At least 73 records · Page 4

A Guideline to Mitigate Interfacial Degradation Processes in Solid‐State Batteries Caused by Cross Diffusion

Abstract Diffusion of transition metals across the cathode–electrolyte interface is identified as a key challenge for the practical realization of solid‐state batteries. This is related to the formation of highly resistive interphases impeding the charge transport across the materials. Herein, the hypothesis that formation of interphases is associated with the incorporation of Co into the Li 7 La 3 Zr 2 O 12 lattice representing the starting point of a cascade of degradation processes is investigated. It is shown that Co incorporates into the garnet structure preferably four‐fold coordinated as Co 2+ or Co 3+ depending on oxygen fugacity. The solubility limit of Co is determined to be around 0.16 per formula unit, whereby concentrations beyond this limit causes a cubic‐to‐tetragonal phase transition. Moreover, the temperature‐dependent Co diffusion coefficient is determined, for example, D 700 °C = 9.46 × 10 −14 cm 2 s −1 and an activation energy E a = 1.65 eV, suggesting that detrimental cross diffusion will take place at any relevant process condition. Additionally, the optimal protective Al 2 O 3 coating thickness for relevant temperatures is studied, which allows to create a process diagram to mitigate any degradation with a minimum compromise on electrochemical performance. This study provides a tool to optimize processing conditions toward developing high energy density solid‐state batteries.

Chemistry↗

Discharge Rate‐Driven Li 2 O 2 Growth Exhibits Unconventional Morphology Trends in Solid‐State Li‐O 2 Batteries

Solid-state lithium oxygen batteries (LOBs) are known for their enhanced safety, higher electrochemical stability, and improved energy density compared to liquid-state LOBs. However, the investigation of solid-state LOBs is limited with little understanding of their discharge and charge processes. In this work, a polymer-based solid-state LOB is used to investigate the effect of discharge rate on lithium peroxide (Li 2 O 2 ) formation, the oxygen evolution reaction (OER), and cycle performance. Notably, we observe a counterintuitive trend: Li 2 O 2 particle size increases with increasing discharge current density, in contrast to liquid systems. This behavior arises from inherent space charge layers that restrict Li⁺ transport under high current, and spatially heterogeneous active sites at the solid electrolyte–cathode interface, directly evidenced by small angle X-ray scattering (SAXS), which govern nucleation accessibility and promote site-selective Li 2 O 2 growth. Furthermore, higher current densities improve ORR and OER efficiency but accelerate anode degradation, while lower currents promote side reactions. These opposing effects result in a trade-off that defines an optimal discharge rate (0.1 mA cm -2 ) for maximizing cycle life. This study provides a new mechanistic perspective on discharge-driven processes in solid-state LOBs and offers practical guidelines for performance optimization in future high-energy battery systems.

Discharge current density↗

The Role of Catholyte Modulation in Suppressing the Initial Capacity Fade of Zinc Electrolytic Manganese Dioxide Coin Cells

Despite its potential for zinc–manganese oxide batteries, electrolytic manganese dioxide (EMD) can experience capacity fade due to a deficiency in the Mn 2+ supply at the cathode electrolyte interphase (CEI) from side reactions, even in the presence of an electrolyte additive. In this work, electrolyte loading modulation at the cathode electrolyte interface (CEI) was correlated with Zn∥EMD cell capacity retention and cycling performance, as a proposed measure to curb the initial capacity fade observed in EMD. Initial galvanostatic charge/discharge cycling, with varied electrolyte loading, revealed severe capacity fade (from ~188 to 10 mAh g –1 for the highest loading of 200 μL) within the first 15 cycles. Such a decrease in cell capacity is correlated with the formation of a Mn 4+ deposit on the current collector and consequently, the Mn 2+ depletion at CEI, as was supported by elemental and Raman analyses. Interestingly, confinement of the electrolyte to the CEI at a lower (≤15 μL) electrolyte loading mitigated Mn 4+ side-deposition, maintaining the cell capacity at >80% over the first 15 cycles. Interfacial Mn supply/depletion could be monitored via voltammetric analysis based on changes of the Zn 2+ insertionreduction peak. Additional galvanostatic experiments corroborated the voltammetric interpretation and the proposed degradation pathway in the studied cell conditions. The outcomes of this work provide practical insight into coin-cell design and configuration strategies for developing Zn∥EMD batteries.

