At least 73 records · Page 4

Thick section aluminum weldments for SRB structures

The Space Shuttle Solid Rocket Booster (SRB) forward and aft skirts were designed with fracture control considerations used in the design data. Fracture control is based on reliance upon nondestructive evaluation (NDE) techniques to detect potentially critical flaws. In the aerospace industry, welds on aluminum in the thicknesses (0.500 to 1.375 in.) such as those encountered on the SRB skirts are normally welded from both sides to minimize distortion. This presents a problem with the potential presence of undefined areas of incomplete fusion and the inability to detect these potential flaws by NDE techniques. To eliminate the possibility of an undetectable defect, weld joint design was revised to eliminate blind root penetrations. Weld parameters and mechanical property data were developed to verify the adequacy of the new joint design.

Bayless, E.↗

Laser Welding Of Contoured Thin-Wall Housings

Superalloy parts joined with less distortion. Carbon dioxide laser beam directed by optics in numerically controlled robot arm welds shell-type turbopump housings having complicated shapes. 5-kW laser, following single programmed three-dimensional pass, produces high-quality, full-penetration weld pass in age-hardenable nickel superalloy. Operator easily programs robot by using teaching pendant to track weld joint and keeps laser focused on workpiece while following contour of shell. Shells welded in rapid succession, with minimal change in setup for each.

Spiegel, Lyle B.↗

Creep performance and microstructure of grade 91 steel weldments with integrated welding and thermal processing

Ferritic-Martensitic steel welds typically require post weld heat treatment (PWHT) to restore toughness and high temperature performance. This off-line thermal process reduces disparities between weld and base metal, but can cause distortion, cracking, or simply be impractical due to assembly size and joint non-uniformity. Here we show integrated welding and thermal processing applied to modified 9Cr-1Mo (Grade 91) steel, favored for advanced power generation applications, performed in real time through the addition of a secondary heat source near the primary weld head. Optimal integrated processing reduces weld fusion and heat affected zone hardness by 125 HV, approaching performance of conventional 730 °C, 60 min PWHT processing. Microstructures and mechanical performance are compared for mechanized GTAW welds, with equivalent lifetimes noted in cross-weld creep rupture tests up to 234 MPa at 550 °C, and up to 104 MPa at 650 °C. The integrated process was validated on a Grade 91 pressure vessel with multipass cold wire feed GTAW. After 550 °C, 71.4 bar thermomechanical cyclic testing, the maximum weld hardness is <350 HV.

36 MATERIALS SCIENCE↗

The variable polarity plasma arc welding process: Characteristics and performance

Significant advantages of the Variable Polarity Plasma Arc (VPPA) Welding Process include faster welding, fewer repairs, less joint preparation, reduced weldment distortion, and absence of porosity. The power distribution was analyzed for an argon plasma gas flow constituting the fluid in the VPPA Welding Process. The major heat loss at the torch nozzle is convective heat transfer; in the space between the outlet of the nozzle and the workpiece; radiative heat transfer; and in the keyhole in the workpiece, convective heat transfer. The power absorbed at the workpiece produces the molten puddle that solidifies into the weld bead. Crown and root widths, and crown and root heights of the weld bead are predicted. The basis is provided for an algorithm for automatic control of VPPA welding machine parameters to obtain desired weld bead dimensions.

Hung, R. J.↗

Characteristics and performance of the variable polarity plasma arc welding process used in the Space Shuttle external tank

Significant advantages of the Variable Polarity Plasma Arc (VPPA) Welding Process include faster welding, fewer repairs, less joint preparation, reduced weldment distortion, and absence of porosity. Flow profiles and power distribution of argon plasma gas as a working fluid to produce plasma arc jet in the VPPA welding process was analyzed. Major loss of heat transfer for flow through the nozzle is convective heat transfer; for the plasma jet flow between the outlet of the nozzle and workpiece is radiative heat transfer; and for the flow through the keyhole of the workpiece is convective heat transfer. The majority of the power absorbed by the keyhole of the workpiece is used for melting the solid metal workpiece into a molten metallic puddle. The crown and root widths and the crown and root heights can be predicted. An algorithm for promoting automatic control of flow parameters and the dimensions of the final product of the welding specification to be used for the VPPA Welding System operated at MSFC are provided.

