Search NASA⌕ Search

SEARCH · Search NASA

Results for “U(Mo)”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Micro-tensile testing of neutron-irradiated Al/Zr and Zr/U-Mo diffusion bonds

This study focuses on micro-tensile testing of neutron-irradiated Al/Zr and Zr/U-Mo diffusion bonds, which are integral to the structure and performance of nuclear fuel plates used in the fuel being developed for U.S. high-power research reactors. During fabrication, two distinct diffusion bonds occur—one at the Zr/U-10Mo interface via roll bonding, and the Zr/Al interface via hot isostatic pressing at 833 K. This work utilizes micro-tensile testing specimens approximately 7 × 7 × 18 μm 3 , which are sufficiently large to encompass the identified diffusion zones to evaluate the failure strength and identify the failure location. For the Zr/Al interface, all failures occurred in the bulk aluminum. The average yield strength, ultimate strength, and strain at failure for the two parent samples were: 125 ± 10 MPa, 139 ± 24 MPa, 156 ± 21 MPa, 185 ± 14 MPa, 37.9 ± 5.6 %, and 29.7 ± 3.4 %, respectively. For specimens across the Zr/U-Mo interface, failures occurred either in the bulk Zr or U-Mo, with no failures observed in the diffusion region. For specimens that failed in the bulk Zr the failure strength and strain for the two parent samples were 570 MPa, 710 ± 131 MPa, and 43.3 %, 27.3 ± 6.6 % respectively. The specimens that failed in the bulk U-Mo had failure strengths and strains of 596 ± 32 MPa, 548 ± 124 MPa, and 2.2 ± 1.3 %, 1.5 ± 0.6 % respectively. In conclusion, these findings support the development of accurate thermo-mechanical models for irradiated fuel performance by identifying the mechanical limits and failure locations within the bonded regions.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The role of UC inclusions in the development of fission gas bubble superlattice neutron-irradiated monolithic U-10Mo fuels

Uranium Carbide (UC) inclusions are the most prevalent impurities in Uranium-Molybdenum (U-Mo) fuel and are considered undesirable because they could potentially affect fuel performance. This work revealed that, like grain boundaries (gBs), UC inclusions could help facilitate the formation of the fission gas bubble superlattice (GBS). The GBS is a highly organized complex defect structure that can effectively store fission gases, thereby inhibiting fuel swelling. Transmission electron microscopy (TEM) showed that GBS self-organization can initiate at the UC/U-Mo interfaces in U-10Mo fuel irradiated to low fission density. Furthermore, this study also revealed that the UC boundary in U-10Mo irradiated to low fission density is wavy and periodic in morphology and that GBS formation is semi-coherent with the UC boundary. Because the initiation of GBS occurs at gBs and UC/U-Mo interfaces, the fission gas inventory is always highest at those regions compared to the U-Mo grain interior. Consequently, at higher fission densities, it is likely that high burnup structure (HBS) development via grain refinement will begin at gBs and UC/U-Mo interfaces.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Non-destructive analysis of swelling in the EMPIrE fuel test

The European Mini-Plate Irradiation Experiment (EMPIrE) was designed to support the development and testing of a coated uranium-molybdenum (U-Mo) dispersion fuel for the conversion of select high-performance research reactors (HPRRs) to utilize low-enriched uranium (LEU). To aid in the development of the coated fuel form, the EMPIrE test included several plate designs and irradiated them in the Idaho National Laboratory (INL) Advanced Test Reactor (ATR) at a high meat power density (~21 kW/cm 3 ) and to high fuel particle fission densities (~6.4 × 10 21 fissions/cm 3 ). These conditions mimic the bounding conditions of the BR-2 reactor in Belgium, where a concurrent irradiation experiment was performed, and exceed those previously explored in dispersion U-Mo fuel plates. A local fuel swelling analysis, as determined through high-fidelity, post-irradiation mini-plate profilometry, was used along with statistical methods to non-destructively evaluate the overall performance and separate the effects of convoluted fabrication variables. While some effects observed with this non-destructive analysis were subtle, others had more significant, and possibly competing, effects on the fuel swelling behavior. In closing, these observations will be examined further with destructive examinations to more fully assess them as the fuel design is developed and qualified.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

