Search NASA⌕ Search

SEARCH · Search NASA

Results for “LIB cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

The Role of Metal Oxides in Li-S Batteries: A High-Areal-Capacity Sulfur Composite Cathode Investigation

Compared to lithium-ion batteries (LIB), lithium-sulfur (Li-S) batteries have low cost and high theoretical specific energy (2510 Wh/kg or about 10 times of the LIB). However, Li-S batteries have several challenges, including large volume expansion, poor utilization of the end products, sluggish kinetics of polysulfides, and crossover, so-called the "shuttle effect". To address these issues, we have introduced metal oxides to the Li-S electrode to develop a metal-oxide-sulfur composite electrode. We aim to use metal oxides to assist the Li-S formation (dissociation) during discharge (charge) cycles. We elect to focus on LIB-based metal oxides to ensure that the added material can contribute storage capacity to the battery. Our cathodes are fabricated by both the conventional slurry casting and air-controlled electrospray. LIB electrode materials, such as Li(Ni 0.6 Mn 0.6 Co 0.2 )O 2 , LiMn 2 O 4 , Li 2 TiO 3 , etc, were incorporated with the sulfur-carbon composite and their charge-discharge performances are compared. We found that the presence of metal oxides increased sulfur utilization with stable cycling performance, even in cells with high areal capacities. To unveil the interactions between lithium metal oxides and sulfur, the cathodes were analyzed by various characterization techniques, including scanning electron microscopy, X-ray diffraction, thermogravimetric analysis, and electrochemistry. The analysis of the role of the oxides will be presented along with the reaction mechanism.

25 ENERGY STORAGE↗

An overview of various critical aspects of low-cobalt/cobalt-free Li-ion battery cathodes

Cathodes of lithium-ion batteries (LIBs) significantly impact the environmental footprint, cost, and energy performance of the battery-pack. Hence, sustainable production of Li-ion battery cathodes is critically required for ensuring cost-effectiveness, environmental benignity, consumer friendliness, and social justice. Battery chemistry largely determines individual cell performance as well as the battery pack cost and life cycle greenhouse gas emission. Continuous manufacturing platforms improve production efficiency in terms of product yield, quality and cost. Spent-battery recycling ensures the circular economy of critical elements that are required for cathode production. Innovations in fast-charging LIBs are particularly promising for sustainable e-mobility with a reduced carbon footprint. This article provides an overview of these research directions, emphasizing strategies for low-cobalt cathode development, recycling processes, continuous production and improvement in fast-charging capability.

25 ENERGY STORAGE↗

Unraveling the nature of sulfide ions in hydrometallurgical recycling of NCM622 cathode material

The use of lithium-ion batteries (LIBs) has increased dramatically since its initial inception in the late 20th century. Such a surge in the LIB market and industry has resulted in a huge demand for mineral resources. Besides, the large scale of production will lead to massive amounts of waste batteries in the end. As such, recycling is seen as an end-of-pipe process to resolve sustainability and environmental concerns. The hydrometallurgical recycling is considered to be the most prominent method to recover cathode materials from spent LIBs owing to its high leaching efficiency and low energy costs. A series of procedures including pretreatment of the spent LIBs, acid leaching of the black mass, chemical co-precipitation of the hydroxide precursor, and sintering of the cathode active material need to be operated precisely. In this aspect, the impurities introduced during the process could pose a serious threat to the reaction stability as well as recycling consistency. Here, the impact of sulfide ions on recovered LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) cathode material with the method of hydrometallurgy is first investigated in detail. This study shows that hydrometallurgical process is not obviously influenced by sulfide impurity. No signs of secondary phase or impurity inclusion are spotted in synthesized cathodes. Under 5 at % sulfide concentration conditions, the obtained NCM622 cathode exhibits a capacity of 159.4 mAh/g after 100 cycles at 1/3C, which is at the same level as virgin benchmark. The difference in rate performance between cathodes with and without additional sulfide is less than 2 % or even smaller. In short, the results indicate a neutral status of sulfide ions in hydrometallurgical recycling.