Hung, R. J.↗

Thermal Stir Welding Development at Marshall Space Flight Center

Solid state welding processes have become the focus of welding process development at NASA's Marshall Space Flight Center. Unlike fusion weld processes such as tungsten inert gas (TIG), variable polarity plasma arc (VPPA), electron beam (EB), etc., solid state welding processes do not melt the material during welding. The resultant microstructure can be characterized as a dynamically recrystallized morphology much different than the casted, dentritic structure typical of fusion weld processes. The primary benefits of solid state processes over fusion weld processes include superior mechanic properties and the elimination of thermal distortion and residual stresses. These solid state processes attributes have profoundly influenced the direction of advanced welding research and development within the NASA agency. Thermal Stir Welding (TSW) is a new solid state welding process being developed at the Marshall Space Flight Center. Unlike friction stir welding, the heating, stirring and forging elements of the weld process can be decoupled for independent control. An induction coil induces energy into a workpiece to attain a desired plastic temperature. An independently controlled stir rod, captured within non-rotating containment plates, then stirs the plasticized material followed by forging plates/rollers that work the stirred weld joint. The independent control (decoupling) of heating, stirring and forging allows, theoretically, for the precision control of microstructure morphology. The TSW process is being used to evaluate the solid state joining of Haynes 230 for ARES J-2X applications. It is also being developed for 500-in (12.5 mm) thick commercially pure grade 2 titanium for navy applications. Other interests include Inconel 718 and stainless steel. This presentation will provide metallurgical and mechanical property data for these high melting temperature alloys.

Ding, Robert J.↗

Localized material compression to correct distortion in wire arc additive manufacturing

Wire Arc Additive Manufacturing (WAAM) is an advanced manufacturing technology which utilizes welding systems to generate three dimensional geometries in a layer-by-layer fashion. Distortion or warping of a print substrate and WAAM components due to thermally induced residual stresses is an ongoing challenge limiting the widespread adoption of WAAM technologies for producing components. In this manuscript, a novel approach is described to address thermal distortion in deposited components by applying lateral compressions along the length of the deposited material. To demonstrate this method, a series of single-track walls were printed and compressed at evenly spaced intervals using a modified hydraulic cutter tool. The jaws of the tool were modified to compress material rather than to shear it. A mathematical model was developed to relate the curvature of the deposited material to the volume of compression required to eliminate this distortion. Validation of this model was performed using 3D scan data to compare the change in wall curvature induced by compression to the volume of the applied compressions. Substrate deflection was also compared against a control wall, and implementation of wall compression reduced maximum deflections by 93% across a series of four depositions and subsequent compressions. Wall cross sections were also analyzed to determine the impact of compression on material hardness and grain structure. The results demonstrate that successively placed lateral compressions can effectively control and potentially eliminate bending distortion in printed parts. This methodology can be further developed to form a robust model for correction of thermally-induced distortion in WAAM components.

Additive manufacturing↗

Integration of NASA-sponsored studies on aluminum welding

The results are presented of numerous studies relating to aluminum alloy welding. The subjects covered include: (1) effects of porosity on weld joint performance, (2) sources of porosity, (3) weld thermal effects, (4) residual stresses and distortion, and (5) manufacturing process system control.

