Search NASA⌕ Search

SEARCH · Search NASA

Results for “TITANIUM OXIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Defining the Shape Density of Cerium Oxide and Titanium Dioxide Aerosol

The “shape density” of CeO 2 (cerium oxide) powder (American Elements, Los Angeles CA) is estimated to be 0.82 ± 0.02 g cm -3 and the shape density for TiO 2 (titanium dioxide) powder (American Elements, Los Angeles CA) is estimated as 0.54 ± 0.01 g cm -3 . The “shape density” is defined as the measured loose density (ASTM 2018 and ASTM 2021) of a powder divided by the ICRP (International Commission on Radiological Protection) default aerosol shape factor (Valetin 2002). This information is used for experimental measurements of the RRF (respirable release factor) and other respirable source term parameter (US DOE 1994) experiments at the Los Alamos National Laboratory (LANL). The shape density is the input parameter to the TSI Inc (Shoreview MN) AIM (Aerosol Instrument Manager) software for the TSI model 3321 APS (Aerodynamic Particle Sizer) (Figure 1).

61 RADIATION PROTECTION AND DOSIMETRY↗

Electrochemical and Chemical Reactivities of Titanium Oxide-Based Materials with a Chloroaluminate Ionic Liquid Electrolyte for Aluminum Batteries

Here, by selecting three different types of electrode materials, we intended to better understand the Al 3+ intercalation chemistry of titanium oxide-based frameworks with an acidic chloroaluminate electrolyte. In agreement with previous reports, we confirmed that the native interstitial sites of anatase TiO 2 are less prone to accommodate Al 3 + than Li + or Na + ions, while introducing cationic vacancies largely increases the electrochemical storage capacity. Upon the first cycle, the highest reversible capacity, up to 277 mAh/g, was obtained for a hydrated layered structure featuring cationic vacancies. Total scattering data showed that the insertion of Al 3+ ions induced a strong distortion of the framework. In addition, combined 27 Al MAS NMR and DFT calculations revealed that in oxy-hydroxylated vacant sites, the coordination mode of Al 3+ ions depends on the arrangement of anions around vacancies inducing the occurrence of 4-, 5-, and 6-fold coordination modes. Further cycling experiments revealed a progressive capacity fading for all electrode materials. Using cyclic voltammetry on the used electrolyte, we evidenced that a partial dissolution has occurred, which is more pronounced for the layered hydrate compound, and that solubilized species are electrochemically active, giving rise to specific signatures in both CVs and galvanostatic experiments. Raman spectroscopy enabled us to characterize these species, which are derived from the Ti-Cl system. The solubilized species, however, eventually precipitated, as shown by a purple deposit observed on the separator and tentatively assigned to TiCl 3 , known to be insoluble in this medium. By providing further information on the Al 3+ intercalation chemistry and a better understanding of the electrochemical and chemical reactivities of electrode materials, this work will enable progress to be made in the development of aluminum-ion batteries.

Al3+-ion insertion chemistry↗

Effect of alloy chemistry and exposure conditions on the oxidation of titanium

Multiwall is a new thermal protection system concept for advanced space transportation vehicles. The system consists of discrete panels made up of multiple layers of foil gage metal. Titanium is the proposed candidate metal for multiwall panels in the reentry temperature range up to 675 C. Oxidation and embrittlement are the principal concerns related to the use of Ti in heat shield applications. The results of a broad study on the oxidation kinetics of several titanium alloys subjected to different exposure conditions are described. The alloys include commercially pure titanium, Ti-6Al-4V, and Ti-6Al-2Sn-4Zr-2Mo. Oxidation studies were performed on these alloys exposed at 704 C in 5-760 torr air pressure and 0 to 50% relative humidity. The resulting weight gains were correlated with oxide thickness and substrate contamination. The contamination depth and weight gains due to solid solutioning were obtained from microhardness depth profiles and hardness versus weight percent oxygen calibration data.

