Atomic Structural Features of Stacking Faults and Domain Connections in the Li- and Mn-Rich Cathode

Li- and Mn-rich layered oxides (LMRs), a class of earth-abundant materials for rechargeable Li-ion battery cathodes, crystallize into layered structures of two different symmetries: C2/m represented by Li 2 MnO 3 and R$\overline{3}$m represented by LiMn 0.5 Ni 0.5 O 2 . Fundamental questions about how the C2/m and R$\overline{3}$m domains spatially correlate within the same oxide grain and how the C2/m stacking faults arrange themselves when this happens still remain. Here, by using integrated differential phase contrast imaging in scanning transmission electron microscopy (STEM-iDPC), we probe the structural and compositional details of a prototypical, cobalt-free LMR material, 0.3Li 2 MnO 3 •0.7LiMn 0.5 Ni 0.5 O 2 (Li 1.13 Mn 0.57 Ni 0.3 O 2 ). The connection between the C2/m and R$\overline{3}$m domains is found to be abrupt, facilitated by the small lattice mismatch between the two structures. Stacking faults in the C2/m domains feature atomic plane shifting that accommodates stacking sequence changes, which explains why the stacking faults form in a random manner. Furthermore, a local disordering mechanism was identified to correlate with the C2/m stacking faults. Chemically, it is found that Ni coexists with Mn at the transition metal sites within the nominal Li 2 MnO 3 domain. As a result, this study demonstrates that STEM-iDPC is a very useful tool for capturing all the elements in a single image, revealing atomic details on domain connections and stacking faults in the LMRs.

Li-rich and Mn-rich oxides↗

Impact of surface coating on electrochemical and thermal behaviors of a Li-rich Li 1.2 Ni 0.16 Mn 0.56 Co 0.08 O 2 cathode

Lithium-rich layered oxide materials are considered as potential cathode materials for future high-performance lithium-ion batteries (LIBs) owing to their high operating voltage and relatively high specific capacity. However, perceptible issues such as poor rate performance, poor capacity retention, and voltage degradation during cycling need to be improved before the successful commercialization of the material. In this report, zirconia coated Li 1.2 Ni 0.16 Mn 0.56 Co 0.08 O 2 2 = 1.0, 1.5 and 2.0 wt%) materials are synthesized using a sol–gel assisted ball milling approach. A comparison of structural, morphological and electrochemical properties is examined to elucidate the promising role of ZrO 2 coating on the performance of the NMC cathode. A uniform and homogeneous ZrO 2 coating is observed on the surface of NMC particles as evident by TEM elemental mapping images. The ZrO 2 coated NMCs exhibit significantly improved electrochemical performance at a higher C-rate as compared to pristine material. 1.5% ZrO 2 coated NMC demonstrates better cycling stability (95% capacity retention) than pristine NMC (77% capacity retention) after 50 cycles. All ZrO 2 coated NMC materials demonstrated improved thermal stability compared to pristine material. The difference in onset temperature of 2 wt% ZrO 2 coated and pristine NMC is 20 °C. The improved electrochemical performance of ZrO 2 coated NMC can be attributed to the stabilization of its surface structure due to the presence of ZrO 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Perspective—Potential Benefit of Li-Rich Cathode Materials: Reduction of Co and Ni Content Rather than Achievement of Ultra-High Capacities

In the conventional cycling protocol for lithium and manganese rich NMC layered oxides (LMRNMC), the upper cutoff voltage V cut is extended to ~ 4.8, to achieve capacities of similar to 250 mAh g -1 . With this mode of operation, structural rearrangements result in voltage fade upon cycling. Herein, a strategy is proposed to avoid these structural rearrangements based on (a) restricting V cut to values < ~ 4.6 to shut down the bulk instabilities, and (b) application of a (preferably) semi-coherent coating that protects the surface oxygen. The potential benefit of this strategy would be to minimize Co and Ni content, compared to Ni-rich NMC.

25 ENERGY STORAGE↗