Apollo 14 very low titanium glasses - Melting experiments in iron-platinum alloy capsules

This paper describes two techniques that have been developed to produce Fe-Pt alloy capsules for hgh-pressure experiments, and reports liquidus-phase relations of the Apollo 14 very low titanium glasses determined using Fe-rich capsules (a/Fe/ approximately 0.6). The liquid is multiply saturated with olivine and clinopyroxene at equal to or greater than 22 kbar. The multiple saturation is at least 3 kbar higher than that determined using pure Fe capsules and corresponds to a source region at least 60 km deeper if olivine and clinopyroxene were the residual phases. However, independent data on iron activity or oxygen fugacity of the glasses are still needed in order to choose a container of optimum composition. Preliminary experiments in Fe-poor alloy capsules suggest that the valence state of iron and the crystallization sequence in the melt have changed, possibly as a result of oxidizing materials entrapped during the iron-plating processes. The FeO content of the charge decreases linearly with increasing run duration in experiments using pure Fe capsules. The observation that iron-rich globules grow with time suggests that the equilibrium Fe (bleb) + Fe2O3 (liq) = 3 FeO (liq) might be established in the liquid at high pressure. If this explanation is correct, an appreciable amount of 'FeO' in the liquid could actually be Fe2O3, and some natural lunar volcanic glasses may contain ferric iron as well.

Chen, H.-K.↗

Effect of Nuclear Radiation on Materials at Cryogenic Temperatures

The tensile properties for 33 polycrystalline structural materials including aluminum, titanium, nickel and iron alloys were obtained at -256.5 C (30 deg R) after irradiation exposure at this temperature to 10(exp 17) nvt (E greater than 0.5 Mev), at -256.5 C without previous irradiation, and at approximately 27 C (540 deg R) without previous irradiation. The data were evaluated statistically to permit identification of cryogenic effects and nuclear-cryogenic effects. A number of conclusions were drawn regarding suitability of certain of the materials for use in nuclear-cryogenic applications and regarding the need for further investigation.

NEUTRON BOMBARDMENT↗

The resistance to embrittlement by a hydrogen environment of selected high strength iron-manganese base alloys

Fe-16Mn and Fe-25Mn base alloys, which had been cold worked to yield strength levels of 201 and 178 KSI, were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature under the loading conditions employed in this investigation. Transmission electron microscopy established that bands of epsilon phase martensite and fcc mechanical twins were formed throughout the fcc matrix when these alloys were cold worked. In the cold worked alloys a high density of crystal defects were observed associated with both types of strain induced structures, which should contribute significantly to the strengthening of these alloys. High strength iron base alloys can be produced which appear to have some resistance to degradation of mechanical properties in a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

Influence of Chemical Composition on Rupture Properties at 1200 Degrees F. of Forged Chromium-Cobalt-Nickel-Iron Base Alloys in Solution-Treated and Aged Condition

The influence of systematic variations of chemical composition on rupture properties at 1200 degrees F. was determined for 62 modifications of a basic alloy containing 20 percent chromium, 20 percent nickel, 20 percent cobalt, 3 percent molybdenum, 2 percent tungsten, 1 percent columbium, 0.15 percent carbon, 1.7 percent manganese, 0.5 percent silicon, 0.12 percent nitrogen and the balance iron. These modifications included individual variations of each of 10 elements present and simultaneous variations of molybdenum, tungsten, and columbium. Laboratory induction furnace heats were hot-forged to round bar stock, solution-treated at 2200 degrees F., and aged at 1400 degrees F. The melting and fabrication conditions were carefully controlled in order to minimize all variable effects on properties except chemical composition. Information is presented which indicates that melting and hot-working conditions play an important role in high-temperature properties of alloys of the type investigated.

