Perfluoro Aryl Boronic Esters as Chemical Shuttle Additives in Lithium Ion Batteries

Redox shuttles could provide an added measure of control for lithium ion batteries beyond that which is provided by the battery management system. Redox shuttles, which are electrolyte additives, provide electrochemical overcharge protection. Since they possess a reduction-oxidation potential that is slightly above the maximum cathode potential during normal use, they should cause no degradation in cell performance during normal operation, but should shuttle excess electrons during overcharge conditions, effectively limiting the full cell voltage. The goals of the Chemical Shuttle Additives program were to discover and implement a redox shuttle that is compatible with large format lithium ion cells utilizing LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NMC) cathode material and to understand the mechanism of redox shuttle action. Many redox shuttles, both commercially available and experimental, were tested and much fundamental information regarding the mechanism of redox shuttle action was discovered. In particular, studies surrounding the mechanism of the reduction of the oxidized redox shuttle at the carbon anode surface were particularly revealing. Shuttles that were evaluated in various lithium ion cell chemistries include: • 2-(pentafluorophenyl)-tetrafluoro-1,3,2-benzodioxaborole (BDB) supplied by Argonne National Laboratory (ANL), Lemont, Illinois; • 2,5-di-tert-butyl-1,4-dimethoxybenzene (DDB) supplied by 3M, St. Paul, Minnesota; • Li 2 B 12 F 12 supplied by Air Products, Allentown, Pennsylvania (pure compound) and Showa Denko, Japan (in electrolyte); • 1,4-bis(2-methoxyethoxy)-2,5-di-tert-butyl-benzene (ANL-RS2) supplied by Argonne National Laboratory (ANL), Lemont, Illinois; and • A 4.5V class redox shuttle supplied by Argonne National Laboratory (ANL), Lemont, Illinois Although redox shuttles with an appropriate redox potential and sufficient chemical and electrochemical stability for cells utilizing cathodes with potentials higher and lower than that of NMC, a redox shuttle that is viable for use in large format lithium ion cells with NMC cathodes was not found. The effect of the anode on the capacity loss of lithium ion cells with redox shuttles in cells utilizing lithium, lithium titanate, or graphite cells was studied. Molecular imprinting of the redox shuttle molecule during solid electrolyte interphase (SEI) layer formation likely contributes to the successful reduction of oxidized redox shuttle species at carbon anodes. This helps understand how a carbon anode covered with an SEI layer, that is supposed to be electrically insulating, can reduce the oxidized form of a redox shuttle.

25 ENERGY STORAGE↗

A Comparative Study of Degradation Behaviors of LiFePO 4 , LiMn 2 O 4 , and LiNi 0.8 Mn 0.1 Co 0.1 O 2 in Different Aqueous Electrolytes

Aqueous Li-ion batteries (ALIBs) are an important class of battery chemistries owing to the intrinsic non-flammability of aqueous electrolytes. However, water is detrimental to most cathode materials and could result in rapid cell failure. Identifying the degradation mechanisms and evaluating the pros and cons of different cathode materials are crucial to guide the materials selection and maximize their electrochemical performance in ALIBs. Here, in this study, we investigate the stability of LiFePO 4 (LFP), LiMn 2 O 4 (LMO) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC) cathodes, without protective coating, in three different aqueous electrolytes, i.e., salt-in-water, water-in-salt, and molecular crowding electrolytes. The latter two are the widely reported "water-deficient electrolytes." LFP cycled in the molecular crowding electrolyte exhibits the best cycle life in both symmetric and full cells owing to the stable crystal structure. Mn dissolution and surface reduction accelerate the capacity decay of LMO in water-rich electrolyte. On the other hand, the bulk structural collapse leads to the degradation of NMC cathodes. LMO demonstrates better full-cell performance than NMC in water-deficient aqueous electrolytes. LFP is shown to be more promising than LMO and NMC for long-cycle-life ALIB full cells, especially in the molecular crowding electrolyte. However, none of the aqueous electrolytes studied here provide enough battery performance that can compete with conventional non-aqueous electrolytes. This work reveals the degradation mechanisms of olivine, spinel, and layered cathodes in different aqueous electrolytes and yields insights into improving electrode materials and electrolytes for ALIBs.

