Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Hybrid Al Casting + AM Components for Automotive Applications

Although casting Aluminum (Al) alloys is widely used for automotive application, the conventional casting process is showing limitations for modern vehicle production. A hybrid manufacturing method that is capable of fabricating automotive structures with tailored functionality and tuned attributes at a high production rate is proposed in this project, utilizing the merits of conventional casting methods and additive manufacturing (AM) methods. Ford is interested in supplementing conventional casting processes (e.g., shape casting, high pressure die casting) with local modifications to geometry and microstructure using additive manufacturing techniques. Two additive manufacturing methods, wire-arc and laser hot-wire directed energy deposition AM process, were evaluated by deposition of 4043 filler wire onto high-pressure die cast and permanent mold cast Al-Si alloys. The feasibility of this hybrid manufacturing method was determined through trial deposition and evaluation of defects, microstructure, and mechanical properties. Laser hot-wire deposition was found to be beneficial for this application with low porosity, a refined microstructure, and mechanical properties similar to those reported in the literature for 4043. The mechanical properties of the interface between the A356 casting and deposited 4043 were found to be controlled by the weaker deposit material.

36 MATERIALS SCIENCE↗

In Situ Prediction of Microstructure and Mechanical Properties in Laser-Remelted Al-Si Alloys: Towards Enhanced Additive Manufacturing

Laser surface remelting of aluminum alloys has emerged as a promising technique to enhance mechanical properties through refined microstructures. This process involves rapid cooling rates ranging from 10 3 to 10 8 °C/s, which increase solid solubility within aluminum alloys, shifting their eutectic composition to a larger value of silicon content. Consequently, the resulting microstructure combines a strengthened aluminum matrix with silicon fibers. This study focuses on the laser scanning of Al-Si aluminum alloy to reduce the size of aluminum matrix spacings and transform fibrous silicon particles from micrometer to nanometer dimensions. Analysis revealed that the eutectic structure contained 17.55% silicon by weight, surpassing the equilibrium eutectic composition of 12.6% silicon. Microstructure dimensions within the molten zones, termed ‘melt pools’, were extensively examined using Scanning Electron Microscopy (SEM) at intervals of approximately 20 μm from the surface. A notable increase in hardness, exceeding 50% compared to the base plate, was observed in the melt pool regions. Thus, it is exemplified that laser surface remelting introduces a novel strengthening mechanism in the alloy. Moreover, this study develops an in situ method for predicting melt pool properties and dimensions. A predictive model is proposed, correlating energy density and spectral signals emitted during laser remelting with mechanical properties and melt pool dimensions. This method significantly reduces characterization time from days to seconds, offering a streamlined approach for future studies in additive manufacturing.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of the AA7075 Tube Fabricated using Shear Assisted Processing and Extrusion (ShAPE)

Shear Assisted Processing and Extrusion (ShAPE) experimental setup and tooling were adopted for extruding thin-walled AA7075 aluminum tube from as-cast non-homogenized billet material in a single run. The mechanical and microstructural characterizations were performed on the extrudate in the as-extruded condition without subsequent heat treating. It was shown that the ShAPE process developed a significantly refined microstructure with uniform and almost equiaxed grain structure on both hoop and axial cross-sections of the extrudate as well as through the thickness of the material. The pole figures and inverse pole figures of the EBSD data showed an strong shear texture development, and it was found out that axial shear is the dominant deformation mechanism in the regions near the inner surface of the tube, while combined axial and torsional shears are the two dominant modes of deformation near the outer surface of the extrudate. As for the mechanical properties, there was an increase of 150% and 73% in the yield and ultimate strengths of the tube produced using ShAPE process, respectively, and a 18% decrease in maximum uniform plastic elongation compared to the conventionally extruded AA7075-O tube.

Shear Assisted Processing and Extrusion, Friction ↗

Multi analysis of the effect of grain size on the dynamic behavior of microalloyed steels

This study presents some aspects of multiscale analysis and modeling of variously structured materials behavior in quasi-static and dynamic loading conditions. The investigation was performed for two different materials of common application: high strength microalloyed steel (HSLA, X65), and as a reference more ductile material, Ti-IF steel. The MaxStrain technique and one pass hot rolling processes were used to produce ultrafine-grained and coarse-grained materials. The efficiency and inhomogeneity of microstructure refinement were examined because of their important role in work hardening and the initiation and growth of fracture under tensile stresses. It is shown that the combination of microstructures characterized by their different features contributes to the dynamic behavior and final properties of the product. In particular, the role of solute segregation at grain boundaries as well as precipitation of carbonitrides in coarse and ultrafine-grained structures is assessed. The predicted mechanical response of ultrafine-grained structures, using modified KHL model is in reasonable agreement with the experiments. This is a result of proper representation of the role of dislocation structure and the grain boundary and their multiscale effects included in this model.

