Search NASA⌕ Search

SEARCH · Search NASA

Results for “ball milling”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Thermal Evolution of Internal Strain in Doped PbTe

Recent improvements in the efficiency of heat-to-electricity energy conversion in lead chalcogenide thermoelectrics involve reducing the thermal conductivity by incorporating large amounts of internal strain. The extent to which typical lead chalcogenide processing techniques (such as doping, ball milling, and densification) increase internal strain and dislocation density must be quantified to improve materials design. In this study, neutron powder diffraction is leveraged to evaluate the internal strain introduced by ball milling in doped and undoped powders. Doping with Na and/or Eu increases internal strain beyond ball milling alone, with the greatest increase from combining the two dopants. Strain recovery occurs in each powder above 400 K but can be suppressed by co-doping, indicating a strong dopant–dislocation interaction in this system. Therefore, high-temperature processing of PbTe powders should be avoided if high internal strain is desired. Low-temperature densification and/or rapid pressing techniques may be key to maintaining internal strain in the final pressed pellet. The diffraction peak asymmetry and correlated elastic softening measured in pressed PbTe pellets in past studies were not observed in the precursor powders measured here, suggesting that measurements of the Debye temperature on final pressed pellets are required to examine the influence of defect-induced elastic softening on thermal conductivity. This work provides key guidance for defect engineering to maximize internal strain and thermoelectric performance in PbTe thermoelectrics.

36 MATERIALS SCIENCE↗

Fabrication, oxidation, and combustion of nanoscale magnesium diboride and tetraboride

The difficult ignition of boron decreases the combustion efficiency of boron-loaded, fuel-rich propellants. One approach to solving this problem involves the use of magnesium diboride (MgB2), which ignites easier than boron. Magnesium tetraboride (MgB4) offers greater energy density owing to its higher boron content. However, the effect of B/Mg ratio on the ignition and combustion is unknown. Additionally, while nanoscale MgB₂ particles and quasi-2D structures were recently recognized as promising energetic additives, the oxidation and combustion properties of nanoscale MgB₄ have not been explored. The objectives of the present work included synthesis, purification, and high-energy ball milling of MgB2 and MgB4 powders as well as investigation of their thermal decomposition, oxidation, and combustion. The MgB2 and MgB4 powders were fabricated by combustion synthesis in the chemical oven mode and by heating Mg/B mixtures in a tube furnace. The latter method was superior in the synthesis of MgB4. Oxide impurities in the synthesized powders were removed by acid leaching. Nanoscale powders were obtained by high-energy ball milling. Thermal decomposition and oxidation of the obtained MgB₂ and MgB₄ powders were investigated by conducting non-isothermal thermogravimetric analysis (TGA) at temperatures up to 1550 °C in argon and oxygen flows. Combustion of B, MgB₂, and MgB₄ powders with oxygen at atmospheric pressure was studied in a windowed chamber using laser ignition and high-speed video recording. The TGA has shown multi-step decomposition of both magnesium borides in an argon environment. The maximum oxidation rate of MgB4 in oxygen was observed at a much lower temperature than in the case of MgB2. In the combustion experiments, both magnesium borides burned much faster than submicron boron. Ball milling of the borides further increased their burning rates. It has been concluded that nanoscale magnesium tetraboride is a promising ingredient for fuel-rich propellants owing to its high energy density, efficient oxidation, and rapid combustion.

Molina, Andre [The University of Texas at El Paso]↗

Particle size reduction of Si3N4 with Si3N4 milling hardware

The grinding of Si3N4 powder using reaction bonded Si3N4 attrition, vibratory, and ball mills with Si3N4 media was examined. The rate of particle size reduction and the change in the chemical composition of the powder were determined in order to compare the grinding efficiency and the increase in impurity content resulting from mill and media wear for each technique. Attrition and vibratory milling exhibited rates of specific surface area increase that were approximately eight times that observed in ball milling. Vibratory milling introduced the greatest impurity pickup.

Herbell, T. P.↗

Particle-size reduction of Si3N4 powder with Si3N4 milling hardware

The grinding of Si3N4 powder using reaction bonded Si3N4 attrition, vibratory, and ball mills with Si3N4 media was examined. The rate of particle size reduction and the change in the chemical composition of the powder were determined in order to compare the grinding efficiency and the increase in impurity content resulting from mill and media wear for each technique. Attrition and vibratory milling exhibited rates of specific surface area increase that were approximately eight times that observed in ball milling. Vibratory milling introduced the greatest impurity pickup.