IER 517: Molybdenum Critical Experiment Design [Slides]

In nuclear fuels, U-Mo metallic fuels are used in new space reactor designs and new research reactor fuels. MITR, MURR, and NBSR reactors plan on converting from different HEU fuels to a U-Mo HALEU fuel. In spend nuclear fuel, 95 Mo is one of the 15 main absorbing fission products in irradiated LWR fuel. This makes it important for criticality safety studies in transportation and reprocessing. In structural materials. Molybdenum is found commonly in alloys that make up the structural materials of nuclear reactors such as type 316 SS. Molybdenum helps to improve high temperature performance and corrosion resistance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Design and Fabrication Options Trade Study for Metallic Fuel without Internal Sodium Bonding

Nuclear fuels using alloys of uranium, or metallic fuels, have many beneficial properties. The classical metallic fuel design uses a loose fitting cylindrical “slug” of fuel placed inside stainless-steel cladding tubes where the gap is filled with sodium. This sodium bond is liquid at operating temperature and conducts heat from the slug to the cladding, especially in early life before fuel swells into contact with the cladding. Despite the benefits of sodium bonding, there is a desire to develop metallic fuel technologies without it chiefly to reduce chemical reaction hazards in spent fuel storage from sodium fast reactors operating on once-through fuel cycles. Elimination of the sodium bond may also help unlock potential benefits for fuel fabrication, reactor neutronics, and compatibility with other types of reactors. Creating a sodium-free metallic fuel revolves around the problem of manufacturing fuel slug geometries which are in close contact with the cladding at beginning of life to facilitate heat transport while alleviating fuel-cladding chemical interactions (FCCI) at this interface and providing enough free volume to accommodate fuel swelling. Accelerating development and qualification of this fuel system will require careful selection of design and manufacturing options. To this end, a design trade-off study was performed to evaluate candidate options. Several design and manufacturing options were assessed, weighted, scored, and ranked with respect to fabrication, normal reactor operation, off-normal scenarios, and back-end considerations. This effort was performed both for “baseline” needs, which represented a once-through fuel cycle at temperatures and burnups known to be viable for sodium-bonded metallic fuel, and for “enhanced” needs to represent opportunities for closed fuel cycles and/or more aggressive temperatures/burnups. The outcomes of this study prioritized a baseline technology using U-Zr alloy with additives to mitigate FCCI, produced in annular slug geometry by continuous casting, clad in austenitic stainless-steel alloy, and followed by a final step to swage the cladding down to close the gap. This study prioritized an enhanced fuel technology using U-Mo alloy, also produced by continuous casting into an annular geometry, followed by coating/plating with an FCCI barrier on the slug, again with a final step to swage the cladding diameter down using oxide dispersion strengthened steel. It was noted that development of the enhanced fuel technology would entail more risk, thus U-Zr alloy was put forth as a backup to U-Mo if challenges are encountered with FCCI barriers, and advanced ferritic/martensitic steels are put forth as a backup to oxide dispersion strengthened steels if swaging and welding are found unworkable.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Nuclear Fuel and Pu Redox Studies from The Glenn T. Seaborg Institute at Idaho National Laboratory