25 ENERGY STORAGE↗

Understanding Structural and Compositional Evolution during NMC Cathode Direct Recycling via Solid-State NMR

Recycling end-of-life lithium-ion batteries (LIBs) to recover high-value cathode materials such as LiNixMnyCozO2 (NMC) is driven by economical, geopolitical, and sustainability needs. There has been recent interest in direct recycling methods to improve efficiency and recovery of materials, including ionothermal, hydothermal, solid-state, or redox mediator methods. In conjunction with recycling process development, detailed structural characterization is necessary in order to understand the mechanisms and efficacy of cathode recycling steps. Solid-state nuclear magnetic resonance (NMR) spectroscopy is a unique tool that can probe Li coordination, bulk and surface environments, and transition metal ordering in recycled and upcycled NMC cathodes. Here, 6,7Li, 1H, and 19F NMR spectroscopy to probe structural and compositional changes as well as surface impurities that may form during each step in NMC direct recycling is utilized. During relithiation, Li reinsertion into the NMC lattice is observed. During upcycling, where the goal is to increase the Ni content in the NMC, incorporation of Ni-rich phases into the bulk Li environment is observed. Surface impurities formed during processing were also identified. These studies provide valuable information for optimizing recycling processes to reach targeted cathode composition and structure that can enable electrochemical performance comparable to or better than pristine materials.

36 MATERIALS SCIENCE↗

In situ inorganic conductive network formation in high-voltage single-crystal Ni-rich cathodes

High nickel content in LiNi x Co y Mn z O 2 (NCM, x ≥ 0.8, x + y + z = 1) layered cathode material allows high specific energy density in lithium-ion batteries (LIBs). However, Ni-rich NCM cathodes suffer from performance degradation, mechanical and structural instability upon prolonged cell cycling. Although the use of single-crystal Ni-rich NCM can mitigate these drawbacks, the ion-diffusion in large single-crystal particles hamper its rate capability. Herein, we report a strategy to construct an in situ Li 1.4 Y 0.4 Ti 1.6 (PO 4 ) 3 (LYTP) ion/electron conductive network which interconnects single-crystal LiNi 0.88 Co 0.09 Mn 0.03 O 2 (SC-NCM88) particles. The LYTP network facilitates the lithium-ion transport between SC-NCM88 particles, mitigates mechanical instability and prevents detrimental crystalline phase transformation. When used in combination with a Li metal anode, the LYTP-containing SC-NCM88-based cathode enables a coin cell capacity of 130 mAh g -1 after 500 cycles at 5 C rate in the 2.75-4.4 V range at 25 °C. Tests in Li-ion pouch cell configuration (i.e., graphite used as negative electrode active material) demonstrate capacity retention of 85% after 1000 cycles at 0.5 C in the 2.75-4.4 V range at 25 °C for the LYTP-containing SC-NCM88-based positive electrode.

25 ENERGY STORAGE↗

An unwanted guest in the electrochemical oxidation of high-voltage Li-ion battery electrolytes: the life of highly reactive protons

Lithium-ion batteries (LIBs) are central to the urgent societal need to decarbonize both transportation and energy storage on the grid. Unfortunately, despite their attractive energy/power density, as well as high coulombic and energy efficiencies, further improvement of this technology – especially their durability – is desperately needed. To support these efforts, our study focuses on fundamental understanding of the decomposition pathways for LIB electrolytes at the cathode–electrolyte interface (CEI), as the nature of these reactions directly controls the extent to which cell capacity and voltage decays in these systems. In this study, we employ electrochemical methods, coupled with product analysis using NMR spectroscopy and mass spectrometry, to determine the decomposition mechanisms in both model and technologically relevant electrolytes. Remarkably, we discovered the electrochemical formation of protons with high chemical activity, comparable to known superacids, at potentials relevant to practical Li-ion batteries. Their reactivity toward every individual component of the CEI provides a unified thermochemical origin for a myriad of side reactions that are commonly associated with the electrochemical reaction. In particular, electrochemically generated protons react with intact EC molecules to form CO 2 and other short and long chain ethers. They also undergo an acid–base reaction with LiPF 6 , to form the weaker acid HF, and with the cathode active material, leaching transition metals into the electrolyte. Collectively, the results of this study all point to the urgent need to either mitigate this proton formation or introduce benign harvesting additives via new electrolyte design strategies.

