At least 73 records · Page 4

An ultra-thin buffer layer for Ge epitaxial layers on Si

Using an Fe{sub 3}Si insertion layer, we study epitaxial growth of Ge layers on a Si substrate by a low-temperature molecular beam epitaxy technique. When we insert only a 10-nm-thick Fe{sub 3}Si layer in between Si and Ge, epitaxial Ge layers can be obtained on Si. The detailed structural characterizations reveal that a large lattice mismatch of {approx}4% is completely relaxed in the Fe{sub 3}Si layer. This means that the Fe{sub 3}Si layers can become ultra-thin buffer layers for Ge on Si. This method will give a way to realize a universal buffer layer for Ge, GaAs, and related devices on a Si platform.

36 MATERIALS SCIENCE↗

Doped LZO buffer layers for laminated conductors

A laminated conductor includes a metallic substrate having a surface, a biaxially textured buffer layer supported by the surface of the substrate, the biaxially textured buffer layer comprising LZO and a dopant for mitigating metal diffusion through the LZO, and a biaxially textured conductor layer supported by the biaxially textured buffer layer.

Paranthaman, Mariappan Parans↗

Carbon doped GaN buffer layer using propane for high electron mobility transistor applications: Growth and device results

The creation of a semi insulating (SI) buffer layer in AlGaN/GaN High Electron Mobility Transistor (HEMT) devices is crucial for preventing a current path beneath the two-dimensional electron gas (2DEG). In this investigation, we evaluate the use of a gaseous carbon gas precursor, propane, for creating a SI GaN buffer layer in a HEMT structure. The carbon doped profile, using propane gas, is a two stepped profile with a high carbon doping (1.5 × 10{sup 18 }cm{sup −3}) epitaxial layer closest to the substrate and a lower doped layer (3 × 10{sup 16 }cm{sup −3}) closest to the 2DEG channel. Secondary Ion Mass Spectrometry measurement shows a uniform incorporation versus depth, and no memory effect from carbon doping can be seen. The high carbon doping (1.5 × 10{sup 18 }cm{sup −3}) does not influence the surface morphology, and a roughness root-mean-square value of 0.43 nm is obtained from Atomic Force Microscopy. High resolution X-ray diffraction measurements show very sharp peaks and no structural degradation can be seen related to the heavy carbon doped layer. HEMTs are fabricated and show an extremely low drain induced barrier lowering value of 0.1 mV/V, demonstrating an excellent buffer isolation. The carbon doped GaN buffer layer using propane gas is compared to samples using carbon from the trimethylgallium molecule, showing equally low leakage currents, demonstrating the capability of growing highly resistive buffer layers using a gaseous carbon source.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High spin polarization in epitaxial Fe 4 N thin films using Cr and Ag as buffer layers

Fe 4 N thin films with (001) texture were prepared by reactive sputtering on MgO substrates, utilizing either a Cr or Ag buffer layer to facilitate the epitaxial growth. X-ray diffraction, atomic force microscopy, and vibrating sample magnetometry measurements show that the Fe 4 N thin film grown on the Ag buffer layer is superior to that grown on the Cr buffer layer. The point contact Andreev reflection measurement was then conducted, and the spin polarizations were determined to be 61.1% and 81.3% for Fe 4 N thin films with Cr and Ag buffer layers, respectively. The 81.3% spin polarization is significantly higher than the ratio reported previously for Fe 4 N and is comparable with that of state-of-the-art Heusler alloys. This result is in agreement with the theoretical prediction on the discrepancy between the two differently defined spin polarizations for Fe 4 N. Moreover, our study indicates that an optimized growth process for Fe 4 N thin films is crucial for achieving a high spin polarization and that true half-metallicity could potentially be realized with Fe 4 N. Furthermore the high spin polarization of Fe 4 N combined with its low fabrication temperature and simple composition makes Fe 4 N a competitive candidate to be a half-metallic ferromagnet in spintronic devices.