Herbell, T. P.↗

Sustainable and Green Production of Nanostructured Cellulose by a 2-Step Mechano-Enzymatic Process

Nanostructured cellulose (NC) represents an emerging sustainable biomaterial for diverse biotechnological applications; however, its production requires hazardous chemicals that render the process ecologically unfriendly. Using commercial plant-derived cellulose, an innovative strategy for NC production based on the combination of mechanical and enzymatic approaches was proposed as a sustainable alternative to conventional chemical procedures. After ball milling, the average length of the fibers was reduced by one order of magnitude (down to 10–20 μm) and the crystallinity index decreased from 0.54 to 0.07–0.18. Moreover, a 60 min ball milling pre-treatment followed by 3 h Cellic Ctec2 enzymatic hydrolysis led to NC production (15% yield). Analysis of the structural features of NC obtained by the mechano-enzymatic process revealed that the diameters of the obtained cellulose fibrils and particles were in the range of 200–500 nm and approximately 50 nm, respectively. Interestingly, the film-forming property on polyethylene (coating ≅ 2 μm thickness) was successfully demonstrated and a significant reduction (18%) of the oxygen transmission rate was obtained. Altogether, these findings demonstrated that nanostructured cellulose could be successfully produced using a novel, cheap, and rapid 2-step physico-enzymatic process that provides a potential green and sustainable route that could be exploitable in future biorefineries.

59 BASIC BIOLOGICAL SCIENCES↗

Novel processing route for design and manufacturing of metal toughened nanoceramics: Al–Al 2 O 3 nanocermets

Monolithic alumina is a highly brittle ceramic with a very low fracture toughness, making it an unreliable material for mechanical and structural applications. Ceramic-metal composites (cermets) are the subject of intensive interest to obtain materials which can address the intrinsic brittleness of ceramics without compromising their high strength and light weight. In the present investigation, aluminium-alumina (Al–Al 2 O 3 ) nanocermets were developed. The nanocermets possessed the toughness of Al phase and the strength of reinforced nano Al 2 O 3 particles. Here, the nanocermets green bodies were prepared such that upon sintering each adjacent Al 2 O 3 grain was conformally coated with a continuous Al film. Mechanical milling via a combination of cryo-milling and ball-milling was used to prepare Al–Al 2 O 3 nano-powder mixture. Spark plasma sintering was used to consolidate the green nanocermets. Results show that specimens prepared from 35 h milled powders exhibited superior mechanical properties as compared to other nanocermets, with an improvement in microhardness, elastic modulus, compressive strength, and flexural strength by 88%, 78%, 69% and 40% with respect to sintered pure Al. The indentation toughness of 35 h milled nanocermet showed an increment of 12.5% with respect to sintered pure Al 2 O 3 . Characterization techniques such as XRD, SEM, HR-TEM, X-ray tomography were employed to investigate the phase evolution and structural morphology, while FEM simulations were performed for understanding the crack propagation mechanisms in nanocermets.

36 MATERIALS SCIENCE↗

Cleaning Internal-Weld Splatter

Splattered metal produced by welding can be easily removed from inaccessible areas by method resembling ball milling. Hard steel balls are vibrated inside welded unit so that they "scrub away" excess metal on interior side of weld joint.

Snodgrass, R.↗

Effect of V Content on Corrosion Behavior of Al-V Alloys Produced by Mechanical Alloying and Subsequent Spark Plasma Sintering

Al-V alloys produced via high-energy ball milling have been reported to show simultaneous improvement of corrosion resistance and mechanical properties compared to traditional Al alloys. In these alloys, V content plays a crucial role in increasing or decreasing the corrosion resistance. Therefore, the effect of V and microstructure on corrosion of high-energy ball milled and subsequently spark plasma sintered Al-xV alloys (x = 2, 5, 10 at%) has been studied. Cyclic potentiodynamic polarization tests and electrochemical impedance spectroscopic analysis revealed the increment of V content up to 5 at% enhanced the corrosion resistance of the alloy. However, highly heterogeneous microstructure in Al-10 at%V resulted in significant localized corrosion over the immersion time. The electrochemical impedance spectroscopy studies over 14 days of immersion revealed underlying corrosion mechanisms.