Ilic, Stefan [Argonne National Laboratory (ANL), A↗

Targeted masking enables stable cycling of LiNi 0.6 Co 0.2 Mn 0.2 O 2 at 4.6V

Layered LiNi x Co y Mn 1–x-y O 2 (NCM, or NCMxy(1-x-y)) is a dominant family of cathode materials for lithium-ion batteries (LIBs) due to its high energy density. Among all NCM cathode materials, NCM622 possess the optimal energy density at high potential (≥ 4.6 V vs. Li/Li + ). However, the practical application of NCM622 at high voltage (≥ 4.6 V) is limited by its parasitic reactions and associated safety concerns. Completely physical isolation has been considered as the main approach to mitigate the parasitic reaction. It has also been previously demonstrated that the interface reaction has active site selectivity, and that the reactivity of the active sites can effectively suppressed by blocking the chemically active sites. Herein, a targeted masking by LiFePO 4 @C nanoplates is reported to unlock the stable performance of NCM622 up to 4.6 V vs. Li/Li + . The (targeted masked-NCM622)|graphite pouch cell shows 86.5% capacity retention after 1000 cycles and its maximum temperature during thermal runaway is dramatically reduced from 570 °C to 415 °C. Systematic in/ex situ characterizations, first-principles calculations and half/pouch targeted LiFePO 4 @C covers the surface of NCM partcell evaluation prove that PO 4 3- is preferentially adsorbed on transition metal sites, stabilizing both the transition metal ions and oxygen ions on the surface against the ethylene carbonate-containing traditional electrolyte even under high voltage (≥ 4.6 V vs. Li/Li + ). Furthermore, this work opens up new venue for rational design of high-performance cathode materials through a low-cost and scalable decoration process, and reveal a new understanding of interfacial activity of materials.

25 ENERGY STORAGE↗

Synthetic Control of Kinetic Reaction Pathway and Cationic Ordering in High-Ni Layered Oxide Cathodes

Nickel-rich layered transition metal oxides, LiNi 1-x (MnCo) x O 2 (1-x ≥ 0.5), are appealing candidates for cathodes in next-generation lithium-ion batteries (LIBs) for electric vehicles and other large-scale applications, due to their high capacity and low cost. However, synthetic control of the structural ordering in such a complex quaternary system has been a great challenge, especially in the presence of high Ni content. Herein, synthesis reactions for preparing layered LiNi 0.7 Mn 0.15 Co 0.15 O 2 (NMC71515) by solid-state methods are investigated through a combination of time-resolved in situ high-energy X-ray diffraction and absorption spectroscopy measurements. The real-time observation reveals a strong temperature dependence of the kinetics of cationic ordering in NMC71515 as a result of thermal-driven oxidation of transition metals and lithium/oxygen loss that concomitantly occur during heat treatment. Through synthetic control of the kinetic reaction pathway, a layered NMC71515 with low cationic disordering and a high reversible capacity is prepared in air. The findings may help to pave the way for designing high-Ni layered oxide cathodes for LIBs

25 ENERGY STORAGE↗

Ni-Rich Li[Ni x MnyCo 1– x – y ]O 2 Single Crystals as Superior Fast Charge Cathodes for Lithium-Ion Batteries

The utilization of single-crystal (SC) Li[Ni x MnyCo 1-x-y ]O 2 (NMC) cathodes has facilitated unparalleled performance in commercial high-energy lithium-ion batteries (LIBs). In the current study, we evaluate the application of SC cathodes in fast charge (FC)-LIBs where particle cracking is a predominant failure mechanism. Ni-rich SC-NMC samples with various compositions, sizes, and shapes are synthesized and investigated for their influence on FC performance. We reveal the necessity of utilizing smaller SCs (<1 μm) as larger sizes (>2 μm) experience significant particle-level lithium concentration gradients under FC conditions. To improve lithium transport and minimize side reactivities, we strategically expose the (104) crystal facets on the surface. Exceptional performance was observed on an optimized SC-LiNi 0.80 Mn 0.05 Co 0.15 O 2 , delivering a discharge capacity of 165 mAh/g even after 150 cycles at 6C charge. Our study not only demonstrates the promise of SC-NMC but also provides the key insights for the design and optimization of advanced cathodes for FC-LIBs.

