Search NASA⌕ Search

SEARCH · Search NASA

Results for “Eutectic solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Directionally solidified ceramic eutectics

The aligned structures which result from the directional solidification (DS) of ceramic eutectics are of interest because of their potential for use in electronic devices and as structural materials. Techniques for growing DS ceramic eutectics are briefly discussed. The principles and controlling parameters of DS eutectic growth are described. The criteria for plane-front growth and the effect of growth rate on interlamellar or interfiber spacing are discussed. Examples of the effect of growth parameters on the alignment of the microstructure are given. Examples of the mechanical properties of directionally solidified oxide-oxide ceramics are also cited.

Ashbrook, R. L.↗

Influence of convection of eutectic morphology

Experimental data are given for BiMn/Bi rod eutectic and Fe3C/Fe lamellar eutectic solidified in low gravity. Eutectic spacing is summarized for various alloy systems solidified in low gravity. On-eutectic and off-eutectic models are evaluated with respect to the low-gravity solidification data. The models examined are inadequate for quantitative prediction of phase spacing for on-eutectic solidification in low gravity.

Curreri, P. A.↗

Use of Microgravity to Control the Microstructure of Eutectics

This grant began in June of 1996. Its long term goal is to be able to control the microstructure of directionally solidified eutectic alloys, through an improved understanding of the influence of convection. The primary objective of the present projects is to test hypotheses for the reported influence of microgravity on the microstructure of three fibrous eutectics (MnBi-Bi, InSb-NiSb, Al3Ni-Al). A secondary objective is to determine the influence of convection on the microstructure of other eutectic alloys. Two doctoral students and a masters student supported as a teaching assistant were recruited for this research. Techniques were developed for directional solidification of MnBi-Bi eutectics with periodic application of current pulses to produce an oscillatory freezing rate. Image analysis techniques were developed to obtain the variation in MnBi fiber spacing, which was found to be normally distributed. The mean and standard deviation of fiber spacing were obtained for several freezing conditions. Eighteen ampoules were prepared for use in the gradient freeze furnace QUELD developed at Queen's University for use in microgravity. Nine of these ampoules will be solidified soon at Queen's in a ground-based model. We hope to solidify the other nine in the QUELD that is mounted on the Canadian Microgravity Isolation Mount on MIR. Techniques are being developed for directional solidification of the Al-Si eutectic at different freezing rates, with and without application of accelerated crucible rotation to induce convection. For the first time, theoretical methods are being developed to analyze eutectic solidification with an oscillatory freezing rate. In a classical sharp-interface model, we found that an oscillatory freezing rate increases the deviation of the average interfacial composition from the eutectic, and increases the undercooling of the two phases by different amounts. This would be expected to change the volume fraction solidifying and the fiber spacing. Because of difficulties in tracking the freezing interfaces of the two solid phases, a phase-field model is also being developed. A paper demonstrating application of phase field methods to periodic structures has been submitted for publication.

Wilcox, William R.↗

Processing and Mechanical Properties of NiAl-Based In-Situ Composites

In-situ composites based on the NiAl-Cr eutectic system were successfully produced by containerless processing and evaluated. The NiAl-Cr alloys had a fibrous microstructure while the NiAl-(Cr,Mo) alloys containing 1 at. percent or more molybdenum exhibited a lamellar structure. The NiAl-28Cr-6Mo eutectic displays promising high temperature strength while still maintaining a reasonable room temperature fracture toughness when compared to other NiAl-based materials. The Laves phase NiAlTa was used to strengthen NiAl and very promising creep strengths were found for the directionally solidified NiAl-NiAlTa eutectic. The eutectic composition was found to be near NiAl-15.5Ta (at. percent) and well aligned microstructures were produced at this composition. An off-eutectic composition of NiAl-14.5Ta was also processed, consisting of NiAl dendrites surrounded by aligned eutectic regions. The room temperature toughness of these two phase alloys was similar to that of polycrystalline NiAl even with the presence of the brittle Laves phase NiAlTa. Polyphase in-situ composites were generated by directional solidification of ternary eutectics. The systems investigated were the Ni-Al-Ta-X (X=Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and both the eutectic composition and temperature were determined. Of these ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr,Al)NiTa-Cr eutectic was intermediate between those of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, David Ray↗

Orbital Processing of Aligned Magnetic Composites

Experiments will be conducted on the space shuttle in which aligned, two-phase magnetic composites will be grown by plane front directional solidification. The objectives are to: (1) identify and quantitatively evaluate the influences of gravitationally driven thermo-solutal convection on contained plane front solidification of binary, eutectic, off-eutectic, and peritectic magnetic composites; (2) to evaluate the effectiveness of micro-g processing as a means of damping convection; and (3) to evaluate the uniqueness of micro-g processing relative to the best of terrestrial convection damping.