36 MATERIALS SCIENCE↗

Improvement of the CIGS solar cell performance: structure based on a ZnS buffer layer

Cu(In,Ga)Se{sub 2} (CIGS) based thin film solar cells are the most efficient thin-film solar cells today. The non-toxic and wide band-gap zinc sulphide (ZnS) is a promising material to replace the cadmium sulfide (CdS) as the buffer layer in CIGS based solar cells. In this work we present a simulation study of a CIGS based solar cell with a buffer layer of ZnS, using the simulator Silvaco-Atlas. Our primary simulation shows a 22.6% efficiency of the CIGS solar cell with the CdS buffer layer which is comparable to reported and highest experimental results. However, the simulated efficiency of the CIGS solar cell with the ZnS buffer layer as high as 23.54% was achieved. The effects of layer parameters like the thickness, the acceptor and donor densities of the CIGS absorber and ZnS buffer layers and the CBO on the photovoltaic parameters of the ZnS/CIGS solar cell are optimized in order to improve the performance of the ZnS/CIGS solar cell. The highest efficiency of 27.33% is achieved when the ZnS buffer and the CIGS absorber layers have thicknesses of 0.025 µm and 4 µm with acceptor and donor densities of 6 × 10{sup 17} cm{sup −3} and 10{sup 18} cm{sup −3}, respectively and a CBO in the range − 0.05 to 0.05 eV. The present results of simulation can help the development of the solar cells with higher conversion efficiency and low cost.

14 SOLAR ENERGY↗

Epitaxial NbN/AlN/NbN tunnel junctions on Si substrates with TiN buffer layers

We have developed epitaxial NbN/AlN/NbN tunnel junctions on Si (100) substrates with a TiN buffer layer. A 50-nm-thick (200)-oriented TiN thin film was introduced as the buffer layer for epitaxial growth of NbN/AlN/NbN trilayers on Si substrates. The fabricated NbN/AlN/NbN junctions demonstrated excellent tunneling properties with a high gap voltage of 5.5 mV, a large I{sub c}R{sub N} product of 3.8 mV, a sharp quasiparticle current rise with a ΔV{sub g} of 0.4 mV, and a small subgap leakage current. The junction quality factor R{sub sg}/R{sub N} was about 23 for the junction with a J{sub c} of 47 A/cm{sup 2} and was about 6 for the junction with a J{sub c} of 3.0 kA/cm{sup 2}. X-ray diffraction and transmission electron microscopy observations showed that the NbN/AlN/NbN trilayers were grown epitaxially on the (200)-orientated TiN buffer layer and had a highly crystalline structure with the (200) orientation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Towards III-V solar cells on Si: Improvement in the crystalline quality of Ge-on-Si virtual substrates through low porosity porous silicon buffer layer and annealing

A comparison between the crystalline quality of Ge grown on bulk Si and on a low porosity porous Si (pSi) buffer layer using low energy plasma enhanced chemical vapor deposition is reported. Omega/2Theta coupled scans around the Ge and Si (004) diffraction peaks show a reduction of the Ge full-width at half maximum (FWHM) of 22.4% in presence of the pSi buffer layer, indicating it is effective in improving the epilayer crystalline quality. At the same time atomic force microscopy analysis shows an increase in root means square roughness for Ge grown on pSi from 38.5 nm to 48.0 nm, as a consequence of the larger surface roughness of pSi compared to bulk Si. The effect of 20 minutes vacuum annealing at 580°C is also investigated. The annealing leads to a FWHM reduction of 23% for Ge grown on Si and of 36.5% for Ge on pSi, resulting in a FWHM of 101 arcsec in the latter case. At the same time, the RMS roughness is reduced of 8.8% and of 46.5% for Ge grown on bulk Si and on pSi, respectively. The biggest improvement in the crystalline quality of Ge grown on pSi with respect to Ge grown on bulk Si observed after annealing is a consequence of the simultaneous reorganization of the Ge epilayer and the buffer layer driven by energy minimization. A low porosity buffer layer can thus be used for the growth of low defect density Ge on Si virtual substrates for the successive integration of III-V multijunction solar cells on Si. The suggested approach is simple and fast –thus allowing for high throughput-, moreover is cost effective and fully compatible with subsequent wafer processing. Finally it does not introduce new chemicals in the solar cell fabrication process and can be scaled to large area silicon wafers.