36 MATERIALS SCIENCE↗

Promising performance of sulfide catholytes compared to halide alternatives in NMC811 cathodes for sheet-type sulfide solid-state batteries

Sulfide-based solid-state batteries (SSBs) show promise in achieving energy densities over 350 Wh/kg, yet challenges persist with their incorporation of high-voltage, nickel-rich layered oxide cathodes, such as LiNi₀.₈Mn₀.₁Co₀.₁O₂ (NMC811), due to the poor oxidation stability of sulfide solid-state electrolytes (SSEs) like Li₆PS₅Cl (LPSCl). Although halide SSEs such as Li₃InCl₆ (LIC) and Li₃YCl₆ (LYC) have previously shown promise in stabilizing high-voltage NMC cathodes, our research reveals that sulfide SSE catholytes, particularly when combined with surface-coated NMC cathodes, deliver superior performance. Here, this investigation assesses the cycling stability of various catholytes—LPSCl, LIC, Li₁₀GeP₂S₁₂ (LGPS), combined LIC-LPSCl, and LYC-LPSCl—in SSBs with LiNbO₃-coated NMC811 cathodes against sheet-type LPSCl separators. Findings indicate that while LGPS-based cathodes maintain higher capacity retention, they yield lower deliverable capacity, and LIC cathodes experience significant electrochemical degradation. Importantly, our results underscore that sulfide SSE catholytes, in conjunction with LiNbO₃-coated cathodes, optimize the cathode-electrolyte interphase (CEI), enhancing both kinetics and mass transport. These insights provide a strategic direction for optimizing catholyte composition in the development of sheet-type sulfide-based SSBs.

Catholyte↗

Electron Delocalization Enables Sulfone-based Single-solvent Electrolyte for Lithium Metal Batteries

Li-metal batteries (LMB), although providing high energy density, face the grand challenge of identifying good electrolyte solvents for cycling. Common solvents are either only stable against lithium metal anode or only stable against LiNi x MnyCo 1-x-y O 2 (NMC) cathode. There is significant effort trying to increase the cathode stability for ether electrolytes, which are in general stable against lithium metal anode. In comparison, there is much less effort trying to increase the anode stability of electrolytes that are stable against NMC cathode. One example is the sulfone-based electrolyte. It has good cathode stability but is hindered from practical application because of (1) high viscosity and poor wetting capability and (2) poor anode stability. Here, we solve these issues by modifying the sulfone molecules using resonance and electron withdrawing effect. The viscosity is significantly reduced by delocalizing the electrons through introducing additional oxygen on the molecular backbone and applying appropriate fluorination. The resulting molecule 2,2,2-trifluoroethyl mesylate (TFEM) has decreased Lewis basicity and less reactivity toward Li + . In conclusion, the electrolyte based on TFEM as single solvent enables cycling of LMB under harsh conditions of low N/P ratio (21 mg/cm 2 NMC811 and 50 μm Li) with 90 % capacity retention after 160 cycles at C/3 discharge rate.

25 ENERGY STORAGE↗

Electron Delocalization Enables Sulfone-based Single-solvent Electrolyte for Lithium Metal Batteries

Li-metal batteries (LMB), although providing high energy density, face the grand challenge of identifying good electrolyte solvents for cycling. Common solvents are either only stable against lithium metal anode or only stable against LiNi x Mn y Co 1-x-y O 2 (NMC) cathode. There is significant effort trying to increase the cathode stability for ether electrolytes, which are in general stable against lithium metal anode. In comparison, there is much less effort trying to increase the anode stability of electrolytes that are stable against NMC cathode. One example is the sulfone-based electrolyte. It has good cathode stability but is hindered from practical application because of (1) high viscosity and poor wetting capability and (2) poor anode stability. Here, we solve these issues by modifying the sulfone molecules using resonance and electron withdrawing effect. The viscosity is significantly reduced by delocalizing the electrons through introducing additional oxygen on the molecular backbone and applying appropriate fluorination. The resulting molecule 2,2,2-trifluoroethyl mesylate (TFEM) has decreased Lewis basicity and less reactivity toward Li + . The electrolyte based on TFEM as single solvent enables cycling of LMB under harsh conditions of low N/P ratio (21 mg/cm 2 NMC811 and 50 μm Li) with 90 % capacity retention after 160 cycles at C/3 discharge rate.

25 ENERGY STORAGE↗

High–Nickel NMA: A Cobalt–Free Alternative to NMC and NCA Cathodes for Lithium–Ion Batteries

High-nickel LiNi 1–x–y Mn x Co y O 2 (NMC) and LiNi 1–x–y Co x Al y O 2 (NCA) are the cathode materials of choice for next-generation high-energy lithium-ion batteries. Both NMC and NCA contain cobalt, an expensive and scarce metal generally believed to be essential for their electrochemical performance. Herein, a high-Ni LiNi 1–x–y Mn x Al y O 2 (NMA) cathode of desirable electrochemical properties is demonstrated benchmarked against NMC, NCA, and Al–Mg-codoped NMC (NMCAM) of identical Ni content (89 mol%) synthesized in-house. Despite a slightly lower specific capacity, high-Ni NMA operates at a higher voltage by ≈40 mV and shows no compromise in rate capability relative to NMC and NCA. In pouch cells paired with graphite, high-Ni NMA outperforms both NMC and NCA and only slightly trails NMCAM and a commercial cathode after 1000 deep cycles. Further, the superior thermal stability of NMA to NMC, NCA, and NMCAM is shown using differential scanning calorimetry. Here, considering the flexibility in compositional tuning and immediate synthesis scalability of high-Ni NMA very similar to NCA and NMC, this study opens a new space for cathode material development for next-generation high-energy, cobalt-free Li-ion batteries.

