Search NASA⌕ Search

SEARCH · Search NASA

Results for “SiC/SiC Composites”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Development of Advanced Environmental Barrier Coatings for SiC/SiC Composites at NASA GRC: Prime-Reliant Design and Durability Perspectives

Environmental barrier coatings (EBCs) are considered technologically important because of the critical needs and their ability to effectively protect the turbine hot-section SiC/SiC ceramic matrix composite (CMC) components in harsh engine combustion environments. The development of NASA's advanced environmental barrier coatings have been aimed at significantly improved the coating system temperature capability, stability, erosion-impact, and CMAS resistance for SiC/SiC turbine airfoil and combustors component applications. The NASA environmental barrier coating developments have also emphasized thermo-mechanical creep and fatigue resistance in simulated engine heat flux and environments. Experimental results and models for advanced EBC systems will be presented to help establishing advanced EBC composition design methodologies, performance modeling and life predictions, for achieving prime-reliant, durable environmental coating systems for 2700-3000 F engine component applications. Major technical barriers in developing environmental barrier coating systems and the coating integration with next generation composites having further improved temperature capability, environmental stability, EBC-CMC fatigue-environment system durability will be discussed.

Environmental barrier coatings (EBCs)↗

C-Coupon Studies of SiC/SiC Composites: Acoustic Emission Monitoring - Part 1

Modal acoustic emission (AE) was used to monitor the acoustic activity during room temperature and elevated temperature c-coupon tests for a variety of SiC/SiC systems including composites containing Sylramic (trademark), ZMI (trademark), or Hi-Nicalon (trademark) fibers with melt-infiltrated or polymer-infiltrated SiC matrices. Modal AE proved excellent at monitoring matrix cracking in the curved portion of the C-coupon specimen with increasing load. This included the load at which the first AE event occurred and the location of AE events during the test that were, presumably, caused by the formation and growth of interlaminar cracks and, at higher loads, transverse cracks. Graphical techniques were employed to estimate the load for first AE. It was determined that for this test with these material systems, the first AE could be estimated within the load range bounded by the load at which initial deviation from linearity of the load-displacement curve occurs and the load where the 98% offset of the linear regression fit intercepted the load-displacement curve. The calculation of interlaminar tensile (ILT) stress from the load for first AE was determined for all the systems. Ultimate ILT strength usually corresponded to ILT stress determined from the ultimate load to failure of the C-coupon test, which was considerably higher than the first cracking stress.

Morscher, Gregory N.↗

High-Temperature Mechanical Tensile Testing of Unidirectional Sic/Sic Composites Using A Versatile Lamp Furnace

Silicon carbide (SiC) based ceramic matrix composites (CMCs) are of interest for high-temperature structural applications, including use in turbine engine components. To understand damage mechanisms and predict durability of these systems, in-depth knowledge of their behavior at ambient and high temperatures is necessary. A method for high temperature testing of SiC/SiC minicomposite specimens up to 1500oC in both tensile fast fracture and creep conditions to investigate their thermomechanical behavior will be presented. This method utilizes a novel radiation heat furnace, equipped with infrared lamps with ellipsoidal reflectors, to heat the specimen at the furnace center in user-defined atmospheres. The housing structure of the lamps allows for observation of the specimen during testing using optical methods and for conducting other experimental studies. The goal is to employ nondestructive health monitoring techniques in-situ, including acoustic emission (AE), electrical resistance (ER), and digital image correlation (DIC) to evaluate damage initiation and evolution in the minicomposite specimens during tensile testing. Results from mechanical testing and nondestructive techniques will be presented. Electron microscopy and X-ray micro-computed tomography were used to further characterize specimen damage after testing.