The Glenn T. Seaborg Institute at Idaho National Laboratory (INL-GTSI) focuses on advancing fundamental research in the actinide sciences by providing unique opportunities to early career scientists and engineers to gain experience studying the actinide elements and their associated systems. The INL-GTSI is built from three focus areas that are based on the expertise and supporting infrastructure at INL and include solid state chemistry and physics, solution phase chemistry and physics, and forensic and isotope science. INL is the lead Laboratory for nuclear energy research and development in the U. S. and the research on nuclear fuels performed under the INL-GTSI gives good examples of solid state studies. Uranium-Molybdenum (U-Mo) alloys are leading fuel candidates for conversion of high performance research and test reactors to low-enriched fuels. During irradiation, generated fission gas accumulates into bubbles and self-organizes into a gas bubble superlattice (GBS) that effectively stores fission gases and inhibits fuel swelling. A study on the early self- organizing behavior of the GBS shows that not only grain boundaries but the interfaces between the U-Mo matrix and uranium carbide (UC) impurities are important to GBS formation.[1] In solution, understanding the complex redox behavior of plutonium in aqueous environments is critical for establishing optimized nuclear waste reprocessing solvent systems and storage tank environments. INL-GTSI researchers have produced an experimentally validated multi-scale model of the gamma radiation induced behavior of plutonium ions in concentrated aqueous HNO3 solutions.[2] Here, gamma radiation effected only minimal steady state changes in the redox distribution of the plutonium oxidation states. The redox cycling between Pu(IV) and Pu(III) is demonstrated to be mediated by the •OH/NO3• radical oxidation of Pu(III) and the H2O2/HNO3 driven reduction of Pu(IV). The INL-GTSI offers young researchers the unique chance to work directly with actinide bearing materials in a U. S. National Laboratory environment. Further topical areas of interest to the INL-GTSI include, but are not limited to, fundamental actinide properties, structure/property (electronic, magnetic, thermal) relations, actinide quantum criticality, f- electron interactions, electron correlations, computational studies, new phases, defect effects, interface interactions, isotope production and separation, forensic analytical chemistry, structure and dynamic properties of actinides in non-aqueous media, separations chemistry and kinetics for advanced nuclear fuel cycles, radiation effects, and innovative and advanced ligand design for complexation of the actinides.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Demonstration of Dimensional and Microstructural Postirradiation Examination Capabilities on MiniFuel Disk Specimens

This work demonstrates two new MiniFuel postirradiation examination (PIE) capabilities, laser profilometry and serial sectioning, for future use on alpha-U specimens for the upcoming Mini-99 irradiation campaign. Representative U–Mo disk specimens—3 mm in diameter and approximately 0.75 mm in thickness—were subjected to dimensional measurements using standard calipers, as well as a new Keyence CL-3000 series laser profilometry system designed to measure the surface of both sides of the disk simultaneously. The laser profilometry system captured thickness gradients across the specimens as large as 0.2 mm. Additionally, because of the limitations inherent to the use of calipers, caliper measurements consistently overestimated the initial volume of MiniFuel disk specimens compared to the laser profilometry method by up to 5%. However, the results show that optimal data collection and analysis procedures are crucial to avoiding significant artifacts during data collection that can lead to large errors (approximately 10%). Serial sectioning using a combination of ion milling and electron imaging was also demonstrated for the analysis of micron-sized control volumes. Nanometer- to micron-scale porosity was resolved on a representative U–Mo specimen before irradiation, even when the surface of the specimen appeared free of porosity. Future efforts to relate microstructural features (porosity, fission product distributions, and so on) to macroscale effects (dimensional changes, thermal conductivity degradation) require accurate characterization methods such as those demonstrated in this work. These advanced PIE capabilities will be applied to optimized alpha-U specimens for the upcoming Mini-99 neutron irradiation campaign.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Synergistic double-atom catalysts of metal-boron anchored on g-C 2 N for electrochemical nitrogen reduction: Mechanistic insight and catalyst screening

The rational design of a novel catalytic center with a sound basis remains both challenging and rewarding for the electrochemical reduction of N 2 (eNRR), which has provided a feasible route for achieving clean and sustainable NH 3 production under ambient conditions. Herein, using density functional theory calculations, we demonstrate that hybrid metal (M)-boron (B) double-atom catalysts (DACs) embedded in g-C 2 N substrate (M-B@C 2 N, M = 3d, 4d and 5d transition metals) can achieve both high catalytic activity and high selectivity in eNRR. The proposed M-B@C 2 N DACs have exhibited impressive feasibility and stability thanks to the resilient and robust C 2 N substrate with abundant pyridinic N atoms distributed among right-sized pore structures. Our results reveal that like the metal center, the embedded B atom can actively involve in Ntriple bondN bond activation via π*-backdonation mechanism concomitant with the substantial charge transfer to adsorbed *N 2 , leading to sizable Nsingle bondN bond elongation. Accordingly, both adsorption energy and Nsingle bondN bond length of *N 2 can be employed as catalytic descriptors for predicting eNRR activity in terms of the limiting potentials (UL). Using high-throughput screening method, we found that six M-B@C 2 N candidates have stood out as the outstanding electrocatalysts for driving eNRR, namely, M = Ti (U L = 0 V), Mo (U L = 0 V), Nb (U L = -0.04 V), W (U L = -0.23 V), Zr (U L = -0.26 V), V (U L = -0.28 V). The underlying origin is attributed to the balanced and constrained N-affinity of M-B dual site working in synergy, which can thus be used as one important guide of catalyst design.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Early self-organization of fission gas bubble superlattice formation in neutron-irradiated monolithic U-10Mo fuels

