Tensile strain measurements of ceramic fibers using scanning laser acoustic microscopy

A noncontacting technique using scanning laser acoustic microscopy for making in situ tensile strain measurements of small diameter fibers was implemented for the tensile strain analysis of individual Nicalon SiC fibers (nominal diameter 15 microns). Stress versus strain curves for the fibers were plotted from the experimental data. The mean elastic modulus of the fibers was determined to be 185.3 GPa. Similar measurements were made for Carborundum SiC fibers (nominal diameter 28 microns) and Saphikon sapphire fibers (nominal diameter 140 microns), yielding and elastic modulus of 401 and 466.8 GPa, respectively.

Kent, Renee M.

Mechanical properties of particulate composites based on a body-centered-cubic Mg-Li alloy containing boron

The effect of substituting the Mg metal in Mg-B composites by a Mg-14 wt pct Li solid solution on the ductility of the resulting composite was investigated using elastic modulus measurements on the P/M composite material prepared with a dispersion of B particles (in a vol pct range of 0-30) in a matrix of Mg-14 wt pct Li-1.5 wt pct Al. It was found that the elastic modulus of the composites increased rapidly with increasing boron, with specific stiffness values reaching about two times that of most structural materials. The values of the compression and tensile strengths increased significantly with boron additions. Good tensile ductility was achieved at the level of 10 vol pct B. However, at 20 vol pct B, the Mg-Li composite exhibited only limited tensile ductility (about 2 percent total elongation).

Whalen, R. T.

Application of an Elongated Kelvin Model to Space Shuttle Foams

Spray-on foam insulation is applied to the exterior of the Space Shuttle s External Tank to limit propellant boil-off and to prevent ice formation. The Space Shuttle foams are rigid closed-cell polyurethane foams. The two foams used most extensively on the Space Shuttle External Tank are BX-265 and NCFI24-124. Since the catastrophic loss of the Space Shuttle Columbia, numerous studies have been conducted to mitigate the likelihood and the severity of foam shedding during the Shuttle s ascent to space. Due to the foaming and rising process, the foam microstructures are elongated in the rise direction. As a result, these two foams exhibit a non-isotropic mechanical behavior. In this paper, a detailed microstructural characterization of the two foams is presented. The key features of the foam cells are summarized and the average cell dimensions in the two foams are compared. Experimental studies to measure the room temperature mechanical response of the two foams in the two principal material directions (parallel to the rise and perpendicular to the rise) are also reported. The measured elastic modulus, proportional limit stress, ultimate tensile stress and the Poisson s ratios for the two foams are compared. The generalized elongated Kelvin foam model previously developed by the authors is reviewed and the equations which result from this model are presented. The resulting equations show that the ratio of the elastic modulus in the rise direction to that in the perpendicular-to-rise direction as well as the ratio of the strengths in the two material directions is only a function of the microstructural dimensions. Using the measured microstructural dimensions and the measured stiffness ratio, the foam tensile strength ratio and Poisson s ratios are predicted for both foams. The predicted tensile strength ratio is in close agreement with the measured strength ratios for both BX-265 and NCFI24-124. The comparison between the predicted Poisson s ratios and the measured values is not as favorable.

Sullivan, Roy M.

Influence of Processing Parameters on the Mechanical Properties of 3D Printed Borosilicate Particulate Reinforced Polymer Composites

Emerging composite materials are expanding the potential of additive manufacturing and enabling applications previously restricted by traditional manufacturing methods. The multi-phase nature of these composite materials combined with the complex in-ternal geometry of additively manufactured parts have enabled unique behavior, and potentially new applications. Additionally, these materials can be pyrolyzed to create dense metal, ceramic, and glass parts with geometries typically not achievable by tra-ditional processes. Additive manufacturing of borosilicate glass-based systems can open new applications in nuclear engineering, astronomy, and bone regrowth therapy. To elucidate the process-parameter relationship of borosilicate-polylactic acid (PLA) composites, mechanical testing was conducted and compared with a pure polylactic acid polymer baseline. Test specimens were fabricated by fused-filament fabrication with minimal post-processing. Yield strength, ultimate strength, and elastic modulus were calculated from stress-strain curves. Optical and scanning electron microscopy were conducted to observe the specimen microstructure before and after testing. The highest compressive yield strength for the composite was 28.22 MPa, and the highest compressive yield strength for PLA was 49.30 MPa. Print orientation was found to benefit the composite material but have a detrimental effect on the pure matrix material. An elastic modulus of 2.66 GPa was recorded for the borosilicate-PLA composite at 100% infill, 1 shell wall, and layer lines parallel to compression axis. Microscopy revealed that lower modulus composite specimens had the particulates re-distributed within the matrix. Tensile testing was done according to a polymer testing standard, which caused difficulties obtaining consistent fracture within the gauge length.

