Search NASA⌕ Search

SEARCH · Search NASA

Results for “EPDM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Swell Behavior of Elastomers with a Hydrothermal Liquefaction Bio-Crude and a Fast Pyrolysis Bio-Oil

The compatibility of seventeen elastomer materials with two heavy biofuels (fast pyrolysis bio-oil and hydrothermal liquefaction (HTL) bio-crude) and diesel was assessed through volume change measurements. The elastomers included two fluorocarbons, six acrylonitrile rubbers (NBRs), and one each of fluorosilicone, neoprene, polyurethane, silicone, epichlorohydrin rubber (ECO), a blend of polyvinyl chloride and NBR (OZO), styrene butadiene rubber (SBR), hydrogenated NBR (HNBR) and ethylene propylene diene monomer (EPDM). The specimens were immersed in each test fuel for four weeks at 50°C and then measured for volume change. Afterwards, the specimens were dried, and the volume was remeasured. Ingeneral, the bio-oil produced unacceptable swelling in the fluoroelastomers, ECO, OZO, neoprene, polyurethane, SBR, HNBR, EPDM, silicone and five of the NBRs. In most cases, the HTL bio-crude produced lower (though still unacceptable) swelling than the bio-oil. Materials that showed good compatibility with the HTL biocrude were the fluoroelastomers, OZO, and silicone.

Kass, Michael↗

TRITIUM EFFECTS ON DYNAMIC MECHANICAL PROPERTIES OF POLYMERIC MATERIALS

Dynamic mechanical analysis has been used to characterize the effects of tritium gas (initially 1 atm. pressure, ambient temperature) exposure over times up to 2.3 years on several thermoplastics-ultrahigh molecular weight polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE), and Vespel{reg_sign} polyimide, and on several formulations of elastomers based on ethylene propylene diene monomer (EPDM). Tritium exposure stiffened the elastic modulus of UHMW-PE up to about 1 year and then softened it, and reduced the viscous response monotonically with time. PTFE initially stiffened, however the samples became too weak to handle after nine months exposure. The dynamic properties of Vespel{reg_sign} were not affected. The glass transition temperature of the EPDM formulations increased approximately 4 C. following three months tritium exposure.

08 HYDROGEN↗

High-pressure hydrogen decompression in sulfur crosslinked elastomers

High-pressure storage and cyclic (de)pressurization of hydrogen gas is known to result in degradation and failure of gas canisters, hoses, linings, and O-rings as the relatively small hydrogen molecule can readily permeate most materials. Hence, identifying material compositions that are less susceptible to hydrogen-induced damage is of significant importance to the hydrogen energy infrastructure. Here, we use classical atomistic molecular dynamics simulations to study hydrogen exposed ethylene-propylene-diene monomer (EPDM) rubber, an elastomer typically used in O-rings. We make chemical modifications to the model by adjusting the crosslink density and report on gas solubility, diffusivity, and molecular restructuring in response to rapid decompression. Our simulations indicate that increases in crosslink density can reduce volumetric expansion during decompression and result in smaller free volume pore sizes. However, these favorable properties for sealing materials come with a tradeoff. At pressure, crosslinks introduce extra free volume, providing potential sites for gas localization, the precursor to cavitation-induced failure.

08 HYDROGEN↗

Effects of high-pressure hydrogen exposure on filler-elastomer adhesion

Elastomers are known to gain enhanced mechanical properties through compounding with nanosized filler particles such as silica or carbon black. Filler dispersion and filler-polymer interfacial strength are key contributing factors to this improvement. The interfacial strength is critical to part lifetime in pressurized gas sealing applications such as O-rings, where weak binding between the filler particle and polymer matrix can lead to internal void structures. With the aim to build a fundamental understanding of precursors to pressurized hydrogen-induced failure in elastomers, we use all-atom molecular dynamics simulations to study the impact of hydrogen oversaturation on filler-polymer interaction strength. We systematically study the interface between a commonly used elastomer, ethylene-propylene-diene monomer (EPDM) and silica by varying gas concentration, crosslink density, and surface chemistry. Our simulations predict that decompression leads to a localization of excess gas near the interface. In conclusion, we demonstrate that this localized gas can weaken interfacial adhesion and quantify the interaction using thermodynamic approaches.

