Engineering Approaches to Dendrite free Lithium Anodes
This is the Final Technical Report of the work that was completed related to development of dendrite free anodes for Li-metal batteries. The report contains full details of all the strategies that were employed to overcome this pernicious problems of dendrite formation of lithium metal during cycling of Li-metal and Li-ion batteries. Various approaches were developed to understand the formation of dendrites and mitigation strategies were then developed to overcome this severe problem. In doing so novel multi-component alloys as well as structurally isomorphous alloys have been developed. In addition coating strategies were also developed to overcome the formation of dendrites. The novel approaches related to development of novel alloys using economic cost effective and scalable approaches. The new approaches will easily advance the science of lithium metal alloys and dendrite free anodes including current collectors. Development of this new technology will have immense benefit to providing new high energy density batteries of tremendous benefit to the public since cost effective and safe high energy density batteries will be possible with this new technology.
Valuation of Anode Materials for High-Performance Lithium Batteries: From Graphite to Lithium Metal and Beyond
Lithium-ion batteries have revolutionized energy storage, yet advanced technologies such as electric vehicles and eVTOLs demand even higher performance and safety. Anodes, the negative electrodes, are crucial in enhancing batteries’ safety, lifespan, and fast-charging capabilities. This review paper comprehensively evaluates the progression of anode materials from traditional graphite to advanced anodes like lithium metal. Graphite anodes, with a capacity of 372 mAh g −1 , enabled the first commercial lithium-ion batteries, but future applications require higher energy densities and fast-charging capabilities. Emerging anode materials, including alloying, and conversion types, as well as lithium metal, offer significantly higher capacities, with lithium metal offering a theoretical capacity of 3 860 mAh g −1 . However, these advanced anodes face challenges such as volume expansion, high surface reactivity, sluggish Li+ kinetics, and unstable lithium deposition morphologies. Here, this review critically examines the electrochemical performance, interfacial properties, mechanical attributes, and stability issues of various anode materials. It further discusses solid electrolyte interphase (SEI) formation, strategies for enhancing interface stability, and the requirements of anodes for solid-state batteries. Additionally, the review explores potential solutions for limitations with each anode type, highlights innovative anode-free architectures, and evaluates the current and future trends of battery anode industries. Ultimately, this paper aims to guide the development of high-performance anode materials, paving the way for the next generation of efficient, reliable lithium batteries.
MHD flow in liquid metal blankets: Major design issues, MHD guidelines and numerical analysis
The design of breeding blankets represents the major challenge for fusion reactor engineering because of performance requirements and severe operating conditions in terms of heat load and neutron flux. Liquid metal alloys such as lead-lithium, due to their lithium content, can be used to breed tritium, one of the plasma fuel components, and owing to their high thermal conductivity, they may serve as coolants. On the other hand, there are technical issues related to the fact that the liquid metals are electrically conducting and interact with the plasma-confining magnetic field. Induced electric currents and generated electromagnetic forces affect velocity and pressure distribution in the blankets. Magnetohydrodynamic (MHD) flows for fusion applications have been often investigated in simplified geometries, such as pipes, ducts, bends, with focus on their fundamental features. These analyses are essential, since results remain valid as background for the development of blanket designs, even when a concept is dismissed. However, the conceptual study of fusion blankets requires to take into account the global multiple effects, that arise when the full system is considered. Progress made in fusion-related MHD research results from combined numerical and experimental activities. In this paper we review and summarize features of 2D and 3D MHD flows that are typical in liquid metal blankets, together with available correlations for MHD pressure losses. This knowledge can provide simple design MHD guidelines that support a preliminary estimate of MHD effects in a blanket concept, in terms of pressure drop and flow distribution.
Evolution of solid electrolyte interphase and active material in the silicon wafer model system
Alloying anode materials for lithium-ion batteries, such as silicon (Si), are an important focus of materials research due to the demand for increased energy density for electric vehicles and stationary grid storage. However, progress towards next generation anode materials has been hindered by poor capacity retention due to the instability of the Si active material and the solid electrolyte interphase (SEI). Herein, the evolution of the active Si material and the SEI are simultaneously investigated from the perspective of chemical, structural, morphological, and electronic evolution in the Si wafer model system through its cycling life, using time-of-flight secondary ion mass spectrometry (TOF-SIMS), scanning transmission electron microscopy (STEM), atomic force microscopy (AFM), and scanning spreading resistance microscopy (SSRM). The results illustrate a dynamic evolution of the SEI and active Si material through cycling. Through an improved understanding of evolution of SEI and Si active material within the Si wafer model system, mitigation strategies may be designed to extend the lifetime of Si anodes.