36 MATERIALS SCIENCE↗

Microstructure of irradiated AGR TRISO particle buffer layers as measured by X-ray computed tomography

Shrinkage of the initially low-density buffer layer in tristructural isotropic (TRISO) coated fuel particles during irradiation is a well-known phenomenon with potential implications for fission product and actinide transport, as well as potential pyrocarbon fracture that in some cases has been observed to impact particle performance. During post-irradiation examination, the buffer layer's structure is commonly determined using 2D microscopy of a particle cross section or a series of particle cross sections at staggered depths. Although these methods provide a general idea of the irradiated buffer microstructure, they do not provide a full picture of the TRISO coating microstructure. By contrast, x-ray computed tomography (XCT) provides full 3D imaging of the TRISO particle. Particles from various compacts irradiated for the Advanced Gas Reactor Fuel Development and Qualification Program were imaged using XCT. Some of these particles were selected because of abnormal fission product inventories (e.g., low 137 Cs), whereas others were randomly selected from the center of the fission product inventory distribution. Qualitative and quantitative analysis techniques were applied to the randomly selected particles as representatives of typical TRISO behavior to study the post-irradiation structure of the buffer layer. These results showed that, while separation of the buffer and inner pyrolytic carbon layers was a common behavior during the radiation-induced shrinkage of the buffer, a portion of the original buffer/inner pyrolytic carbon interface remained intact throughout irradiation in nearly all cases. Furthermore, these results also indicated clear trends in the degree of buffer densification with irradiation temperature and fluence.

36 MATERIALS SCIENCE↗

Reliability of Small Molecule Organic Photovoltaics with Electron-Filtering Compound Buffer Layers

Electron-filtering compound buffer layers (EF-CBLs) improve charge extraction in organic photovoltaic cells (OPVs) by blending an electron-conducting fullerene with a wide energy gap exciton-blocking molecule. It is found that devices with EF-CBLs with high glass transition temperatures and a low crystallization rate produce highly stable morphologies and devices. The most stable OPVs employ 1:1 2,2',2"-(1,3,5-benzenetriyl tris-[1-phenyl-1H-benzimidazole] TPBi:C 70 buffers that lose <20% of their initial power conversion efficiency of 6.6 ± 0.6% after 2700 h under continuous simulated AM1.5G illumination, and show no significant degradation after 100 days of outdoor aging. When exposed to 100-sun (100 kW m -2 ) concentrated solar illumination for 5 h, their power conversion efficiencies decrease by <8%. Moreover, it is found that the reliability of the devices employing stable EF-CBLs has either reduced or no dependence on operating temperature up to 130 °C compared with BPhen:C 60 devices whose fill factors show thermally activated degradation. The robustness of TPBi:C 70 devices under extreme aging conditions including outdoor exposure, high temperature, and concentrated illumination is promising for the future of OPV as a stable solar cell technology.

14 SOLAR ENERGY↗

X-ray Microdiffraction from α-Ti 0.04 Fe 1.96 O 3 (0001) Epitaxial Film Grown Over α-Cr 2 O 3 Buffer Layer Boundary

Ti-doped hematite (α-Ti 0.04 Fe 1.96 O 3 ) film grown over patterned α-Cr 2 O 3 buffer layer on α-Al 2 O 3 (0001) substrate was characterized with synchrotron X-ray microdiffraction. The film was grown by oxygen plasma assisted molecular beam epitaxy method. The film growth mode was correlated to buffer layer boundary and Ti concentration variation. Epitaxial α-Ti 0.04 Fe 1.96 O 3 film was formed on bare substrate adjacent to the buffer layer. The epitaxial film was connected laterally to a strain-relaxed epitaxial α-Ti 0.04 Fe 1.96 O 3 film grown on the buffer layer. On bare α-Al2O3 substrate with diminished Ti concentration only a small portion of α-Ti x Fe 1-x O 3 film was epitaxial either as coherent to the substrate or strain-relaxed form.

