Search NASA⌕ Search

SEARCH · Search NASA

Results for “Hydrogen Degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

The resistance to embrittlement by a hydrogen environment of selected high strength iron-manganese base alloys

Fe-16Mn and Fe-25Mn base alloys, which had been cold worked to yield strength levels of 201 and 178 KSI, were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature under the loading conditions employed in this investigation. Transmission electron microscopy established that bands of epsilon phase martensite and fcc mechanical twins were formed throughout the fcc matrix when these alloys were cold worked. In the cold worked alloys a high density of crystal defects were observed associated with both types of strain induced structures, which should contribute significantly to the strengthening of these alloys. High strength iron base alloys can be produced which appear to have some resistance to degradation of mechanical properties in a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

Effects of Surface Treatments on Secondary Electron Emission from CVD Diamond Films

Secondary electron emission (SEE) properties of polycrystalline diamond films grown by chemical vapor deposition (CVD) were measured. The total secondary yield (sigma) from as-grown samples was observed to be as high as 20 at room temperature and 48 while heating at 700 K in vacuum. Electron-beam-activated, alkali-terminated diamond films have shown stable values of sigma as high as 60 when coated with CsI and similarly high values when coated with other alkali halides. Diamond coated with BaF2 had a stable sigma of 6, but no enhancement of the SEE properties was observed with coatings of Ti or Au. Hydrogen was identified to give rise to this effect in as-grown films. However, electron beam exposure led to a reduction in sigma values as low as 2. Exposure to a molecular hydrogen environment restored sigma to its original value after degradation, and enabled stable secondary emission during electron beam exposure. Atomic hydrogen and hydrogen plasma treatments were performed on diamond/Mo samples in an attempt to increase the near-surface hydrogen concentration which might lead to increased stability in the secondary emission. Raman scattering analysis, scanning electron microscopy, and Auger electron spectroscopy (AES) confirmed that hydrogen plasma and atomic hydrogen treatments improved the quality of the CVD diamond significantly. Elastic recoil detection (ERD) showed that heating as-grown diamond targets to 7OO K, which was correlated with an increase in sigma, removed contaminants from the surface but did not drive hydrogen from the diamond bulk. ERD showed that the hydrogen plasma treatment produced an increase in the hydrogen concentration in the near-surface region which did not decrease while heating in vacuum at 700 K, but no improvement in the SEE properties was observed.

Mearini, G. T.↗

Performance of 3rd electrode cells in OAO.

The OAO 2 satellite employed nickel-cadmium batteries with auxiliary (signal) electrodes for overcharge control. During the early life of the satellite, these third-electrode signals provided an orbit-by-orbit indication of the overcharge received by the batteries. By ground command, the battery charger was adjusted on a need basis to provide optimum recharge conditions as indicated by the third-electrode signals during all phases of spacecraft operation and orientation. After more than two years, an unusual degradation in third-electrode signals was observed, providing the first indication of battery degradation. The present paper examines the operation of the battery system and analyzes the battery degradation mechanism. The abnormal performance of the third electrode is related to cell-voltage divergence during periods of overcharge. Cells that had a higher cell voltage showed signs (third-electrode degradation) of small amounts of hydrogen gas generation.

Ford, F. E.↗

Thermal performance of gaseous-helium-purged tank-mounted multilayer insulation system during ground-hold and space-hold thermal cycling and exposure to water vapor

An experimental investigation was conducted to determine (1) the ground-hold and space-hold thermal performance of a multilayer insulation (MLI) system mounted on a spherical, liquid-hydrogen propellant tank and (2) the degradation to the space-hold thermal performance of the insulation system that resulted from both thermal cycling and exposure to moisture. The propellant tank had a diameter of 1.39 meters (4.57ft). The MLI consisted of two blankets of insulation; each blanket contained 15 double-aluminized Mylar radiation shields separated by double silk net spacers. Nineteen tests simulating basic cryogenic spacecraft thermal (environmental) conditions were conducted. These tests typically included initial helium purge, liquid-hydrogen fill and ground-hold, ascent, space-hold, and repressurization. No significant degradation of the space-hold thermal performance due to thermal cycling was noted.