Aeronautics↗

Hermeticity of SiC/SiC composite and monolithic SiC tubes irradiated under radial high-heat flux

Demonstration of hermetic SiC fiber–reinforced SiC matrix composite cladding under normal operating environments has been identified as one of the most critical feasibility issues for accident-tolerant fuel cladding in light-water reactors. This study provides critical experimental data needed for understanding the effects of irradiation on hermeticity. SiC composite and monolithic tubes were neutron-irradiated to 2 displacements per atom with and without a nominal radial heat flux of 0.6 MW/m2 to produce a simulated in-pile stress state for the normal operation of a light-water reactor. The through-thickness temperature gradient under irradiation results in a gradient in swelling, which causes a significant stress buildup. Such irradiation-induced stress was modeled using a commercial finite element analysis code. The radial heat flux–irradiation synergism was experimentally investigated by constructing a special irradiation capsule and evaluating the helium hermeticity of the specimens. The simulated stress state exhibited a near equi-biaxial tensile axial and hoop stress of ~150 MPa at the inner surface of the SiC composite tube. This stress level is potentially beyond the matrix cracking stress. Degradation of hermeticity of the SiC composite tubes was observed after irradiation, indicating irradiation-induced cracking, whereas the irradiated monolithic SiC tubes remained hermetic. In conclusion, the results indicate that loss of hermeticity caused by radiation-induced microcracking is a potential issue for SiC composite cladding, depending on the magnitude of the temperature gradients. Coating the outer surface of the cladding was identified as a mitigation strategy that might overcome the cracking issue.

36 MATERIALS SCIENCE↗

Radiation-induced bowing of SiC/SiC composites under neutron flux gradients—integral experimental data for model validation

Here, the radiation-induced swelling of SiC and its composites, including strong dependencies on temperature and dose, can drive significant lateral bowing in the presence of temperature and/or dose gradients. In recent years, simulations have been performed to assess the extent of bowing in SiC composite light-water reactor (LWR) fuel cladding and boiling water reactor (BWR) channel boxes. However, to date, no integral experimental data exist to validate these models. This work provides the first experimental bowing evaluation of three ∼380 mm long SiC composite specimens irradiated under varying neutron dose gradients (∼50°C–60°C, 0.03–0.06 dpa): two tubes (∼9.8 mm diameter) and a miniature BWR channel box (∼30 mm square). The measured radiation-induced length swelling (∼0.3%–0.7% linear) was consistently 10%–21% higher than values obtained from 3D finite element structural analyses with inputs from 3D radiation transport calculations. This discrepancy could be at least partially explained by differences in dose rate (∼10 -8 dpa/s) compared to the literature data (∼10-6 dpa/s) used to establish the dose-to-swelling correlations in the model. Nevertheless, the modeled bowing magnitudes (<2 mm) obtained from finite element analyses and simple analytical equations were within the bounds of the experimental measurements for all specimens. With improved confidence in the ability to predict the structural response and measure the macroscopic deformations, future experiments will target transient bowing under neutron flux gradients at representative LWR temperatures and assess whether grid spacers can mitigate the tens of millimeters of bowing that would otherwise be expected in ∼4 m long LWR components.

bowing↗

Stress rupture of SiC/SiC composite tubes under high-temperature steam

SiC-fiber–reinforced SiC matrix composite cladding for light water reactor fuel elements must withstand high-temperature steam oxidation in a loss-of-coolant accident scenario (LOCA). Current composite designs include an outer monolithic SiC layer, in part, to increase steam oxidation resistance. However, it is not clear how such a structure would behave under high-temperature steam in the case when the monolithic layer cracks and carbon interphases and SiC fibers are exposed to the environment. To fill this knowledge gap, stress-rupture tests of prototypic SiC composite cladding at 1000°C under steam and inert environments were conducted. The applied stress was ~120 MPa, which was beyond the initial cracking stress. The failure lifetime under steam was 400–1300 s, while 75% of the composite specimens did not fail after 3 h of total exposure under inert gases. Microstructural observations suggest that steam oxidation activated slow crack growth in the fibers, which led to failure of the composite. The results from this study suggest that stress rupture in steam environments could be a limiting factor of the cladding under reactor LOCA conditions.

