At least 73 records · Page 4

Improved oxidation-resistant carbon and graphite materials

A variety of silicon-carbide treated carbon and graphite products were prepared, and oxidation and strength properties determined. Carbon and graphite materials used in the preliminary study include fiber, tape, felt, foam, bulk, and laminar configurations. The silicon-carbide treatment used in preparing the oxidation resistant specimens employs either vacuum or ultrasonic impregnation of various silicone-silicon mixtures into the matrix material. The impregnation phase is followed by controlled thermal reaction at which time the silicon carbide is synthesized and takes the form of an integral protective boundary layer. Thickness of the layer ranges from a fraction of a mil to 10 mils, depending on the matrix material and processing parameters. Oxidation resistance of all the silicon-carbide-treated specimens investigated was found to be significantly improved. Mechanical strengths of the laminar composites were also found to be somewhat improved. At room temperature the specific strength of the silicon-carbide treated fibers and tapes was degraded to some extent; however, their relative strengths were significantly increased at elevated temperatures in oxidizing atmosphere.

Muir, H. M.↗

The Effect of Hydrogen Annealing on the Oxidation Resistance of Four EPM Single Crystal Superalloys

Four single crystal EPM (enabling propulsion materials) developmental airfoil superalloys were hydrogen annealed at 1300 C for up to 100 hours to remove sulfur and improve oxidation resistance. Although the 1100 and 1150 C cyclic oxidation resistance was remarkably improved by annealing for 24 or 100 hours, the behavior was still considerably inferior to that of commercially available single crystal superalloys, especially those that are either Y-doped or hydrogen annealed. Excessive degradation in the developmental alloys appeared to be correlated with low Cr contents and, to a lesser extent, high Co and Re contents.

Smialek, James L.↗

Cyclic oxidation resistance of a reaction milled NiAl-AlN composite

Based upon recent mechanical property tests a NiAl-AlN composite produced by cryomilling has very attractive high temperature strength. This paper focuses on the oxidation resistance of the NiAl-AlN composite at 1473 and 1573 K as compared to that of Ni-47Al-0.15Zr, one of the most oxidation resistant intermetallics. The results of cyclic oxidation tests show that the NiAl-AlN composite has excellent properties although not quite as good as those of Ni-47Al-0.15Zr. The onset of failure of the NiAl-AlN was unique in that it was not accompanied by a change in scale composition from alumina to less protective oxides. Failure in the composite appears to be related to the entrapment of AlN particles within the alumina scale.

Lowell, Carl E.↗

ZrB{sub 2}-SiC-Ta{sub 4}HfC{sub 5}/Ta{sub 4}HfC{sub 5} Oxidation-Resistant Dual-Layer Coating Fabricated by Spark Plasma Sintering for C/C Composites

In this work, a ZrB{sub 2}-SiC-Ta{sub 4}HfC{sub 5}/Ta{sub 4}HfC{sub 5} oxidation-resistant dual-layer coating was fabricated to improve the oxidation resistance of carbon–carbon (C/C) composites. The coating was prepared by pack cementation combined with the slurry paste method. Spark plasma sintering was used in the procedure. The as-prepared dual-layer coating was approximately 110 μm, and no distinct interface was observed between the coating and the matrix. The isothermal oxidation test results showed that the dual coating effectively prevented C/C composites from oxidizing. The weight loss of the coated samples was only 3.3 and 9.5% after oxidation at 1773 K for 20 h and ten thermal shock cycles between 1773 K and room temperature in air, respectively. The pores and microcracks were the main reason for the failure of the coating.

36 MATERIALS SCIENCE↗

Ceramic reinforced zirconium alloy nuclear fuel cladding with intermediate oxidation resistant layer

The invention relates to compositions and methods for coating a zirconium alloy (e.g., ceramic-containing) cladding tube for use with fuel rods in a nuclear water reactor. The coating includes an intermediate oxidation resistant layer and a SiC containing layer at least partially deposited on the intermediate oxidation resistant layer. The SiC containing layer can include a plurality of fibers. The SiC containing layer may also be on the outer surface of end plugs. The invention provides improved capability for the zirconium alloy cladding to withstand normal and accident conditions in the nuclear water reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Silicon carbide as an oxidation-resistant high-temperature material. 1: Oxidation and heat corrosion behavior

The oxidation and corrosion behavior of SiC (in the form of a SiC powder) and hot-pressed and reaction-bound material were studied. The excellent stability of SiC in an oxidizing atmosphere is due to the development of protective SiO2 coatings. Any changes in these protective layers (e.g., due to impurities, reaction with corrosive media, high porosity of SiC, etc.) lead in most cases to increased rates of oxidation and thus restrict the field of SiC application.