25 ENERGY STORAGE↗

Simultaneous Stabilization of LiNi 0.76 Mn 0.14 Co 0.10 O 2 Cathode and Lithium Metal Anode by Lithium Bis(oxalato)borate as Additive

Abstract The long‐term cycling performance, rate capability, and voltage stability of lithium (Li) metal batteries with LiNi 0.76 Mn 0.14 Co 0.10 O 2 (NMC76) cathodes is greatly enhanced by lithium bis(oxalato)borate (LiBOB) additive in the LiPF 6 ‐based electrolyte. With 2 % LiBOB in the electrolyte, a Li∥NMC76 cell is able to achieve a high capacity retention of 96.8 % after 200 cycles at C/3 rate (1 C=200 mA g −1 ), which is the best result reported for a Ni‐rich NMC cathode coupled with Li metal anode. The significantly enhanced electrochemical performance can be ascribed to the stabilization of both the NMC76 cathode/electrolyte and Li‐metal‐anode/electrolyte interfaces. The LiBOB‐containing electrolyte not only facilitates the formation of a more compact solid–electrolyte interphase on the Li metal surface, it also forms a enhanced cathode electrolyte interface layer, which efficiently prevents the corrosion of the cathode interface and mitigates the formation of the disordered rock‐salt phase after cycling. The fundamental findings of this work highlight the importance of recognizing the dual effects of electrolyte additives in simultaneously stabilizing both cathode and anode interfaces, so as to enhance the long‐term cycle life of high‐energy‐density battery systems.

Zhao, Wengao↗

Value-creating upcycling of retired electric vehicle battery cathodes

The electrification revolution in the automobile and other industries demands annual production capacity of batteries of at least 10 2 GWh, which presents a twofold challenge: supply of key materials such as cobalt and nickel and recycling when batteries are retired from use. Pyrometallurgical and hydrometallurgical recycling are currently used in industry but suffer from complexity, high costs, and secondary pollution. Here we report a molten-salt-based method for direct recycling (MSDR) that is environmentally benign and creates value on the basis of a techno-economic analysis using real-world data and price information. We also experimentally demonstrate the feasibility of MSDR by upcycling a low-nickel polycrystalline LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC) cathode material into Ni-rich (Ni > 65%) single-crystal NMCs with increased energy density (>10% increase) and outstanding electrochemical performance (>94% capacity retention after 500 cycles). This work may open opportunities for closed-loop recycling of electric vehicle batteries and manufacturing of next-generation NMC cathode materials.

25 ENERGY STORAGE↗

Cabs Milestone I3 Report: Demonstration of Ability to Construct 3D Meshes of Electrodes Using Reconstructions from Micro-Tomography

Mesoscale (100s of particles) electrochemical-thermal-mechanical models and simulations of NMC cathodes are a critical outcome of the CABS project. These simulations require mesostructure geometries and commensurate computational meshes on which to perform the simulations. While these geometries can be generated using a variety of methods, the highest-fidelity approach is to reconstruct the geometry directly from 3D experimental data/measurements. In this milestone report, we demonstrate our ability to create 3D computational meshes using the Conformal Decomposition Finite Element Method (CDFEM) on a selection of NMC cathodes that were imaged using X-Ray Computed Micro-Tomography (X-Ray CT, or simply XCT).

97 MATHEMATICS AND COMPUTING↗

High-Energy and High-Power NMP-Free, Designer NMC 811 Cathodes with Ultra-Thick Architectures Processed by Electrophoretic Deposition

This project focused on electrode engineering and reducing the weight of inactive components in the battery cells. Additionally, the project focused on optimizing the ‘electrophoretic deposition’ technique developed by PPG industries for aqueous processing of electrodes. During this project team has screened several binders suitable for electrophoretic deposition of electrodes. Additionally, we developed a nice strategy to deposit a low cost and scalable oxide coating on the surface of cathode materials. ORNL team performed the research under this CRADA at DOE’s Battery Manufacturing Facility (BMF) at ORNL.