Sumner, I. E.↗

NASA Engineering and Safety Center Technical Bulletin No. 21-01: Experimental and Computational Study of Cavitation in Hydrogen Peroxide

Cavitation in liquid propulsion systems can lead to performance degradation and hardware failures. The NESC sponsored an investigation to measure and model cavitation in pressurized hydrogen peroxide fl ow. The experimentally measured and computationally predicted cavitation lengths were compared as a function of cavitation number. The measured and predicted data exhibited close agreement over the range of pressures and temperatures studied, and no calibration of the cavitation model coefficients was needed.

NESC Technical Bulletin No. 21-01↗

Material technology

Advanced high pressure O2/H2 propulsion systems as exemplified by the Space Shuttle Main Engine (SSME) create challenging operating environments for materials. Many components operate in either hydrogen or hydrogen-steam environments which may significantly degrade the performance of common alloys. The objective of the materials technology projects is to develop and evaluate candidate materials for application in advanced high pressure O2/H2 propulsion systems. These new and improved materials are to improve the durability or performance of the SSME or derivative engine. The program includes projects on the following topics: (1) Hydrogen Resistant Alloys; (2) High Pressure O2 Ignition and Burning; (3) Improved Turbine Blades; (4) Improved Turbine Disk Material; (5) Impact Reactivity in High Pressure O2; and Fiber Reinforced Superalloys.

Dreshfield, R. L.↗

The effect of microstructure on hydrogen embrittlement of the nickel-base superalloy, Udimet 700

Material from a single heat of cast and wrought Udimet 700 was processed and/or heat treated to produce five material conditions with identical chemical compositions but with distinct microstructural variations, and then evaluated for susceptibility to hydrogen embrittlement. Two prealloyed powder conditions exhibited significantly improved resistance to hydrogen embrittlement, as compared to wrought material. No degradation in notch or smooth tensile strengths occurred, and average ductilities of 25 percent reduction of area were determined for 2 hydrogen evaluation procedures. For the most severe hydrogenation procedure, ductility levels were reduced to 15 percent. These improvements were attributed to cleaner grain boundaries and decreases grain size.

Gray, H. R.↗

The effect of microstructure on hydrogen embrittlement of the nickel base superalloy, Udimet 700

Material from a single heat of cast and wrought Udimet 700 was processed and/or heat treated to produce five material conditions with identical chemical compositions but with distinct microstructural variations, and then evaluated for susceptibility to hydrogen embrittlement. Two prealloyed powder conditions exhibited significantly improved resistance to hydrogen embrittlement, as compared to wrought material. No degradation in notch or smooth tensile strengths occurred, and average ductilities of 25 percent reduction of area were determined for 2 hydrogen evaluation procedures. For the most severe hydrogenation procedure, ductility levels were reduced to 15 percent. These improvements were attributed to cleaner grain boundaries and decreased grain size.

Gray, H. R.↗

Sintered plaque characteristics

The structural transformations occurring during sintering, the fabrication of a slurry produced sintered plaque, are detailed. Degradation of the positive electrode in performance in cycling in a nickel hydrogen battery were traced to the quality of the sintered plaque. Electrode degradation was found to be a limiting factor in the battery cycle life. Details of microstructural characterization and distribution of pores, examination of plastic flow during shrinkage, and observations of the rounding of nickel powder particles during the slurry process are presented.

Vaidyanathan, H.↗

Effect of hydrogen on the strength and microstructure of selected ceramics

Ceramics in monolithic form and as composite constituents in the form of fibers, matrices, and coatings are currently being considered for a variety of high-temperature applications in aeronautics and space. Many of these applications involve exposure to a hydrogen-containing environment. The compatibility of selected ceramics in gaseous high-temperature hydrogen is assessed. Environmental stability regimes for the long term use of ceramic materials are defined by the parameters of temperature, pressure, and moisture content. Thermodynamically predicted reactions between hydrogen and several monolithic ceramics are compared with actual performance in a controlled environment. Morphology of hydrogen attack and the corresponding strength degradation is reported for silicon carbide, silicon nitride, alumina, magnesia, and mullite.

Herbell, Thomas P.↗

Effect of hydrogen on the strength and microstructure of selected ceramics

Ceramics in monolithic form and as composite constituents in the form of fibers, matrices, and coatings are currently being considered for a variety of high-temperature applications in aeronautics and space. Many of these applications involve exposure to a hydrogen-containing environment. The compatibility of selected ceramics in gaseous high-temperature hydrogen is assessed. Environmental stability regimes for the long term use of ceramic materials are defined by the parameters of temperature, pressure, and moisture content. Thermodynamically predicted reactions between hydrogen and several monolithic ceramics are compared with actual performance in a controlled environment. Morphology of hydrogen attack and the corresponding strength degradation is reported for silicon carbide, silicon nitride, alumina, magnesia, and mullite.