Laser Powder Bed Fusion Additive Manufacture Nb1Zr Development
Next generation fission and fusion nuclear reactors require materials that can withstand operating temperatures greater than 500 °C, neutron irradiation doses of up to 200 displacements per atom (dpa), and potentially corrosive coolants such as the alkali liquid metals sodium, lithium, and NaK (Na33K eutectic alloy). Refractory alloys, such as Nb1Zr (Nb-1wt%Zr) and Molybdenum alloy TZM (Mo-0.5wt%Ti-0.08wt%Zr) have been traditionally considered viable candidates for advanced fission and fusion reactor concepts. However, it is relatively difficult to generate complex geometries of interest from these alloys using traditional manufacturing methods. In addition, there needs to be a concentrated effort to address refractory metal challenges at elevated temperature operation. In order to generate complex geometries of interest, modern manufacturing techniques are considered to increase the technological readiness level (TRL), cost-effectiveness, and schedule savings. This work focused on the continued development of laser powder bed fusion (L-PBF) additive manufacturing (AM) to improve both design flexibility, evaluate microstructure and properties, and ultimately accelerate the TRL and qualification of these processes and alloys for components to potentially be put into service. Niobium alloy Nb1Zr was identified through a down-selection process outlined in previous reports as a candidate to develop in L-PBF AM. Historically, Nb1Zr had been explored for high temperature fast spectrum fission reactors for both terrestrial and space applications. Molybdenum alloy TZM has also been considered for these reactor concepts due to exceptional high-temperature strength, creep resistance, and stability under irradiation. L-PBF AM of TZM has previously been investigated at LANL under the Microreactor program, NASA, ORNL, and in academia. However, due to the crack prone nature of TZM, L-PBF AM of TZM resulted in significant microcracking and additional development is required to pursue viable maturation. Other AM methods have been found to be more successful in printing TZM, and those alternatives approaches are discussed in this effort. The efforts detailed in this report focused on continued development of Nb1Zr through L-PBF and development of TZM via L-PBF and electron powder bed fusion (E-PBF). The objective of this work was to further the development of these AM techniques for the chosen refractory alloys, elucidating and addressing associated challenges through characterization of several demonstration builds. At LANL, Nb1Zr builds were completed using an EOS M290 and M400 machines, and a refractory alloy-dedicated L-PBF system, the Xact Metal XM200G, was installed. The XM200G primary purpose was to do the Nb1Zr parameter development process; however, due to difficulties associated with the machine installation and qualification process, it was decided to pivot development to the larger M400 and M290 machines. Although the supply of Nb1Zr powder was limited, it was sufficient to generate sub-scale metallographic specimens for the purpose of parameter development. This was first accomplished on the EOS M400 then the M290 due to machine schedule availability. Further development of TZM has been initiated at the University of Texas El Paso (UTEP) under contract with LANL to use both a heated build envelope L-PBF machine and E-PBF machine that have been found in the literature to mitigate microcracking. UTEP was provided with TZM powder and build plates to support parallel TZM parameter development across both machines. As part of the contract, UTEP will also be conducting microstructural characterization once optimized process parameters have been identified. The optimized process parameters for each machine will be used to generate a series of metallographic, mechanical, and surface finish specimens for subsequent characterization and testing. In the next section, we provide a detailed discussion of the methodology used for investigating the feasibility of leveraging these alloys for use in advanced reactor applications.
New High-Performance Pb-Based Nanocomposite Anode Enabled by Wide-Range Pb Redox and Zintl Phase Transition
Explore the source record for details and available documents.