36 MATERIALS SCIENCE↗

Influence of Rare Earth Ce Additions on Microstructure and Mechanical Properties of Experimental Pipeline Steels

Herein, the effect of Ce additions ranging from 57 to 263 ppm is evaluated for an experimental pipeline steel. Compared to the Ce-free steel, progressive Ce additions result in a slightly refined microstructure, significantly improve transverse impact properties, and slightly increase strength. All these observations can be attributed to the gradual transformation of Mn sulfide and Mn–Si–Al oxide inclusions to Ce-containing oxide/sulfides. In particular, the inclusions consist exclusively of sub-5 μm spherical Ce 2 O 2 S particles upon near-stoichiometric additions of Ce, considering the oxygen and sulfur impurity level of the steel. In conclusion, the results suggest that Ce is a potentially promising alloying addition for next-generation pipeline steels by replacing overtly deleterious inclusions with potentially beneficial ones.

36 MATERIALS SCIENCE↗

Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP)

Thermal stability of the ultra-fine grained (UFG) microstructure of magnesium AZ31 alloy was investigated. UFG microstructure was achieved by a combined two-step severe plastic deformation process: the extrusion (EX) and subsequent equal-channel angular pressing (ECAP). This combined process leads to refined microstructure and enhanced microhardness. Specimens with UFG microstructure were annealed isochronally at temperatures 150–500 °C for 1 h. The evolution of microstructure, mechanical properties and dislocation density was studied by electron backscatter diffraction (EBSD), microhardness measurements and positron annihilation spectroscopy (PAS). The coarsening of the fine-grained structure at higher temperatures was accompanied by a gradual decrease of the microhardness and decrease of dislocation density. Mechanism of grain growth was studied by general equation for grain growth and Arrhenius equation. Activation energies for grain growth were calculated to be 115, 33 and 164 kJ/mol in temperature ranges of 170–210 °C, 210–400 °C and 400–500 °C (443–483 K, 483–673 K and 673–773 K), respectively. - Highlights: • Microhardness of UFG AZ31 alloy decreases with increasing annealing temperature. • This fact has two reasons: dislocation annihilations and/or grain growth. • The activation energies for grain growth were calculated for all temperature ranges.

36 MATERIALS SCIENCE↗

Microstructural characterization in dissimilar friction stir welding between 304 stainless steel and st37 steel

In the present study, 3 mm-thick plates of 304 stainless steel and st37 steel were welded together by friction stir welding at a welding speed of 50 mm/min and tool rotational speed of 400 and 800 rpm. X-ray diffraction test was carried out to study the phases which might be formed in the welds. Metallographic examinations, and tensile and microhardness tests were used to analyze the microstructure and mechanical properties of the joint. Four different zones were found in the weld area except the base metals. In the stir zone of the 304 stainless steel, a refined grain structure with some features of dynamic recrystallization was evidenced. A thermomechanically-affected zone was characterized on the 304 steel side with features of dynamic recovery. In the other side of the stir zone, the hot deformation of the st37 steel in the austenite region produced small austenite grains and these grains transformed to fine ferrite and pearlite and some products of displacive transformations such as Widmanstatten ferrite and martensite by cooling the material after friction stir welding. The heat-affected zone in the st37 steel side showed partially and fully refined microstructures like fusion welding processes. The recrystallization in the 304 steel and the transformations in the st37 steel enhanced the hardness of the weld area and therefore, improved the tensile properties of the joint. - Highlights: Black-Right-Pointing-Pointer FSW produced sound welds between st37 low carbon steel and 304 stainless steel. Black-Right-Pointing-Pointer The SZ of the st37 steel contained some products of allotropic transformation. Black-Right-Pointing-Pointer The material in the SZ of the 304 steel showed features of dynamic recrystallization. Black-Right-Pointing-Pointer The finer microstructure in the SZ increased the hardness and tensile strength.