Reynolds, E E↗

Bosch Carbon Catalyst Regeneration in Water II: Analysis of Bosch Catalyst Beads Throughout the Initial Regeneration Process

Catalyst integrity is an important factor in reactor longevity since it changes the effectiveness of a reaction. A Carbon Formation Reactor (CFR), used within Series Bosch (S-Bosch), utilizes an iron alloy catalyst to convert carbon monoxide and hydrogen into water and solid carbon. The catalyst promotes the formation of carbon to such an extent that pressure-causing clogs form within the reactor and reaction sites on the catalyst become limited. To remove carbon from both the reactor and the surface of the iron alloy catalyst, a technique was developed that utilizes water, an In-Situ Resource Utilization (ISRU) Resource, and agitation to regenerate the reactor. To ascertain catalyst integrity throughout this regenerative process, sample catalyst beads were taken before and after the carbon formation reaction, and then after the regeneration process. Additionally, wastewater from the regeneration process was sampled. The sampled beads and wastewater were observed under a Scanning Electron Microscopy (SEM) microscope and the beads were chemically etched to determine if the catalyst had degraded at any point during this process, and if catalyst was lost. Minimal catalyst degradation was observed after carbon formation in the CFR.

regeneration↗

Bosch Carbon Catalyst Regeneration in Water II: Analysis of Bosch Catalyst Beads Throughout the Initial Regeneration Process

Catalyst integrity is an important factor in reactor longevity since it changes the effectiveness of a reaction. A Carbon Formation Reactor (CFR), used within Series Bosch (S-Bosch), utilizes an iron alloy catalyst to convert carbon monoxide and hydrogen into water and solid carbon. The catalyst promotes the formation of carbon to such an extent that pressure-causing clogs form within the reactor and reaction sites on the catalyst become limited. To remove carbon from both the reactor and the surface of the iron alloy catalyst, a technique was developed that utilizes water, an In-Situ Resource Utilization (ISRU) Resource, and agitation to regenerate the reactor. To ascertain catalyst integrity throughout this regenerative process, sample catalyst beads were taken before and after the carbon formation reaction, and then after the regeneration process. Additionally, wastewater from the regeneration process was sampled. The sampled beads and wastewater were observed under a Scanning Electron Microscopy (SEM) microscope and the beads were chemically etched to determine if the catalyst had degraded at any point during this process, and if catalyst was lost. Minimal catalyst degradation was observed after carbon formation in the CFR.

Series Bosch↗

Normal evaporation of binary alloys

In the study of normal evaporation, it is assumed that the evaporating alloy is homogeneous, that the vapor is instantly removed, and that the alloy follows Raoult's law. The differential equation of normal evaporation relating the evaporating time to the final solute concentration is given and solved for several important special cases. Uses of the derived equations are exemplified with a Ni-Al alloy and some binary iron alloys. The accuracy of the predicted results are checked by analyses of actual experimental data on Fe-Ni and Ni-Cr alloys evaporated at 1600 C, and also on the vacuum purification of beryllium. These analyses suggest that the normal evaporation equations presented here give satisfactory results that are accurate to within an order of magnitude of the correct values, even for some highly concentrated solutions. Limited diffusion and the resultant surface solute depletion or enrichment appear important in the extension of this normal evaporation approach.

Li, C. H.↗

Tantalum modified ferritic iron base alloys

Strong ferritic alloys of the Fe-CR-Al type containing 0.4% to 2% tantalum were developed. These alloys have improved fabricability without sacrificing high temperature strength and oxidation resistance in the 800 C (1475 F) to 1040 C (1900 F) range.

Oldrieve, R. E.↗

Phosphoran pyroxene and olivine in silicate inclusions in natural iron-carbon alloy, Disko Island, Greenland

A survey of literature data on the P contents of olivine, pyroxene, and garnet in mantle xenoliths and the bulk P contents of mantle xenoliths shows that available data is ambiguous as to whether mantle P is primarily contained in silicates or in phosphates, even though phosphates are rarely observed in mantle xenoliths. Garnet probably contains more of the mantle's P than olivine or pyroxene. Bulk P contents of mantle xenoliths vary significantly. Estimation of the primitive mantle P content from xenoliths requires interpretation of the partial melting and contamination histories of the xenoliths.

Goodrich, C. A.↗

Advanced thermal barrier system bond coatings for use on nickel-, cobalt- and iron-base alloy substrates

New and improved Ni-, Co-, and Fe-base bond coatings have been identified for the ZrO2-Y2O3 thermal barrier coatings to be used on Ni-, Co-, and Fe-base alloy substrates. These bond coatings were evaluated in a cyclic furnace between 1120 and 1175 C. It was found that MCrAlYb (where M = Ni, Co, or Fe) bond coating thermal barrier systems have significantly longer lives than MCrAlY bond coating thermal barrier systems. The longest life was obtained with the FeCrAlYb thermal barrier system followed by NiCrAlYb and CoCrAlYb thermal barrier systems in that order.