Masubuchi, K.↗

Experimental Study of Residual Stresses in Hybrid Laser Arc and Submerged Arc-Welded 10-mm-Thick Low-Carbon Steel Plates

Offshore structures are constantly exposed to a multihazard marine environment that threatens their structural integrity. This imposes a high risk for extensive structural failures while various deterioration mechanisms may degrade the available capacity of the structures. Thus, no reliable decisions can be reached regarding design, operation, and survivability of the structures unless a deep comprehension of their fatigue performance is available, including welding-induced residual stresses. In particular, the continuous increase in size of the weldments for the offshore wind industry needs special attention with regard to welding-induced residual stresses, as they can reduce fatigue life, promote distortion, and contribute to stress corrosion cracking. Thus, the current design methods and increased structural dimensions as well as new design and manufacturing methods need to be inspected, understood, and optimized. Related to this, there is a growing need for evaluation of the effect of welding methods with various heat input density distributions. This article deals with the influence of welding method on the welding-induced residual stresses in 10-mm-thick low-carbon structural steel plates. The residual stresses are investigated in hybrid laser-arc welded and submerged arc butt-welded steel plates by means of experimental temperature profile measurements and neutron diffraction measurements and in accordance with existing production procedures. The residual stresses were measured at three different depths in the plates. The goal of the analysis is to gain a comprehensive understanding of the distribution and development of residual stresses in relation to the welding method for better control of the residual stresses and distortion. Furthermore, the repeatability of the neutron diffraction measurements is also investigated and reported in this article.

36 MATERIALS SCIENCE↗

Control of Weld Residual Stress in a Thin Steel Plate through Low Transformation Temperature Welding Consumables

Low transformation temperature welding (LTTW) consumables are characterized by a low martensite start temperature and a large fraction of martensite forming in the weld. It can efficiently reduce the tensile residual stress because the volume expansion associated with the martensitic transformation compensates for the thermal contraction during cooling. In this work, a LTTW wire, designated as EH200B, was created for the arc welding of advanced high-strength steel thin plates. In comparison to conventional ER70S-3 wires, this LTTW wire generated an opposite distortion pattern. Neutron diffraction measurements along the center thickness of the welded plates showed the maximum residual stress along the longitudinal direction (LD) in the weld region, and the heat-affected zone (HAZ) immediately adjacent to the weld region was reduced from ~330 MPa to below 240 MPa by using the LTTW wire. A finite element (FE) model was developed to predict the residual stress distributions of the plates welded under these two wires. The simulation results showed reasonable agreement with the volume-average neutron diffraction data. Compressive residual stress in the weld region using the LTTW wire was predicted by the FE method. Electron backscattered diffraction and x-ray diffraction measurements confirmed ~90% martensite was present in the LTTW weld. The fatigue life of DP980 steel lap joint panels using EH200B wire nearly doubled that of ER70S-3 wire. This improvement was attributed to the high strength and low LD residual stress in the weld and HAZ immediately adjacent to the weld.

36 MATERIALS SCIENCE↗

Stress characterization for friction-stir-welded electric vehicle battery trays with application of neutron diffraction

The battery tray is an essential component that protects and controls battery-cell temperatures in electric and plug-in hybrid vehicles. The functional stress limit of the battery tray heavily depends on the residual stress acquired from the manufacturing process. Consequently, exceeding the stress limit of the battery tray during operation could compromise the battery-cell banks and may risk the vehicle's safety. Hence, understanding residual stress formation is vital for design and safety concerns. Here, in the current study, AA 6061-plates were friction stir welded to an A365 high-pressure die-cast battery tray to create sealed coolant channels in the battery tray. However, this multi-material lap friction stir weld introduces residual stress into the battery tray, resulting in distortion. This distortion was mitigated using burnishing or coining operations, though straightening the battery tray had initially unknown effects on the residual stress. Therefore, neutron diffraction was utilized to characterize residual stresses after straightening. The results indicate that the friction stir welding (FSW) operation generated residual stresses exceeding the yield strength of the material, consequently deforming the battery tray by ±3 mm from the pre-weld geometry. The burnishing operation reduced the residual stresses below the material's yield strength while restoring the tray to within ±0.75 mm of the pre-weld geometry. Similarly, the coining operation restored the battery tray to within ±0.75 mm of the pre-weld geometry, however, increasing the number of locations where the residual stress exceeds the yield strength of the material.