25 ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

Understanding and Mitigating the Dissolution and Delamination Issues Encountered with High-Voltage LiNi 0.5 Mn 1.5 O 4

In our initial study on the high-voltage 5 V cobalt-free spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode, we discovered a severe delamination issue in the laminates when cycled at a high upper cut-off voltage (UCV) of 4.95 V, especially when a large cell format was used. This delamination problem prompted us to investigate further by studying the transition metal (TM) dissolution mechanism of cobalt-free LNMO cathodes, and as a comparison, some cobalt-containing lithium nickel manganese cobalt oxides (NMC) cathodes, as the leachates from the soaking experiment might be the culprit for the delamination. Unlike other previous reports, we are interested in the intrinsic stability of the cathode in the presence of a baseline Gen2 electrolyte consisting of 1.2 M of LiPF 6 in ethylene carbonate/ethyl methyl carbonate (EC/EMC), similar to a storage condition. The electrode laminates (transition metal oxides, transition metal oxides, TMOs, coated on an Al current collector with a loading level of around 2.5 mAh/cm 2 ) or the TMO powders (pure commercial quality spinel LNMO, NMC, etc.) were stored in the baseline solution, and the transition metal dissolution was studied through nuclear magnetic resonance, such as 1 H NMR, 19 F NMR, scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS) and inductively coupled plasma mass spectrometry (ICP-MS). Significant electrolyte decomposition was observed and could be the cause that leads to the TM dissolution of LNMO. To address this TM dissolution, additives were introduced into the baseline electrolyte, effectively alleviating the issue of TM dissolution. The results suggest that the observed delamination is caused by electrolyte decompositions that lead to etching, and additives such as lithium difluorooxalato borate and p-toluenesulfonyl isocyanate can alleviate this issue by forming a firm cathode electrolyte interface. This study provides a new perspective on cell degradation induced by electrode/electrolyte interactions under storage conditions.

25 ENERGY STORAGE↗

Operating Stresses and Their Effects on Degradation of LSM-Based SOFC Cathodes

The performance of solid oxides fuel cells (SOFCs) with four different Mn excess of lanthanum strontium manganite (LSM) -based cathodes were examined under different temperatures (1,000 °C, 900 °C), current densities (0, 380, and 760 mA cm -2 ), and cathode atmospheres (p O 2 )=0.1,0.15,0.21) for durations ranging from 58 to 1,008 h. Each yttria-stabilized zirconia (YSZ) electrolyte-supported “button” cell had a porous Ni/YSZ composite anode and a porous LSM/YSZ composite cathode. The cells’ output voltage versus time were recorded and electrochemical impedance spectroscopy (EIS) and linear sweep voltammetry (LSV) measurements were performed every 24 hours. The total area specific resistance (ASR) was calculated from these measurements. The values of ASR from both EIS and LSV were comparable between each other but lower than that from durability test. Distribution of relaxation times (DRT) analysis was performed to investigate the electrochemical processes and their corresponding relaxation frequencies as well as their attributions to the total ASR. The series resistance and parallel resistance that obtained from the equivalent circuit fit of the Nyquist plot were higher at low temperature and low p O 2 regardless of LSM compositions. The area of the peaks derived from DRT analysis increased with time during individual tests. The microstructures of the tested cells were examined using scanning electron microscopy and energy-dispersive x-ray spectroscopy (SEM/EDS). Manganese oxide particles were observed near the cathode-electrolyte interface after prolonged (1,008 h) testing in air of a cell with LSM of 11% manganese excess, and after a short test (58 h) under low oxygen (p O 2 = 0.10) in a cell with LSM of 5% manganese excess. However, the role of MnOx in cell degradation is still unknown.

08 HYDROGEN↗

Structure, Chemistry, and Charge Transfer Resistance of the Interface between Li 7 La 3 Zr 2 O 12 Electrolyte and LiCoO 2 Cathode