Self-organization of defect superlattices in far-from-equilibrium systems presents a promising way to mitigate swelling concerns in nuclear materials. The gas bubble superlattice (GBS) is a highly ordered, three-dimensional complex defect structure that can retain fission gasses in Uranium-Molybdenum (U-Mo) fuels. Transmission electron microscopy (TEM) investigation of monolithic U-10Mo fuel irradiated to 1.15 × 10 21 fissions/cm 3 and 1.30 × 10 21 fissions/cm 3 revealed that early-stage ordering preferentially occurs at the grain boundaries (GB) and that the critical bubble size for complete ordering is ~3 nm. Once formed at the GB, the GBS extends towards the grain interior; however, the spread in distance from the GB varies likely depending on the type and strength of the GB sink. TEM results also showed a possible correlation between the growth and evolution of the intragranular disordered bubbles and large dislocation networks. The fission product distribution in and outside of the GBS was also investigated confirming the presence of xenon in the GBS, as well as other fission products including cesium, barium, lanthanum, and cerium.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Atom probe tomography of segregation at grain boundaries and gas bubbles in neutron irradiated U-10 wt% Mo fuel

During neutron irradiation to fission densities > 5.2 × 10 21 fiss/cm 3 , Xe agglomerates forming gas bubbles of varying size within the U-Mo fuel matrix. Herein, segregation of fission products to Xe bubbles and grain boundaries (GB) were studied using atom probe tomography (APT). Segregation behavior was found to vary among GBs, small bubbles (<10 nm), and larger bubbles (>10 nm). Solid fission products were enriched at GBs and larger bubbles, but not at small bubbles. Finally, a denuded zone was identified adjacent to a > 10 nm Xe gas bubble and a GB.

36 MATERIALS SCIENCE↗

Integrated simulation of U-10Mo monolithic fuel swelling behavior

Here, a separate computational branch has been implemented within the DART (Dispersion Analysis Research Tool) computational code to simulate the swelling behavior of U-10Mo monolithic fuel under the operating conditions of high-power research and test reactors (RTRs). The monolithic branch of the DART code implements a mechanistic rate-theory-based fission-gas-behavior model for the calculation of fission gas swelling, as well as a suite of thermal, physical, and mechanical models to take into account various processes occurring in RTR fuels during irradiation. In order to accurately simulate and eventually predict U-10Mo monolithic fuel irradiation behavior, the code uses materials properties calculated with lower length-scale computational methods, such as gas atom diffusivity and U-Mo surface energy from atomic simulations and grain-morphology-specific recrystallization kinetics (recrystallized fuel volume fractions vs. fission density) predicted using the phase-field method. The remainder of fission gas behavior parameters used in the model were calibrated with measured intergranular bubble size distributions. With this integrated simulation approach, the swelling behavior of U-10Mo monolithic fuel was simulated for various initial grain sizes at different operating conditions and compared with measured data. Furthermore, because limited experimental data exist for parameter calibration detailed sensitivity studies for the important parameters used in the fission gas behavior model were performed in order to examine their impact on both intergranular gas bubble morphology at low fission density, and on total porosity at high fission density.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Behavior of the Mo, Tl, and U isotope systems during differentiation in the Kilauea Iki lava lake