36 MATERIALS SCIENCE↗

Investigation of Friction Stir Welding and Laser Engineered Net Shaping of Metal Matrix Composite Materials

The improvement in weld quality by the friction stir welding (FSW) process invented by TWI of Cambridge, England, patented in 1991, has prompted investigation of this process for advanced structural materials including Al metal matrix composite (Al-MMC) materials. Such materials can have high specific stiffness and other potential beneficial properties for the extreme environments in space. Developments of discontinuous reinforced Al-MMCs have found potential space applications and the future for such applications is quite promising. The space industry has recognized advantages of the FSW process over conventional welding processes such as the absence of a melt zone, reduced distortion, elimination of the need for shielding gases, and ease of automation. The process has been well proven for aluminum alloys, and work is being carried out for ferrous materials, magnesium alloys and copper alloys. Development work in the FSW welding process for joining of Al-MMCs is relatively recent and some of this and related work can be found in referenced research publications. NASA engineers have undertaken to spear head this research development work for FSW process investigation of Al-MMCs. Some of the reported related work has pointed out the difficulty in fusion welding of particulate reinforced MMCs where liquid Al will react with SiC to precipitate aluminum carbide (Al4C3). Advantages of no such reaction and no need for joint preparation for the FSW process is anticipated in the welding of Al-MMCs. The FSW process has been best described as a combination of extrusion and forging of metals. This is carried out as the pin tool rotates and is slowly plunged into the bond line of the joint as the pin tool's shoulder is in intimate contact with the work piece. The material is friction-stirred into a quality weld.

Ravinder M. Diwan↗

Counterrotating-Shoulder Mechanism for Friction Stir Welding

A counterrotating-shoulder mechanism has been proposed as an alternative to the mechanism and fixtures used in conventional friction stir welding. The mechanism would internally react most or all of the forces and torques exerted on the workpiece, making it unnecessary to react the forces and torques through massive external fixtures. In conventional friction stir welding, a rotating pin tool is inserted into, and moved along, a weld seam. As the pin tool moves, it stirs together material from the opposite sides of the seam to form the weld. A large axial plunge force must be exerted upon the workpiece through and by the pin tool and a shoulder attached above the pin tool in order to maintain the pressure necessary for the process. The workpiece is secured on top of an anvil, which supports the workpiece against the axial plunge force and against the torque exerted by the pin tool and shoulder. The anvil and associated fixtures must be made heavy (and, therefore, are expensive) to keep the workpiece stationary. In addition, workpiece geometries must be limited to those that can be accommodated by the fixtures. The predecessor of the proposed counterrotating-shoulder mechanism is a second-generation, self-reacting tool, resembling a bobbin, that makes it possible to dispense with the heavy anvil. This tool consists essentially of a rotating pin tool with opposing shoulders. Although the opposing shoulders maintain the necessary pressure without need to externally apply or react a large plunge force, the torque exerted on the workpiece remains unreacted in the absence of a substantial external fixture. Depending on the RPM and the thickness of the workpiece, the torque can be large. The proposed mechanism (see figure) would include a spindle attached to a pin tool with a lower shoulder. The spindle would be coupled via splines to the upper one of three bevel gears in a differential drive. The middle bevel gear would be the power-input gear and would be coupled to the upper and lower bevel gears. The lower bevel gear would be attached to the upper shoulder and would slide and rotate freely over the spindle. The spindle would be fastened by its threaded upper end to an external submechanism that would exert axial tension on the spindle to load the workpiece in compression between the shoulders. By reducing or eliminating (relative to the use of a self reacting tool) the torque that must be reacted externally, the use of the proposed tool would reduce the tendency toward distortion or slippage of the workpiece. To begin a weld, the spindle would be inserted through a hole in the workpiece or run-on tab at the beginning of the seam and fastened to the loading submechanism. Rotation and axial loading would be increased gradually from zero and, after a time to be determined by trial and error, translation along the weld seam would be increased gradually from zero to a steady weld speed. The weld would be ended by running the mechanism off the workpiece or, if the lower shoulder were detachable, by detaching the lower shoulder from the spindle and pulling the pin tool out.