25 ENERGY STORAGE↗

Evaluation of Gas Formation and Consumption Driven by Crossover Effect in High-Voltage Lithium-Ion Batteries with Ni-Rich NMC Cathodes

Gas formation during lithium-ion battery (LIB) cycling impacts the stability and safety of these batteries, especially for those containing Ni-rich NMC cathodes. In this paper, the cycling performance and gassing behavior of NMC811/graphite full cells with 4.2 and 4.4 V upper cutoff voltages were first compared. We report cells with a 4.2 V upper cutoff voltage had good cycling stability, exhibiting a capacity retention of 96.8% after 100 cycles and generated little gas. On the other hand, cells with a 4.4 V upper cutoff voltage lost over 25% of initial capacity after 100 cycles and generated large amounts of gas in the first 10 cycles. Electrochemical cycling of anode and cathode symmetric cells was implemented to isolate gases formed at the electrode. Gas chromatography–mass spectrometry, Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy, and scanning transmission electron microscopy were used to characterize the gas formation and associated material surfaces and structural properties. It was found that CO2 and fluorinated alkanes were the dominant gases evolved on the cathode side during cycling to 4.4 V. Gas crossover to the anode led to the depletion of gaseous products, which stabilized the cell performance to some extent. However, the growing surface reconstruction layer at the cathode, the thickening of the solid electrolyte interphase layer at the anode, and the gradual depletion of lithium inventory collectively contributed to the continuous capacity loss of full cells cycled to 4.4 V.

25 ENERGY STORAGE↗

Electrode Separation and Froth Flotation for the Recovery of Li-ion Battery Cathode Materials

Increasing use of Li-ion batteries (LIBs) will significantly increase the quantity of LIB waste generated from end-of-life batteries. Spent LiCoO 2 (LCO) battery cathodes contain significant quantities of valuable metals, making them good candidates for recycling. Typical recycling processes rely on high temperatures (pyrometallurgy) and chemical leachants (hydrometallurgy) to completely decompose the cathode and enable material recovery. Direct recycling processes and recovery of active material from electrode scrap do not benefit from such destructive recycling, and an efficient means of separating the cathode active material from the inactive components (e.g., polyvinylidene fluoride (PVDF) binder, conductive carbon) is needed. Here, we explore PVDF removal from LCO cathodes by two separate methods, evaluating their suitability for coupling to subsequent separation by froth flotation (FF). We show that washing electrodes in the solvent PolarClean (PC) dissolves PVDF away from LCO cathodes, enabling separation of the remaining LCO and conductive carbon by FF. The process is suitable for use with both pristine and cycled LCO electrodes, and the pristine recovered material can be used to prepare electrodes capable of cycling at 140 mAh/g. In conclusion, this demonstrates the suitability of coupled PC washing and FF separation for recycling both end-of-life batteries and scrap electrode material.

Batteries↗

Sustainable bioleaching of lithium-ion batteries for critical materials recovery

The demand for lithium-ion batteries (LIBs) has increased substantially over the last few decades due to their longer lifetime, greater resistance to self-discharge, and higher output voltage compared to other battery types. With the global trend of electrifying vehicle fleets, the number of LIBs reaching their end-of-life (EOL) is expected to grow substantially in the next decade. These EOL LIBs represent a significant secondary source of materials (e.g., Li, Co, Ni, Mn) that can be recovered and reused in LIBs or other products. In this study, we developed a bioleaching process that could recover critical materials from EOL LIBs in an economical and environmentally sustainable manner under industrially relevant conditions. Black mass, i.e., cathode-containing powder, prepared from EOL LIBs was leached using a biolixiviant produced from corn stover by Gluconobacter oxydans bacteria. Iron(II) was used as a reducing agent to promote metal dissolution. Techno-economic analysis (TEA) estimated a potential average profit margin of 21% for processing 10,000 t of black mass per year, which represents approximately 30% of the available black mass in the US in 2020. Life cycle assessment (LCA) demonstrated that bioleaching of spent LIBs could be more environmentally sustainable than alternative hydrometallurgical recovery methods such as hydrochloric acid leaching (16-19 kg vs. 43-91 kg CO 2 equivalent global warming potential per kg of recovered cobalt). The TEA results are highly dependent on the cost of black mass production, which varies by EOL LIB collection and transportation costs. Finally, emerging technologies for deactivating used LIBs for fire safety at collection centers will allow the transport of EOL LIBs as non-hazardous materials, lower the cost of preparing black mass and thereby increase economic prospects for EOL LIBs recycling using this approach.

