Search NASA⌕ Search

SEARCH · Search NASA

Results for “controlled spalling”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Real-time measurements of temperature, pressure and moisture profiles in High-Performance Concrete exposed to high temperatures during neutron radiography imaging

High-Performance Concrete (HPC) is particularly prone to explosive spalling when exposed to high temperature. Although the exact causes that lead to spalling are still being debated, moisture transport during heating plays an important role in all proposed mechanisms. In this study, slabs made of high-performance, low water-to-binder ratio mortars with addition of superabsorbent polymers (SAP) and polypropylene fibers (PP) were heated from one side on a temperature-controlled plate up to 550 °C. A combination of measurements was performed simultaneously on the same sample: moisture profiles via neutron radiography, temperature profiles with embedded thermocouples and pore pressure evolution with embedded pressure sensors. Spalling occurred in the sample with SAP, where sharp profiles of moisture and temperature were observed. No spalling occurred when PP-fibers were introduced in addition to SAP. The experimental procedure described here is essential for developing and verifying numerical models and studying measures against fire spalling risk in HPC.

42 ENGINEERING↗

Shock-Wave Proprieties of High-Strength Ceramics

The shock and release response of a suite of high-strength ceramics has been investigated with controlled planar impact methods and velocity interferometry diagnostics. The study provides Hugoniot, yield and post-yield compressive strength, phase transformation and tensile spall material properties data for these ceramics.

36 MATERIALS SCIENCE↗

Microstructure, Processing, Performance Relationships for High Temperature Coatings

HVOF coating have shown high resistance to corrosion in fossil energy applications and it is generally accepted that mechanical failure, e.g. cracking or spalling, ultimately will determine coating lifetime. The high velocity oxygen-fuel method (HVOF) of applying coatings is one of the most commercially viable and allows the control of various parameters including powder particle velocity and temperature which influence coating properties, such as residual stress, bond coat strength and microstructure. Methods of assessing the mechanical durability of coatings are being developed in order to explore the relationship between HVOF spraying parameters and the mechanical properties of the coating and coating bond strength. The room temperature mechanical strength, as well as the resistance of the coating to cracking/spalling during thermal transients, is of considerable importance. Eddy current, acoustic emission and thermal imaging methods are being developed to detect coating failure during thermal cycling tests and room temperature tensile tests. Preliminary results on coating failure of HVOF FeAl coatings on carbon steel, as detected by eddy current measurements during thermal cycling, are presented. The influence of HVOF coating parameters of iron aluminides - applied to more relevant structural steels, like 316 SS and Grade 91 steel, - on coating durability will be explored once reliable methods for identification of coating failure have been developed.

20 FOSSIL-FUELED POWER PLANTS↗

Microstructure, Processing, Performance Relationships for High Temperature Coatings

HVOF coatings have shown high resistance to corrosion in fossil energy applications and it is generally accepted that mechanical failure, e.g. cracking or spalling, ultimately will determine coating lifetime. The high velocity oxygen-fuel method (HVOF) for applying coatings is one of the most commercially viable and allows the control of various parameters including powder particle velocity and temperature which influence coating properties, such as residual stress, bond coat strength and microstructure. The mechanical durability of coatings is being assessed using a dual eddy current coil method to monitor crack formation in real time during thermal cycling. Absolute impedence signals from two coils, which interrogate two different areas on the sample, are collected. Crack detection can be determined from the differential signal generated from these absolute signals. The coils are operated at two different frequencies, resulting in two differential signals used for crack detection. Currently this crack detection method is being used to elucidate the influence of thermal cycling temperature and coating thickness on cracking. Recent results (cycles to failure) will be presented for FeAl coatings thermally sprayed (HVOF) onto carbon steel to two coating thicknesses (160 microns and 250 microns thick) and subsequently cycled at temperatures up to 700oC. Thinner coatings exhibit greater resistance to cracking. Ultimately the resistance to cracking will be used to explore the relationship between HVOF spraying parameters, the mechanical properties of the coating and coating bond strength to develop optimized thermal spray parameters. To this end thermal spray coatings (FeAl and Fe3Al) have been applied to additional alloy substrates (Grade 91 steel, 316 SS, etc.) relevant to the fossil industry. Future plans also include a direct comparison to conventional weld overlay coatings currently used in the industry as well as exploration of new coatings. The room temperature mechanical strength and coating adhesion to the substrate is also of considerable importance. Eddy current methods are being developed to detect coating failure during room temperature tensile tests to optimize surface preparation as well as aid in the optimization of the HVOF thermal spray parameters.