Nunes, Arthur C., Jr.↗

Results of Uranium Dioxide-Tungsten Irradiation Test and Post-Test Examination

A uranium dioxide (UO2) fueled capsule was fabricated and irradiated in the NASA Plum Brook Reactor Facility. The capsule consisted of two bulk UO2 specimens clad with chemically vapor deposited tungsten (CVD W) 0.762 and 0.1016 cm (0.030-and 0.040-in.) thick, respectively. The second specimen with 0.1016-cm (0.040-in.) thick cladding was irradiated at temperature for 2607 hours, corresponding to an average burnup of 1.516 x 10 to the 20th power fissions/cu cm. Postirradiation examination showed distortion in the bottom end cap, failure of the weld joint, and fracture of the central vent tube. Diametral growth was 1.3 percent. No evidence of gross interaction between CVD tungsten or arc-cast tungsten cladding and the UO2 fuel was observed. Some of the fission gases passed from the fuel cavity to the gas surrounding the fuel specimen via the vent tube and possibly the end-cap weld failure. Whether the UO2 loss rates through the vent tube were within acceptable limits could not be determined in view of the end-cap weld failure.

Collins, J. F.↗

Metal Cutting Theory and Friction Stir Welding Tool Design

Friction Stir Welding (FSW) is a relatively new industrial process that was invented at The Weld Institute (TWI, United Kingdom) and patented in 1992 under research funded by in part by the National Aeronautics and Space Administration (NASA). Often quoted advantages of the process include good strength and ductility along with minimization of residual stress and distortion. Less well advertised are the beneficial effects of this solid state welding process in the field of occupational and environmental safety. It produces superior weld products in difficult to weld materials without producing any toxic fumes or solid waste that must be controlled as hazardous waste. In fact, it reduces noise pollution in the workspace as well. In the early days of FSW, most welding was performed on modified machine tools, in particular on milling machines with modified milling cutters. In spite of the obvious milling heritage of the process, the techniques and lessons learned from almost 250 years of successful metalworking with milling machines have not been applied in the field of modern Friction Stir Welding. The goal of the current research was to study currently successful FSW tools and parameterize the process in such a way that the design of new tools for new materials could be accelerated. Along the way, several successful new tooling designs were developed for current issues at the Marshall Space Flight Center with accompanying patent disclosures

Payton, Lewis N.↗

Advanced Process Possibilities in Friction Crush Welding of Aluminum, Steel, and Copper by Using an Additional Wire

Joining sheet metal can be problematic using traditional friction welding techniques. Friction crush welding (FCW) offers a high speed process which requires a simple edge preparation and can be applied to out-of-plane geometries. In this work, an implementation of FCW was employed using an additional wire to weld sheets of EN AW5754 H22, DC01, and Cu-DHP. The joint is formed by bringing together two sheet metal parts, introducing a wire into the weld zone and employing a rotating disk which is subject to an external force. The requirements of the welding preparation and the fundamental process variables are shown. Thermal measurements were taken which give evidence about the maximum temperature in the welding center and the temperature in the periphery of the sheet metals being joined. The high welding speed along with a relatively low heat input results in a minimal distortion of the sheet metal and marginal metallurgical changes in the parent material. In the steel specimens, this FCW implementation produces a fine grain microstructure, enhancing mechanical properties in the region of the weld. Aluminum and copper produced mean bond strengths of 77 and 69 pct to that of the parent material, respectively, whilst the steel demonstrated a strength of 98 pct. Using a wire offers the opportunity to use a higher-alloyed additional material and to precisely adjust the additional material volume appropriate for a given material alignment and thickness.