36 MATERIALS SCIENCE↗

Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing

An Al–10Ce-8Mn (wt%) alloy was designed and fabricated by laser powder bed fusion additive manufacturing (AM). The rapid cooling rates of the AM process produced a refined microstructure with a large fraction of reinforcing intermetallic phases. The tensile properties of the alloy were characterized in the as-fabricated state and following thermal exposure. The properties of the as-fabricated microstructure showed exceptional high-temperature performance and strength retention at elevated temperatures up to 400 °C relative to benchmark wrought Al and AM Al alloy properties. Characterization of the microstructure and thermodynamic modeling of the ternary Al–Ce–Mn system rationalized the solidification and solid-state phase transformations. Finally, analysis of the relevant strengthening mechanisms for both the as-fabricated and thermally exposed conditions was performed.

36 MATERIALS SCIENCE↗

Characterization of Multilayered Multipass Friction Stir Weld on ASTM A572 G50 Steel

A multilayered multipass friction stir weld (MM-FSW) on ASTM A572 Grade 50 steel was characterized to understand its potential application for thick-section structures. The 15-mm-thick section was fabricated by stacking up three steel plates and then friction stir welding the plates together in a total of 5 passes. The unique butt/lap joint configuration encountered in the multilayer weld was examined to understand the effect of tool rotation direction on the joint quality especially the formation of hooking defect. Charpy V-notch impact toughness tests showed generally higher impact toughness energy for the stir zone than the base metal with a ductile fracture mode. The microhardness value was measured from 195 to 220 HV in the stir zone, while the base metal showed an average value of 170 HV. The microstructure in the stir zone and the adjacent heat affected zone was quantified using Optical and Scanning Electron Microscopy (SEM) including Electron Backscatter Diffraction (EBSD). The increased toughness and hardness were correlated with the refined microstructure in stir zone, resulting from severe plastic deformation and subsequent dynamic recrystallization during friction stir welding.

Lim, Yong Chae↗

Microstructures and mechanical properties of compositionally complex Co-free FeNiMnCr 18 FCC solid solution alloy

Recently, a structurally-simple but compositionally-complex FeNiCoMnCr high entropy alloy was found to have excellent mechanical properties (e.g., high strength and ductility). To understand the potential of using high entropy alloys as structural materials for advanced nuclear reactor and power plants, it is necessary to have a thorough understanding of their structural stability and mechanical properties degradation under neutron irradiation. Furthermore, this requires us to develop a similar model alloy without Co because material with Co will make post-neutron-irradiation testing difficult due to the production of the 60 Co radioisotope. In order to achieve this goal, a FCC-structured single-phase alloy with a composition of FeNiMnCr 18 was successfully developed. This near-equiatomic FeNiMnCr 18 alloy has good malleability and its microstructure can be controlled by thermomechanical processing. By rolling and annealing, the as-cast elongated-grained-microstructure is replaced by homogeneous equiaxed grains. The mechanical properties (e.g., strength and ductility) of the FeNiMnCr 18 alloy are comparable to those of the equiatomic FeNiCoMnCr high entropy alloy. Both strength and ductility increase with decreasing deformation temperature, with the largest difference occurring between 293 and 77 K. Extensive twin-bands which are bundles of numerous individual twins are observed when it is tensile-fractured at 77 K. No twin bands are detected by EBSD for materials deformed at 293 K and higher. Ultimately the unusual temperature-dependencies of UTS and uniform elongation could be caused by the development of the dense twin substructure, twin-dislocation interactions and the interactions between primary and secondary twinning systems which result in a microstructure refinement and hence cause enhanced strain hardening and postponed necking.

36 MATERIALS SCIENCE↗

Effect of pre-cold rolling on the evolution of microstructure, microtexture, and mechanical properties of the mushy state rolled in-situ Al-4.5Cu-5TiB2 composite

