Thermodynamics and kinetics of reactions in protective coating systems
Investigations of fluoride activated packs with Al:Ni ratios greater than 50 a/o prove that the specimen surface is not in equilibrium with the pack at high Al:Ni ratios but that an activity gradient exists between pack and specimen. Therefore, gaseous diffusion and possibly surface reactions play a role in determining the overall rate of Al deposition in such packs. Noticeable differences in coating behavior have been obtained in packs activated with chloride and iodide, and it appears that poorest results are obtained with iodides, better with chlorides, and best with fluorides. A numerical method has been perfected for calculating rates of solid-state diffusion controlled coating formation, allowing for the variation of diffusivity with composition in the NiAl phase. Layer growth rates can now be accurately predicted from a knowledge of the surface and substrate compositions. Furthermore, the correct diffusion profiles are obtained by this method. These differ substantially from the profile obtained when the diffusivity is assumed constant.