mechanical testing

Tensile properties of SiC/aluminum filamentary composites - Thermal degradation effects

Aluminium metal matrix composites with a low cost fiber, e.g. SiC, provide for an attractive combination of high elastic modulus and longitudinal strengths coupled with a low density. SiC (volume fraction 0.55)-aluminum (6061) systems have been studied in order to optimize fiber composite strength and processing parameters. A comparison of two SiC/aluminum composites produced by AVCO and DWA is provided. Fiber properties are shown to alter composite tensile properties and fracture morphology. The room temperature tensile strengths appear to be insensitive to thermal exposures at 500 C up to 150 h. The elastic modulus of the composites also appears to be stable up to 400 C, however variations in the loss modulus are apparent. The fracture morphology reflects the quality of the interfacial bond, fiber strengths and fiber processing.

Skinner, A.

Effects of Cryogenic Temperature on Fracture Toughness of Core-Shell Rubber (CSR) Toughened Epoxy Nanocomposites

This study investigated the effects of core-shell rubber (CSR) nanoparticles on the mechanical properties and fracture toughness of an epoxy resin at ambient and liquid nitrogen (LN2) temperatures. Varying amounts of Kane Ace MX130 toughening agent were added to a commercially available EPON 862/Epikure W epoxy resin. Elastic modulus was calculated using quasi-static tensile data. Fracture toughness was evaluated by the resulting breaking energy measured in Charpy impact tests conducted on an instrumented drop tower. The size and distribution of the CSR nanoparticles were characterized using Transmission Electron Microscopy (TEM) and Small Angle X-ray Scattering (SAXS). Scanning Electron Microscopy (SEM) was used to study the fracture surface morphology. The addition of the CSR nanoparticles increased the breaking energy with negligible change in elastic modulus and ultimate tensile stress (UTS). At ambient temperature the breaking energy increased with increasing additions of the CSR nanoparticles, while at LN2 temperatures, it reached a maximum at 5 wt% CSR concentration. KEY WORDS: liquid nitrogen (LN2) properties, fracture toughness, core-shell rubber (CSR).

Wang, J.

Effects of Core-Shell Rubber (CSR) Nanoparticles on the Cryogenic Fracture Toughness of CSR Modified Epoxy

This study investigated the effects of core-shell rubber (CSR) nanoparticles on the mechanical properties and fracture toughness of an epoxy resin at ambient and liquid nitrogen (LN2) temperatures. Varying amounts of Kane Ace(Registered TradeMark) MX130 and Kane Ace(Registered TradeMark) MX960 toughening agent were added to a commercially available EPON 862/Epikure W epoxy resin. Elastic modulus was calculated using quasi-static tensile data. Fracture toughness was evaluated by the resulting breaking energy measured in Charpy impact tests conducted on an instrumented drop tower. The size and distribution of the CSR nanoparticles were characterized using Transmission Electron Microscopy (TEM) and Small Angle X-ray Scattering (SAXS). Scanning Electron Microscopy (SEM) was used to study the fracture surface morphology. The addition of the CSR nanoparticles increased the breaking energy with negligible change in elastic modulus and ultimate tensile stress (UTS). At ambient temperature the breaking energy increased with increasing additions of the CSR nanoparticles up to 13.8wt%, while at LN2 temperatures, it reached a plateau at much lower CSR concentration.

Wang, Jun

Evaluation of urethane for feasibility of use in wind turbine blade design

A preliminary evaluation was conducted of the use of cast urethane as a possible material for low-cost blades for wind turbines. Specimen test data are presented for ultimate tensile strength, elastic modulus, flexural strain, creep, and fatigue properties of a number of urethane formulations. Data are also included for a large-scale urethane blade section composed of cast symmetrical half-profiles tested as a cantilever beam. Based on these results, an analysis was conducted of a full-scale blade design of cast urethane that meets the design specifications of the rotor blades for the NASA/DOE experimental 100-kW MOD-0 wind turbine. Because of the low value of elastic modulus for urethane (around 457 000 psi), the design loads would have to be carried by metal reinforcement. Considerations for further evaluation are noted.