Herbell, Thomas P.↗

Ultrastable reference frequency distribution utilizing a fiber optic link

The Frequency Standards Laboratory at the Jet Propulsion Laboratory (JPL) is responsible for the generation and distribution of ultra-stable reference frequency in NASA's Deep Space Network (DSN). Certain assemblies and components of the Radio Science and VLBI systems are located in the cones of tracking antennas hundreds of meters from the Frequency and Timing Subsystem's frequency standards. The very stringent requirements of these users challenge the performance of state-of-the-art frequency sources as well as the associated signal distribution system. The reference frequency distribution system described is designed around a low temperature coefficient of delay (TCD) optical fiber. On-site measurements of the fiber optic link alone indicate 100 MHz phase noise performance on the order of -120 dBc at 1 Hz from the carrier and Allan deviation on the order of parts in 10(exp 16) at 1000 seconds averaging time. The measured phase noise and stability of the link indicate that the performance characteristics of the hydrogen maser frequency standards are not degraded by the distribution system. Thus, optical fibers and electro-optic devices as distribution media appear to be a viable alternative to the classical coaxial cable distribution systems.

Calhoun, Malcolm↗

Thermomechanical behavior of a polynorbornadiene

A high-temperature linear amorphous hydrocarbon polymer synthesized cationically from 2,5-norbornadiene was studied thermomechanically with respect to physical transitions and stability in nitrogen. The glass transition temperature was determined to be 320 C (at less than 1 cps), which is probably the highest known for a linear hydrocarbon addition polymer. The thermomechanical technique of torsional braid analysis, together with thermogravimetric analysis, differential thermal analysis, infrared analysis, and solubility studies, was used to investigate the sequential events of the glass transition and degradation. The polymer is of particular interest since it is a high-temperature plastic which in the bulk form would probably need to be processed at high speeds in the vicinity of the glass transition temperature in an inert atmosphere. The presence of tertiary hydrogen atoms should render it amenable to degradation by the earth's environment.

Roller, M. B.↗

Thermal oxidative degradation reactions of perfluoroalkylethers

The mechanisms operative in thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes are investigated. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids is not established. It was determined that this behavior is not associated with hydrogen end groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres is dependent on the surface/volume ratio. Once a limiting ratio is reached, a steady rate appears to be attained. Based on elemental analysis and oxygen consumption data, CF2OCF2CF2O2, no. CF2CF2O, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys is much more drastic in the case of Fomblin Z fluids than that observed for the hexafluoropropene derived materials. The effectiveness of antioxidation anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys is very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appears to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes this takes place to a much lesser degree with M-50.

Paciorek, K. L.↗

Effects of Hydrogen on Tantalum Nitride Resistors

In this paper we report on observations of degradation of thin film Tantalum Nitride chip resistors in a hermetically sealed hybrid. The observations have been attributed to the reaction of residual Palladium with desorbed Hydrogen on the surface of the resistor film. Hydrogen gas has been observed to desorb from various sources within the sealed hybrid as a result of temperature elevation. The hydrogen gas has been reported to undergo a reaction with elements such as Platinum and Palladium causing device degradation in Gallium Arsenide Field Effect Transistors. The experimental procedures and data relating to this observation along with a discussion of available risk mitigation techniques will be presented.