Polymer-Stabilized Liquid Metal Nanoparticles as a Scalable Current Collector Engineering Approach Enabling Lithium Metal Anodes
Dendrites and dead lithium formation over prolonged cycling have long been challenges that hinder the safe implementation of metallic Li anodes. In this study, we employ polymer-stabilized liquid metal nanoparticles (LM-P NPs) of eutectic gallium indium (EGaIn) to create uniform Li nucleation sites enabling homogeneous lithium electrodeposition. Block copolymers of poly(ethylene oxide) and poly(acrylic acid) (PEO-b-PAA) were grafted onto the EGaIn surface, forming stabilized, well-dispersed NPs. Using a scalable spray coating approach, LM-P NPs were fabricated on copper current collectors, providing lithiophilic PEO sites and interactive carboxyl groups to guide Li deposition. The Li-EGaIn alloying process greatly reduced the Li + diffusion barrier, enabling fast Li transport through the coating layer, resulting in decreased nucleation overpotential. Therefore, about five times lower Li nucleation overpotential was obtained on the LM-P modified Cu with an optimal composition of the polymers than the bare Cu substrates. DFT computations was used to reveal the binding properties between the LM-P layer and Li. Due to the regulated Li plating/stripping process, as-obtained 30 μm Li anodes paired with LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NCM8 11 ) with a negative/positive electrode capacity (N/P) ratio ~ 10 exhibited stable cycling performance at 0.5C for over 250 cycles, with an average Coulombic efficiency of 99.55%. Ultrathin Li (1 μm) anodes with an N/P ratio ~ 0.6 were also demonstrated in Li|LiFePO 4 cells, which examined the stabilization of Li by LM-P NPs and monitored practical loadings of Li anodes that are close to anode-free systems.
A self-healing liquid metal anode with PEO-Based polymer electrolytes for rechargeable lithium batteries
In this study, a Ga-Sn liquid metal alloy material is demonstrated as a self-healing anode system due to its fluidity via operando synchrotron-based transmission X-ray microscopy and X-ray diffraction experiments. Cracks formed due to volume expansions can be recovered by the fluidity of the liquid metals. By incorporating with a poly(ethylene oxide) (PEO)-based electrolyte at 60°C, the Ga-Sn anode shows a reversible lithium insertion and extraction process with a high initial discharge specific capacity of 682 mAh g -1 , followed by delivering a capacity of 462 mAh g -1 in the second cycle at C/20 rate. Furthermore, compared with its solid counterparts, the Ga-Sn liquid metal anode demonstrates a better capability to maintain its mechanical integrity and better contact with PEO solid electrolytes due to its advantageous features of the liquid. This study suggests a potential strategy to use liquid metal alloys with polymer solid electrolyte to solve the anode challenges in rechargeable lithium batteries.
In-situ formation of stable interface towards Li-in anode for halide solid-state electrolyte
Halide-based solid-state electrolytes (SSEs) are promising candidates for next-generation all-solid-state lithium batteries (ASSLBs) due to their high ionic conductivity and chemical stability. However, their poor interfacial compatibility with lithium metal anode and Li-In alloy significantly hinder practical application due to the requirement for a protective interlayer. In this study, a novel approach to overcome this limitation is presented by introducing iron (Fe) doping into Li 3 InCl 6 (LIC), which enables direct and stable contact with lithium-indium (Li-In) metal without a protective interlayer. Thermodynamic and computational analyses identified Fe 3+ as a suitable dopant based on its similar reduction potential to In 3+ and structural compatibility within the halide lattice. The synthesized 10 at. % Fe-doped LIC exhibits high phase purity, retained ionic conductivity, and notably improved interfacial stability. Full-cell tests using Fe-LIC achieve over 300 cycles with 80 % capacity retention. At the same time, symmetric Li-In/ Fe-LIC/ Li-In cells sustain over 500 h of operation, representing the first reported long-term cycling of LIC-based ASSLB without a protective interlayer. In conclusion, this work establishes Fe doping as an effective strategy to stabilize halide SSEs of In system against Li-In alloy, thereby simplifying cell architecture and advancing the development of safer, high-performance halide-based solid-state electrolytes.
Beyond Volume Variation: Anisotropic and Protrusive Lithiation in Bismuth Nanowire
Materials storing energy via an alloying reaction are promising anode candidates in rechargeable lithium-ion batteries (LIBs) due to their much higher energy density than the current graphite anode. Until now, the volumetric expansion of such electrode particles during lithiation has been considered as solely responsible for cycling-induced structural failure. Here, we report different structural failure mechanisms using single-crystalline bismuth nanowires as the alloying-based anode. The Li–Bi alloying process exhibits a two-step transition, that is, Bi–Li 1 Bi and Li 1 Bi–Li 3 Bi. Interestingly, the Bi–Li 1 Bi phase transition occurs not only in the bulk Bi nanowire but also on the particle surface showing its characteristic behavior. The bulk alloying kinetics favors a Bi-(012)-facilitated anisotropic lithiation, whose mechanism and energetics are further studied using the density functional theory calculations. More importantly, the protrusion of Li 1 Bi nanograins as a result of anisotropic Li–Bi alloying is found to dominate the surface morphology of Bi particles. The growth kinetics of Li 1 Bi protrusions is understood atomically with the identification of two different controlling mechanisms, that is, the dislocation-assisted strain relaxation at the Bi/Li 1 Bi interface and the short-range migration of Bi supporting the off-Bi growth of Li 1 Bi. As loosely rooted to the bulk substrate and easily peeled off and detached into the electrolyte, these nanoscale protrusions developed during battery cycling are believed to be an important factor responsible for the capacity decay of such alloying-based anodes at the electrode level.