Unnam, J.↗

Oxidation of commercial purity titanium

The oxidation kinetics of commercial purity Ti-A55 exposed to laboratory air in the 593-760 C temperature range were continuously monitored by thermogravimetric analysis. The oxide thickness was measured by microscopy, and the substrate contamination was estimated from microhardness measurements. The microhardness depth profiles were converted to oxygen composition profiles using calibration depth. The oxygen diffusion coefficient in alpha-Ti appears to be approximately concentration-independent in the 1-10 at. pct oxygen range. Diffusion coefficient for oxygen in TiO2 has been estimated as a function of temperature and is found to be about 50 times the value in alpha-Ti. The metallographically prepared cross sections of the oxidized specimens revealed a 'moving boundary' in the substrate, parallel to the oxide-metal interface. This boundary was associated with a specific oxygen level of 5.0 + or - 0.5 at. pct. It occurred at a distance from the oxide-metal interface which was correlatable with temperature and time of exposure. The diffusion coefficient corresponding to the composition of this moving boundary is in excellent agreement with the effective diffusion coefficient for the substrate contamination.

Unnam, J.↗

Theoretical Investigation of the Hydrogenation of Cyclohexene Catalyzed by Supported Single-Atom Sites on Redox Noninnocent LiMn 2 O 4 and Li 2 Mn 2 O 4 Surfaces

Here, the tuning of catalyst activity via stereoelectronic modulation of the active-site structure remains a grand challenge in heterogeneous catalysis. In homogeneous catalysis, the redox noninnocent ligands can be introduced to organometallic fragments to donate electrons to the metal center and fine-tune the catalytic activity. Analogously, lithium-ion battery materials, such as lithium manganese oxide (LMO), lithium titanium oxides (LTO), etc., can serve as redox noninnocent catalyst support to modulate the electronic structures of the active site via lithiation, hence tuning the catalytic activity of supported active sites. Experimentally, the Ni single-atom site was supported on LiMn 2 O 4 via oxidative grafting and exhibited no catalytic activity toward the hydrogenation of cyclohexene. After introducing additional Li into the catalyst support forming Li 2 Mn 2 O 4 , the Ni single-atom site becomes active, with the catalytic rates increasing as a function of the lithiation for Li/Mn ratios >0.9. In this paper, density functional theory (DFT) calculations are performed to study the Ni site structure via X-ray absorption near edge structure (XANES) simulations and investigate the electronic properties of Ni single-atom site before and after the addition of intercalated lithium in the LMO spinel structure. Furthermore, the study of the reaction mechanism is also carried out to understand the thermodynamically and kinetically favored pathways. XANES simulation suggests that the Ni single-atom site is likely to stay in the Li channel of the spinel support structure and form an octahedral structure. After Li intercalation, the Ni site becomes less positively charged, indicating the partial reduction of the Ni site. The simulated reaction energy profile over the LiMn 2 O 4 support exhibits high-energy barriers (1.07 eV) for the hydrogenation of cyclohexene; however, the Li 2 Mn 2 O 4 support is able to better stabilize low-coordinated ion sites and improve ion mobility, leading to lower overall energy barriers (0.64 eV). The reduced and low-coordinated ion site, thus, can better stabilize the reaction intermediates and promote hydrogenation reaction. Similarly, other transition metal ions (Fe, Co, and Cu) are also considered over the LiMn 2 O 4 and Li 2 Mn 2 O 4 catalyst supports for hydrogenation reaction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploiting Fixed Charge at Selective Contacts for Silicon Photovoltaics