Stable molybdenum (Mo), thallium (Tl), and uranium (U) isotope ratios were determined in a suite of samples from the 1959 Kilauea eruption and from Kilauea Iki lava lake with the aim of understanding the effects of igneous differentiation on these isotope systems. The samples range from olivine cumulate with MgO up to 27% to internal differentiates with MgO less than 3%, representing a tholeiitic differentiation series. Molybdenum, Tl, and U behave incompatibly during differentiation, and Mo and U isotope ratios do not systematically vary amongst the different samples. δ 98 Mo values range from -0.17 to -0.31‰ and δ 238 U values range from -0.20 to -0.38‰. Most individual analyses for both isotope systems overlap within measurement uncertainty (± ~0.7 and ~ 0.6, respectively). Mean δ 98 Mo and δ238U values are -0.22 ± 0.08‰ (2σ) and - 0.29 ± 0.09‰ (2σ), respectively, which overlap with Pacific mid ocean ridge basalt (MORB). In contrast, Tl isotopes show small but resolvable variations, with ε 205 Tl ranging from +1.20 to -1.38. The most negative ε 205 Tl values are confined to some of the lowest [Tl] samples, but the ε 205 Tl values do not otherwise vary smoothly with MgO or [Tl]. Possible mechanisms for thallium isotope fractionation are considered (e.g., degassing, water leaching, sulfide fractionation) but none are found to be satisfactory. Overall, the lack of resolvable variation in the Mo and U isotope systems and the small magnitude of heterogeneity in the Tl isotope system indicate that differentiation in tholeiitic systems is unlikely to be a major contributor to global variation in these isotope systems.

58 GEOSCIENCES↗

Evaluation of Oak Ridge National Laboratory Health Physics Research Reactor Operation Data for Critical Benchmark Creation

The Oak Ridge National Laboratory (ORNL) Health Physics Research Reactor (HPRR) was a research reactor designed and built at ORNL in 1961. The critical assembly used a highly enriched uranium and molybdenum alloy as the fuel and could be operated in steady-state or burst modes. The HPRR has recently been the object of an investigation to create a criticality benchmark. Such benchmarks are very important, as they are used primarily to show the accuracy of newly developed modeling codes and to help experimental validation and reactor licensing. The evaluated experiments considered in this paper were carried out between 1974 and 1986 from various HPRR activities such as steady-state subcritical, steady-state critical, and burst prompt super-critical operations of the reactor for dosimetry, irradiation, or training purposes. By using the HPRR experimental logbook information and the as-built drawings of the critical assembly, a highly detailed model of the HPRR was created with SCALE 6.2.4/KENO-VI, and a first version of a critical benchmark of the HPRR was developed following the International Criticality Safety Benchmark Evaluation Project (ICSBEP) guidelines for thorough description and uncertainty/sensitivity quantification. Unfortunately, in most of the evaluated experiments, the obtained difference between calculated and experimental k eff is around 1,000 pcm, corresponding to a relative error of approximately 1%, beyond the quality standards of the ICSBEP recommending a relative error below 0.1%. Moreover, the derived experimental uncertainty is high, around 4% relative, mainly due to the U-Mo fuel density uncertainty, but also from numerous other factors. For these reasons, the creation of a valuable critical benchmark from HPRR operation data is thus far compromised. In this paper, the different steps of the experiments’ evaluation are summarized, and the reasons for the experimental/calculation discrepancies and potential ways to solve them are explored. This paper also aims to remind us always to exercise considerable care when performing experimental work, and to record all the data possible for potential future uses.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Interfacial Analysis of Blister Formation in U-10Mo Mini-Plates

A thorough investigation of potential failure mechanisms builds confidence in the performance of monolithic U-10wt%Mo (U-10Mo) fuel plates. The lowenriched uranium (LEU) fuel system is currently undergoing qualification as a high U-density fuel that can be used to convert United States high-performance research reactors from high-enriched uranium (HEU) operation. This will require establishing fuel operational limits such that fission products and a coolable geometry are retained, even during off-normal reactor operation conditions [1]. Such off-normal conditions can subject the fuel plates to temperatures where the internal pressure of precipitated fission gasses result in a permanent deformed, raised area of the cladding, referred to as a blister. These blisters can reduce the local coolability of a fuel plate and can even close coolant channels of a fuel assembly, so blistered plates are considered failed regardless of whether the fuel is truly breached. Historically, a marginto- failure is established through out-of-pile blister threshold testing of irradiated fuel plates. This is accomplished by incrementally heating irradiated fuel plates until blisters are observed. This reveals the temperature threshold that would have resulted in a blister if a plate experienced them at those irradiation conditions [2]. While the blister testing itself reveals the temperatures at which the cladding mechanical integrity was exceeded, a more thorough investigation of the interface evolution in proximity to formed blisters may reveal mechanisms as to the blister formation and retention of fission gases. Previous studies have explored potential underlying mechanisms in historical plates that may have been close to blistering [3]; however, this work is the first exploration of blister tested irradiated plates, fabricated by a commercial vendor—another requirement for qualification of the fuel system [1]. The Mini-plate 1 (MP-1) experiment was the first in a series of irradiation and post-irradiation examination (PIE) campaigns to qualify the U-10Mo monolithic fuel system. It consisted of commercially fabricated 25.4×101.5 mm Al-clad mini-plates with a monolithic U-10Mo foil coated in a Zr diffusion barrier. The primary MP-1 PIE campaign was previously completed. Among the suit of examinations was a blister testing campaign, where plates were incrementally annealed in 25°C increments until blisters were observed or a maximum temperature of 550°C was reached [4]. The previously blistered plates from this campaign were revisited in this work.