Larson, D. J.↗

Structure-property relationships in eutectic composites

The preparation of a composite material of eutectic composition directly from the molten state is investigated. The manufacture of eutectic composites by unidirectional solidification is reviewed, and it is shown how two-phase composite structures of given relative volume fraction can be produced with a range of particle sizes. Crystallographic relationships and the thermal stability of interfaces in controlled eutectic structures are examined, the mechanical behavior of aligned eutectic microstructures is discussed, and characteristics of eutectic composites having mechanical properties of engineering significance are evaluated. Specific properties of the Ni-Nb eutectic alloy are reviewed to demonstrate the effect of structure control (through directional solidification) on the mechanical response of a eutectic composite. It is noted that unidirectionally solidified eutectic composites possess highly aligned and thermally stable microstructures and also exhibit excellent combinations of strength and ductility to very high temperature levels.

Hertzberg, R. W.↗

Development and Processing of Nickel Aluminide-Carbide Alloys

With the upper temperature limit of the Ni-based superalloys attained, a new class of materials is required. Intermetallics appear as likely candidates because of their attractive physical properties. With a relatively low density, high thermal conductivity, excellent oxidation resistance, high melting point, and simple crystal structure, nickel aluminide (NiAl) appears to be a potential candidate. However, NiAl is limited in structural applications due to its low room temperature fracture toughness and poor elevated temperature strength. One approach to improving these properties has been through the application of eutectic composites. Researchers have shown that containerless directional solidification of NiAl-based eutectic alloys can provide improvement in both the creep strength and fracture toughness. Although these systems have shown improvements in the mechanical properties, the presence of refractory metals increases the density significantly in some alloys. Lower density systems, such as the carbides, nitrides, and borides, may provide NiAl-based eutectic structure. With little or no information available on these systems, experimental investigation is required. The objective of this research was to locate and develop NiAl-carbide eutectic alloys. Exploratory arc-melts were performed in NiAl-refractory metal-C systems. Refractory metal systems investigated included Co, Cr, Fe, Hf, Mo, Nb, Ta, Ti, W, and Zr. Systems containing carbides with excellent stability (i.e.,HfC, NbC, TaC, TiC, and ZrC) produced large blocky cubic carbides in an NiAl matrix. The carbides appeared to have formed in the liquid state and were randomly distributed throughout the polycrystalline NiAl. The Co, Cr, Fe, Mo, and W systems contained NiAl dendrites with a two-phase interdendritic microconstituent present. Of these systems, the NiAl-Mo-C system had the most promising microstructure for in-situ composites. Three processing techniques were used to evaluate the NiAl-Mo-C system: arc-melting, slow cooling, and containerless directional solidification. Arc-melting provided a wide range of compositions in an economical and simple fashion. The slow cooled ingots provided larger ingots and slower cooling rates than arc-melting. Directional solidification was used to produce in-situ composites consisting of NiAl reinforced with molybdenum carbides.

Newport, Timothy Scott↗

Solidification and Morphological Evolution of Al-Si Eutectics in Convector-Diffusive Conditions

The Al-Si material system is an important and has been studied for over half century with a focus on industrial applications in high strength and high conductivity alloys. A great deal of researches have been focused on controlling the morphology and hence performance through the addition of small impurities and by processing conditions. Most of the structure-property correlations are based on the post solidified micromorphology and growth conditions. This material system is unique and has been explored for heat spreader, controlling coefficient of expansion by adjusting composition of silicon and in designing composites. The Al-Si system is very interesting system for understanding the dendritic (Al-rich side) eutectic transition. Recently this system has been of great interest because of its applications in designing heat spreader, low temperature flux to grow SiC large substrates and in controlling the coefficient of expansion of Al-based alloys. We have performed extensive experiments to understand eutectic transition and to understand the morphological evolution in presence of impurities. We will discuss the results of dendritic transition into faceted long grains in convector-diffusive conditions. In this presentation we will present morphological transition in presence of carbon impurity and development of novel morphology.