36 MATERIALS SCIENCE↗

Water Vapor Resistant SiC/SiC Composite for Hydrogen-Based Turbines (Final Scientific Technical Report)

New material innovations are needed for the extreme environments of next generation, hydrogen-fueled turbine engines. Ceramic matrix composites (CMCs) offer high-temperature capability but are susceptible to degradation in high-temperature water vapor. Pratt & Whitney’s (P&W) baseline silicon carbide (SiC)/SiC CMC was initially applied to design a component in a hydrogen-fueled engine, verifying the existence of a design space and extracting boundary conditions to inform testing parameters. Several material innovations, including two fibers, interface coatings (IFC), and self-healing matrices (SHM), were investigated to improve high-temperature performance in water vapor. A boron-doped pyrocarbon (B-PyC) IFC and a SHM matrix with layers of zirconium nitride (ZrN) or zirconium diboride (ZrB 2 ) were developed to fabricate minicomposites with either standard Hi-Nicalon™ Type S (HNS) fibers or new Tyranno® SA4 fibers (SA4). The B-PyC IFC is functional but lacks in providing improved durability. A matrix consisting of thick layers of SiC and thin layers of ZrB 2 shows promise as a SHM that can effectively seal matrix cracks in this extreme environment. Minicomposites with HNS fibers generally outperform those with SA4 fibers.

08 HYDROGEN↗

Failure mechanisms of 3-D woven SiC/SiC composites under tensile and flexural loading at room and elevated temperatures

Nicalon silicon carbide 3D yarn with silicon carbide matrix composites made through a chemical vapor infiltration (CVI) process were investigated under tensile and flexural loading at 23, 1200 and 1550 C in air. The effectiveness of a chemical vapor deposition (CVD) SiC surface coating was also evaluated in severe oxidizing environment. Acoustic emission sensors and in situ optical microscopy were used at room temperature to monitor the failure mechanisms. It is shown that the level of tensile stress at which nonlinear behavior begins is not drastically reduced at 1200 and 1550 C when composites were protected by a SiC surface coating. Extensive fiber pull-out was observed only in the 1550 C specimen. Similar behaviors were also found in flexural specimens.

Chulya, Abhisak↗

Characterizing the Properties of a Woven SiC/SiC Composite Using W-CEMCAN Computer Code

A micromechanics based computer code to predict the thermal and mechanical properties of woven ceramic matrix composites (CMC) is developed. This computer code, W-CEMCAN (Woven CEramic Matrix Composites ANalyzer), predicts the properties of two-dimensional woven CMC at any temperature and takes into account various constituent geometries and volume fractions. This computer code is used to predict the thermal and mechanical properties of an advanced CMC composed of 0/90 five-harness (5 HS) Sylramic fiber which had been chemically vapor infiltrated (CVI) with boron nitride (BN) and SiC interphase coatings and melt-infiltrated (MI) with SiC. The predictions, based on the bulk constituent properties from the literature, are compared with measured experimental data. Based on the comparison. improved or calibrated properties for the constituent materials are then developed for use by material developers/designers. The computer code is then used to predict the properties of a composite with the same constituents but with different fiber volume fractions. The predictions are compared with measured data and a good agreement is achieved.

Murthy, Pappu L. N.↗

Design, Fabrication, and Testing of Ceramic Joints for High Temperature SiC/SiC Composites

Various issues associated with the design and mechanical evaluation of joints of ceramic matrix composites are discussed. The specific case of an affordable, robust ceramic joining technology (ARCJoinT) to join silicon carbide (CG-Nicalon(sup TM)) fiber-reinforced-chemically vapor infiltrated (CVI) silicon carbide matrix composites is addressed. Experimental results are presented for the time and temperature dependence of the shear strength of these joints in air up to 1200 C. From compression testing of double-notched joint specimens with a notch separation of 4 mm, it was found that the apparent shear strength of the joints decreased from 92 MPa at room temperature to 71 MPa at 1200 C. From shear stress-rupture testing in air at 1200 C it was found that the shear strength of the joints decreased rapidly with time from an initial shear strength of 71 to 17.5 MPa after 14.3 hr. The implications of these results in relation to the expected long-term service life of these joints in applications at elevated temperatures are discussed.