EPDM↗

In situ investigation of high-pressure hydrogen-induced swelling in elastomers and its correlation with material properties

The resistance of elastomeric materials to high-pressure hydrogen-induced damage is essential for ensuring the reliability of hydrogen infrastructure. Here, in this study, we systematically investigated the swelling behavior and hydrogen transport properties of four elastomer types – EPDM, NBR, FKM, and HNBR – using a custom in-situ view cell system capable of real-time monitoring during decompression from pressures up to 96.5 MPa. Each elastomer was formulated with and without fillers and plasticizers to assess the effects of formulation on swelling response. Thermal desorption analysis (TDA) was employed to determine equilibrium hydrogen content and diffusion coefficients, providing insight into gas uptake and mobility within each material. Correlation analyses using Pearson and Spearman coefficients revealed that the diffusion coefficient showed a stronger relationship with swelling behavior than hydrogen content, highlighting the dominant role of hydrogen mobility. Filled elastomers, particularly those with carbon black, consistently showed reduced swelling due to enhanced stiffness and reduced diffusivity. These results deepen our understanding of diffuso-mechanical interactions in elastomers and support the rational design of sealing materials for high-pressure hydrogen systems.

EPDM↗

Interfacial Effects on the Dielectric Properties of Elastomer Composites and Nanocomposites

Elastomer-based composites and nanocomposites are discussed, with the emphasis on the filler and interfacial effects on their dynamics, and the resulting manifestation in their macroscopic dielectric or mechanical response. Specifically, selected polydimethylsiloxane (PDMS)/barium-titanate and styrene-butadiene rubber (SBR)/graphene oxide nanocomposites are discussed, as examples where controlled spatial distribution of filler (structured composites) gives rise to significantly different dielectric and thermomechanical behaviors. Also, ethylene–propylene–diene (EPDM)/carbon black (CB) composites are presented, as examples of systems that exhibit an abnormal temperature dependence of dielectric relaxation; and this response is discussed in the context of CB cluster polarization and quantified through a simple scaling model of the same. Finally, multi-filler EPDM/CB/ceramic elastomer nanocomposites are discussed, as examples of systems with antagonistic interfacial effects between conductive and dielectric fillers, as well as with strong interphase responses that can overwhelm the dielectric contributions from the fillers; in these systems, interphasial responses result in counter-intuitive dielectric behaviors and in strong deviations from standard design principles typically employed in the design of dielectric composite systems.

Li, Bo↗

In situ friction and wear behavior of rubber materials incorporating various fillers and/or a plasticizer in high-pressure hydrogen

Polymers are used routinely for equipment and infrastructure in hydrogen vehicle refueling stations, but significant gaps remain in understanding their hydrogen compatibility. The tribological properties of these materials in a high-pressure hydrogen environment is important in preventing component failure and the need for frequent replacement. We present in situ tribological studies on model rubbers, which include common fillers and plasticizer, using an in situ tribometer developed previously. Results suggest a clear, yet complicated, combined effect of the high-pressure hydrogen and the additives on the tribological performance of the chosen materials, as compared to matching experiments performed in ambient air. We find that the additives improved wear resistance in EPDM but deteriorated that in NBR due to disparate additive-polymer interactions.