Singh, N. B.↗

Simulating the Effect of Space Vehicle Environments on Directional Solidification of a Binary Alloy

Space microgravity missions are designed to provide a microgravity environment for scientific experiments, but these missions cannot provide a perfect environment, due to vibrations caused by crew activity, on-board experiments, support systems (pumps, fans, etc.), periodic orbital maneuvers, and water dumps. Therefore, it is necessary to predict the impact of these vibrations on space experiments, prior to performing them. Simulations were conducted to study the effect of the vibrations on the directional solidification of a dendritic alloy. Finite element ca!cu!attie?ls were dme with a simd2titcr based on a continuum model of dendritic solidification, using the Fractional Step Method (FSM). The FSM splits the solution of the momentum equation into two steps: the viscous intermediate step, which does not enforce continuity; and the inviscid projection step, which calculates the pressure and enforces continuity. The FSM provides significant computational benefits for predicting flows in a directionally solidified alloy, compared to other methods presently employed, because of the efficiency gains in the uncoupled solution of velocity and pressure. finite differences, arises when the interdendritic liquid reaches the eutectic temperature and concentration. When a node reaches eutectic temperature, it is assumed that the solidification of the eutectic liquid continues at constant temperature until all the eutectic is solidified. With this approach, solidification is not achieved continuously across an element; rather, the element is not considered solidified until the eutectic isotherm overtakes the top nodes. For microgravity simulations, where the convection is driven by shrinkage, it introduces large variations in the fluid velocity. When the eutectic isotherm reaches a node, all the eutectic must be solidified in a short period, causing an abrupt increase in velocity. To overcome this difficulty, we employed a scheme to numerically predict a more accurate value for the rate of change of fraction of liquid as the liquid in an element solidifies. The new method enables us to contrast results of simulations in which the alloy is subjected to no gravity or a steady-state acceleration versus simulations when the alloy is subjected to vibration disturbances; therefore, the effect of vibration disturbances can be assessed more accurately. To assess the impact of these vibration-perturbations, transient accelerometer data from a space shuttle mission are used as inputs for the simulation model. These on-orbit acceleration data were obtained from the Microgravity Science Division at Glenn Research Center (GRC- MSD) and are applied to the buoyancy term of the momentum equation in a simulation of a Pb-5.8 wt. % Sb alloy that solidifies in a thermal gradient of 4000 K/m and a translation velocity of 3 p d s . Figure 2 shows the vertical velocity of a node that begins in the all-liquid region and subsequently solidifies; the vibrations are applied at 5000 seconds in this simulation. An important difficulty, common to all solidification models based on finite elements or 2 The magnitudes of the velocity oscillations that are vibration-induced are very small and acceptable. The biggest concern is whether the concentration of the liquid near the dendrite tips is distorted because of the vibration-induced perturbations. Results for this case show no concentration oscillations present in the all-liquid region.

Westra, D. G.↗

Directionally solidified pseudo-binary eutectics of Ni-Cr-(Hf, Zr)

A pseudo-binary eutectic, in which the intermetallic Ni7Hf2 reinforces the Ni-Cr solid solution phase, was previously predicted in the Ni-Cr-Hf system by a computer analysis. The experimental determination of pseudo binary eutectic compositions and the directional solidification of the Ni-Cr-Hf, Zr, and Ni-Cr-Zr eutectic alloys are discussed. To determine unknown eutectics, chemical analyses were made of material bled from near eutectic ingots during incipient melting. Nominal compositions in weight percent of Ni-18.6Cr-24.0HF, Ni19.6Cr-12.8Zr-2.8Hf, and Ni-19.2Cr-14.8Zr formed aligned pseudo-binary eutectic structures. The melting points were about 1270 C. The reinforcing intermetallic phases were identified as noncubic (Ni,Cr)7Hf2 and (Ni,Cr)7(Hf,Zr)2, and face centered cubic (Ni,Cr)5Zr. The volume fraction of the reinforcing phases were about 0.5.