36 MATERIALS SCIENCE↗

Multi-scale and multi-technic microstructure analysis of a linear friction weld of the metastable-β titanium alloy Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) towards a new Post-Weld Heat Treatment

Highlights: • Soft joint showing sharp macro-zones and marked by asymmetrical process effects • Gradient of thermomechanical loads identified through progressive stages of transformation • Highly textured recrystallized β grains at the joint core with distorted β lattice • Lattices, phase fractions, microstructures and hardness homogenized after heat treatment - Abstract: Linear Friction Welding (LFW) is a solid-state joining process producing narrow joints mainly developed for the aircraft industry. The Thermo-Mechanical Processing (TMP) loads imposed on the material cause complex microstructure transformations. This study aimed at characterizing the local microstructures and crystallographic configurations to identify the mechanisms impacting the stability and the mechanical properties of a Ti17 LFW joint with the objective of establishing an innovative homogenizing Post-Weld Heat Treatment (PWHT). The process caused a narrow zone of ±2 mm from the friction interface to reach the isothermal α → β transformation temperature under a heating rate of 500 K/s followed by quenching (−100 K/s). The TMP resulted in the formation a ±3 mm wide soft Process Affected Zone (PAZ) delimited by three characteristic zones: the Welding Line (WL width ≈ 400 μm), The Thermo-Mechanically Affected Zone (TMAZ width ≈ 1 mm) and the Heat Affected Zone (HAZ). β TMP resulted in the total dissolution of the α phase in the joint core (WL + TMAZ) and formed strongly textured {110}<111> β recrystallized grains in the WL by continuous dynamic recrystallization of squeezed prior-β grains in the TMAZ. α + β TMP led to a gradual loss of hardness in the HAZ whose microstructure is similar to the one of the base material (BM) but is subject to gradual α laths dissolution due to the local temperatures experienced during LFW. A PWHT consisting in a β annealing followed by an α + β ageing resulted in a uniformly hardened weld with a homogenized Widmanstätten microstructure in the whole assembly.

36 MATERIALS SCIENCE↗

Helium pressure increase inside GPHS clads: implications for formation of distended clads

Distension of GPHS clads has generally been attributed to gas buildup inside the clad. The bulging vent frit cover can be caused only by gas pressure, since the vent cover is isolated from the fuel by the vent frit. Gas generation is the only change expected as the oxide fuel ages. However, several data suggest that gas pressure is not the origin of the distension of the clad body. Gas pressure sufficient to distend the iridium body of the clad would be on the order of 1500 psi. This high pressure is very unlikely to be reached inside a GPHS clad, because the vent frit cover weld cannot sustain high pressures. Every distended clad that has been examined has an open vent frit, suggesting that the vent frit cover eventually opens on all distended GPHS clads. No gas pressure has been observed in any distended clad. In addition, the vent frit cover is sufficiently thin, about 2 grains thick, that diffusion of helium through the intact cover is possible and almost certainly occurs. Conversely, no clad has ever been definitively observed to distend after venting. Removal of the vent cover allows free escape of any radiolytically generated helium. However, there is little data on the behavior of vented GPHS. The vent cover is seldom removed at LANL, and vent covers are not removed on clads that will be stored. The vent covers are known to have been removed from the four clads residing in a module which was stored for 8 years. Expansion of the fuel is more likely to provide sufficient force on the iridium clad to distort the iridium metal. Radiographs indicate that the fuel inside a distended GPHS clad is also distended, filling all or most of the interior volume of the GPHS. No radiograph shows the fuel expanded and in contact with the weld shield and the distorted side of the GPHS clad without distension. However, radiography is infrequently done on stored clads unless they exhibit distension, so the dimensions of fuel in normal clads are not generally known.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