Highlights: • Microstructure-Microtexture evolution study of the mushy state rolled composite (MRC) and MRC with pre-cold rolling (PCMRC). • The Microstructure and microtexture were characterized using SEM, EBSD, and TEM. • Exactly opposite trends in micro-hardness variation across the thickness of MRC and PCMRC were discussed. • The PCMRC exhibited the best combination of hardness, strength, and ductility. • A proper microstructure-microtexture-property correlation was established with experimental evidence. The mushy state rolling has been found as a promising technique for near-net forming of the cast Al-4.5 wt% Cu-5 wt% TiB{sub 2} in-situ composite to obtain microstructural refinement and moderate mechanical properties. Cold rolling with 30% reduction in thickness was carried out before mushy state rolling, for achieving a relatively more homogeneous distribution of CuAl{sub 2}-TiB{sub 2} particles as well as an appropriate microstructure to enhance the mechanical properties. A comparative investigation on the microstructural and microtextural evolution, along with mechanical properties of both the mushy state rolled composite (MRC) and pre-cold rolled mushy-state rolled composite (PCMRC) was performed, and the microstructure-property correlation was established. The PCMRC exhibited the lowest homogenized lengthscale parameter (L{sub H} 29 μm) indicating the maximum uniformity of particle distribution, computed with the help of multi-scalar analysis of area fractions (MSAAF) technique. Electron back-scattered diffraction (EBSD) and transmission electron microscopy (TEM) studies revealed the presence of fine sub-grains within centrally located deformed Al grains due to dynamic recovery, as well as the particle stimulated nucleation of equiaxed fine Al grains by dynamic recrystallization or rapid solidification of liquid near edges for both the investigated composites. The PCMRC displayed a superior combination of hardness (96.82 ± 4.5 HV{sub 5kgf}), 40% higher ultimate tensile strength (301.4 ± 1.8 MPa), and 68% more uniform elongation (30.8% ± 0.5%), compared to the MRC. The improvement in mechanical properties is attributed to the uniform particle distribution and presence of both higher density of low angle boundaries and recrystallized grains adjacent to the particles, obtained from prior cold rolling.

36 MATERIALS SCIENCE↗

Enhanced strength and ductility of a tungsten-doped CoCrNi medium-entropy alloy

Developing metallic materials with a good combination of strength and ductility has been an unending pursuit of materials scientists. The emergence of high/medium-entropy alloys (HEA/MEA) provided a novel strategy to achieve this. In this work, we also strengthened a strong-and-ductile MEA using a traditional solid solution strengthening theory. The selection of solute elements was assisted by mechanical property and microstructure predictive models. Extensive microstructural characterizations and mechanical tests were performed to verify the models and to understand the mechanical behavior and deformation mechanisms of the designated CoCrNi–3W alloy. Our results show good experiment-model agreement. The incorporation of 3 at.% W into the ternary CoCrNi matrix increased its intrinsic strength by ~20%. External strengthening through microstructural refinement led to a yield strength nearly double that of the parent alloy, CoCrNi. The increase in strength is obtained with still good ductility when tested down to 77 K. Nanoscale twin boundaries are observed in the post-fracture microstructure under 77 K. Finally, the combination of strength and ductility after W additions deviate from the traditional strength-ductility-trade-off contour.

36 MATERIALS SCIENCE↗

Martensitic transformation induced strength-ductility synergy in additively manufactured maraging 250 steel by thermal history engineering

Maraging steels are known for their exceptional strength but suffer from limited work hardening and ductility. Here, in this study, we report an intermittent printing strategy to tailor the microstructure and mechanical properties of maraging 250 steel via tuning the thermal history during wire-arc directed energy deposition. By introducing a dwell time between adjacent layers, the maraging 250 steel is cooled below the martensite start temperature, triggering thermally-driven martensitic transformation during the printing process. Thermal cycling during subsequent layer deposition results in the formation of reverted austenite which shows a refined microstructure and induces elemental segregation between martensite and reverted austenite. The Ni enrichment in the austenite promotes stabilization of the reverted austenite upon cooling to room temperature. The reverted austenite is metastable during deformation, leading to strain-induced martensitic transformation under loading. Specifically, a 3 min interlayer dwell time produces a maraging 250 steel with approximately 8% reverted austenite, resulting in improved work hardening via martensitic transformation induced plasticity during deformation. Meanwhile, the higher cooling rate and refined prior austenite grains lead to substantially refined martensitic grains (by approximately fivefold) together with an increased dislocation density. With 3 min interlayer dwell time, the yield strength of the printed maraging 250 steel increases from 836 MPa to 990 MPa, and the uniform elongation is doubled from 3.2% to 6.5%. This intermittent deposition strategy demonstrates the potential to tune the microstructure of maraging steels for achieving strength-ductility synergy by engineering the thermal history during additive manufacturing.

Additive manufacturing↗

Microstructures and Properties of Medium Manganese Sheet Steels - Strategies and Opportunities

Medium manganese steels, with 3 to 10 wt pct Mn, have been shown to be capable of being thermally-processed to produce sheet products with a variety of strength-ductility combinations and thus are receiving considerable attention as candidates for 3rd generation advanced high strength steels (3GAHSS). The steels typically contain refined microstructures with characteristic microstructural dimensions of 1 to 2 µm and consist of significant amounts of retained austenite in a fine grained ferritic matrix. Strategies for development of medium manganese steels are reviewed and results of recent property predictions based on composite modeling are presented. The importance of controlling austenite stability is illustrated with data on medium Mn (7 and 10 wt pct.), low carbon (0.1 and 0.15 wt pct) steels. Important forming variables (strain, strain rate, and temperature) are discussed, along with a consideration of yield point elongation, present in many medium Mn steels.