36 MATERIALS SCIENCE↗

Microstructural Transitions during Powder Metallurgical Processing of Solute Stabilized Nanostructured Tungsten Alloys

Exploiting grain boundary engineering in the design of alloys for extreme environments provides a promising pathway for enhancing performance relative to coarse-grained counterparts. Due to its attractive properties as a plasma facing material for fusion devices, tungsten presents an opportunity to exploit this approach in addressing the significant materials challenges imposed by the fusion environment. Here, we employ a ternary alloy design approach for stabilizing W against recrystallization and grain growth while simultaneously enhancing its manufacturability through powder metallurgical processing. Mechanical alloying and grain refinement in W-10 at.% Ti-(10,20) at.% Cr alloys are accomplished through high-energy ball milling with transitions in the microstructure mapped as a function of milling time. We demonstrate the multi-modal nature of the resulting nanocrystalline grain structure and its stability up to 1300 °C with the coarser grain size population correlated to transitions in crystallographic texture that result from the preferred slip systems in BCC W. Field-assisted sintering is employed to consolidate the alloy powders into bulk samples, which, due to the deliberately designed compositional features, are shown to retain ultrafine grain structures despite the presence of minor carbides formed during sintering due to carbon impurities in the ball-milled powders.

36 MATERIALS SCIENCE↗

Effects of carbon substitution on magnetic properties and magnetocaloric effects in Mn 65-x Ga 17 C 18+x compounds

This study involved the tuning of the magnetic, magnetocaloric, and room-temperature structural properties of Mn 65-x Ga 17 C 18+x (0 ≤ x ≤ 4) compounds prepared using a high-energy ball milling (HEBM) technique. This study indicates that the crystal structure of all the compounds can be described as an anti-perovskite cubic structure with the Pm-3m space group and the crystal cell volume decreases with increasing carbon concentration. The system shows a first-order structural phase transition at a temperature T=T M between two cubic phases having different magnetic structures. The phases are characterized by antiferromagnetic (AFM) and ferromagnetic (FM) -like behavior at low (T < T M ) and high (T M > T) temperature regions, respectively. A suppression of the AFM phase was observed with increasing C concentration. The temperature-induced first-order transitions (FOTs) were found to possess a small thermal hysteresis in the magnetization (~2-3 K) in an applied magnetic field of H = 50 kOe. Magnetic entropy changes estimated from isothermal magnetization curves indicate that the largest value of the magnetic entropy change of |ΔS M | = 2.1 J kg -1 K -1 for x = 4 with ΔH = 50 kOe, with a relative cooling power (RCP) of ~190 J kg -1 . Furthermore, high-energy ball milling (HEBM), a scalable technique, has been demonstrated as a viable method to synthesize magnetocaloric materials with substantial RCP values.

36 MATERIALS SCIENCE↗

Effects of mechanically alloying Al 2 O 3 and Y 2 O 3 additives on the liquid phase sintering behavior and properties of SiC

In order to improve the sintering of SiC, mixtures of Al 2 O 3 and Y 2 O 3 powders are commonly included as sintering additives. The aim of this work was to use mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures as sintering additives to promote liquid phase sintering of SiC using spark plasma sintering. The results showed that milling reduced the particle size of the powders and led to the formation of complex oxide phases (YAP, YAM, and YAG) at low temperatures. As the ball milling time increased, the mass loss of specimens sintered with mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures decreased, and accordingly the relative density increased. However, the hardness and flexural strength of sintered SiC specimens first increased and then decreased. Because the specimens prepared with oxides milled for a long time contained too much YAG/YAP and accordingly too much liquid at sintering temperature. This negatively affected the mechanical properties of the SiC specimens because of the increased volume of the complex oxide phases, which have inferior mechanical properties to SiC, in the sintered specimens. In conclusion, when the ball milling time was 6h, the hardness (24.02 GPa) and flexural strength (655.61 MPa) of the SiC specimens reached maximum values.