Singh, Mrityunjay↗

Growth of Matrix Cracks During Intermediate Temperature Stress Rupture of a SiC/SiC Composite in Air

The crack density of woven Hi-Nicalon(sup TM) (Nippon Carbon, Japan) fiber, BN interphase, melt-infiltrated SiC matrix composites was determined for specimens subjected to tensile stress rupture at 815 C. A significant amount of matrix cracking occurs due to the growth of fiber-bridged microcracks even at stresses below the run-out condition. This increased cracking corresponded to time dependent strain accumulation and acoustic emission activity during the constant load test. However, the portion of the rupture specimens subjected to cooler temperatures (< 600 C than the hot section had significantly lower crack densities compared to the hotter regions. From the acoustic emission and time dependent strain data it can be inferred that most of the matrix crack growth occurred within the first few hours of the tensile rupture experiment. The crack growth was attributed to an interphase recession mechanism that is enhanced by the presence of a thin carbon layer between the fiber and the matrix as a result of the composite fabrication process. One important consequence of matrix crack growth at the lower stresses is poor retained strength at room temperature for specimens that did not fail.

Morscher, Gregory N.↗

Mechanical Behavior of Notched SiC/SiC Composites

Gas turbine components such as combustor liners or turbine vanes are subject to regions of high stress-concentration, e.g., attachment to the frame or at cooling holes. Ceramic matrix composites (CMCs) are potential materials for high temperature applications in gas turbines. They offer some capability to relieve stress at regions of high stress-concentration via matrix damage accumulation. In this study notch sensitivity was examined for woven SiC fiber reinforced, melt-infiltrated SiC matrix composites with a BN interphase, utilizing either Hi-Nicalo(TM) fibers or the stiffer Sylramic fibers. The double-edge notched tensile test approach was used for a wide range of notch sizes and specimen widths. Both composite systems exhibited mild notch sensitivity similar to other CMC systems. Acoustic emission, detected during the tensile tests, indicated that matrix cracking occurred around notches at net-section stresses below the stress where matrix cracking first occurs in unnotched specimens. However, thermoelastic stress analysis did not show any measurable stress relief around notches after the specimens were preloaded.

Morscher, Gregory N.↗

Room Temperature Creep Of SiC/SiC Composites

During a recent experimental study, time dependent deformation was observed for a damaged Hi-Nicalon reinforced, BN interphase, chemically vapor infiltrated SiC matrix composites subjected to static loading at room temperature. The static load curves resembled primary creep curves. In addition, acoustic emission was monitored during the test and significant AE activity was recorded while maintaining a constant load, which suggested matrix cracking or interfacial sliding. For similar composites with carbon interphases, little or no time dependent deformation was observed. Evidently, exposure of the BN interphase to the ambient environment resulted in a reduction in the interfacial mechanical properties, i.e. interfacial shear strength and/or debond energy. These results were in qualitative agreement with observations made by Eldridge of a reduction in interfacial shear stress with time at room temperature as measured by fiber push-in experiments.

Morscher, Gregory N.↗

Stress-Rupture and Stress-Relaxation of SiC/SiC Composites at Intermediate Temperature