Lieblein, S.

Resilient and Corrosion-Proof Rolling Element Bearings Made from Superelastic Ni-Ti Alloys for Aerospace Mechanism Applications

Mechanical components (bearings, gears, mechanisms) typically utilize hard materials to minimize wear and attain long life. In such components, heavily loaded contact points (e.g., meshing gear teeth, bearing ball-raceway contacts) experience high contact stresses. The combination of high hardness, heavy loads and high elastic modulus often leads to damaging contact stress. In addition, mechanical component materials, such as tool steel or silicon nitride exhibit limited recoverable strain (typically less than 1 percent). These material attributes can lead to Brinell damage (e.g., denting) particularly during transient overload events such as shock impacts that occur during the launching of space vehicles or the landing of aircraft. In this paper, a superelastic alloy, 60NiTi, is considered for rolling element bearing applications. A series of Rockwell and Brinell hardness, compressive strength, fatigue and tribology tests are conducted and reported. The combination of high hardness, moderate elastic modulus, large recoverable strain, low density, and intrinsic corrosion immunity provide a path to bearings largely impervious to shock load damage. It is anticipated that bearings and components made from alloys with such attributes can alleviate many problems encountered in advanced aerospace applications.

DellaCorte, Christopher

Influence of extended exposure in space on mechanical properties of high-toughness graphite-epoxy composite material (A0019)

Graphite-epoxy composites are promising candidates for structural use in space vehicles because of their high strength and elastic modulus properties. The problem of low fracture toughness was solved by use of recently developed techniques of intermittent interlaminar bonding. Before this material can be adapted for space use, however, confidence must be gained that its mechanical properties are not degraded by exposure to the space environment. The objective of this experiment is to test the effect of extended exposure to a space environment on the mechanical properties of a specially toughened T300/5208 graphite-epoxy composite material. Specimens made by recently developed techniques of intermittent interlaminar bonding will be exposed and afterward tested for fracture toughness, tensile strength, and elastic modulus. The approach of this experiment is to provide a frame on which the specimens can be mounted with their flat sides normal to the Long Duration Exposure Facility radius, each specimen with an unobstructed exposure of about 2 pi sr. The specimens will be mounted so that they neither fracture from high stress nor fail from excessive heating during launch and return.

Felbeck, D. K.

Effect of Sintering on Mechanical and Physical Properties of Plasma-Sprayed Thermal Barrier Coatings

The effect of sintering on mechanical and physical properties of free-standing plasma-sprayed ZrO2-8 wt% Y2O3 thermal barrier coatings (TBCs) was determined by annealing them at 1316 C in air. Mechanical and physical properties of the TBCs, including strength, modes I and II fracture toughness, elastic modulus, Poisson s response, density, microhardness, fractography, and phase stability, were determined at ambient temperature as a function of annealing time ranging from 0 to 500 h. All mechanical and physical properties, except for the amount of monoclinic phase, increased significantly in 5 to 100 h and then reached a plateau above 100 h. Annealing resulted in healing of microcracks and pores and in grain growth, accompanying densification of the TBC s body due to the sintering effect. However, an inevitable adverse effect also occurred such that the desired lower thermal conductivity and good expansivity, which makes the TBCs unique in thermal barrier applications, were degraded upon annealing. A model was proposed to assess and quantify all the property variables in response to annealing in a normalized scheme. Directionality of as-sprayed TBCs appeared to have an insignificant effect on their properties, as determined via fracture toughness, microhardness, and elastic modulus measurements.

Choi, Sung R.

Readily fiberizable glasses having a high modulus of elasticity

New glass compositions yield composites having higher moduli of elasticity and specific moduli of elasticity than commercially available glasses. Over a reasonable temperature range the glasses have a viscosity of about 20,000 poises. They consist of silica, alumina, magnesia, and beryllia, plus at least one uncommon oxide.

Bacon, J. F.