Weiler, James↗

Influence of Microstructure on the Fatigue Crack Growth of A516 in Hydrogen

Some day hydrogen may be used as a viable energy storage and transport medium within the United States. Hydrogen gas may be used to dilute and extend our present methane supply as a blend or may even be used in its pure elemental form as a primary fuel. Independent of the methods of production, storage, and distribution, the interaction of hydrogen with its containment material will play an integral role in the success of a hydrogen energy program. Presently, the selection of hydrogen containment materials can be made such that the material will remain reasonably free from environmental degradation; however, costly alloying additions are required. Unfortunately, high alloy steels are economically prohibitive when large-scale hydrogen energy storage, transmission, and conversion systems are desired. Therefore, in order to implement such hydrogen energy systems in the future, existing low-cost materials must be improved via mechanical, thermal, or thermo-mechanical processing methods or new low-cost materials which are compatible with hydrogen must be developed. Originally, low strength, low alloy steels at room temperature were thought to be immune to hydrogen gas embrittlement, since no sustained load crack growth is observed. However, results of Clark in HY8O and Nelson in SAE 1020 have shown that the fatigue crack growth rate can be greatly accelerated in the presence of hydrogen gas. In recent results reported by Louthan and Mucci, the smooth bar fatigue life of an A1068 pipeline steel was reduced up to a factor of ten when the tests were performed in a 13.8 MPa hydrogen environment. These results suggest that the selection of material for structures designed to operate in hydrogen under cyclic loads must include consideration of hydrogen/metal fatigue interaction. Although the hydrogen/metal fatigue interaction can be severe in low strength low alloy steels, the degree of degradation may be altered by the underlying ferrous microstructure. At present, no correlation between microstructure and degree of hydrogen susceptibility exists for low strength steels. However, in high strength steels, susceptibility to hydrogen embrittlement has been shown to be strongly sensitive to the metallurgical microstructure. In addition, compositional effects and grain size can 703 Some day hydrogen may be used as a viable energy storage and transport medium within the United States. Hydrogen gas may be used to dilute and extend our present methane supply as a blend or may even be used in its pure elemental form as a primary fuel. Independent of the methods of production, storage, and distribution, the interaction of hydrogen with its containment material will play an integral role in the success of a hydrogen energy program. Presently, the selection of hydrogen containment materials can be made such that the material will remain reasonably free from environmental degradation; however, costly alloying additions are required. Unfortunately, high alloy steels are economically prohibitive when large-scale hydrogen energy storage, transmission, and conversion systems are desired. Therefore, in order to implement such hydrogen energy systems in the future, existing low-cost materials must be improved via mechanical, thermal, or thermo-mechanical processing methods or new low-cost materials which are compatible with hydrogen must be developed.

Wachob, Harry F.↗

Fiber optic reference frequency distribution to remote beam waveguide antennas

In the NASA/JPL Deep Space Network (DSN), radio science experiments (probing outer planet atmospheres, rings, gravitational waves, etc.) and very long-base interferometry (VLBI) require ultra-stable, low phase noise reference frequency signals at the user locations. Typical locations for radio science/VLBI exciters and down-converters are the cone areas of the 34 m high efficiency antennas or the 70 m antennas, located several hundred meters from the reference frequency standards. Over the past three years, fiber optic distribution links have replaced coaxial cable distribution for reference frequencies to these antenna sites. Optical fibers are the preferred medium for distribution because of their low attenuation, immunity to EMI/IWI, and temperature stability. A new network of Beam Waveguide (BWG) antennas presently under construction in the DSN requires hydrogen maser stability at tens of kilometers distance from the frequency standards central location. The topic of this paper is the design and implementation of an optical fiber distribution link which provides ultra-stable reference frequencies to users at a remote BWG antenna. The temperature profile from the earth's surface to a depth of six feet over a time period of six months was used to optimize the placement of the fiber optic cables. In-situ evaluation of the fiber optic link performance indicates Allan deviation on the order of parts in 10(exp -15) at 1000 and 10,000 seconds averaging time; thus, the link stability degradation due to environmental conditions still preserves hydrogen maser stability at the user locations. This paper reports on the implementation of optical fibers and electro-optic devices for distributing very stable, low phase noise reference signals to remote BWG antenna locations. Allan deviation and phase noise test results for a 16 km fiber optic distribution link are presented in the paper.

Calhoun, Malcolm↗

Thermal oxidative degradation reactions of perfluoroalklethers

The objective of this contract was to investigate the mechanisms operative in thermal and thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids has not been established. It was determined that this behavior was not associated with hydrogen end-groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres was found to be dependent on the surface/volume ratio. Once a limiting ratio was reached, a steady rate appeared to be attained. Based on elemental analysis and oxygen consumption data, -CF2OCF2CF2O-, not -CF2CF2O-, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys was found to be much more drastic in the case of Fomblin Z fluids than that observed for the hexalfuoropropane oxide derived materials. The effectiveness of antioxidation/anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys was very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appeared to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes; this took place to a much lesser degree with M-50.

Paciorek, K. L.↗