Kuang, Wenbin↗

Coupled diffusion-deformation-damage model for polymers used in hydrogen infrastructure

The soft materials used in the infrastructure of hydrogen storage and distribution systems are vulnerable because exposure to high-pressure hydrogen can lead to mechanical damage and property degradation. Some materials, such as polymers, can undergo mechanical failure due to a phenomenon wherein hydrogen gas diffuses through the polymer chains and occupies preexisting cavities or voids inside the polymer material. If the hydrogen gas pressure is reduced more quickly than hydrogen can diffuse back out of the polymer which is necessary for some applications, the trapped hydrogen gas instead escapes by rupturing the material, causing surface blistering or permanent damage. In this study, a continuum mechanics-based fully coupled diffusion-deformation model with damage is developed to predict the stress distribution and damage propagation while the polymer undergoes rapid decompression failure. The hyperelastic material model, along with the maximum principal strain failure theory, was chosen for this study as it represents the nonlinear material response with brittle failure observed in uniaxial tensile tests perfectly. EPDM polymer was chosen for this study because of its commercial availability and common use in hydrogen storage and distribution system. It has superior mechanical properties, high and low temperature resistance, and certain compounds work well in hydrogen gas. This work is useful for design engineers to alter the parameters while manufacturing polymer composites to increase their performance in a high-pressure hydrogen environment.

Kulkarni, Shank S.↗

The compatibility performance of fuel system elastomers with two dioxolane molecules as blends with diesel

The compatibility of 17 elastomers with two dioxolane molecules was assessed by volume change and hardness measurements. Each molecule was blended with diesel in concentrations of 0, 10, 20 and 30 wt.%. The elastomers included two fluorocarbons, six acrylonitrile butadiene rubbers (NBRs), and one each of fluorosilicone, chloroprene rubber (CR), polyurethane, styrene butadiene rubber (SBR), hydrogenated NBR (HNBR), a blend of NBR and PVC (OZO), epichlorohydrin/ ethylene oxide (ECO), ethylene propylene diene monomer (EPDM), and silicone. Specimens of each elastomer were immersed in the test fuels for a period of 4 weeks and measured for property change. Afterwards they were dried at 60°C for 20 h and remeasured. The results showed that the dioxolanes were suitable with many of the elastomers and that the performances were essentially the same for both molecules. The dioxolanes were found to either have negligible impact beyond neat diesel or they produced a small increase in swell. This minimal impact is attributed to the fact that the solubility parameters (especially those associated with polarity and hydrogen bonding) of the dioxolanes are similar to those of diesel. As a result, little change in solubility and hence swell occurred when dioxolane was added to the diesel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Normetex Pump Alternatives Study

A mainstay pump for tritium systems, the Normetex scroll pump, is currently unavailable because the Normetex company went out of business. This pump was an all-metal scroll pump that served tritium processing facilities very well. Current tritium system operators are evaluating replacement pumps for the Normetex pump and for general used in tritium service. An all-metal equivalent alternative to the Normetex pump has not yet been identified. 1. The ideal replacement tritium pump would be hermetically sealed and contain no polymer components or oils. Polymers and oils degrade over time when they contact ionizing radiation. 2. Halogenated polymers (containing fluorine, chlorine, or both) and oils are commonly found in pumps. These materials have many properties that surpass those of hydrocarbon-based polymers and oils, including thermal stability (higher operating temperature) and better chemical resistance. Unfortunately, they are less resistant to degradation from ionizing radiation than hydrocarbon-based materials (in general). 3. Polymers and oils can form gaseous, condensable (HF, TF), liquid, and solid species when exposed to ionizing radiation. For example, halogenated polymers form HF and HCl, which are extremely corrosive upon reaction with water. If a pump containing polymers or oils must be used in a tritium system, the system must be designed to be able to process the unwanted by-products. Design features to mitigate degradation products include filters and chemical or physical traps (eg. cold traps, oil traps). 4. Polymer components can work in tritium systems, but must be replaced regularly. Polymer components performance should be monitored or be regularly tested, and regular replacement of components should be viewed as an expected normal event. A radioactive waste stream must be established to dispose of used polymer components and oil with an approved disposal plan developed based on the facility location and its regulators. Polymers have varying resistances to ionizing radiation - aromatic polymers such as polyimide Vespel (TM) and the elastomer EPDM (ethylene propylene diene monomer) have been found to be more resistant to degradation in tritium than other polymers. This report presents information to help select replacement pumps for Normetex pumps in tritium systems. Several pumps being considered as Normetex replacement pumps are discussed.