36 MATERIALS SCIENCE↗

Long wavelength emitting GaInN quantum wells on metamorphic GaInN buffer layers with enlarged in-plane lattice parameter

Metamorphic (i.e., linear composition graded) GaInN buffer layers with an increased in-plane lattice parameter, grown by plasma-assisted molecular beam epitaxy, were used as templates for metal organic vapor phase epitaxy (MOVPE) grown GaInN/GaInN quantum wells (QWs), emitting in the green to red spectral region. A composition pulling effect was observed allowing considerable higher growth temperatures for the QWs for a given In composition. The internal quantum efficiency (IQE) of the QWs was determined by temperature and excitation power density dependent photoluminescence (PL) spectroscopy. An increase in IQE by a factor of two was found for green emitting QWs grown on metamorphic GaInN buffer compared to reference samples grown on standard GaN buffer layers. The ratio of room temperature to low temperature intensity PL of the red emitting QWs were found to be comparable to the PL efficiency of green emitting QWs, both grown on metamorphic GaInN buffers. The excitation density and well width dependence of the IQE indicate a reduction of the quantum confined Stark effect upon growth on GaInN buffer layers with increased in-plane lattice parameter.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of dopent on the structural and optical properties of ZnS thin film as a buffer layer in solar cell application

In order to find the suitable alternative of toxic CdS buffer layer, deposition of pure ZnS and doped with Al by chemical bath deposition method have been reported. Further as grown pure and doped thin films have been annealed at 150°C. The structural and surface morphological properties have been characterized by X-Ray diffraction (XRD) and Atomic Force Microscope (AFM).The XRD analysis shows that annealed thin film has been polycrystalline in nature with sphalerite cubic crystal structure and AFM images indicate increment in grain size as well as growth of crystals after annealing. Optical measurement data give band gap of 3.5 eV which is ideal band gap for buffer layer for solar cell suggesting that the obtained ZnS buffer layer is suitable in a low-cost solar cell.

36 MATERIALS SCIENCE↗

Buffer layers for REBCO films for use in superconducting devices

A superconducting article includes a substrate having a biaxially textured surface. A biaxially textured buffer layer, which can be a cap layer, is supported by the substrate. The buffer layer includes a double perovskite of the formula A.sub.2B'B''O.sub.6, where A is rare earth or alkaline earth metal and B' and B'' are different transition metal cations. A biaxially textured superconductor layer is deposited so as to be supported by the buffer layer. A method of making a superconducting article is also disclosed.

36 MATERIALS SCIENCE↗

Nanometer-Scale Epitaxial Strain Release in Perovskite Heterostructures Using 'SrAlOx' Sliding Buffer Layers

We demonstrate the strain release of LaAlO{sub 3} epitaxial film on SrTiO{sub 3} (001) by inserting ultra-thin 'SrAlO{sub x}' buffer layers. Although SrAlO{sub x} is not a perovskite, nor stable as a single phase in bulk, epitaxy stabilizes the perovskite structure up to a thickness of 2 unit cells (uc). At a critical thickness of 3 uc of SrAlO{sub x}, the interlayer acts as a sliding buffer layer, and abruptly relieves the lattice mismatch between the LaAlO{sub 3} filmand the SrTiO{sub 3} substrate, while maintaining crystallinity. This technique may provide a general approach for strain relaxation of perovskite film far below the thermodynamic critical thickness. A central issue in heteroepitaxial filmgrowth is the inevitable difference in lattice constants between the filmand substrate. Due to this lattice mismatch, thin film are subjected to microstructural strain, which can have a significan effect on the filmproperties. This challenge is especially prominent in the rapidly developing fiel of oxide electronics, where much interest is focused on incorporating the emergent physical properties of oxides in devices. Although strain can be used to great effect to engineer unusual ground states, it is often deleterious for bulk first-orde phase transitions, which are suppressed by the strain and symmetry constraints of the substrate. While there are some reports discussing the control of the lattice mismatch in oxides using thick buffer layers, the materials choice, lattice-tunable range, and control of misfit dislocations are still limited. In this Letter, we report the fabrication of strain-relaxed LaAlO{sub 3} (LAO) thin film on SrTiO{sub 3} (STO) (001) using very thin 'SrAlO{sub x}' (SAO) buffer layers. Whereas for 1 or 2 pseudo-perovskite unit cells (uc) of SAO, the subsequent LAO filmis strained to the substrate, at a critical thickness of 3 uc the SAO interlayer abruptly relieves the lattice mismatch between the LAO and the STO, although maintaining the relative crystalline orientation between the filmand the substrate. For 4 uc or greater, the perovskite epitaxial template is lost and the LAO filmis amorphous. These results suggest that metastable interlayers can be used for strain release on the nanometer scale.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Buffer layer between a planar optical concentrator and a solar cell