All-solid-state batteries promise significant safety and energy density advantages over liquid-electrolyte batteries. The interface between the cathode and the solid electrolyte is an important contributor to charge transfer resistance. Strong bonding of solid oxide electrolytes and cathodes requires sintering at elevated temperatures. Knowledge of the temperature dependence of the composition and charge transfer properties of this interface is important for determining the ideal sintering conditions. To understand the interfacial decomposition processes and their onset temperatures, model systems of LiCoO 2 (LCO) thin films deposited on cubic Al-doped Li 7 La 3 Zr 2 O 12 (LLZO) pellets were studied as a function of temperature using interface-sensitive techniques. X-ray photoelectron spectroscopy, secondary ion mass spectroscopy, and energy-dispersive X-ray spectroscopy data indicated significant cation interdiffusion and structural changes starting at temperatures as low as 300 °C. La 2 Zr 2 O 7 and Li 2 CO 3 were identified as decomposition products after annealing at 500 °C by synchrotron X-ray diffraction. X-ray absorption spectroscopy results indicate the presence of also LaCoO 3 in addition to La 2 Zr 2 O 7 and Li 2 CO 3 . On the basis of electrochemical impedance spectroscopy and depth profiling of the Li distribution upon potentiostatic hold experiments on symmetric LCO|LLZO|LCO cells, the interfaces exhibited significantly increased impedance, up to 8 times that of the as-deposited samples after annealing at 500 °C. Here, our results indicate that lower-temperature processing conditions, shorter annealing time scales, and CO 2 -free environments are desirable for obtaining ceramic cathode|electrolyte interfaces that enable fast Li transfer and high capacity.

25 ENERGY STORAGE↗

Phase Stability of Garnet Solid-Electrolyte Interfacing with Various Cathodes in All Solid-State Batteries

Garnet-structured Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO) is one of the most promising electrolyte materials for solid-state Li batteries (SS-LiB). The design and fabrication of a good cathode/electrolyte interface is an important criterion for the SS-LiB. In this work, we performed a systematic study on the impact of cathode crystal structure and chemical compositions on their chemical stabilities against the LLZTO at elevated temperatures, which are required for their adhesion during cell fabrication processes. X-ray Diffraction (XRD) and Rietveld refinement analyses revealed the chemical stabilities of various cathode materials in contact with the LLZTO. While layered LiCoO 2 cathode showed good stability in contact with LLZTO to 900 °C, LiNiO 2 or Ni-rich LiNi x Mn y Co 1–x–y O 2 (NMC) cathodes suffered from the formation of La 4 NiLiO 8 due to La-diffusion from LLZTO. Furthermore, Mn-rich LiMn 2 O 4 spinel and layered LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes suffered from the formation of La 2 Zr 2 O 7 due to Li-diffusion and production of Li 2 MnO 3 . As a result, LiNi 0.6 Mn 0.2 Co 0.2 O 2 , having an ideal balance of Ni/Mn/Co composition, or Li 2 MnO 3 containing cathodes such as Li 1.2 Ni 0.15 Mn 0.55 Co 0.1 O 2 were found to have excellent phase stability as the cathodes for LLZTO-based SS-LiBs.

25 ENERGY STORAGE↗

Ionic Interdiffusion at Cathode|Solid-Electrolyte Interface: A Machine Learning–Assisted Multiscale Investigation and Mitigation Strategies

Future lithium batteries are expected to use solid electrolytes to achieve higher energy density and fast charge capabilities. However, most solid electrolytes are thermodynamically unstable against layered oxide cathodes. In this study, the stability of LiCoO2 (LCO) cathode with Li10GeP2S12 (LGPS) solid electrolyte is investigated using ab initio molecular dynamics (AIMD) and machine learning molecular dynamics (MLMD). The propensity of ionic interdiffusion, formation of a passivating interphase layer, and corresponding decay in cell performance is addressed using a continuum model. Large-scale MLMD simulations confirm that the LCO|LGPS interface permits interdiffusion of cobalt (Co) and other ionic species, leading to the formation and growth of a resistive interphase and to dramatic capacity fade even in the first cycle. We examine the literature evidence that incorporating a thin layer of LiNb0.5Ta0.5O3 (LNTO) between LCO and LGPS prevents the interdiffusion of ions. Atomistic simulations suggest that substituting lithium (Li) in LNTO with Co is thermodynamically unfavorable, thereby inhibiting ionic interdiffusion. The stable Nb5+/Ta5+ states form a rigid metal-oxide framework, which consequently also prevents the substitution of niobium (Nb) or tantalum (Ta). However, continuum-level analysis suggests that the higher mechanical stiffness of LNTO can lead to interfacial delamination between the LCO and LNTO. This phenomenon reduces the effectiveness of the protective layer. This paper, therefore, highlights the need to develop novel interlayers that balance low ionic interdiffusion with low mechanical stiffness.