Schlichting, J.↗

The cyclic oxidation resistance at 1200 C of beta-NiAl, FeAl, and CoAl alloys with selected third element additions

The intermetallic compounds Beta-NiAl, FeAl, and CoAl were tested in cyclic oxidation with selected third element alloy additions. Tests in static air for 200 1-hr cycles at 1200 C indicated by specific weight change/time data and x-ray diffraction analysis that the 5 at percent alloy additions did not significantly improve the oxidation resistance over the alumina forming baseline alloys without the additions. Many of the alloy additions were actually deleterious. Ta and Nb were the only alloy additions that actually altered the nature of the oxide(s) formed and still maintained the oxidation resistance of the protective alumina scale.

Barrett, C. A.↗

High Temperature Thermal Stability and Oxidation Resistance of Magnetron-sputtered Homogeneous CrAlON Coatings on 430 Steel

The requirements of low cost and high-temperature corrosion resistance for bipolar interconnect plates in solid oxide fuel cell stacks has directed attention to the use of metal plates with oxidation resistant coatings. We have investigated the performance of steel plates with homogenous coatings of CrAlON (oxynitrides). The coatings were deposited using RF magnetron sputtering, with Ar as a sputtering gas. Oxygen in these coatings was not intentionally added. Oxygen might have come through contaminated nitrogen gas bottle, leak in the chamber or from the partial pressure of water vapors. Nitrogen was added during the growth process to get oxynitride coating. The Cr/Al composition ratio in the coatings was varied in a combinatorial approach. The coatings were subsequently annealed in air for up to 25 hours at 800 deg. C. The composition of the coated plates and the rate of oxidation were characterized using Rutherford backscattering (RBS) and nuclear reaction analysis (NRA). From our results, we conclude that Al rich coatings are more susceptible to oxidation than Cr rich coatings.

36 MATERIALS SCIENCE↗

High-Sensitivity Low-Energy Ion Spectroscopy with Sub-Nanometer Depth Resolution Reveals Oxidation Resistance of MoS 2 Increases with Film Density and Shear-Induced Nanostructural Modifications of the Surface

For decades, density has been attributed as a critical aspect of the structure of sputter-deposited nanocrystalline molybdenum disulfide (MoS 2 ) coatings impacting oxidation resistance and wear resistance. Despite its importance, there are few examples in the literature that explicitly investigate the relationship between the density and oxidation behaviors of MoS 2 coatings. Aging and oxidation are primary considerations for the use of MoS 2 coatings in aerospace applications as they inevitably experience prolonged storage in water and oxygen-rich environments prior to use. Oxidation that is either limited to the first few nanometers or through the bulk of the coating can result in seizure due to high initial coefficients of friction or component failure from excessive wear. High-sensitivity low-energy ion spectroscopy (HS-LEIS) and Rutherford backscattering spectrometry (RBS) are both used to understand the extent of oxidation throughout the first ~10 nanometers of the surface of pure sputtered nanocrystalline MoS 2 coatings after high-temperature aging and how it is impacted by the density of coatings as measured by RBS. Results show that low-density coatings (ρ = 3.55 g/cm 3 ) exhibit a more columnar microstructure and voiding, which act as pathways for oxidative species to penetrate and interact with edge sites, causing severe surface and subsurface oxidation. Furthermore, HS-LEIS of surfaces sheared prior to oxidation reveals that the oxidation resistance of low-density MoS 2 coatings can be significantly improved by shear-induced reorientation of the surface microstructure to a basal orientation and elimination of pathways for oxygen into the bulk through compaction of surface and subsurface voids.

36 MATERIALS SCIENCE↗

Overcoming the thermal conductivity versus oxidation resistance barrier in high-temperature steels

Heat-resistant steels with high chromium additions (≥5 weight percent) are critical for many high temperature energy and manufacturing applications, including heat exchangers, pistons for engines, and dies for metal working and casting. However, while high chromium additions increase oxidation resistance at elevated temperatures, they also compromise thermal conductivity, resulting in a metallurgical trade-off between these two important properties. Here we show that a microstructure with both higher thermal conductivity and improved oxidation resistance at elevated temperatures is achieved in a unique steel with only 1 weight percent chromium, thereby overcoming the long-standing metallurgical trade-off. This is accomplished through a tailored thermal treatment that produces a tempered martensitic matrix with low solute content and a fine dispersion of copper precipitates and molybdenum enriched carbides. A further discovery is that the resultant thermally grown oxide includes an iron-copper-manganese-enriched outer layer that provides high-temperature oxidation protection equivalent to heat-resistant steels with five times the chromium content and 25% lower thermal conductivity.