The goal of this work was to examine and exploit fixed interface charges in ultra-thin (0-3 nm thickness) tunnel dielectric layers sandwiched between silicon and selective contact metal oxides (molybdenum oxide, MoO x , titanium oxide, TiO 2 ). Specifically, the interface fixed charge was varied by changing processing conditions and materials over a wide range and the effect on the current-voltage behavior and the Schottky barrier height was quantified. In budget period 1 (year 1), the objective was to grow aluminum oxide tunnel layers with quantified fixed charge over a range of ~1E12 to ~-2E12 cm -2 and combine these with MoO x and TiO 2 layers on Czochralsi (CZ) mono p- and n-Si, respectively. We sought conditions that maximize fixed charge and minimize Schottky barrier height to MoO x contacts to p-Si. This objective, along with investigating the effects of silicon surface terminations, occupied the majority of the project timeline (Q1-Q8) due to complications with high specific contact resistivity values. In the last two quarters of the project period, the objective was to insert HfO2 layers between Si and aluminum oxide layers to quench the fixed charge for layers with otherwise identical thermal history. Another objective was to lower the barrier height at TiO 2 -based contacts on n-type Si, but that was never investigated completely.

14 SOLAR ENERGY↗

Nucleation-promoting and growth-limiting synthesis of disordered rock-salt Li-ion cathode materials

Disordered rock-salt oxides and oxyfluorides are promising positive electrode materials for high-performance lithium-ion batteries free of nickel and cobalt. However, conventional synthesis methods rely on post-synthesis pulverization to achieve cycling-appropriate particle sizes, offering limited control over particle microstructure and crystallinity. This accelerates degradation and complicates secondary particle processing. Here we present a synthesis strategy that enhances nucleation while suppressing particle growth and agglomeration across various disordered rock-salt compositions, including lithium–manganese–titanium oxide, lithium–manganese–niobium oxide, and lithium–nickel–titanium oxide systems. Applied to Li 1.2 Mn 0.4 Ti 0.4 O 2 , this method yields highly crystalline, well-dispersed sub-200 nm particles that form homogeneous electrode films with stable cycling behavior. Tested in cells with lithium metal as the counter electrode, these electrodes deliver ~200 mAh/g with 85% capacity retention relative to the first cycle after 100 cycles (20 mA/g, 1.5–4.8 V), and an average discharge voltage loss of 4.8 mV per cycle, compared to 38.6% retention and 7.5 mV loss per cycle for electrodes derived from pulverized solid-state particles. This approach suggests a route to enhance the performance and durability of disordered rock-salt electrodes for sustainable lithium-ion batteries.

Batteries↗

Very Long Term Oxidation of Titanium Aluminides Investigated

Titanium aluminides (TiAl) are of great interest for intermediate-temperature (600 to 850 C) aerospace and power-generation applications because they offer significant weight savings over today's nickel alloys. TiAl alloys are being investigated for low-pressure turbine blade applications, exhaust nozzle components, and compressor cases in advanced subsonic and supersonic engines. Significant progress has been made in understanding the fundamental aspects of the oxidation behavior of binary TiAl alloys. However, most of this work has concentrated on short term (<1000 hr), high-temperature (900 to 1000 C) exposures. Also, there is not much data available in the literature regarding the oxidation behavior of the quaternary and higher order engineering alloys. This is especially true for the very long term, low-temperature conditions likely to be experienced during aerospace applications. An investigation at the NASA Glenn Research Center at Lewis Field was undertaken to characterize the long-term oxidation behavior of various model and advanced titanium aluminides for periods up to 7000 hr at 704 C in air using a high-resolution field emission scanning electron microscope. Also, a unique surface treatment technique developed to improve the oxidation resistance of TiAl was evaluated. The alloys included in this investigation are listed in the table. The table also shows typical alloy compositions and the specific weight changes and scale thickness measured for each alloy after exposure to 700 C for 7000 hr in air.

Locci, Ivan E.↗

Detection of H2O and Evidence for TiO VO in an Ultra Hot Exoplanet Atmosphere.