25228↗

Spark plasma sintering of fuel meats for U 3 O 8 based dispersion fuels

Research and test reactors often use dispersion-type fuel due to its increased thermal conductivity and burn-up capabilities compared to conventional fuel. Al-U 3 O 8 (aluminumtriuranium octaoxide) dispersion fuels have several advantages over their competitors, such as higher service temperature and better stability of oxygen stoichiometry. However, the two-step fabrication of dispersion fuel causes undesirable porosity in cold-pressed fuel meats that is preserved in co-extruded fuel plates. To combat this, spark plasma sintering (SPS) was used for the fabrication of Al-15, 20, and 30 vol% U 3 O 8 and 8 and 12 vol% Mo-U 3 O 8 fuel meats for the Al-U 3 O 8 time. The in situ SPS data was used to construct and validate Master Sintering Curves (MSCs) with accuracies in Al fuels at 0.02 g/cm 3 , and Mo fuels at 0.07 and 0.17 g/cm 3 . The as-sintered fuel meats were characterised using x-ray diffraction (XRD) and scanning electron microscopy (SEM) to understand chemical and physical changes following the SPS process. The pellets exhibited very high relative densities, the U 3 O 8 was observed to undergo reduction to UO 2 .

Aluminium↗

Mechanical Properties of Irradiated U-10 wt. %Mo Alloy Degraded by Porosity Development

In this study, a plate-type nuclear fuel consisting of a solid monolithic foil of U-10 wt. %Mo is under development for use in the United States' high-performance research reactors. In support of developing this fuel, the fuel has been fabricated for the first time by a commercial fuel vendor and subsequently irradiated in a test reactor. This provides an opportunity to evaluate postirradiation mechanical properties of the commercially fabricated fuel. Four-point bend testing was conducted on the irradiated U-10Mo samples to generate the fuel material properties, including the modulus of elasticity and the bending strength. Although the material behaves in a brittle manner due to the accumulated porosity, a general trend of strength and modulus reduction was found as fission density increases. The data produced was evaluated using both Weibull statistics and a modulus degradation model with recommendations provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase Equilibria and Thermochemistry of Advanced Fuels: Modeling Burnup Behavior (Final Report)