07 ISOTOPE AND RADIATION SOURCES↗

Basin-Scale Leakage Risks from Geologic Carbon Sequestration: Impact on Carbon Capture and Storage Energy Market Competitiveness

This three-year project, performed by Princeton University in partnership with the University of Minnesota and Brookhaven National Laboratory, examined geologic carbon sequestration in regard to CO 2 leakage and potential subsurface liabilities. The research resulted in basin-scale analyses of CO 2 and brine leakage in light of uncertainties in the characteristics of leakage processes, and generated frameworks to monetize the risks of leakage interference with competing subsurface resources. The geographic focus was the Michigan sedimentary basin, for which a 3D topographical model was constructed to represent the hydrostratigraphy. Specifically for Ottawa County, a statistical analysis of the hydraulic properties of underlying sedimentary formations was conducted. For plausible scenarios of injection into the Mt. Simon sandstone, leakage rates were estimated and fluxes into shallow drinking-water aquifers were found to be less than natural analogs of CO 2 fluxes. We developed the Leakage Impact Valuation (LIV) model in which we identified stakeholders and estimated costs associated with leakage events. It was found that costs could be incurred even in the absence of legal action or other subsurface interference because there are substantial costs of finding and fixing the leak and from injection interruption. We developed a model framework called RISCS, which can be used to predict monetized risk of interference with subsurface resources by combining basin-scale leakage predictions with the LIV method. The project has also developed a cost calculator called the Economic and Policy Drivers Module (EPDM), which comprehensively calculates the costs of carbon sequestration and leakage, and can be used to examine major drivers for subsurface leakage liabilities in relation to specific injection scenarios and leakage events. Finally, we examined the competiveness of CCS in the energy market. This analysis, though qualitative, shows that financial incentives, such as a carbon tax, are needed for coal combustion with CCS to gain market share. In another part of the project we studied the role of geochemical reactions in affecting the probability of CO 2 leakage. A basin-scale simulation tool was modified to account for changes in leakage rates due to permeability alterations, based on simplified mathematical rules for the important geochemical reactions between acidified brines and caprock minerals. In studies of reactive flows in fractured caprocks, we examined the potential for permeability increases, and the extent to which existing reactive transport models would or would not be able to predict it. Using caprock specimens from the Eau Claire and Amherstburg, we found that substantial increases in permeability are possible for caprocks that have significant carbonate content, but minimal alteration is expected otherwise. We also found that while the permeability increase may be substantial, it is much less than what would be predicted from hydrodynamic models based on mechanical aperture alone because the roughness that is generated tends to inhibit flow.

54 ENVIRONMENTAL SCIENCES↗

Preliminary Report: Effects of Irradiation and Thermal Exposure on Elastomeric Seals for Cask Transportation and Storage

A testing and analysis approach to predict the sealing behavior of elastomeric seal materials in dry storage casks and evaluate their ability to maintain a seal under thermal and radiation exposure conditions of extended storage and beyond was developed, and initial tests have been conducted. The initial tests evaluate the aging response of EPDM elastomer O-ring seals. The thermal and radiation exposure conditions of the CASTOR® V/21 casks were selected for testing as this cask design is of interest due to its widespread use, and close proximity of the seals to the fuel compared to other cask designs leading to a relatively high temperature and dose under storage conditions. A novel test fixture was developed to enable compression stress relaxation measurements for the seal material at the thermal and radiation exposure conditions. A loss of compression stress of 90% is suggested as the threshold at which sealing ability of an elastomeric seal would be lost. Previous studies have shown this value to be conservative to actual leakage failure for most aging conditions. These initial results indicate that the seal would be expected to retain sealing ability throughout extended storage at the cask design conditions, though longer exposure times are needed to validate this assumption. The high constant dose rate used in the testing is not prototypic of the decreasingly low dose rate that would occur under extended storage. The primary degradation mechanism of oxidation of polymeric compounds is highly dependent on temperature and time of exposure, and with radiation expected to exacerbate the oxidation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of the Performance of O-rings Made with Different Elastomeric Polymers in Simulated Geothermal Environments at 300°C