Tensile static stress and static strain experiments were performed on woven Sylramic (Dow Corning, Midland, MI) and Hi-Nicalon (Nippon Carbon, Japan) fiber reinforced, BN interphase, melt-infiltrated SiC matrix composites at 815 C. Acoustic emission was used to monitor the damage accumulation during the test. The stress-rupture properties of Sylramic composites were superior to that of Hi-Nicalon Tm composites. Conversely, the applied strain levels that Hi-Nicalon composites can withstand for stress-relaxation experiments were superior to Sylramic composites; however, at a cost of poor retained strength properties for Hi-Nicalon composites. Sylramic composites exhibited much less stress-oxidation induced matrix cracking compared to Hi-Nicalon composites. This was attributed to the greater stiffness and roughness of Sylramic fibers themselves and the lack of a carbon layer between the fiber and the BN interphase for Sylramic composites, which existed in Hi-Nicalon composites. Due to the lack of stress-relief for Sylramic composites, time to failure for Sylramic composite stress-relaxation experiments was not much longer than for stress-rupture experiments when comparing the peak stress condition for stress-relaxation with the applied stress of stress-rupture.

Morscher, Gregory N.↗

C-Coupon Studies of SiC/SiC Composites: Microstructual Characterization - Part 2

A 'C-coupon' was used to measure the interlaminar tensile behavior of five different composite materials: Sylramic/MI (melt infiltration SiC matrix), ZMl/MI, Sylramic/S300, and ZMI and Hi-Nicalon with an S200 matrix at room temperature, 816 C, and 1204 C. Fracture behavior was characterized by field emission scanning electron microscopy, and observed cracking compared with events measured by modal acoustic emission. Both radial and matrix hoop cracking along the inner radius arising from hoop stresses were observed for all material types. In those composites in which the radial cracks were sufficiently wide to view the composite interior, fracture was observed to occur at the fiber BN or BN matrix interface.

Hurwitz, Frances I.↗

Intermediate Temperature Strength Degradation in SiC/SiC Composites

Woven silicon carbide fiber-reinforced, silicon carbide matrix composites are leading candidate materials for an advanced jet engine combustor liner application. Although the use temperature in the hot region for this application is expected to exceed 1200 C, a potential life-limiting concern for this composite system exists at intermediate temperatures (800 +/- 200 C), where significant time-dependent strength degradation has been observed under stress-rupture loading. A number of factors control the degree of stress-rupture strength degradation, the major factor being the nature of the interphase separating the fiber and the matrix. BN interphases are superior to carbon interphases due to the slower oxidation kinetics of BN. A model for the intermediate temperature stress-rupture of SiC/BN/SiC composites is presented based on the observed mechanistic process that leads to strength degradation for the simple case of through-thickness matrix cracks. The approach taken has much in common with that used by Curtin and coworkers, for two different composite systems. The predictions of the model are in good agreement with the rupture data for stress-rupture of both precracked and as-produced composites. Also, three approaches that dramatically improve the intermediate temperature stress-rupture properties are described: Si-doped BN, fiber spreading, and 'outside debonding'.

Morscher, Gregory N.↗

The Velocity and Attenuation of Acoustic Emission Waves in SiC/SiC Composites Loaded in Tension

The behavior of acoustic waves produced by microfracture events and from pencil lead breaks was studied for two different silicon carbide fiber-reinforced silicon carbide matrix composites. The two composite systems both consisted of Hi-Nicalon (trademark) fibers and carbon interfaces but had different matrix compositions that led to considerable differences in damage accumulation and acoustic response. This behavior was primarily due to an order of magnitude difference in the interfacial shear stress for the two composite systems. Load/unload/reload tensile tests were performed and measurements were made over the entire stress range in order to determine the stress-dependence of acoustic activity for increasing damage states. It was found that using the extensional wave velocities from acoustic emission (AE) events produced from pencil lead breaks performed outside of the transducers enabled accurate measurements of the stiffness of the composite. The extensional wave velocities changed as a function of the damage state and the stress where the measurement was taken. Attenuation for AE waveforms from the pencil lead breaks occurred only for the composite possessing the lower interfacial shear stress and only at significantly high stresses. At zero stress after unloading from a peak stress, no attenuation occurred for this composite because of crack closure. For the high interfacial stress composite no attenuation was discernable at peak or zero stress over the entire stress-range of the composite. From these observations, it is believed that attenuation of AE waveforms is dependent on the magnitude of matrix crack opening.

Morscher, Gregory N.↗