Pierce, Dean T. [Oak Ridge National Laboratory (OR↗

Oxidation Resistance and Critical Sulfur Content of Single-Crystal Superalloys

The high-temperature components of a jet turbine engine are made from nickel-base superalloys. These components must be able to withstand high stresses, fatigue, and corrosive reactions with high-temperature gases. Such oxidation resistance is associated with slow-growing Al2O3 scales that remain adherent to superalloy components after many thermal cycles. Historically, good oxidation resistance has been obtained by coating these components with Ni-Cr-Al-Y coatings, where small additions of yttrium (Y) were necessary for scale adhesion. Subsequently, it was found that the Y aids scale adhesion by preventing sulfur from segregating to the scale metal interface and thus preventing the sulfur from weakening the oxide-metal bonds. Y is a difficult element to incorporate in single-crystal superalloy castings, but it was shown in early work at the NASA Lewis Research Center that good adhesion could be obtained for low-sulfur, uncoated, singlecrystal superalloys, without Y additions. Low sulfur contents for these uncoated superalloys were achieved in the laboratory by a high-temperature hydrogen annealing process. This process allows segregation and surface cleaning of sulfur monolayers in a reducing environment. Another approach is to remove sulfur from the alloy in the melting process. The present study was designed to establish a guideline for the minimum level of desulfurization needed to achieve maximum performance. Coupons of various thicknesses of the superalloy PWA 1480 were hydrogen annealed at various times (8 to 100 hr) and temperatures (1000 to 1300 C), resulting in coupons with sulfur contents ranging from about 0.05 to 5 ppm. Cyclic oxidation tests at 1100 C were then used to assess adhesion and spalling. The weight change of one set of 20-mil (0.5-mm) samples, annealed for 20 hr at 1000, 1100, 1200, and 1300 C, is shown in the following figure. Clearly, the effect of the annealing temperature is quite dramatic in that the higher temperatures produced scales that spalled very little, whereas the lower temperatures resulted in severe weight losses comparable to those for the as-received, unannealed sample.

Smialek, James L.↗

Oxidation Resistant, Cr Retaining, Electrically Conductive Coatings on Metallic Alloys for SOFC Interconnects

This report describes significant results from an on-going, collaborative effort to enable the use of inexpensive metallic alloys as interconnects in planar solid oxide fuel cells (SOFCs) through the use of advanced coating technologies. Arcomac Surface Engineering, LLC, under the leadership of Dr. Vladimir Gorokhovsky, is investigating filtered-arc and filtered-arc plasma-assisted hybrid coating deposition technologies to promote oxidation resistance, eliminate Cr volatility, and stabilize the electrical conductivity of both standard and specialty steel alloys of interest for SOFC metallic interconnect (IC) applications. Arcomac has successfully developed technologies and processes to deposit coatings with excellent adhesion, which have demonstrated a substantial increase in high temperature oxidation resistance, stabilization of low Area Specific Resistance values and significantly decrease Cr volatility. An extensive matrix of deposition processes, coating compositions and architectures was evaluated. Technical performance of coated and uncoated sample coupons during exposures to SOFC interconnect-relevant conditions is discussed, and promising future directions are considered. Cost analyses have been prepared based on assessment of plasma processing parameters, which demonstrate the feasibility of the proposed surface engineering process for SOFC metallic IC applications.

30 DIRECT ENERGY CONVERSION↗

Enhanced steam oxidation resistance of uranium nitride nuclear fuel pellets

Here, the steam oxidation resistance of UN and UN-(20 vol%)ZrN fuel pellets is evaluated to enhance understanding of steam corrosion mechanisms in advanced nuclear fuel materials. In situ neutron diffraction shows the modified UN fuel pellets form a (U 0.77 ,Zr 0.23 )N solid-solution and the sole crystalline oxidation product detected in bulk is (U 0.77 ,Zr 0.23 )O 2 . U 2 N 3 is not detected in significant quantities during the steam oxidation of UN or (U 0.77 ,Zr 0.23 )N and stable lattice parameters show that hydriding does not take place. Steam oxidation rates, obtained via sequential Rietveld refinement show how (U 0.77 ,Zr 0.23 )N has a higher activation energy (79 ± 1 kJmol -1 vs. 50 ± 5 kJmol -1 ), higher onset temperature (430 °C vs. 400 °C) and slower reaction rates for steam oxidation up to 616 °C, than pure UN. Throughout, both UN and (U 0.77 ,Zr 0.23 )N exhibit linear (non-protective) oxidation kinetics, signifying that degradation of the fuel pellets is caused by the evolution of gaseous products at the interface followed by oxide scale spallation. This quantitative and mechanistic understanding of material degradation enables better defined operating regimes and points towards (U,Zr)N solid solutions as a promising strategy for the design of advanced nuclear fuel materials with enhanced steam corrosion resistance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