Search NASA⌕ Search

SEARCH · Search NASA

Results for “Dislocation mechanics”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Effect of heat treatment on creep behavior of 316 L stainless steel manufactured by laser powder bed fusion

The objective of this study is to understand the thermal stability of microstructure and its effect on the creep behavior of additively-manufactured 316L stainless steel (AM 316L SS). Creep specimens were fabricated from rods printed by a laser powder bed fusion process. Six different heat treatments, namely 650 °C/1 h, 700 °C/1 h, 750 °C/1 h, 800 °C/1 h, 900 °C/1 h and 1050 °C/1 h were applied to the creep specimens. The heat-treated specimens were creep-tested under the same condition, 550 °C/275 MPa to evaluate the effect of post-build heat treatment on the creep behavior of AM 316L SS. In the temperature range of 650-750 °C, dislocation density within cells, and cell size and wall thickness were affected by the heat treatment, while elemental segregation at boundaries remained unchanged and Mn-enriched Si oxide particles remained stable. In the temperature range of 750-900 °C, concurrent changes were observed in dislocation cell structures, elemental segregation and oxide particles. The 1050 °C-heat treatment removed cell structures and boundary solute segregations, leading to formation of equiaxed grains; Mn-enriched Si oxide particles in the as-built specimen were replaced by more stable Mn-enriched Cr oxides. The creep life of AM 316L SS increased after the heat treatment at 650 °C and then decreased with increasing temperature up to 900 °C where cell/subgrain structures still existed. The creep rate and creep elongation followed an opposite trend. The creep rate can be correlated with the structural parameters of cell/subgrain size and cell wall/boundary thickness and can be rationalized by different strengthening mechanisms of dislocation cells and subgrains. The heat treatment affected strongly the primary and secondary creep but had a minimal effect on the tertiary creep of AM 316L SS.

316L stainless steel↗

Microstructural evaluation of the creep behavior in L-PBF Ni-based superalloys

This presentation at ICAM 2024 Conference focuses on the commonalities and differences in the creep rupture behavior and creep mechanisms for three distinct classes of laser powder-bed fusion (L-PBF) Ni-based superalloys (γ’-precipitate strengthened Haynes® 282®, γ’/γ”/δ-precipitate strengthened Alloy 718, and solid-solution strengthened Alloy 625) as compared to conventionally processed counterparts. A comparison of Larson-Miller parameter plots establishes that these alloys perform statistically within the bounds established for the wrought product, despite having dissimilar microstructural features and other artefacts associated with PBF-LB manufacturing and post-processing heat treatment. To understand the failure and the impact of composition, minor phases, and deformation defects on creep behavior, the fractography has been performed and microstructures have been evaluated in detail with SEM-EDS, EBSD, and HAADF-STEM. The underlying diffusional and dislocation creep mechanisms associated with this microstructural evaluation is discussed. This work is supported by NETL-FWP-1022408 Advanced Turbines.

Sudbrack, Chantal↗

Support of Adhesion Mechanisms in Al 2 O 3 Aerosol Deposition Through Laser-Induced Particle Impact Testing

Aerosol deposition (AD) is a kinetic spray process capable of depositing ceramic coatings at room temperature, but AD process development is generally a laborious exploration of a large process parameter space. Here, this paper presents a case study investigating whether laser-induced particle impact testing (LIPIT) could be applied to expedite development of an alumina (Al 2 O 3 ) coating on nickel (Ni): Specifically, whether LIPIT measurements could predict critical velocities of adhesion on Ni and Al 2 O 3 , and the effect of ball milling the Al 2 O 3 powder. Because LIPIT has a diffraction-limited lower bound on imageable particle size, the usefulness of Al 2 O 3 powder agglomerates as a proxy for single particles was additionally studied. Overall, LIPIT measurements and AD sprays agreed that ball milling dramatically improves adhesion. Additionally, LIPIT measurements of critical velocity of adhesion of Al 2 O 3 powder agglomerates on Ni and Al 2 O 3 substrates (150 meters per second [m/s] and 250 m/s, respectively) quantitatively agreed with predictions from a previously published model based on picoindentation and molecular dynamics simulations. Together, these findings support the established hypothesis that Al 2 O 3 adheres via a dislocation-mediated mechanism in AD, that Al 2 O 3 powder agglomerates adhere as individual constituent particles rather than collectively, and that, for this case study, LIPIT measurements were predictive of AD process parameters.