20 FOSSIL-FUELED POWER PLANTS↗

Discontinuous Inter-Granular Separations (DIGS) in the Gas Nitride Layer of ISS Race Rings

The starboard solar alpha rotary joint (SARJ) race ring on the International space station (ISS) failed due to severe spalling of the outer diameter, 45 degree (outer canted) nitrided surface. Subsequent analysis at NASA-KSC revealed that almost all of the debris generated due to the failure was nitrided 15-5 stainless steel. Subsequent analysis of the nitride control coupons (NCC) at NASA-JSC revealed the presence of discontinuous inter-granular separations (DIGS) in the gas nitride layer. These DIGS were present in the inter-granular networking located in the top 2 mils of the nitride layer. The manufacturer's specification requires the maximum white structure to be 0.0003 inches and intergranular networking below the allowable white structure depth to be cause for rejection; a requirement that the NCCs did not meet. Subsequent testing and analysis revealed that lower DIGS content significantly lowered the probability of nitride spalling in simulated, dry condition runs. One batch of nitride samples with DIGS content similar to the port SARJ (did not fail on orbit) which exhibited almost no nitride spalling after being run on one test rig. Another batch of nitride samples with DIGS content levels similar to the starboard SARJ exhibited significant nitride spalling on the same test rig with the same load under dry conditions. Although DIGS were not the root cause of starboard race ring failure, testing indicates that increased DIGS reduced the robustness of the gas nitride layer under dry operating conditions.

Figert, John↗

Thermal fracture mechanisms in ceramic thermal barrier coatings

Ceramic thermal barrier coatings represent an attractive method of increasing the high temperature limits for systems such as diesel engines, gas turbines and aircraft engines. However, the dissimilarities between ceramics and metal, as well as the severe temperature gradients applied in such systems, cause thermal stresses which can lead to cracking and ultimately spalling of the coating. This paper reviews the research which considers initiation of surface cracks, interfacial edge cracks and the effect of a transient thermal load on interface cracks. The results of controlled experiments together with analytical models are presented. The implications of these findings to the differences between diesel engines and gas turbines are discussed. The importance of such work for determining the proper design criteria for thermal barrier coatings is underlined.

Kokini, K.↗

Thermal fracture mechanisms in ceramic thermal barrier coatings

Ceramic thermal barrier coatings represent an attractive method of increasing the high temperature limits for systems such as diesel engines, gas turbines and aircraft engines. However, the dissimilarities between ceramics and metal, as well as the severe temperature gradients applied in such systems cause thermal stresses which can lead to cracking and ultimately spalling of the coating. This paper reviews the research which considers initiation of surface cracks, interfacial edge cracks and the effect of a transient thermal load on interface cracks. The results of controlled experiments together with analytical models are presented. The implications of these findings to the differences between diesel engines and gas turbines are discussed. The importance of such work for determining the proper design criteria for thermal barrier coatings is underlined.

Kokini, Klod↗

Thermal barrier coatings for thermal insulation and corrosion resistance in industrial gas turbine engines

Four thermal barrier coatings were subjected to a 500-hour gas turbine engine test. The coatings were two yttria stabilized zirconias, calcium ortho silicate and calcium meta titanate. The calcium silicate coating exhibited significant spalling. Yttria stabilized zirconia and calcium titanate coatings showed little degradation except in blade leading edge areas. Post-test examination showed variations in the coating due to manual application techniques. Improved process control is required if engineering quality coatings are to be developed. The results indicate that some leading edge loss of the coating can be expected near the tip.