Experimental Identification and Simulation of Time and/or Rate Dependent Reversible and Irreversible Deformation Regions for both a Titanium and Nickel Alloy

In this paper time and/or rate dependent deformation regions are experimentally mapped out as a function of temperature. It is clearly demonstrated that the concept of a threshold stress (a stress that delineate reversible and irreversible behavior) is valid and necessary at elevated temperatures and corresponds to the classical yield stress at lower temperatures. Also the infinitely slow modulus, (Es) i.e. the elastic modulus of the material if it was loaded at an infinitely slow strain rate, and the "dynamic modulus", modulus, Ed, which represents the modulus of the material if it is loaded at an infinitely fast rate are used to delineate rate dependent from rate independent regions. As demonstrated at elevated temperatures there is a significant difference between the two modulus values, thus indicating both significant time-dependence and rate dependence. In the case of the nickel-based super alloy, ME3, this behavior is also shown to be grain size specific. Consequently, at higher temperatures viscoelastic behavior exist below k (i.e., the threshold stress) and at stresses above k the behavior is viscoplastic. Finally a multi-mechanism, stress partitioned viscoelastic model, capable of being consistently coupled to a viscoplastic model is characterized over the full temperature range investigated for Ti-6-4 and ME3.

Arnold, Steven M.

Ni-Ti Alloys for Aerospace Bearing Applications

Nickel-rich Ni-Ti alloys are emerging candidate materials for aerospace bearing applications. These alloys exhibit a unique combination of physical, chemical, and tribological properties that are highly relevant to challenging aerospace bearings and other mechanical components. Despite being made solely from metals, Ni-Ti alloys are classified as intermetallics with properties akin to both metals and ceramics. For instance, like metals, they are electrically conductive but they tend to be brittle like ceramics. When properly processed, they have high hardness, low elastic modulus and an extensive elastic deformation range that imparts extraordinarily high resilience and resistance to denting. New alloy compositions enable simpler thermal processing and machining and intensive microstructural analyses have helped elucidate the materials science mechanisms governing hardness. In this paper, the application of state-of-art in NiTi alloys for aerospace bearings and mechanical components is explored. In addition to reviewing future trends and remaining challenges, the unique approaches and methods of tailoring bearing design to accommodate NiTis unique properties is discussed.

intermetallics

Minimum film thickness in elliptical contacts for different regimes of fluid-film lubrication

The film-parameter equations are provided for four fluid-film lubrication regimes found in elliptical contacts. These regimes are isoviscous-rigid; viscous-rigid; elastohydrodynamic of low-elastic-modulus materials, or isoviscous-elastic; and elastohydrodynamic, or viscous-elastic. The influence or lack of influence of elastic and viscous effects is the factor that distinguishes these regimes. The film-parameter equations for the respective regimes come from earlier theoretical studies by the authors on elastohydrodynamic and hydrodynamic lubrication of elliptical conjunctions. These equations are restated and the results are presented as a map of the lubrication regimes, with film-thickness contours on a log-log grid of the viscosity and elasticity parameters for five values of the ellipticity parameter. The results present a complete theoretical film-parameter solution for elliptical contacts in the four lubrication regimes.

Hamrock, B. J.

Mechanical properties of brittle materials

Brittle materials are difficult to tensile test because of gripping problems. They either crack in conventional grips or they are crushed. Furthermore, they may be difficult to make into tensile specimens having, for example, threated ends or donut shapes. To overcome the problem, simple rectangular shapes can be used in bending (i.e., a simple beam) in order to obtain the modulus of rupture and the elastic modulus. The equipment necessary consists of a fixture for supporting the specimens horizontally at two points, these points contact points being rollers which are free to rotate. The force necessary to bend the specimen is produced by a tup attached to the crosshead of an Instron machine. Here, the experimental procedure is explained.

Cornwell, L. R.

Nanotubular Toughening Inclusions

Conventional toughening agents are typically rubbery materials or small molecular weight molecules, which mostly sacrifice the intrinsic properties of a matrix such as modulus, strength, and thermal stability as side effects. On the other hand, high modulus inclusions tend to reinforce elastic modulus very efficiently, but not the strength very well. For example, mechanical reinforcement with inorganic inclusions often degrades the composite toughness, encountering a frequent catastrophic brittle failure triggered by minute chips and cracks. Thus, toughening generally conflicts with mechanical reinforcement. Carbon nanotubes have been used as efficient reinforcing agents in various applications due to their combination of extraordinary mechanical, electrical, and thermal properties. Moreover, nanotubes can elongate more than 20% without yielding or breaking, and absorb significant amounts of energy during deformation, which enables them to also be an efficient toughening agent, as well as excellent reinforcing inclusion. Accordingly, an improved toughening method is provided by incorporating nanotubular inclusions into a host matrix, such as thermoset and thermoplastic polymers or ceramics without detrimental effects on the matrix's intrinsic physical properties.

Park, Cheol