We present a primary transit observation for the ultra-hot (Teq approx. 2400 K) gas giant expolanet WASP-121b, made using the Hubble Space Telescope Wide Field Camera 3 in spectroscopic mode across the 1.12-1.64 micron wavelength range. The 1.4 microns water absorption band is detected at high confidence (5.4(sigma)) in the planetary atmosphere. We also reanalyze ground-based photometric light curves taken in the B, r′, and z′ filters. Significantly deeper transits are measured in these optical bandpasses relative to the near-infrared wavelengths. We conclude that scattering by high-altitude haze alone is unlikely to account for this difference and instead interpret it as evidence for titanium oxide and vanadium oxide absorption. Enhanced opacity is also inferred across the 1.12-1.3 micron wavelength range, possibly due to iron hydride absorption. If confirmed, WASP-121b will be the first exoplanet with titanium oxide, vanadium oxide, and iron hydride detected in transmission. The latter are important species in M/L dwarfs and their presence is likely to have a significant effect on the overall physics and chemistry of the atmosphere, including the production of a strong thermal inversion.

Spectroscopy↗

CO Oxidation Catalyzed by Au Dispersed on SBA-15 Modified with TiO2 Films Grown via Atomic Layer Deposition (ALD)

It has been established that gold, when in nanoparticle (NP) form and in contact with reducible oxides, can promote oxidation reactions under mild conditions. Here, we report results from our exploration of the catalytic oxidation of carbon monoxide using catalysts where Au NPs were combined with thin titanium oxide films deposited on SBA-15 using atomic layer deposition (ALD). Both orders of deposition, with TiO2 added either before or after Au dispersion, were tested for two titania film thicknesses amounting to about half and full TiO2 monolayers. The resulting catalysts were characterized using various techniques, mainly electron microscopy and N2 adsorption–desorption isotherms, and the kinetics of the oxidation of CO with O2 were followed using infrared absorption spectroscopy. A synergy between the Au and TiO2 phases as it relates to the bonding and conversion of CO was identified, the tuning of which could be controlled by varying the synthetic parameters. The ALD of TiO2 films proved to be an effective way to maximize the Au-TiO2 interface sites, and with that help with the activation of molecular oxygen.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Guidance and control research

Cesium vapor heat conduction in thermionic energy converters, space charge distribution in neutral plasma, and titanium oxide thin films

THERMIONIC CONVERTER↗

In Situ Scattering Studies of Superconducting Vacancy‐Ordered Monoclinic TiO Thin Films

Abstract The structural and transport properties of vacancy‐ordered monoclinic superconducting titanium oxide (TiO) thin films grown by molecular beam epitaxy are investigated. The evolution of the crystal structure during growth is monitored by in situ synchrotron X‐ray diffraction. Long‐range ordering of Ti and O vacancies in the disordered cubic phase stabilizes the vacancy‐ordered monoclinic TiO phase. The reduced structural disorder arising from vacancy‐ordering is correlated with a superconductor‐metal transition (SMT) in contrast to the superconductor‐insulator transition (SIT) observed in cubic TiO, orthorhombic Ti 2 O 3 , and the Magneli γ − Ti 3 O 5 and γ − Ti 4 O 7 phase. Magnetoresistance measurements for the SIT phases indicate superconducting fluctuations persisting in the normal phase. These results confirm the role of disorder related to Ti and O vacancies and structural inhomogeneity in determining the electronic properties of the normal state of titanium oxide‐based superconductors.

Baksi, Merve↗

Titanium Niobium Oxide: From Discovery to Application in Fast-Charging Lithium-Ion Batteries

Lithium-ion batteries are essential for portable technology and are now poised to disrupt a century of combustion-based transportation. The electrification revolution could eliminate our reliance on fossil fuels and enable a clean energy future; advanced batteries would facilitate this transition. However, owing to the demanding performance, cost, and safety requirements, it is challenging to translate new materials from laboratory prototypes to industrial-scale products. This Perspective describes that journey for a new lithium-ion battery anode material, TiNb 2 O 7 (TNO). TNO is intended as an alternative to graphite or Li 4 Ti 5 O 12 with better rate and safety characteristics than the former and higher energy density than the latter. The high capacity of TNO stems from the multielectron redox of Nb 5+ to Nb 3+ , its operating voltage window well above the Li + /Li reduction potential prevents lithium dendrite formation, and its open crystal structure leads to high-power performance. Nevertheless, the creation of a practical TNO anode was nonlinear and nontrivial. Its history is built on 30 years of fundamental science that preceded its application as a battery anode, and its battery development included a nearly 30-year gap. The insights and lessons contained in this Perspective, many of them acquired firsthand, serve two purposes: (i) to unite the disparate studies of TiNb 2 O 7 into a coherent modern understanding relevant to its application as a battery material and (ii) to highlight briefly some of the challenges faced when scaling up a new material that affect TiNb 2 O 7 as well as new electrode candidates more generally.