Vogan, J. W.↗

Design and fabrication of prototype system for early warning of impending bearing failure

A test program was conducted with the objective of developing a method and equipment for on-line monitoring of installed ball bearings to detect deterioration or impending failure of the bearings. The program was directed at the spin-axis bearings of a control moment gyro. The bearings were tested at speeds of 6000 and 8000 rpm, thrust loads from 50 to 1000 pounds, with a wide range of lubrication conditions, with and without a simulated fatigue spall implanted in the inner race ball track. It was concluded that a bearing monitor system based on detection and analysis of modulations of a fault indicating bearing resonance frequency can provide a low threshold of sensitivity.

Meacher, J.↗

Structural Damage Prediction and Analysis for Hypervelocity Impacts: Handbook

This handbook reviews the analysis of structural damage on spacecraft due to hypervelocity impacts by meteoroid and space debris. These impacts can potentially cause structural damage to a Space Station module wall. This damage ranges from craters, bulges, minor penetrations, and spall to critical damage associated with a large hole, or even rupture. The analysis of damage depends on a variety of assumptions and the area of most concern is at a velocity beyond well controlled laboratory capability. In the analysis of critical damage, one of the key questions is how much momentum can actually be transfered to the pressure vessel wall. When penetration occurs without maximum bulging at high velocity and obliquities (if less momentum is deposited in the rear wall), then large tears and rupture may be avoided. In analysis of rupture effects of cylindrical geometry, biaxial loading, bending of the crack, a central hole strain rate and R-curve effects are discussed.

Elfer, N. C.↗

On the ultimate tensile strength of tantalum

Strain rate, temperature, and microstructure play a significant role in the mechanical response of materials. By using non-equilibrium molecular dynamics simulations, we characterize the ductile tensile failure of a model body-centered cubic metal, tantalum, over six orders of magnitude in strain rate. Molecular dynamics calculations combined with reported experimental measurements show power-law kinetic relationships that vary as a function of dominant defect mechanism and grain size. The maximum sustained tensile stress, or spall strength, increases with increasing strain rate, before ultimately saturating at ultra-high strain rates, i.e. those approaching or exceeding the Debye frequency. The upper limit of tensile strength can be well estimated by the cohesive energy, or the energy required to separate atoms from one another. At strain rates below the Debye frequency, the spall strength of nanocrystalline Ta is less than single crystalline tantalum. This occurs in part due to the decreased flow stress of the grain boundaries; stress concentrations at grain boundaries that arise due to compatibility requirements; and the growing fraction of grain-boundary atoms as grain size is decreased into the nanocrystalline regime. In the present cases, voids nucleate at defect structures present in the microstructure. The exact makeup and distribution of defects is controlled by the initial microstructure and the plastic deformation during both compression and expansion, where grain boundaries and grain orientation play critical roles.

36 MATERIALS SCIENCE↗

Microstructure and corrosion behavior of cast Fe-B alloys dipped into liquid zinc bath

The corrosion behavior of cast Fe-B alloys in a liquid zinc bath was examined. As a result, the as-cast Fe-3.5B alloy displays the best corrosion resistance in all tested specimens owing to its netlike structure of eutectic Fe{sub 2}B against the liquid zinc. XRD and EDS results indicate that the main phases in the corrosion layer are determined to be {delta}, {zeta} and {eta} from the matrix to the zinc zone, respectively. The corrosion process is controlled by the diffusion of zinc atoms and the dissolution mechanism. According to the observations, only three steps occur in the whole dissolution process: the preferential dissolution of {alpha}-Fe, the formation of intermetallic compounds, and the spalling of Fe{sub 2}B caused by cracks that mainly result from the internal stress produced by Fe/Zn phase transformation. The continuous netlike Fe{sub 2}B phase delays the further reaction of Fe/Zn and hinders the diffusion of zinc atoms between the substrate and liquid zinc effectively, improving corrosion resistance of Fe-B alloy in comparison with 1Cr18Ni9Ti stainless steel.