In Situ Alloying Enabled by Active Liquid Metal Filler for Self‐Healing Composite Polymer Electrolytes
Abstract Solid inorganics, known for kinetically inhibiting polymer crystallization and enhancing ionic conductivity, have attracted significant attention in solid polymer electrolytes. However, current composite polymer electrolytes (CPEs) are still facing challenges in Li metal batteries, falling short of inhibiting severe dendritic growth and resulting in very limited cycling life. This study introduces Ga 62.5 In 21.5 Sn 16 (Galinstan) liquid metal (LM) as an active liquid alternative to conventional passive solid fillers, aiming at realizing self‐healing protection against dendrite problems. Compared to solid inorganics, for example silica, LM droplets could more significantly reduce polymer crystallinity and enhance Li‐ion conductivity due to their liquid nature, especially at temperatures below the polymer melting point. More importantly, LMs are unraveled as dynamic chemical traps, which are capable of blocking and consuming lithium dendrites upon contact via in situ alloying during battery operation and further inhibiting dendritic growth due to the lower deposition energy barrier of the formed Li‐LM alloy. As a proof of concept, by strategically designing an asymmetric CPE with the active LM filling, a solid‐state Li/LiFePO 4 battery achieves promising full‐cell functionality with notable rate performance and stable cycle life. This active filler‐mediated self‐healing approach could bring new insights into the battery design in versatile solid‐state systems.
Corrosion sensitivity of nickel-based Alloy Inconel 600 in pressurized water reactor water chemistry: Can KOH replace LiOH?
Lithium hydroxide (LiOH) has been used to balance water acidity against boric acid moderators in the primary water of Western pressurized water reactor (PWR) designs for decades. However, the demand and the cost of lithium-7 has grown significantly since 2015. Potassium hydroxide (KOH) has been identified as a suitable and cost-effective substitute for LiOH and has been used successfully in Russian PWR designs for more than 40 years. However, it is important to know if alloys and water conditions used in Western PWR’s (Alloy 600) are similarly compatible with KOH additions. This work is focused on the aqueous corrosion behaviors of Alloy 600 with LiOH versus KOH additions at normal operating concentrations and crevice water chemistry at simulated PWR primary water conditions. TEM was used to characterize the formed oxide through diffraction analysis; SIMS was used to probe the cation ingress into the material; Atom probe tomography was used to determine the 3D elemental distribution within the oxide/metal structures; finally electrochemical impedance spectroscopy was used to discuss the structure and corrosion resistance of the oxide films. These advanced characterization techniques complement the weight measurments which showed lower mass gain in KOH than LiOH crevice water due to less oxide formation. Overall, the use of KOH as a potential alternative to LiOH in PWR is discussed.
Thermal evaporation of thin Li films
Thermal evaporation of lithium is considered a promising technique for the fabrication of clean lithium thin films for solid-state batteries. Here, in this study, we present a practical investigation of nanometer scale lithium films prepared by evaporation on different substrates. These substrates include Li-alloying and nonalloying metals as well as different classes of solid-state lithium-ion conductors. The deposition rate was also varied. For films less than 100 nm thick, the data show that the deposition rate has the biggest impact on the surface coverage. At 50 Å/s, Li forms small particles <1 μm in diameter while higher deposition rate of 150 Å/s resulted in more uniform film morphology on all the substrates. At the lower deposition rates, the wetting of Li to the substrate will impact the particle morphology. We also used the particles to estimate a contact angle between Li and the substrate to qualitatively compare the adhesion from substrate to substrate. The smallest contact angle was observed from lithium films on Li 7 La 3 Zr 2 O 12 and LiPON (nominal Li 2.94 PO 3.5 N 0.31 ) solid-state electrolytes.