Al2O3↗

Serrated flow in $\mathrm{NaI:Tl}$ scintillator crystals

We report the serrated-flow behavior is an important phenomenon that unveils material-deformation mechanisms, as reported for various kinds of materials. NaI doped with Tl (NaI:Tl) is unique among scintillation materials in that the structure contains glide planes that are linked to serration behavior. In the present work, single crystals of NaI:Tl were subjected to room-temperature compression experiments at different strain rates. The serrated flow was observed, and complexity and multifractal analyses were performed to analyze the serration behavior. The findings revealed that the strain rate had a pronounced effect on the complexity and multifractality of the serrated flow, similar to what has been found in other alloy systems. The results also indicate that there may be a strong link between the complexity of the serrated flow behavior and the heterogeneity of the underlying dynamics. It is expected that the present work could be a step toward a better understanding of the deformation behavior and forgeability of NaI:Tl single crystals.

36 MATERIALS SCIENCE↗

Elimination of oxygen sensitivity in α-titanium by substitutional alloying with Al

Individually, increasing the concentration of either oxygen or aluminum has a deleterious effect on the ductility of titanium alloys. For example, extremely small amounts of interstitial oxygen can severely deteriorate the tensile ductility of titanium, particularly at cryogenic temperatures. Likewise, substitutional aluminum will decrease the ductility of titanium at low-oxygen concentrations. Here, we demonstrate that, counter-intuitively, significant additions of both Al and O substantially improves both strength and ductility, with a 6-fold increase in ductility for a Ti-6Al-0.3 O alloy as compared to a Ti-0.3 O alloy. The Al and O solutes act together to increase and sustain a high strain-hardening rate by modifying the planar slip that predominates into a delocalized, three-dimensional dislocation pattern. Furthermore, the mechanism can be attributed to decreasing stacking fault energy by Al, modification of the “shuffle” mechanism of oxygen-dislocation interaction by the repulsive Al-O interaction in Ti, and micro-segregation of Al and O by the same cause.

36 MATERIALS SCIENCE↗

High-energy synchrotron x-ray study of deformation-induced martensitic transformation in a neutron-irradiated Type 316 stainless steel

An unusual tensile deformation behaviour in the form of a propagating band along the sample gauge was observed in two neutron-irradiated 316 stainless steel samples during room-temperature tests, leading to a combination of high strength and high ductility. These bands were not observed in an unirradiated counterpart. With the help of in situ high-energy synchrotron x-ray diffraction, the phase-specific crystal information was tracked at different deformation levels in each sample. Post-irradiation and post-deformation samples were examined using electron microscopy to characterize various microstructural features. All samples displayed a deformation-induced martensitic phase transformation, which was identified as a second strain-hardening mechanism accompanying the dislocation hardening. The deformation-induced martensitic transformation was rationalized by the effect of applied stress on the effective martensite start temperature. The results showed that the irradiation did not alter the dislocation hardening and the martensitic transformation mechanisms, but the increased yield strength in irradiated materials facilitated the localized phase transformation at the onset of plastic deformation, in contrast to the unirradiated material which required pre-straining. The hardening effect of the martensitic transformation reduced the tendency towards necking and mitigated the loss of ductility in the irradiated material by carrying the deformation in the form of a propagating band. Despite the beneficial effect from the martensitic transformation, this study indicates that this mechanism cannot not be activated at typical operating temperatures of nuclear reactors.