36 MATERIALS SCIENCE↗

The effect of yttrium and thorium on the oxidation behavior of Ni-Cr-Al alloys

The effect of quaternary additions of 0.5% Y, 0.5 and 1.0% Th to a base alloy of Ni-10CR-5Al on the oxidation behavior and mechanism was studied during oxidation in air over the range of 1000 to 1200 C. The presence of yttrium decreased the oxidation kinetics slightly, whereas, the addition of thorium caused a slight increase. Oxide scale adherence was markedly improved by the addition of the quaternary elements. Although a number of oxides formed on yttrium containing alloys, quantitative X-ray diffraction clearly showed that the rate-controlling step was the diffusion of aluminum through short circuit paths in a thin layer of alumina that formed parabolically with time. Although the scale adherence of the yttrium containing alloy was considerably better than the base alloys, spalling did occur that was attributed to the formation of the voluminous YAG particles which grew in a mushroom-like manner, lifting the protective scale off the subrate locally. The YAG particles formed primarily at grain boundaries in the substrate in which the yttrium originally existed as YNi9.

Kumar, A.↗

Ductile-to-brittle transition in spallation of metallic glasses

In this paper, the spallation behavior of a binary metallic glass Cu{sub 50}Zr{sub 50} is investigated with molecular dynamics simulations. With increasing the impact velocity, micro-voids induced by tensile pulses become smaller and more concentrated. The phenomenon suggests a ductile-to-brittle transition during the spallation process. Further investigation indicates that the transition is controlled by the interaction between void nucleation and growth, which can be regarded as a competition between tension transformation zones (TTZs) and shear transformation zones (STZs) at atomic scale. As impact velocities become higher, the stress amplitude and temperature rise in the spall region increase and micro-structures of the material become more unstable. Therefore, TTZs are prone to activation in metallic glasses, leading to a brittle behavior during the spallation process.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Moisture-Induced Delayed Alumina Scale Spallation on a Ni(Pt)Al Coating

Delayed interfacial scale failure takes place after cooling for samples of a Ni(Pt)Al-coated CMSX4 single crystal superalloy, cycled at 1150 C for up to 2000 hr. One sample exhibited premature coating grain boundary wrinkling, alumina scale spallation to bare metal, and a final weight loss of 3.3 mg/cm2 . Spallation under ambient conditions was monitored with time after cooldown and was found to continue for 24 hr. This produced up to 0.05 mg/cm2 additional loss for each hold, accumulating 0.7 mg/cm 2 (20 percent of the total) over the course of the test. After test termination, water immersion produced an additional 0.15 mg/cm2 loss. (A duplicate sample produced much less wrinkling and time dependent spalling, maintaining a net weight gain.) The results are consistent with the general phenomena of moisture-induced delayed spallation (MIDS) of mature, distressed alumina scales formed on oxidation resistant M-Al alloys. Relative ambient humidity is discussed as the factor controlling adsorbed moisture, reaction with the substrate, and hydrogen effects on interface strength.