25 ENERGY STORAGE↗

Modification of Ni-Rich FCG NMC and NCA Cathodes by Atomic Layer Deposition: Preventing Surface Phase Transitions for High-Voltage Lithium-Ion Batteries

The energy density of current lithium-ion batteries (LIBs) based on layered LiMO 2 cathodes (M=Ni, Mn, Co: NMC; M=Ni, Co, Al: NCA) needs to be improved significantly in order to compete with internal combustion engines and allow for widespread implementation of electric vehicles (EVs). In this report, we show that atomic layer deposition (ALD) of titania (TiO 2 ) and alumina (Al 2 O 3 ) on Ni-rich FCG NMC and NCA active material particles could substantially improve LIB performance and allow for increased upper cutoff voltage (UCV) during charging, which delivers significantly increased specific energy utilization. Our results show that Al2O3 coating improved the NMC cycling performance by 40% and the NCA cycling performance by 34% at 1C/₋1C with respectively 4.35V and 4.4V UCV in 2Ah pouch cells. High resolution TEM/SAED structural characterization revealed that Al 2 O 3 coatings prevented surface-initiated layered-to-spinel phase transitions in coated materials which were prevalent in uncoated materials. Lastly, EIS confirmed that Al 2 O 3 -coated materials had significantly lower increase in the charge transfer component of impedance during cycling. In conclusion, the ability to mitigate degradation mechanisms for Ni-rich NMC and NCA illustrated in this report provides insight into a method to enable the performance of high-voltage LIBs.

25 ENERGY STORAGE↗

Complementary Effects of Mg and Cu Incorporation in Stabilizing the Cobalt-Free LiNiO 2 Cathode for Lithium-Ion Batteries

Since the discovery of LiNiO 2 several decades ago, a new era of electric vehicles demanding high-energy-density lithium-ion batteries (LIBs) has recently rebooted the interest in this cathode material to eliminate the dependence on expensive and scarcely available cobalt. However, LiNiO 2 has been plagued by cycle instability, thermal instability, and air instability. We present here an exploration of the mutual interaction of magnesium and copper in stabilizing the cobalt-free LiNiO 2 cathode. Although Mg doping is beneficial for the robustness of the bulk structure of LiNiO 2 , surface characterization results of Mg-doped LiNiO 2 implies the need for further surface protection. To that end, we have incorporated Cu in addition to Mg in that Cu stabilizes the surface of Mg-doped LiNiO 2 by forming a protective stable surface layer without harming the bulk. Notable variations of the surface residual lithium composition (Li Li 2 CO 3 /Li LiOH ) along with the incorporation of stabilizers are also discussed. The harmony between Mg and Cu with as little as 0.5 atom % Mg and 0.3 atom % Cu significantly enhances the specific energy and cycle life of LiNiO 2 . Furthermore, this study demonstrates how the co-incorporation of optimal dopants can help stabilize both the bulk and surface and provides new insights toward developing cobalt-free layered oxide cathodes for high-energy-density LIBs.