36 MATERIALS SCIENCE↗

Metal-ceramic composite powders

A process for manufacturing metal-ceramic composite material powder comprising ball milling metal powder and ceramic nanoparticles to yield a metal-ceramic composite powder comprising ceramic nanoparticles embedded in a metal matrix powder particles; wherein the ball milling is performed using a ceramic milling media and a milling vessel having a ceramic interior surface. Metal matrix nanocomposite powders comprising ceramic nanoparticles imbedded in metal matrix powder particles; wherein the metal matrix powder particles have a spherical shape; wherein there is uniform distribution the ceramic nanoparticles; wherein the nanocomposite powders have good flowability.

Chen, Lianyi↗

Sharpening ball-nose mill cutters

Economical attachment allows faster, more precise grinding. Vibrationless and rigid relation between grinding wheel and cutter allows for extremely high finish and accurate grinding. Leveling device levels flutes with respect to toolholder rotation that generates ball-nose radius. Constant relief around entire profile of cutting edge produces longer tool life.

Burch, C. F.↗

Densification, microstructure, and mechanical properties of Mo–30W alloys fabricated from conditioned powders

Refractory alloys, such as molybdenum-based systems, are attracting growing interest for applications in extreme environments, such as in the nuclear and aerospace industries. Recent advances in sintering technologies, coupled with mechanical alloying, have enabled the tailored design of these alloys by leveraging powder characteristics to control final microstructures and mechanical properties. In this study, Mo-30W alloys were fabricated using electric field-assisted sintering (EFAS) from ball-milled powders with and without hydrogen treatment to investigate the influence of surface oxides on material properties and sintering behavior. The results revealed that samples processed from as-ball-milled powder contained a high density of oxides within the microstructure, whereas oxide presence was significantly reduced in samples fabricated from hydrogen-treated powders. Interestingly, the two powder types led to opposite trends in grain size distribution: samples from untreated powders exhibited grain refinement from sample periphery to the center, while samples from hydrogen-treated powders showed grain coarsening toward the center. This behavior is attributed to temperature gradients present during sintering due to electrical percolation pathway differences during Joule heating. The powder surface oxides may have influenced the temperature distribution and grain evolution. Microhardness profiles measured along both axial and thickness directions were consistent with the grain size distribution. Furthermore, oxide films on powder surfaces have delayed densification by hindering particle necking and atomic diffusion during sintering.

36 - MATERIALS SCIENCE↗

The properties of the nitrogen-vacancy center in milled chemical vapor deposition nanodiamonds

Fluorescent nanodiamonds (FNDs) containing negatively charged nitrogen-vacancy (NV − ) centers are vital for many emerging quantum sensing applications from magnetometry to intracellular sensing in biology. However, developing a scalable fabrication method for FNDs hosting color centers with consistent bulk-like photoluminescence (PL) and spin coherence properties remains a highly desired but unrealized goal. Here, we investigate optimized ball milling of single-crystal diamonds produced via chemical vapor deposition (CVD) and containing 2 ppm of substitutional nitrogen and 0.3 ppm of NV − to achieve this goal. The NV charge state, PL lifetime, and spin properties of bulk CVD diamond samples are directly compared to milled CVD FNDs and commercial high-pressure high-temperature (HPHT) FNDs. We find that on average, the relative contribution of the NV − charge state to the total NV PL is lower and the NV PL lifetime is longer in CVD FNDs compared to HPHT FNDs, both likely due to the lower N s 0 concentration in CVD FNDs. The CVD bulk and CVD FNDs on average show similar average T 1 spin relaxation times of 3.2 ± 0.7 ms and 4.7 ± 1.6 ms, respectively, compared to 0.17 ± 0.01 ms for commercial HPHT FNDs. Our results demonstrate that ball milling of CVD diamonds enables the large-scale fabrication of NV ensembles in FNDs with bulk-like T 1 spin relaxation properties.

chemical vapor deposition↗

Uranium nitride (UN) pellets with controllable microstructure and phase – fabrication by spark plasma sintering and their thermal-mechanical and oxidation properties