99 GENERAL AND MISCELLANEOUS↗

High-Energy and High-Power NMP-Free, Designer NMC 811 Cathodes with Ultra-Thick Architectures Processed by Electrophoretic Deposition

This project focused on electrode engineering and reducing the weight of inactive components in the battery cells. Additionally, the project focused on optimizing the ‘electrophoretic deposition’ technique developed by PPG industries for aqueous processing of electrodes. During this project team has screened several binders suitable for electrophoretic deposition of electrodes. Additionally, we developed a nice strategy to deposit a low cost and scalable oxide coating on the surface of cathode materials. ORNL team performed the research under this CRADA at DOE’s Battery Manufacturing Facility (BMF) at ORNL.

25 ENERGY STORAGE↗

High capacity and stable cathode materials

High energy density cathode materials, such as LiNiXMnYCoZO2 (NMC) cathode materials, with improved discharge capacity (hence energy density) and enhanced cycle life are described. A solid electrolyte, such as lithium phosphate infused inside of secondary particles of the cathode material demonstrates significantly enhanced structural integrity without significant or without any observable particle cracking occurring during charge/discharge processes, showing high capacity retention of more than 90% after 200 cycles at room temperature. In certain embodiments the disclosed cathode materials (and cathodes made therefrom) are formed using nickel-rich NMC and/or are used in a battery system with a non-aqueous dual-Li salt electrolytes.

25 ENERGY STORAGE↗

High capacity and stable cathode materials

High energy density cathode materials, such as LiNixMnyCozO2 (NMC) cathode materials, with improved discharge capacity (hence energy density) and enhanced cycle life are described. A solid electrolyte, such as lithium phosphate infused inside of secondary particles of the cathode material demonstrates significantly enhanced structural integrity without significant or without any observable particle cracking occurring during charge/discharge processes, showing high capacity retention of more than 90% after 200 cycles at room temperature. In certain embodiments the disclosed cathode materials (and cathodes made therefrom) are formed using nickel-rich NMC and/or are used in a battery system with a non-aqueous dual-Li salt electrolytes.

25 ENERGY STORAGE↗

Suppressed oxygen extraction and degradation of LiNixMnyCozO2 cathodes at high charge cut-off voltages

The capacity degradation mechanism in lithium nickel-manganese-cobalt oxide (NMC) cathodes (LiNi1/3Mn1/3Co1/3O2 (NMC333) and LiNi0.4Mn0.4Co0.2O2 (NMC442)) during high-voltage (cut-off of 4.8 V) operation has been investigated. In contrast to NMC442, NMC333 exhibits rapid structural changes including severe micro-crack formation and phase transformation from a layered to a disordered rock-salt structure, as well as interfacial degradation during high-voltage cycling, leading to a rapid increase of the electrode resistance and fast capacity decline. The fundamental reason behind the poor structural and interfacial stability of NMC333 was found to be correlated to its high Co content and the significant overlap between the Co3+/4+ t(2g) and O2- 2p bands, resulting in oxygen removal and consequent structural changes at high voltages. In addition, oxidation of the electrolyte solvents by the extracted oxygen species generates acidic species, which then attack the electrode surface and form highly resistive LiF. These findings highlight that both the structural and interfacial stability should be taken into account when tailoring cathode materials for high voltage battery systems

Environmental Molecular Sciences Laboratory↗

Stabilizing Ni-rich layered cathode for high-voltage operation through hierarchically heterogeneous doping with concentration gradient

High-nickel LiNi x Mn y Co 1-x-y O 2 (NMC) cathodes have demonstrated superior energy density, yet their stability is compromised under high voltage conditions. To address this, here we propose a strategy of heterogeneous doping with a concentration gradient, specifically through Sr–Zr co-modification. We synthesized Ni-rich NMC particles featuring several micron-sized secondary particles composed of micron-sized primary grains. This design aims to harness the structural robustness of single-crystalline grains and the favorable diffusion kinetics of polycrystalline secondary particles. Systematic characterization using a combination of electrochemical measurements and synchrotron analytics reveals an intriguing pattern of hierarchically heterogeneous Sr–Zr co-doping. It demonstrates a depth-dependent concentration gradient at the secondary particle level and competing dopant segregation over the buried grain boundaries. This unique characteristic creates opportunities for enhancing battery performance, particularly by optimizing precursors and implementing advanced modulation techniques. We also investigate the dissolution and precipitation of the cathode's transition metal cations upon high-voltage cycling. These insights suggest that a tailored compositional variation can be a viable approach to effectively design the next-generation high-Ni NMC cathode materials for high-voltage lithium batteries.

36 MATERIALS SCIENCE↗