36 MATERIALS SCIENCE↗

An energetic link between order and strength in metals: A nanocrystalline strength limit in high-entropy alloys and intermetallic compounds

The metallurgy and materials communities have long understood and exploited fundamental links between chemical and structural ordering in metallic solids to tailor their mechanical properties. We extend these ideas to include prediction of the nanocrystalline strength limit in high-entropy alloys and intermetallic compounds, where a breakdown occurs in the classical Hall-Petch strengthening behavior. The highest reported strength achievable through alloying has rapidly climbed and given rise to new classifications of materials with extraordinary properties, with a notable case being nanocrystalline metals. High-entropy alloys (chemically disordered, concentrated solid solutions) and intermetallic compounds are two boundary cases of how tailored order can be used to manipulate mechanical behavior. Here, we show that the complex electronic-structure mechanisms governing the peak strength of alloys and pure metals can be reduced to a few physically meaningful parameters based on their atomic arrangements and used – with no fitting parameters – to predict the maximum strength of these materials. This includes a generalized energy-based accounting for the degree of structural and chemical ordering that allows for rapid and reasonably accurate prediction of peak strength (validated in the nanocrystalline limit) as a function of temperature. Predictions of maximum strength based on the activation energy (with all materials properties derived from DFT calculations or experiments) for a stress-driven transition to an amorphous state is shown to accurately describe the breakdown in Hall-Petch behavior at the smallest crystallite sizes for pure metals, intermetallic compounds, high-entropy alloys, and metallic glasses. Further, this activation energy is also shown to be directly proportional to interstitial electronic charge density, which is a good predictor of ductility, stiffness (moduli), and phase stability in high-entropy alloys and solid metals generally. The proposed framework suggests the possibility of coupling ordering and intrinsic strength to mechanisms like dislocation nucleation, hydrogen embrittlement, and transport properties, such as through correlations between the activation energies for amorphization with stacking-fault and grain boundary energies. It additionally opens the prospect for greatly accelerated structural materials design and development to address materials challenges limiting more sustainable and efficient use of energy.

36 MATERIALS SCIENCE↗

In situ neutron diffraction study of fatigue behavior of CrFeCoNiMo 0.2 high entropy alloy

In situ neutron diffraction measurement was applied to study the low-cycle fatigue behavior of CrFeCoNiMo 0.2 high entropy alloy. A two-step stress-controlled fatigue test with a stress range of 100–460 and 20–500 MPa was employed. The as-cast sample was cycled 129,000 and 61,000 times, respectively, before fracture. The evolution of the lattice strain and peak intensity demonstrates that the main deformation mechanism is dislocation slip, while no evidence of stacking fault was found. A three-stage ratcheting was clearly observed. Under the stress-controlled mode, the experimentally determined dislocation density increases linearly with the ratcheting strain. Here, the increase of the dislocation density results in a decay of the ratcheting strain rate, which stabilizes the structure and is beneficial for fatigue resistance.

36 MATERIALS SCIENCE↗

Decoupling indentation size and strain rate effects during nanoindentation: A case study in tungsten

Materials indented at small scales may simultaneously exhibit indentation size and strain rate effects which complicate the identification of the mechanisms that control deformation and strength. Here, in this work, we explore the possibility that indentation size and rate effects in some materials can be decoupled in a simple way. Nanoindentation tests with various load-time histories were carried out to measure the hardness of a tungsten single crystal over a wide range of indentation depths (~500–3600 nm) and indentation strain rates (~5 ×10 –5 –2 ×10 –1 s –1 ). Under these conditions, this material exhibits significant indentation size and rate effects, but the size effect is, to a good approximation, independent of strain rate. It is shown that this behavior can be understood by the Nix-Gao model for the indentation size effect modified to include the effects of a strain rate dependent friction stress. As a consequence, the size and rate dependencies of the hardness can be expressed as the sum of two independent terms: H($\dot{ε}$ i , h c )=H f ($\dot{ε}$ i ) + (H 0 – H f ) $\sqrt{1+ \frac{h^*}{h_c}}$, where H($\dot{ε}$ i , h c ) is the hardness at given indentation strain rate ($\dot{ε}$ i ) and contact depth (h c ), H f ($\dot{ε}$ i ) is the hardness contributed by the rate dependent friction stress, and (H 0 – H f ) and h* are size and rate independent constants that follow from the Nix-Gao analysis. This formula, together with an expression for the rate dependence of H f , was successfully applied to decouple the indentation size and rate effects observed in tungsten. In addition, the physics underlying the rate independence of indentation size effect is discussed, which provides guidance for application of the proposed approach to other materials.