25 ENERGY STORAGE↗

Rational designs to enable 10-min fast charging and long cycle life in lithium-ion batteries

A daunting challenge in the design of lithium ion batteries (LiBs) is enabling 10-min extreme fast charging (XFC) while achieving appreciable charge acceptance and cycle life. This desirable outcome requires both a comprehensive understanding of LiB operation and aging behavior at different length scales and careful optimization. Lithium plating has been a critical bottleneck because, at XFC rates, it consumes cyclable lithium causing distinct aging and safety concerns even in moderate-loading LiBs. Here, we propose combining multiple solutions, including materials-to-electrode design-to-charging protocols, that are intended to overcome limitations in lithium-ion transport in the electrolyte phase, thus enabling 10-min XFC in LiBs. Some implemented strategies include cathode chemistry, optimized carbon binder domain in the cathode, dual layer anode design, improved separator and advanced electrolyte. Further, innovative charging protocols in moderately loading (~3 mAh/cm 2 anode/2.7 mAh/cm 2 cathode) single-layer pouch cells are proposed, together with demonstrated 10-min XFC with higher charge acceptance between 87.3 and 92.1% (or 2–2.1 mAh/cm 2 ) for 600 cycles without lithium plating. This methodical study with well-defined cells shows promise in combining multiple solution strategies to enable 10-min XFC, charting a pathway to achieve XFC in higher-loading energy-optimized LiBs.

25 ENERGY STORAGE↗

Probing the Complexities of Structural Changes in Layered Oxide Cathode Materials for Li-Ion Batteries during Fast Charge–Discharge Cycling and Heating

The rechargeable lithium-ion battery (LIB) is the most promising energy storage system to power electric vehicles with high energy density and long cycling life. However, in order to meet customers’ demands for fast charging, the power performances of current LIBs need to be improved. From the cathode aspect, layer-structured cathode materials are widely used in today’s market and will continue to play important roles in the near future. The high rate capability of layered cathode materials during charging and discharging is critical to the power performance of the whole cell and the thermal stability is closely related to the safety issues. Therefore, the in-depth understanding of structural changes of layered cathode materials during high rate charging/discharging and the thermal stability during heating are essential in developing new materials and improving current materials. Since structural changes take place from the atomic level to the whole electrode level, combination of characterization techniques covering multilength scales is quite important. Finally, in many cases, this means using comprehensive tools involving diffraction, spectroscopy, and imaging to differentiate the surface from the bulk and to obtain structural/chemical information with different levels of spatial resolution.

25 ENERGY STORAGE↗

Progress in direct recycling of spent lithium nickel manganese cobalt oxide (NMC) cathodes

With the widespread use of lithium-ion batteries (LIBs) in portable electronics and electric vehicles (EVs), the end-of-life (EOL) LIBs are projected to reach 1336 GWh by 2040 under the sustainable development scenario. Proper recycling is urgently needed to minimize the release of hazardous waste and reduce mining activities by reintroducing critical minerals into the supply chain. Lithium nickel manganese cobalt oxide (LiNi x Mn y Co z O 2 , NMCs) cathodes have become dominant in the LIB market, especially with the increasing production of EVs, which are also the most valuable components in EOL LIBs. Unlike pyrometallurgical and/or hydrometallurgical methods, which convert spent NMCs into metals or metal compounds, direct recycling technologies aim to maximize the value of spent cathodes by restoring their degraded structure and composition. Furthermore, this review summarizes direct recycling methods for NMC cathodes published in the last decade and provides insights into the challenges and future development of direct recycling techniques.

Cathode↗

Optimising the geospatial configuration of a future lithium ion battery recycling industry in the transition to electric vehicles and a circular economy

Rapid electrification of the transport system will generate substantial volumes of Lithium-ion-battery (LiB) waste as batteries reach their end-of-life. Much attention focuses on the recycling processes, neglecting a broader systemic view that considers the concentration of the costs and impacts associated with logistics and transportation. This paper provides an economic, environmental and geospatial analysis of a future LiB recycling industry in the UK. Hitherto, state-of-the-art assessment methods have evaluated life cycle impacts and costs but have not considered the geographical layer of the problem. This paper develops a GSC derived supply chain model for the UK electric vehicle and end-of-life vehicle battery industry. Considering both pyrometallurgical and hydrometallurgical recycling technologies, the optimisation process takes into account anticipated EV volumes, and, based on anticipated near-term technological evolution of LiBs, the evolution of the mix of battery cathodes in production, and presents a number of scenarios to show where LiB recycling facilities should ideally be geographically located. An economic and environmental assessment based on a customised EverBatt model is provided.

25 ENERGY STORAGE↗