Kim, Y. G.↗

Directionally solidified pseudo-binary eutectics of Ni-Cr-/Hf,Zr/

This report is concerned with the experimental determination of pseudo binary eutectic compositions and the directional solidification of the Ni-Cr-Hf,Zr, and Ni-Cr-Zr eutectic alloys. To determine unknown eutectics, chemical analyses were made of material bled from near eutectic ingots during incipient melting. Nominal compositions in weight per cent of Ni-18.6Cr-24.0Hf, Ni-19.6Cr-12.8Zr-2.8Hf, and Ni-19.2Cr-14.8Zr formed aligned pseudo-binary eutectic structures. The melting points were about 1270 C. The reinforcing intermetallic phases were identified as noncubic (Ni,Cr)7Hf2 and (Ni,Cr)7(Hf,Zr)2, and face centered cubic (Ni,Cr)5Zr. The volume fraction of the reinforcing phases were about 0.5.

Kim, Y. G.↗

Directional solidification of Bi-Mn alloys using an applied magnetic field

Off-eutectic compositions of Bi-Mn were directionally solidified in applied transverse magnetic fields up to 3 kG, to determine the effects on thermal and solutal convection. Plane front directional solidification of eutectic and near-eutectic Bi-Mn results in a two-phase rodlike morphology consisting of ferromagnetic MnBi rods in a Bi solid solution matrix. Compositions of either side of the eutectic were studied in growth orientations vertically up and down. Temperature gradient was monitored during growth by means of an in-situ thermocouple. For Bi-rich compositions, the magnetic field appeared to increase mixing as determined from thermal, morphological, chemical, and magnetic analyses. For Mn-rich compositions, morphological and chemical analyses suggest some reduction in mixing due to application of the magnetic force. The capability for carrying out directional solidification of Bi-Mn in high longitudinal magnetic fields was established.

Decarlo, J. L.↗

Influence of convection on microstructure

The primary motivation for this research was to determine the cause for space processing altering the microstructure of some eutectics, especially the MnBi-Bi eutectic. Four primary hypotheses were to be tested under this current grant: (1) A fibrous microstructure is much more sensitive to convection than a lamellar microstructure, which was assumed in our prior theoretical treatment. (2) An interface with one phase projecting out into the melt is much more sensitive to convection than a planar interface, which was assumed in our prior theoretical treatment. (3) The Soret effect is much more important in the absence of convection and has a sufficiently large influence on microstructure that its action can explain the flight results. (4) The microstructure is much more sensitive to convection when the composition of the bulk melt is off eutectic. These hypotheses were tested. It was concluded that none of these can explain the Grumman flight results. Experiments also were performed on the influence of current pulses on MnBi-Bi microstructure. A thorough review was made of all experimental results on the influence of convection on the fiber spacing in rod eutectics, including results from solidification in space or at high gravity, and use of mechanical stirring or a magnetic field. Contradictory results were noted. The predictions of models for convective influences were compared with the experimental results. Vigorous mechanical stirring appears to coarsen the microstructure by altering the concentration field in front of the freezing interface. Gentle convection is believed to alter the microstructure of a fibrous eutectic only when it causes a fluctuating freezing rate with a system for which the kinetics of fiber branching differs from that for fiber termination. These fluctuations may cause the microstructure to coarsen or to become finer, depending on the relative kinetics of these processes. The microstructure of lamellar eutectics is less sensitive to freezing rate fluctuations and to gentle convection.

Wilcox, William R.↗

Solidification Behavior of gamma'-Ni3Al Containing Alloys in the Ni-Al-O System

The chemical activities of Al and Ni in gamma(prime)-Ni3Al-containing systems were measured using the multi-cell Knudsen effusion-cell mass spectrometry technique (multi-cell KEMS), over the composition range 8 - 32 at.%Al and temperature range T = 1400 - 1750 K. From these measurements a better understanding of the equilibrium solidification behaviour of gamma(prime)-Ni3Al-containing alloys in the Ni-Al-O system was established. Specifically, these measurements revealed that (1) gamma(prime)-Ni3Al forms via the peritectiod reaction, gamma + Beta (+ A12O3) = gamma (prime) (+ Al2O3), at 1633 +/- 1 K, (2) the {gamma + Beta + Al2O3} phase field is stable over the temperature range 1633 through 1640 K, and (3) equilibrium solidification occurs by the eutectic reaction, L (+ Al2O3) = gamma + Beta (+ Al2O3), at 1640 +/- 1 K and a liquid composition of 24.8 +/- 0.2 at.%Al (at an unknown oxygen content). When projected onto the Ni-Al binary, this behaviour is inconsistent with the current Ni-Al phase diagram and a new diagram is proposed. This new Ni-Al phase diagram explains a number of unusual steady-state solidification structures reported previously and provides a much simpler reaction scheme in the vicinity of the gamma(prime)-Ni3Al phase field.

