after heat treatment and solid solution V of at least 0.20% after heat treatment, and both Cu and Mg are dissolved into the aluminum matrix during the heat treatment and subsequently precipitated during the heat treatment. A process for heat treating an Al—Si—Cu—Mg—Fe—Zn—Mn—Sr-TMs alloy comprises heat treating the alloy to produce a microstructure having a matrix with Zr and V in solid solution after solidification.
This study uses friction stir processing (FSP) for thermomechanical processing of high-pressure die-casting (HPDC) to modify microstructure and improve mechanical properties. FSP is carried out on two different HPDC aluminum alloys: (a) general-purpose, high-iron, HPDC A380 alloy and (b) premium quality, low-iron HPDC Aural-5 alloy in thin wall, flat plate geometry. Subsequent mechanical testing shows ~30 % and ~65 % enhancement in yield strength and tensile ductility. In addition, FSP leads to ~10 times improvement in fatigue life for A380 alloy and ~70 % improvement in fracture toughness for Aural-5 alloy. These findings emphasize the capability of FSP to modify the microstructure of HPDC Al-alloys-based structural components so that they can demonstrate a good combination of strength, ductility, fracture toughness, and high fatigue properties for long-term durability and reliability.
The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.
Residual elements from scrap steel recycling, most notably copper, are known to result in hot shortness during thermomechanical processing and casting. As the concentration of copper and other residuals in steel scrap streams increases, Electric Arc Furnace (EAF) scrap recycling heats commonly use pig iron to dilute residuals below current limits. This work focuses on establishing residual element tolerant compositions and concomitant processing windows that can simultaneously mitigate issues from residuals during thermomechanical processing and, if possible, use these residuals to improve properties, yielding a more sustainable steel manufacturing pathway with a substantially smaller carbon footprint.
Three-dimensionally preserved Ediacaran fossils occur globally within sandstone beds. Sandy siliciclastic deposits of the Ediacaran Wood Canyon Formation (WCF) in the Montgomery Mountains, Nevada, contain two fossil morphologies with similar shapes and sizes: one exhibits mm-scale ridges and a distinct lower boundary and the other is devoid of these diagnostic features. We interpret these as taphomorphs of erniettomorphs, soft-bodied organisms with uncertain taxonomic affinities. We explore the cast-and-mould preservation of both taphomorphs by petrography, Raman spectroscopy, X-ray fluorescence microprobe and X-ray diffraction. All fossils and the surrounding sedimentary matrix contain quartz grains, iron-rich chlorite and muscovite. The ridged fossils contain about 70% larger quartz grains compared to the ridgeless taphomorph, indicating a lower abundance of clay minerals in the ridged fossil. Chlorite and muscovite likely originated from smectite and kaolinite precursors that underwent lower greenschist facies metamorphism. Kaolinite and smectite are inferred to have been abundant in sediments around the ridged fossil, which enabled the preservation of a continuous, distinct, clay- and kerogen-rich bottom boundary. The prevalence of quartz in the ridged fossils of the WCF and in erniettomorphs from other localities also suggests a role for this mineral in three-dimensional preservation of erniettomorphs in sandstone and siltstone deposits.
In this study, we investigate the toughness and resistance to tear of thin-wall high-pressure die-cast (HPDC) aluminum alloys in two different orientations following the implementation of friction stir processing (FSP). The FSP technique was applied to two different HPDC Al-Si alloys: the recyclable-grade, high iron, A380 alloy and the premium-quality, low iron, Aural-5 alloy. Our findings reveal significant tear resistance and strength enhancements for both alloys after FSP modification. Specifically, FSPed A380 alloy requires 126% higher energy to tear, and it has 49% higher tear strength than the HPDC counterpart. Similarly, the tear energy and tear strength of the Aural-5 alloy witness enhancements of 69% and 21%, respectively. In conclusion, these results highlight the potential of FSP as a viable method for augmenting the mechanical properties of HPDC aluminum alloys, thereby opening up new avenues for their utilization in diverse engineering applications for crack obstruction.
The addition of boron to steel alloys results in an increase in both hardenability and casting defects. The casting difficulties are predicted to stem from a metatectic reaction, δ + γ → L + γ, where a fully solidified material begins to locally remelt as the temperature decreases. Another possible source of casting defects is a boride-rich phase that is predicted to remain liquid at low temperatures. To experimentally determine which reaction is the likely source of the casting defects, the predicted reactions and the effect of solute elements on those reactions are investigated. Levitation zone melting is used to control segregation in a ternary Fe–C–B alloy and a commercial 22MnB5 alloy. Carbon segregation and a peritectic reaction result in a peritectic jump during directional solidification where the first directionally solidified (DS) zone undergoes δ-bcc solidification followed by a peritectic jump to steady state planar solidification of γ-fcc in the second DS zone. The presence of other solute elements in the zone melted 22MnB5 alloy lead to a breakdown in the planar solidification front before steady state solidification could be achieved in the second DS zone. With a cellular solid/liquid interface, boron-rich intercellular liquid formed low melting iron boro-carbide particles. The controlled solidification conditions in a levitation zone melter were unable to prevent ~0.003 wt% boron from segregating to high enough levels to form boride particles. Therefore, it is likely that during commercial casting, the formation of the low melting boride phase from interdendritic segregation is a key source of the casting issues.
Mechanically stable and foldable air cathodes with exceptional oxygen reduction reaction (ORR) and oxygen evolution reaction (OER) activities are key components of wearable metal-air batteries. Herein, a directional freeze-casting and annealing approach is reported for the construction of a 3D honeycomb nanostructured, N,P-doped carbon aerogel incorporating in situ grown FeP/Fe 2 O 3 nanoparticles as the cathode in a flexible Zn-air battery (ZAB). The aqueous rechargeable Zn-air batteries assembled with this carbon aerogel exhibit a remarkable specific capacity of 648 mAh g -1 at a current density of 20 mA cm -2 with a good long-term durability, outperforming those assembled with commercial Pt/C+RuO 2 catalyst. Furthermore, such a foldable carbon aerogel with directional channels can serve as a freestanding air cathode for flexible solid-state Zn-air batteries without the use of carbon paper/cloth and additives, giving a specific capacity of 676 mAh g -1 and an energy density of 517 Wh kg -1 at 5 mA cm -2 together with good cycling stability. This work offers a new strategy to design and synthesize highly effective bifunctional air cathodes to be applied in electrochemical energy devices.