Ncube, Musawenkosi K.↗

Stable Cycling with Intimate Contacts Enabled by Crystallinity–Controlled PTFE–Based Solvent–Free Cathodes in All–Solid–State Batteries

All-solid-state batteries (ASSBs) employing Li-metal anodes and inorganic solid electrolytes are attracting great attention due to high safety and energy density for next-generation energy storage devices. However, the volume change of cathode active materials can cause contact loss, resulting in charge carrier isolation, heterogeneous current distribution, and poor electrochemical properties in ASSBs. Here, a simple, yet effective, solvent-free electrode engineering approach with polytetrafluoroethylene (PTFE) as a binder for ASSBs is reported, enabling intimate contact and stable interfaces with the cathode. It is substantiated that the crystallinity of PTFE can be controlled depending on the heat history, and highly crystalline PTFE displays robust mechanical properties. High-nickel LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathode prepared with crystalline PTFE show improved cycle and rate performances in ASSBs. In addition, it is revealed that the intimate contact between cathode particles with a stable cathode electrolyte layer is maintained during cycling by postmortem studies. Furthermore, this simple engineering method can be applied to prepare cathodes with a variety of active materials and solid electrolytes in ASSBs.

25 ENERGY STORAGE↗

Impacts of Solvent Washing on the Electrochemical Remediation of Commercial End-of-Life Cathodes

Changes to surface structure and chemistry occurring throughout the functional lifetime of lithium-ion batteries (LIBs) may impact the effectiveness of end-of-life rejuvenation methods. Solvent washing prior to electrochemical relithiation is shown to both increase relithiation efficacy and beneficially alter the interfacial chemistry of heavily degraded industrial cathode material. Four common solvents (acetone, diethyl carbonate, isopropyl alcohol, propylene carbonate) are employed to investigate the role of varying physicochemical solvent properties on the mechanism of capacity recovery. Electrochemical (dQ/dV, EIS), structural (XRD), and chemical (SPME-GC-MS) analysis techniques are employed to comprehensively analyze solvent-cathode interactions. Highly nucleophilic solvents (acetone, DEC) are found to reduce cathode charge-transfer impedance and enable stable impedance growth throughout subsequent cycling. The use of nucleophilic solvents under mechanically aggressive washing conditions may also enable the reintroduction of bulk lattice oxygen, thereby restoring anionic redox capacity. Further, the four solvents are found to selectively remove a subset of surface species from the aged cathode material, including residual electrolyte, additives, and electrolyte-additive reaction products, which are qualitatively analyzed. Surface species removal by each solvent is correlated with the electrochemical performance of the correspondingly washed cathode, highlighting the importance of an optimized washing protocol to effective remediation in the context of direct LIB recycling. For the material under study, the use of a simple acetone washing protocol prior to electrochemical relithiation enables up to 174% capacity recovery relative to unwashed/relithiated black mass.

ADVANCED PROPULSION SYSTEMS↗

Unveiling the Mechanism of Mn Dissolution Through a Dynamic Cathode‐Electrolyte Interphase on LiMn2O4

Abstract Understanding the formation and evolution of the cathode‐electrolyte interphase (CEI), which forms at the interface between the cathode and electrolyte, is crucial for revealing degradation mechanisms in cathode materials, especially for developing strategies to stabilize the interphase in the strongly oxidizing conditions that evolve at high operating voltages in next‐generation Li‐ion batteries. However, The present understanding of the CEI is challenged by its complex and dynamic nature. In this work, near‐edge X‐ray absorption fine structure spectroscopy, electrochemical characterization, and reactive molecular dynamics simulations are combined to reveal a mechanism for CEI formation and evolution above model LiMn 2 O 4 (LMO) thin‐film electrodes in contact with conventional carbonate‐based electrolytes. It is found that Mn dissolution from LMO can be understood in terms of repetitive Mn 3 O 4 formation and dissolution behavior during cycling, which is closely connected to electrolyte decomposition and a key aspect of the CEI formation and growth. The behavior of the CEI in this model system offers detailed insight into the dynamic chemistry of the interphase, underscoring the important role of electrolyte composition and cathode surface structure in interphase degradation.