This paper aims to evaluate the survival of O-rings made with six different elastomeric polymers, EPDM, type I- and II-FKM, FEPM, FFKM, and FSR, in five different simulated geothermal environments at 300°C. It further defines the relative strengths and weaknesses of the materials in each environment. The environments tested were: 1) non-aerated steam-cooling cycles, 2) aerated steam-cooling cycles, 3) water-based drilling fluid, 4) CO2-rich geo-brine fluid, and, 5) heat-cool water quenching cycles. Following exposure, the extent of oxidation, oxidationinduced degradation, thermal behaviors, micro-defects, permeation depths of ionic species present in environments throughout the O-ring, silicate-related scale-deposition, and changes in mechanical properties were assessed.

36 MATERIALS SCIENCE↗

Performance of Bolted Closure Joint Elastomers Under Cask Aging Conditions

The bolted closure joint of a bare spent fuel cask is susceptible to age-related degradation and potential loss of confinement function under long-term storage conditions. Elastomeric seals, a component of the joint typically used to facilitate leak testing of the primary seal that includes the metallic seal and bolting, is susceptible to degradation over time by several mechanisms, principally via thermo-oxidation, stress-relaxation, and radiolytic degradation under time and temperature condition. Irradiation and thermal exposure testing and evaluation of an ethylene-propylene diene monomer (EPDM) elastomeric seal material similar to that used in the CASTOR® V/21 cask for a matrix of temperature and radiation exposure conditions relevant to the cask extended storage conditions, and development of semiempirical predictive models for loss of sealing force is in progress. A special insert was developed to allow Compressive Stress Relaxation (CSR) measurements before and after the irradiation and/or thermal exposure without unloading the elastomer. A condition of the loss of sealing force for the onset of leakage was suggested. The experimentation and modeling being performed could enable acquisition of extensive coupled aging data as well as an estimation of the timeframe when loss of sealing function under aging (temperature/radiation) conditions may occur.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Design Parameters of a Miniaturized Piezoelectric Underwater Acoustic Transmitter

The Juvenile Salmon Acoustic Telemetry System (JSATS) project supported by the U.S. Army Corps of Engineers, Portland District, has yielded the smallest acoustic fish tag transmitter commercially available to date. In order to study even smaller fish populations and make the transmitter injectable by needles, the JSATS acoustic micro transmitter needs to be further downsized. As part of the transmitter downsizing effort some of the design parameters of the lead zirconate titanate (PZT) ceramic tube transducer in the transmitter were studied, including the type of PZT, the backing material, the necessary drive voltage, the transmitting bandwidth and the length of the transducer. It was found that, to satisfy the 156-dB source level requirement of JSATS, a square wave with a 10-volt amplitude is required to drive 'soft' PZT transducers. PZT-5H demonstrated the best source level performance. For Navy types I and II, 16 volts or 18 volts were needed. Ethylene-propylene-diene monomer (EPDM) closed-cell foam was found to be the backing material providing the highest source level. The effect of tube length on the source level is also demonstrated in this paper, providing quantitative information for downsizing of small piezoelectric transmitters.

47 OTHER INSTRUMENTATION↗

Toxicity of Pyrolysis Gases from Elastomers

The toxicity of the pyrolysis gases from six elastomers was investigated. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acryltonitrile rubber exhibited the greatest toxicity under these test conditions; carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, Carlos J.↗

Effect of heating rate on toxicity of pyrolysis gases from some elastomers

The effect of heating rate on the toxicity of the pyrolysis gases from six elastomers was investigated, using a screening test method. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acrylonitrile rubber exhibited the greatest toxicity under these test conditions, and carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, C. J.↗