Copland, Evan↗

Processing eutectics in space

The investigations of directional solidification have indicated the necessity of establishing a secure foundation in earth-based laboratory processing in order to properly assess low-gravity processing. Emphasis was placed on evaluating the regularity of microstructure of the rod-like eutectic Al-Al3Ni obtained under different conditions of growth involving the parameters of thermal gradient, solidification rate, and interfacial curvature. In the case of Al-Al3Ni, where the Al3Ni phase appears as facets rods, solidification rate was determined to be a controlling parameter. Zone melting of thin eutectic films showed that for films of the order of 10 to 20 micrometers thick, the extra surface energy appears to act to stabilize a regular microstructure. The results suggest that the role of low-gravity as provided in space-laboratory processing of materials is to be sought in the possibility of generating a higher thermal gradient in the solidifying ingot for a given power input-output arrangement than can be obtained under normal one-g processes.

Douglas, F. C.↗

SPAR VI Technical Report for Experiment 76-22: Directional Solidification of Magnetic Composites

Samples of eutectic Bi/MnBi were directionally solidified during a low-g interval aboard the SPAR 6 flight and in a l-g environment under identical furnace velocity and thermal conditions. The Bi/MnBi eutectic is characterized by a regular rod eutectic whose morphology may be sensitive to thermo-solutal convection and by its components, MnBi, which is ferromagnetic. Morphological analyses on samples show statistically smaller interrod spacings and rod diameters with respect to samples grown under identical solidification furnace conditions in l-g. An adjustment between the interrod spacing, growth velocity, and total undercooling at the solidification interface is proposed. Morphological analyses on samples grown in l-g indicate little difference between results for different growth orientations with respect to the gravity vector. The magnetic properties are significantly affected, however, by the presence of a nonequilibrium magnetic phase and the nonequilibrium phase transforms to the equilibrium ferromagnetic phase during isothermal heat treatment.

Pirich, R. G.↗

Shape of two-dimensional solidification interface during directional solidification by continuous casting

An analysis was made of the two-dimensional solidification of an ingot being cooled and withdrawn vertically downward from a mold consisting of parallel walls of finite length. Heat transfer analysis shows how the flatness of the interface is related to the ingot thickness, the withdrawal rate, the heat addition from the superheated liquid metal, and the temperature difference available for cooling. This provides an understanding of the conditions that will yield a maximum rate of casting while achieving the desired flatness of the interface. The results are interpreted with respect to the conditions for obtaining an aligned eutectic structure by directional solidification. In this process an additional constraint must be included that relates the ingot withdrawal rate and the heat transfer rate from the liquid metal to the solidification interface.

Siegel, R.↗

Microstructural Characterization of a Directionally-Solidified Ni-33 (at. %)Al-31Cr-3Mo Eutectic Alloy as a Function of Withdrawal Rate

The Ni-33 (at. %)Al-3lCr-3Mo eutectic alloy was directionally-solidified (DS) at different rates, V(sub I), varying between 2.5 to 508 mm/ h. Detailed qualitative and quantitative metallographic and chemical analyses were conducted on the directionally-solidified rods. The microstructures consisted of eutectic colonies with parallel lamellar NiAl/(Cr,Mo) plates for solidification rates at and below 12.7 mm/ h. Cellular eutectic microstructures were observed at higher solidification rates, where the plates exhibited a radial pattern. The microstructures were demonstrated to be fairly uniform throughout a 100 mm length of the DS zone by quantitative metallography. The average cell size, bar-d, decreased with increasing growth rate to a value of 125 microns at 508 mm/ h according to the relation bar-d (microns) approx. = 465 V(sup -0.22, sub I), where V(sub I) is in mm/ h. Both the average NiAl plate thickness, bar-Delta(sub NiAl), and the interlamellar spacing, bar-lambda, were observed to be constant for V(sub I) less than or = 50.8 mm/ h but decreased with increasing growth rate above this value as 0.93 bar-Delta(sub NiAl)(microns) = 61.2 V(sup -0.93, sub I) and bar-lambda (microns) = 47.7 V(sup -0.64, sub I), respectively. The present results are detailed on a microstructural map. Keywords Optical microscopy, microstructure, compounds intermetallic, directional solidification

Raj, S. V.↗