Ou, Wenhan↗

Microstructural Insights into Performance Loss of High-Voltage Spinel Cathodes for Lithium-ion Batteries

Spinel-structured LiNi x Mn 2-x O 4 (LNMO), with low-cost earth-abundant constituents, is a promising high-voltage cathode material for lithium-ion batteries. Even though extensive electrochemical investigations have been conducted on these materials, few studies have explored correlations between their loss in performance and associated changes in microstructure. Here, down to the atomic scale, the structural evolution of these materials is investigated upon the progressive cycling of lithium-ion cells. Transgranular cracking is revealed to be a key feature during cycling; this cracking is initiated at the particle surface and leads to the penetration of electrolytes along the crack path, thereby increasing particle exposure to the electrolyte. The lattice structure on the crack surface shows spatial variances, featuring a top layer of rock-salt, a sublayer of a Mn 3 O 4 -like arrangement, and then a mixed-cation region adjacent to the bulk lattice. The transgranular cracking, along with the emergence of local lattice distortion, becomes more evident with extended cycling. Further, phase transformation at primary particle surfaces and void formation through vacancy condensation is found in the cycled samples. All these features collectively contribute to the performance degradation of the battery cells during electrochemical cycling.

25 ENERGY STORAGE↗

Dual Passivation of Cathode and Anode through Electrode–Electrolyte Interface Engineering Enables Long-Lifespan Li Metal–SPAN Batteries

The reliability and durability of lithium metal (Li 0 )–sulfur batteries are largely limited by the undesired Li 0 plating-stripping irreversibility and the detrimental polysulfide dissolution, yet approaches that can simultaneously address the above anodic and cathodic problems are scarce. In this study, we report the stable operation of a Li 0 -SPAN (sulfurized polyacrylonitrile) battery via an anode–cathode dual-passivation approach. By combination of a fluorinated localized high concentration electrolyte (LHCE) and a Li 3 N-forming additive (TMS-N 3 ), robust and highly conductive electrode passivation layers are formed in situ on the surface of both the Li 0 anode and the SPAN cathode. The resulting highly reversible, dendrite-free, and high-density Li 0 plating morphology enables a high Coulombic efficiency of 99.4%. Advanced tender energy X-ray spectroscopy also reveals the eliminated Li 2 S formation and minimized polysulfide dissolution in SPAN cathodes, leading to a high capacity of 580 mAh/g SPAN and stable cycling with negligible capacity decay (0.7%) for 800 cycles. This electrode–electrolyte interphase engineering strategy has tackled the major limitations of Li–S batteries in both ether- and carbonate-based electrolyte systems and under a wide temperature range from –10 to +50 °C, thus providing insightful guidelines for the rational design of highly durable and high-energy-density Li 0 -S batteries.

25 ENERGY STORAGE↗

Effect of Electrolytes on the Cathode-Electrolyte Interfacial Stability of Fe-Based Layered Cathodes for Sodium-Ion Batteries

Iron (Fe)-based layered oxide cathodes that employ Fe 3+ /Fe 4+ redox reaction present a family of attractive cathode materials for sodium-ion batteries as iron is abundant, low-cost, and environmentally benign. However, their electrochemical performance is not yet satisfactory and requires further improvement. In this study, we investigate the effect of electrolytes on the electrochemical performance of α -NaFeO 2 , a prototypical model of Fe-based layered cathodes. First, we established the critical impact of the poor cathode-electrolyte interfacial stability on cell performances. Systematic electrochemical tests and material characterizations further revealed the degradation mechanism in which the highly reactive Fe 4+ state in the charged Na 1−x FeO 2 electrodes promotes severe electrolyte decomposition and subsequent growth of a thick interface layer that leads to impedance rise and performance degradation. In addition, the superior performance of NaPF 6 over NaClO 4 and the beneficial effect of the FEC additive are reported.

25 ENERGY STORAGE↗

Basics of the scanning electrochemical microscope and its application in the characterization of lithium-ion batteries: a brief review

A scanning electrochemical microscope (SECM) can directly monitor electrochemical processes at interfaces of electrodes and electrolytes and has been used as an analytical tool for lithium-ion battery (LIB) studies. Through SECM, we can visualize the electrochemical reactivities of active species in LIBs in-situ during cycling. This review begins with introducing SECM-based LIB research and then summarizes the working mechanism and operating modes of the technique as well as combinations of SECM with other techniques for LIB studies. We review the results with a focus on the interfacial properties, surface reactions and electrochemical activity of different electrode materials for LIBs. The investigations of battery degradation, kinetic parameters and electrolyte swelling by SECM are also discussed. Finally, the current limitations and perspectives are also described regarding future developments.