Dense uranium mononitride (UN) pellets with controlled microstructures and tailored grain size from large-grained to a few microns are synthesized by spark plasma sintering (SPS) combined with high energy ball milling. The impacts of the sintering conditions on fuel microstructure, grain size, physical density, and phase behavior are systematically investigated, and the thermal-mechanical properties and oxidation behavior of the SPS densified UN pellets are characterized. Higher sintering temperatures and longer ball milling durations and thus finer starting UN powders promote sintering and densification, and dense UN pellets above 95% theoretical density can be achieved by SPS at 1873 K for 10 min. UN phase purity is maintained in the SPS-densified pellets sintered at a lower temperature and short duration. A phase heterogeneity with secondary UO 2 or uranium sesquinitride (U 2 N 3 ) occurs for the UN pellets sintered at higher temperatures using finer UN powders. The hardness and fracture toughness of the SPS-densified UN pellets increase with smaller grain sizes and higher densities to 7.9 GPa and 3.5 MPa m 1/2 , respectively. Furthermore, both small (1–2 μm) and large grain-sized (30–50 µm) UN pellets exhibit good thermal conductivity. Dynamic oxidation testing by a thermogravimetric analyzer in air shows that the onset temperature for oxidation varies with microstructure and phase heterogeneity of the SPS densified UN pellets. Particularly, the smaller-grained (micron-sized) UN pellets containing uranium oxides and U 2 N 3 display lower weight gain and significantly-reduced oxidation kinetics, and full oxidation completes at a temperature above 1173 K when tested with a ramp rate of 10 K/min.

36 MATERIALS SCIENCE↗

Doping effect of Al in LLZO

Lithium ion batteries have become a common use in most electronic devices and transportation. However, the use of liquid electrolytes poses a serious safe hazard due to their high flammability. The narrow operating temperature and voltage windows also limit further improvement of the energy density.Solid-state lithium batteries with the use of more stable and safer solid electrolyte have garnered much attention and could be the future choice for battery technology. A promising potential candidate for the solid electrolyte component is the garnet type Li 7 La 3 Zr 2 O 12 (LLZO) ceramic material since it possesses high ionic conductivity at room temperature and enables the use of high capacity lithium anode and high voltage/capacity cathodes.However, to form the stable cubic phase of LLZO and high densification,high sintering temperatures above 1100°C is typically required, which causes Lithium loss of the system.Many studieshave been taken to dop LLZO with various precursors such as Ga, Ta, and Al to stabilize the cubic structure and reduce calcination temperature, while the doping effect on sintering densification is still unclear. In this study Al doping along with ball milling were explored to stabilize the cubic phase of LLZO and improve densification, while reducing the amount of impurity phases. Samples were synthesized from the precursors Li 2 CO 3 , Al 2 O 3 , La 2 O 3 , and ZrO 2 by ball milling followed by heat treatment for 12 hours at 1000°C. XRD with Rietveld fitting was used to determine the two phases of LLZO (cubic, tetragonal) and other possible secondary phases. Furthermore,SEM with top and cross sectional views was conducted to investigate the morphology and microstructure of sintered pellets.

36 MATERIALS SCIENCE↗

Support of Adhesion Mechanisms in Al 2 O 3 Aerosol Deposition Through Laser-Induced Particle Impact Testing

Aerosol deposition (AD) is a kinetic spray process capable of depositing ceramic coatings at room temperature, but AD process development is generally a laborious exploration of a large process parameter space. Here, this paper presents a case study investigating whether laser-induced particle impact testing (LIPIT) could be applied to expedite development of an alumina (Al 2 O 3 ) coating on nickel (Ni): Specifically, whether LIPIT measurements could predict critical velocities of adhesion on Ni and Al 2 O 3 , and the effect of ball milling the Al 2 O 3 powder. Because LIPIT has a diffraction-limited lower bound on imageable particle size, the usefulness of Al 2 O 3 powder agglomerates as a proxy for single particles was additionally studied. Overall, LIPIT measurements and AD sprays agreed that ball milling dramatically improves adhesion. Additionally, LIPIT measurements of critical velocity of adhesion of Al 2 O 3 powder agglomerates on Ni and Al 2 O 3 substrates (150 meters per second [m/s] and 250 m/s, respectively) quantitatively agreed with predictions from a previously published model based on picoindentation and molecular dynamics simulations. Together, these findings support the established hypothesis that Al 2 O 3 adheres via a dislocation-mediated mechanism in AD, that Al 2 O 3 powder agglomerates adhere as individual constituent particles rather than collectively, and that, for this case study, LIPIT measurements were predictive of AD process parameters.

Al2O3↗