Smialek, James L.↗

Cratering Equations for Zinc Orthotitanate Coated Aluminum

The final STS-125 servicing mission (SM4) to the Hubble Space Telescope (HST) in May of 2009 saw the return of the 2nd Wide Field Planetary Camera (WFPC2) aboard the shuttle Discovery. This hardware had been in service on HST since it was installed during the SM1 mission in December of 1993 yielding one of the longest low Earth orbit exposure times (15.4 years) of any returned space hardware. The WFPC2 is equipped with a 0.8 x 2.2 m radiator for thermal control of the camera electronics (Figure 1). The space facing surface of the 4.1 mm thick aluminum radiator is coated with Z93 zinc orthotitanate thermal control paint with a nominal thickness of 0.1 0.2 mm. Post flight inspections of the radiator panel revealed hundreds of micrometeoroid/orbital debris (MMOD) impact craters ranging in size from less than 300 to nearly 1000 microns in diameter. The Z93 paint exhibited large spall areas around the larger impact sites (Figure 2) and the craters observed in the 6061-T651 aluminum had a different shape than those observed in uncoated aluminum. Typical hypervelocity impact craters in aluminum have raised lips around the impact site. The craters in the HST radiator panel had suppressed crater lips, and in some cases multiple craters were present instead of a single individual crater. Humes and Kinard observed similar behavior after the WFPC1 post flight inspection and assumed the Z93 coating was acting like a bumper in a Whipple shield. Similar paint behavior (spall) was also observed by Bland2 during post flight inspection of the International Space Station (ISS) S-Band Antenna Structural Assembly (SASA) in 2008. The SASA, with similar Z93 coated aluminum, was inspected after nearly 4 years of exposure on the ISS. The multi-crater phenomena could be a function of the density, composition, or impact obliquity angle of the impacting particle. For instance, a micrometeoroid particle consisting of loosely bound grains of material could be responsible for creating the multiple craters. Samples were obtained from the HST largest craters for examination by electron microscope equipped with x-ray spectrometers to determine impactor source (micrometeoroid or orbital debris). In an attempt to estimate the MMOD particle diameters that produced these craters, this paper will present equations for spall diameter, crater depth and crater diameter in Z93 coated aluminum. The equations will be based on hypervelocity impact tests of Z93 painted aluminum at the NASA White Sands Test Facility. Equations inputs for velocities beyond the testable regime are expected from hydrocode simulations of Z93 coated aluminum using CTH and ANSYS AUTODYN.

Hyde, James↗

RDS-21 Face-Gear Surface Durability Tests

Experimental fatigue tests were performed to determine the surface durability life of a face gear in mesh with a tapered spur involute pinion. Twenty-four sets of gears were tested at three load levels: 7200, 8185, and 9075 lb-in face gear torque, and 2190 to 3280 rpm face gear speed. The gears were carburized and ground, shot-peened and vibro-honed, and made from VIM-VAR Pyrowear 53 steel per AMS 6308. The tests produced 17 gear tooth spalling failures and 7 suspensions. For all the failed sets, spalling occurred on at least one tooth of all the pinions. In some cases, the spalling initiated a crack in the pinion teeth which progressed to tooth fracture. Also, spalling occurred on some face gear teeth. The AGMA endurance allowable stress for a tapered spur involute pinion in mesh with a face gear was determined to be 275 ksi for the material tested. For the application of a tapered spur involute pinion in mesh with a face gear, proper face gear shim controlled the desired gear tooth contact pattern while proper pinion shim was an effective way of adjusting backlash without severely affecting the contact pattern.

Lewicki, David G.↗

High Temperature Materials for Chemical Propulsion Applications

Radiation or passively cooled thrust chambers are used for a variety of chemical propulsion functions including apogee insertion, reaction control for launch vehicles, and primary propulsion for planetary spacecraft. The performance of these thrust chambers is limited by the operating temperature of available materials. Improved oxidation resistance and increased operating temperatures can be achieved with the use of thermal barrier coatings such as zirconium oxide (ZrO2) and hafnium oxide (HfO2). However, previous attempts to include these materials showed cracking and spalling of the oxide layer due to poor bonding. Current research at NASA's Marshall Space Flight Center (MSFC) has generated unique, high temperature material options for in-space thruster designs that are capable of up to 2500 C operating temperatures. The research is focused on fabrication technologies to form low cost Iridium,qF_.henium (Ir/Re) components with a ceramic hot wall created as an integral, functionally graded material (FGM). The goal of this effort is to further de?celop proven technologies for embedding a protective ceramic coating within the Ir/Re liner to form a robust functional gradient material. Current work includes the fabrication and testing of subscale samples to evaluate tensile, creep, thermal cyclic/oxidation, and thermophysical material properties. Larger test articles have also being fabricated and hot-fire tested to demonstrate the materials in prototype thrusters at 1O0 lbf thrust levels.

Elam, Sandra↗