The effect of inserting a buffer layer between a periodically multilayered isotropic dielectric (PMLID) material acting as a planar optical concentrator and a photovoltaic solar cell was theoretically investigated. The substitution of the photovoltaic material by a cheaper dielectric material in a large area of the structure could reduce the fabrication costs without significantly reducing the efficiency of the solar cell. Both crystalline silicon (c-Si) and gallium arsenide (GaAs) were considered as the photovoltaic material. We found that the buffer layer can act as an antireflection coating at the interface of the PMLID and the photovoltaic materials, and the structure increases the spectrally averaged electron-hole pair density by 36% for c-Si and 38% for GaAs compared to the structure without buffer layer. Numerical evidence indicates that the optimal structure is robust with respect to small changes in the grating profile.

14 SOLAR ENERGY↗

Degradation of Mg-doped zinc oxide buffer layers in thin film CdTe solar cells

Cadmium Sulphide is the conventional n-type buffer layer used in thin film Cadmium Telluride solar cells. It is well known that Cadmium Sulphide causes optical losses and sulphur diffuses into the absorber during high temperature activation. Sputter-deposited Mg-doped ZnO (MZO) has been shown to be an attractive buffer layer for Cadmium Telluride solar cells due to its transparency and tuneable band gap. It is also stable to high temperature processing and avoids diffusion of elements into the cadmium telluride absorber during the cadmium chloride activation treatment. However, degradation is observed in solar cells incorporating MZO buffer layers. Analysis of the MZO film surface potential has revealed significant fluctuations in the thin film work function once the layer is exposed to the atmosphere following deposition. These fluctuations are attributed to the high reactivity to water vapour of the MgO contained in the MZO films. This has been analysed using X-ray Photoelectron Spectroscopy to determine corresponding changes in the surface chemistry. The Zinc Oxide component is relatively stable, but the analysis shows that MgO forms a Mg(OH) 2 layer on the MZO surface which forms a secondary barrier at the MZO/CdTe interface and/or at the interface between MZO and the Fluorine-doped SnO 2 . This affects the Fill Factor and as a consequence it degrades the conversion efficiency.

14 SOLAR ENERGY↗

Epitaxial Electrodeposition of Wide Bandgap Cuprous Bromide on Silver via a Silver Bromide Buffer Layer

Cuprous halides are an important class of wide bandgap p-type semiconductors used in opto-electronics. Cuprous bromide (CuBr) shows potential for short-wavelength devices due to a large exciton binding energy (108 meV) and near-ultraviolet bandgap (3.1 eV). However, the growth of high-quality epitaxial CuBr films by electrodeposition has remained a challenge. Here, we introduce a low-cost electrochemical procedure for producing epitaxial CuBr(111) on a Ag(111) substrate by a [111]-oriented silver bromide (AgBr) buffer layer. The AgBr buffer layer forms during the electrodeposition of the CuBr. The mismatch between CuBr(111) and AgBr(111) is –1.3%. A plausible mechanism for nucleation and growth of the epitaxial CuBr is proposed. X-ray techniques including high resolution X-ray diffraction and X-ray pole figures are used to determine the epitaxial relationship. CuBr(100) is also produced on a Ag(100) surface by a AgBr(100) buffer layer that is rotated in-plane 45° relative to the Ag(100) surface. In conclusion, this in-plane rotation reduces the lattice mismatch from +39.5% for an unrotated film to –1.4% for a 45° rotated film.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of buffer layer growth temperature on epitaxial GaN films deposited by magnetron sputtering

Epitaxial GaN films were deposited by reactive sputtering of a GaAs target in 100 % nitrogen at 700 deg. C on ZnO buffer layers grown at different substrate temperatures over sapphire substrates. High resolution X-ray diffraction measurements and the corresponding analysis show that the growth temperature of buffer layers significantly affects the micro-structural parameters of GaN epilayer, such as lateral coherence length, tilt and twist, while the vertical coherence length remains unaffected. The optimum substrate temperature for buffer layer growth has been found to be 300 deg. C. High epitaxial quality GaN film grown on such a buffer layer exhibited micro strain of 1.8x10{sup -4} along with screw and edge type dislocation densities of 7.87x10{sup 9} and 1.16x10{sup 11}, respectively.

36 MATERIALS SCIENCE↗