42 ENGINEERING↗

The influence of temperature on the strain-hardening behavior of Fe-22/25/28Mn-3Al-3Si TRIP/TWIP steels

In this work, the influence of temperature and stacking fault energy (SFE) on the strain-hardening behavior and critical resolved shear stress for twinning was investigated for three Fe–22/25/28Mn–3Al–3Si wt.% transformation- and twinning-induced plasticity (TRIP/TWIP) steels. The SFEs were calculated by two different methods, density functional theory and statistical thermodynamic modeling. The dislocation structure, observed at low levels of plastic deformation, transitions from “planar” to “wavy” dislocation glide with an increase in temperature, Mn content, and/or SFE. The change in dislocation glide mechanisms from planar to wavy reduces the strain hardening rate, in part due to fewer planar obstacles and greater cross slip activity. Additionally, the alloys exhibit a large decrease in strength and ductility with increasing temperature from 25 to 200 °C, attributed to a substantial reduction in the thermally activated component of the flow stress, predominate suppression of TRIP and TWIP, and a significant increase in the critical resolved shear stress for mechanical twinning. Interestingly, the increase in SFE with temperature had a rather minor influence on the critical resolved shear stress for mechanical twinning, and other temperature dependent factors which likely play a more dominant role are discussed.

36 MATERIALS SCIENCE↗

Polymorphic structure of $\langle a \rangle$-type screw dislocation cores in $\alpha$-Ti

The dislocation core structure has a significant role in determining the dominant slip plane and the magnitude of the Peierls stress for a dislocation. An important challenge when studying dislocation cores is to determine the stable and metastable core morphologies, and then relate these structures to the dynamics of the dislocations. ere this study introduces a method for identifying core structures that are metastable at zero temperature. Application of this method to $\langle$a$\rangle$-type screw dislocations in α-Ti (as described using an empirical potential) reveals a multitude of (meta)stable nonplanar cores. Molecular dynamics studies show how the competing metastable core structures determine the properties of the dislocations at temperature and under a range of non-Schmid stresses.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Doping Metallic Grain Boundaries to Control Atomic Structure and Damage Tolerance (Final Report)

The interfaces between crystals, known as grain boundaries, often act as sites for crack and void nucleation during plastic deformation of metallic materials. While it is known that interfacial character and structural state can greatly influence this damage nucleation process, the current level of control over such details is extremely limited. The objective of this project was to obtain a fundamental understanding of how metallic grain boundary structure can be controlled through intelligent doping, with the idea of inducing planned grain boundary phases or complexions. The effect of complexion structure on dislocation accommodation mechanisms was studied, to improve the field’s understanding of damage nucleation at interfaces. While mechanical damage was the primary focus, the project showed that amorphous complexions can also improve a material’s resistance to radiation damage, providing a single materials design concept that can address multiple important technological areas. This research used a combination of computational, experimental, and characterization techniques to isolate and understand the importance of nanoscale grain boundary structure and interfacial chemistry. The fundamental insights provided by this project enable the creation of advanced engineering metals with improved damage tolerance.