Lithium nitrate salt-assisted CO 2 absorption for the formation of corrosion barrier layer on AZ91D magnesium alloy
The formation of Mg–Li–C–O barrier layer on AZ91D Mg alloy using LiNO 3 -assisted thermal CO 2 treatment provides a pathway to utilize excessive CO 2 for corrosion protection of AZ91D.
Batteries (2021 Annual Progress Report)
This document summarizes the progress of VTO battery R&D projects supported during the fiscal year 2021 (FY 2021). In FY 2021, the DOE VTO battery R&D funding was approximately $\$$115 million. Its R&D focus was on the development of high-energy batteries for EVs as well as very high-power devices for hybrid vehicles. The electrochemical energy storage roadmap (which can be found at the EERE Roadmap web page2) describes ongoing and planned efforts to develop electrochemical storage technologies for EVs. To advance battery technology, which can in turn improve market penetration of PEVs, the program investigates various battery chemistries to overcome specific technical barriers, e.g., battery cost, performance, life (both the calendar life and the cycle life), its tolerance to abusive conditions, and its recyclability/sustainability. VTO R&D has had considerable success, lowering the cost of EV battery packs to $\$$185/kWh in 2019 (representing more than 80% reduction since 2008) yet even further cost reduction is necessary for EVs to achieve head-to-head cost competitiveness with ICEs (without Federal subsidies). In addition, today’s batteries also need improvements in such areas as their ability to accept charging at a high rate, referred to as extreme fast charging (XFC) (15 minute charge) – to provide a “refueling” convenience similar to ICEs, and the ability to operate adequately at low temperatures. Research into “next-gen lithium-ion” batteries which would provide such functionalities is one of the R&D focus areas. VTO is funding research on both “next gen” chemistries (which employ an alloy anode and/or a high voltage cathode) and beyond lithium-ion (BLI) chemistries (which can, for example, employ a lithium metal anode).
Tuning working potential of silicon-phosphorus anode via microstructure control for high-energy lithium-ion batteries
The primary research on anode materials of lithium-ion batteries have been focused on increasing the specific capacity, while the working potential that is also closely related to the practical energy density of batteries has been paid much less attention. In this paper, starting from micrometer-sized silicon and black phosphorus, we have reported a high-energy silicon-phosphorus/carbon anode (denoted as mSPC) via a high-energy ball milling process, which demonstrates an average discharge working potential of 0.3 volts versus lithium, together with a high reversible capacity of > 2000 mAh/g, high initial coulombic efficiency of 84%, excellent cycle stability, and superior rate capability up to 15 A/g. Furthermore, in situ focused-ion-beam scanning electron microscopy reveals that the volume change of the mSPC anode during repeated (de) lithiation is effectively alleviated. In contrast, starting from nanometer-sized silicon, the resulted anode (denoted as nSPC) not only presents a lower reversible capacity (~1200 mAh/g), but also exhibits a higher charge/discharge working potential, leading to reduced energy density. Our results indicate the importance of composition/structure control in tailoring the working potential and specific capacity of alloying-type anodes towards high-energy lithium-ion batteries.
Ca Metal Batteries and Sn Anode Alloying: Resolving Misconceptions in Ca–Sn Alloy Formation
Ca metal anode suffers from surface passivation and struggles to effectively plate and strip in conventional Ca electrolytes, making the development of alloy anode for calcium metal battery essential. This work systematically and carefully evaluates the electrochemical formation and feasibility of the Sn anode and its possibility of alloying with Ca using a combination of cyclic voltammetry, scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM/EDS), X-ray diffraction (XRD), and synchrotron transmission X-ray microscopy (TXM). Electrochemical measurements and SEM/EDS analyses indicate apparent Ca alloy formation. However, detailed XRD and TXM characterization reveal substantial lithium-ion involvement when lithium metal is employed as the reference electrode, even in electrolytes with high Ca salt concentrations. These findings highlight a significant risk of misinterpretation: Although limited Ca–Sn alloying may occur, the faster kinetics of Li + can dominate the alloying process, leading to a Li-driven reactions at the Sn anode. In contrast, cells constructed with Ca metal as both reference and counter electrodes exhibit distinct redox features only during the initial cycles, followed by rapid cell failure. The high oxidation currents induce severe Ca passivation, occurring nearly concurrently with Sn dealloying. Overall, this study provides critical insight into the practical limitations and common experimental artifacts associated with Ca metal battery systems and underscores the necessity for rigorous cell design and cautious interpretation when evaluating alloy chemistry in multivalent Ca-based batteries.