36 MATERIALS SCIENCE↗

The role of grain orientation in microstructure evolution of pure aluminum processed by equal channel angular pressing

A new approach describing the role of crystallographic orientation in the microstructural refinement of commercially pure aluminum during the successive passes of equal channel angular pressing (ECAP) is introduced. The study is based on analysis of X-ray diffraction texture data that is used to calculate the geometrical position of crystallographic slip planes with respect to the shearing plane of the ECAP die. The angular deviations of {l_brace}111{r_brace} slip planes from the macroscopic deformation plane for different processing routes were calculated and compared. The microstructure evolution was investigated using electron back-scattered diffraction (EBSD). The grain size and grain boundary character distribution obtained for each processing route are related to the angles between {l_brace}111{r_brace} planes and the shearing plane. It was shown that the more effective routes in grain refinement have higher angles between {l_brace}111{r_brace} slip planes and the shearing plane. - Research Highlights: {yields} The grain refinement of commercially pure aluminum during ECAP highly depends on the processing routes. {yields} The differences between the processing routes could be explained by the crystallographic orientations of the grains which become parallel to the shearing plane and direction. {yields} Texture results could be used to calculate the angle between the slip planes of the grains and the shearing plane of the ECAP die. {yields} The routes making higher angles between {l_brace}111{r_brace} planes and the shearing plane result in better grain refinement during the process.

36 MATERIALS SCIENCE↗

Microstructural and Property Evolution of Continuous Columnar-Grained Polycrystalline Copper during Extreme Plastic Deformation at Room Temperature

An extreme extensibility with a true strain of 11.12 has been obtained for continuous columnar-grained (CCG) polycrystalline copper at room temperature, which was cold-drawn from a 10-mm-diameter as-cast rod into a 38.5-μm-diameter ultra-fine wire without any intermediate softening heat treatment. During the extreme plastic deformation, the ultimate tensile stress increased from 140 MPa for as-cast CCG copper to 525 MPa for the deformed sample at a true stain of 11.12, while the relative electrical conductivity maintained a high value of 97.6% IACS. On this basis, CCG copper is an excellent raw material for the fabrication of ultra-fine wires with both high strength and high electrical conductivity. The original columnar grains experienced grain subdivision and formed fibrous grains along the drawing direction with a fibrous longitudinal morphology and curly transverse microstructure at medium to high strain. The subdivision of the fibrous grains then went on as the extreme plastic deformation continued. Large amounts of strain-induced boundaries and microstructural refinement facilitated the storage of abundant glide dislocations created by extreme plastic deformation. Thus, extreme plastic extensibility can be achieved through continuous work hardening of CCG copper.

36 MATERIALS SCIENCE↗

Thermo-mechanical behavior of hypoeutectic Ni-Y-Zr alloys

Microstructure refinement and optimized alloying can improve metallic alloy performance: stable nanocrystalline (NC) alloys with immiscible second phases, e.g., Cu-Ta, are stronger than unstable NC alloys and their coarse-grained (CG) counterparts, but higher melting point matrices are needed. Hypoeutectic, CG Ni-Y-Zr alloys were produced via arc-melting to explore their potential as high-performance materials. Microstructures were studied to determine phases present, local composition and length scales, while heat treatments allowed investigating microstructural stability. Alloys had a stable, hierarchical microstructure with ~250 nm ultrafine eutectic, ~10 µm dendritic arm spacing and ~1 mm grain size. Hardness and uniaxial compression tests revealed that mechanical properties of Ni-0.5Y-1.8Zr (in wt%) were comparable to Inconel 617 despite the small alloying additions, due to its hierarchical microstructure. Here, uniaxial compression at 600 °C showed that ternary alloys outperformed Ni-Zr and Ni-Y binary alloys in flow stress and hardening rates, which indicates that the Ni 17 Y 2 phase was an effective reinforcement for the eutectic, which supplemented the matrix hardening due to increased solubility of Zr. Results suggest that ternary Ni-Y-Zr alloys hold significant promise for high temperature applications.

36 MATERIALS SCIENCE↗