36 MATERIALS SCIENCE↗

A mechanistic model for creep and thermal aging in Alloy 709

This report describes a physics-based model for creep and thermal aging in Alloy 709. Alloy 709 is an advanced austenitic alloy, targeted for use in future Sodium Fast Reactors (SFRs) and other advanced reactors. The material has superior high temperature properties compared to currently qualified 316 and 304 stainless steels. However, the available creep and thermal aging test database for Alloy 709 is significantly more limited compared to the historical materials. The physics-based model developed here is one way to accelerate the qualification of the material by providing more accurate long-term predictions for creep properties and thermal aging, compared to current empirical time-extrapolate techniques. The crystal plasticity finite element model is used to predict the deformation and failure of alloy 709. The same setup for the CPFE model is used in both the baseline model calibration process and the simulation campaigns for parameter inference. Specific constitutive choices are made for Alloy 709 to capture the primary deformation mechanisms. The dislocation creep formulation developed by Hu and Cocks is extended to account for coupled precipitation formation and the grain boundary cavitation model developed by Sham, Needleman, et al. is used to model grain boundary cavitation-induced failure. A novel update algorithm is proposed to render the semi-discrete constitutive update for the Sham-Needleman model unconditionally stable. A progressive calibration approach is adopted based on the observations that several types of material responses can be effectively decoupled. A surrogate model is trained based on full-fledged CPFE simulations to accelerate the forward model evaluations, and stochastic variational inference (SVI) is used to calibrate the unknown microstructural model parameters. The calibrated mechanistic model is used to predict the long-term creep life of Alloy 709, and the predictions are compared against classical empirical approaches.

36 MATERIALS SCIENCE↗

Doping Metallic Grain Boundaries to Control Atomic Structure and Damage Tolerance

Grain boundaries often act as sites for crack and void nucleation during plastic deformation of metallic materials. While it is known that grain boundary character and structure can greatly influence this damage nucleation process, the current level of control over such details is limited. The objective of this project was to obtain a fundamental understanding of how metallic grain boundary structure can be controlled through intelligent doping, with the idea of inducing planned amorphous grain boundary phases or complexions. The effect of amorphous complexion structure on dislocation accommodation mechanisms was studied, to improve the field’s understanding of damage nucleation at a promising type of interface. Different microstructural descriptors were studied, as grain boundaries can have large variations and complexity of local structure, and influence the mechanical damage resistance of these features was tested. Nanocrystalline systems that contain amorphous grain boundary complexions were prioritized, as these have more extreme variations in interfacial structure and damage tolerance, with an emphasis on isolating the importance of complexion population (type, thickness, etc.), network topology, local structure, and local chemistry. This research used a combination of computational, experimental, and characterization techniques to isolate and understand the importance of nanoscale grain boundary structure and interfacial chemistry. Amorphous grain boundary complexions were found to clearly increase a material’s resistance to mechanical damage, with the local distribution of structural short-range order within the complexions found to be an important descriptor for damage and the proposed focus of future work in this area.

36 MATERIALS SCIENCE↗

Probing the Damage Recovery Mechanism in Irradiated Stainless Steels Using In-Situ Microcantilever Bending Test

Single crystalline microcantilevers are fabricated from the base metal and heat-affected zone (HAZ) of a laser welded, neutron irradiated austenitic stainless steel, for scanning electron microscope (SEM) in-situ bending. In the HAZ, cantilevers exhibit higher yield point and lower crack tip blunting displacement than in the base metal and unirradiated archive specimen. These results suggest that radiation-induced defects harden the base metal, whereas the HAZ exhibits annealing of defects leading to mechanical softening. Dislocation nucleation ahead of the crack tip is responsible for ductile blunting behavior and provides a pathway to mitigating helium-induced cracking during weld repairs of irradiated materials.

36 MATERIALS SCIENCE↗

Medium-Range Order Resists Deformation in Metallic Liquids and Glasses

In crystals, lattice defects, such as dislocations, control mechanical deformation. Similarly, it is widely believed that even in glasses and liquids some kinds of defects, strongly disordered regions, play a major role in deformation. To identify defects researchers focused on the nature of the short-range order (SRO) in the nearest neighbor cage of atoms. However, recent results by experiment, simulation and theory raise serious questions about this assumption. They suggest that the atomic medium-range order (MRO) provides resistance against flow at the atomic level. Because the MRO is a bulk property, it implies that defects play only a limited role. This new insight is supported by the density wave theory which shows that the MRO is driven by a top-down global force, rather than being a consequence of the SRO in the bottom-up manner, and the MRO provides stiffness to resist deformation. We briefly summarize the density wave theory, show that the MRO is related to ductility of metallic glasses, and discuss the implications on the role of the MRO in the atomic-level mechanism of deformation.

36 MATERIALS SCIENCE↗