Achieving the goal of developing advanced fuel concepts that meet the DOE objectives of being robust, demonstrating high performance, and are more tolerant of accident conditions than current fuel systems will require a thorough understanding of the thermophysical and thermochemical properties of the constituent materials. Non-oxide fuel systems are being explored under the Advanced Fuels Program that hold significant promise for improved performance and accident tolerance, including the uranium silicide-based system considered in the current work. Prospective cladding materials currently considered that contribute to improved accident tolerance include silicon carbide composites and ferritic alloys (Fe-Cr-Al base compositions). Thus, the effort developed thermochemical models and values, supported with targeted experiments, to evaluate the ferritic alloy and silicon carbide composite cladding systems in contrast to current zirconium alloy cladding. The developed detailed understanding will serve to aid in relatively early screening of candidate systems to avoid wasted effort, guide development of new fuel forms, and to provide a basis for predicting and modeling fuel performance. Major deliverables for the project included: Thermochemical assessment and models of phases in the U-Si and U-Si-N systems; thermochemical evaluation supported by experimental measurements of fuel-cladding interactions of silicide fuel with baseline zirconium, ceramic composite, and ferritic alloy cladding; thermochemical assessment and models of phases supported by experimental measurements for silicide fuel with key fission products provided in a dataset and reported in refereed publications. Within the project a significantly refined U-Si phase diagram was developed and reported that now includes homogeneity ranges for key phases, such at the U 3 Si 2 proposed fuel phase, and settles issues with regard to uncertainty in the stability of some phases. Computational efforts together with key experiments has determined phase formation in interactions between U 3 Si 2 and Zircaloy-4 cladding material, a ferritic FeCrAlY alloy of interest as an advanced cladding material, and silicon carbide, also of interest as a fiber-reinforced composite cladding. As expected, very significant reactions occur between U3Si2 and Zircaloy-4, with much less interaction at higher temperatures for the ferritic alloy, and finally interactions with SiC only in the region of contact. A potentially major issue is the stability of U 3 Si 2 fuel that has undergone significant burnup. The result is the loss of the uranium metal, liberating silicon, and the formation of concomitant fission product elements that either dissolve in the U 3 Si 2 phase or form independent, and possibly silicide phases. A combination of experimental determinations of phase formation of U 3 Si 2 reacted with representative fission products yttrium, gadolinium, cerium, zirconium, and molybdenum and first principles calculations has helped understand the fuel chemistry. The behavior of the U 3 Si 2 phase and the partitioning of silicon to possible fission product phases with burnup was thus determined, with significant dissolution in U 3 Si 2 of cerium, gadolinium, zirconium, and plutonium predicted along with independent phase formation of a U-Mo-Si ternary phase, yttrium silicide, and elemental selenium. It can be concluded that at significant burnup there will be a very minor amount of the U 3 Si 2 fuel phase that will decompose to a lower silicide or a uranium alloy as silicon preferentially forms a secondary phase.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Materials Data on U6Al39Mo8 by Materials Project

U6Mo8Al39 crystallizes in the hexagonal P6_3/mcm space group. The structure is three-dimensional. U is bonded in a 4-coordinate geometry to one U, three Mo, and thirteen Al atoms. The U–U bond length is 3.18 Å. There are two shorter (3.28 Å) and one longer (3.63 Å) U–Mo bond lengths. There are a spread of U–Al bond distances ranging from 3.05–3.50 Å. There are three inequivalent Mo sites. In the first Mo site, Mo is bonded to three equivalent U and nine Al atoms to form a mixture of distorted face and corner-sharing MoU3Al9 cuboctahedra. There are a spread of Mo–Al bond distances ranging from 2.64–2.77 Å. In the second Mo site, Mo is bonded in a cuboctahedral geometry to twelve Al atoms. There are six shorter (2.65 Å) and six longer (2.86 Å) Mo–Al bond lengths. In the third Mo site, Mo is bonded in a distorted q6 geometry to two equivalent U and ten Al atoms. There are a spread of Mo–Al bond distances ranging from 2.52–2.74 Å. There are six inequivalent Al sites. In the first Al site, Al is bonded in a 2-coordinate geometry to one U, two Mo, and three equivalent Al atoms. There are one shorter (2.70 Å) and two longer (2.89 Å) Al–Al bond lengths. In the second Al site, Al is bonded in a 2-coordinate geometry to two equivalent U, two Mo, and two Al atoms. There are one shorter (2.87 Å) and one longer (2.99 Å) Al–Al bond lengths. In the third Al site, Al is bonded in a 12-coordinate geometry to two equivalent U, one Mo, and nine Al atoms. There are two shorter (2.78 Å) and two longer (2.98 Å) Al–Al bond lengths. In the fourth Al site, Al is bonded in a 12-coordinate geometry to four equivalent U, two equivalent Mo, and six Al atoms. Both Al–Al bond lengths are 2.73 Å. In the fifth Al site, Al is bonded in a 3-coordinate geometry to two equivalent U and three Mo atoms. In the sixth Al site, Al is bonded in a distorted linear geometry to two equivalent Mo atoms.

36 MATERIALS SCIENCE↗