25 ENERGY STORAGE↗

Oxide-Encapsulated Ruthenium Oxide Catalysts for Selective Oxygen Evolution in Unbuffered pH-Neutral Seawater

Direct seawater electrolysis is a promising approach to producing green hydrogen in water-scarce environments using renewable energy. However, the undesirable chlorine evolution reaction and hypochlorite evolution reaction compete with the desired oxygen evolution reaction (OER) at the anode electrocatalyst. This issue is most pronounced in unbuffered pH-neutral solutions due to local acidification resulting from the OER. To overcome this challenge, this study provides a comprehensive evaluation of the use of silicon oxide (SiO x ) and titanium oxide (TiO x ) nanoscale overlayers coated on metallic ruthenium (Ru) and ruthenium oxide (RuO x ) thin film electrodes and their ability to block chloride ions from reaching active sites during operation in an unbuffered 0.6 M NaCl electrolyte. Using a combination of (electro)analytical techniques, encapsulated RuO x anodes are shown to effectively suppress Cl - transport to buried catalyst active sites while allowing for the desired OER to occur, leading to increases in OER faradaic efficiency at moderate overpotentials. Evidence for the ability of SiO x overlayers to block Cl - ions from reaching the active buried interface was obtained by monitoring the ν(O-H) stretching mode of OH adsorbates using in situ Raman spectroscopy. Here, this study also reports trade-offs between the activity, selectivity, and stability of bare and encapsulated Ru and RuO x electrocatalysts, finding that the magnitude of these trade-offs strongly depends on the complex interplay between electrode architecture, material properties, and catalytic performance, especially in unbuffered pH-neutral seawater.

58 GEOSCIENCES↗

Probing the active sites of oxide encapsulated electrocatalysts with controllable oxygen evolution selectivity

Electrocatalysts encapsulated by nanoscopic overlayers can control the rate of redox reactions at the outer surface of the overlayer or at the buried interface between the overlayer and the active catalyst, leading to complex behavior in the presence of two competing electrochemical reactions. This study investigated oxide encapsulated electrocatalysts (OECs) comprised of iridium (Ir) thin films coated with an ultrathin (2–10 nm thick) silicon oxide (SiO x ) or titanium oxide (TiO x ) overlayer. The performance of SiO x |Ir and TiO x |Ir thin film electrodes towards the oxygen evolution reaction (OER) and Fe(II)/Fe(III) redox reactions were evaluated. An improvement in selectivity towards the OER was observed for all OECs. Overlayer properties, namely ionic and electronic conductivity, were assessed using a combination of electroanalytical methods and molecular dynamics simulations. SiO x and TiO x overlayers were found to be permeable to H 2 O and O 2 such that the OER can occur at the MO x |Ir (M = Ti, Si) buried interface, which was further supported with molecular dynamics simulations of model SiO 2 coatings. In contrast, Fe(II)/Fe(III) redox reactions occur to the same degree with TiO x overlayers having thicknesses less than 4 nm as bare electrocatalyst, while SiO x overlayers inhibit redox reactions at all thicknesses. This observation is attributed to differences in electronic transport between the buried interface and outer overlayer surface, as measured with through-plane conductivity measurements of wetted overlayer materials. These findings reveal the influence of oxide overlayer properties on the activity and selectivity of OECs and suggest opportunities to tune these properties for a wide range of electrochemical reactions.

08 HYDROGEN↗