Search NASA⌕ Search

SEARCH · Search NASA

Results for “dislocation density”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Dislocation density in fine grain-size spark-plasma sintered aluminum measured using high brightness synchrotron radiation

In this study, three-dimensional orientation mapping of samples of aluminum prepared by spark plasma sintering (SPS) with average grain sizes of 5 μm and 1 μm has been carried out using high-brightness synchrotron radiation, from which the geometrically necessary dislocation (GND) density has been determined. The low average measured GND density values confirm that the SPS process can be used to produce samples containing grains with dislocation density similar to that of fully recrystallized coarse-grained samples. Values of GND density are also compared to those obtained from electron back-scatter diffraction studies on the same material, highlighting the significantly higher angular resolution of the synchrotron data. For the 5 μm grain-size sample the measured GND density can account for a large fraction of the previously observed positive Hall-Petch deviation of this material. For the 1 μm grain-size sample, however, the GND-based strengthening contribution is much smaller than the reported positive Hall-Petch deviation, such that the additional strength may be reliably associated with dislocation source-limited strengthening.

36 MATERIALS SCIENCE↗

In Situ Tensile Testing of Single Crystal Molybdenum Alloy Fibers with Various Dislocation Densities in a Scanning Electron Microscope

In-situ tensile tests have been performed in a dual beam focused ion beam and scanning electron microscope on as-grown and prestrained single-crystal molybdenum-alloy (Mo-alloy) fibers. The fibers had approximately square cross sections with submicron edge lengths and gauge lengths in the range of 9-41 {mu}m. In contrast to previously observed yield strengths near the theoretical strength of 10 GPa in compression tests of {approx}1-3-{mu}m long pillars made from similar Mo-alloy single crystals, a wide scatter of yield strengths between 1 and 10 GPa was observed in the as-grown fibers tested in tension. Deformation was dominated by inhomogeneous plastic events, sometimes including the formation of Lueders bands. In contrast, highly prestrained fibers exhibited stable plastic flow, significantly lower yield strengths of {approx}1 GPa, and stress-strain behavior very similar to that in compression. A simple, statistical model incorporating the measured dislocation densities is developed to explain why the tension and compression results for the as-grown fibers are different.

36 MATERIALS SCIENCE↗

Subgrain geometrically necessary dislocation density mapping in spalled Ta in three dimensions

Here, in this work, the intragranular distributions of the densities of geometrically necessary dislocations (GNDs) generated in a polycrystalline tantalum (Ta) sample loaded in shock compression to spall are investigated. The sample studied is a highly resolved three-dimensional (3D) map of the orientations, grain boundary morphology, and voids across a 0.276mm 3 (with sample dimensions of 688.5µm x 669µm x 600µm) region of the microstructure about the spall plane obtained by TriBeam tomography. We present a formulation for calculating the crystallographic screw and edge character GND densities at a material point within body centered cubic (BCC) crystals when provided any number of potential slip systems or modes. Combining the 3D characterization, GND formulation, and a sample containing ≈ 6000 grains, we sought statistically relevant correlations between GND density per grain with grain size, grain orientation, void formation, and proximity from the spall plane. We show that GND density per grain increases with decreasing distance from the spall plane. Most grains had heterogeneously distributed GND densities but were free of any detectable voids, at least within the ≈ 1.5µm resolution of the characterization technique. It is found that the GND density for most grains is insensitive to grain size and grain orientation. Only the fraction of grains with the highest GND densities tended to have a [001] parallel to shock-direction orientation. Intragranular 3D maps of GNDs reveals that grains that contain voids have high GND density concentrations in the intragranular region immediately surrounding the void. The local intragranular GND mapping also showed voids that are connected to grain boundaries preferred to grow into the grain with the larger size, regardless of orientation.

36 MATERIALS SCIENCE↗

Evaluation of threading dislocation densities in In- and N-face InN

The threading dislocation (TD) structure and density has been studied in In- and N-face InN films grown on GaN by plasma-assisted molecular beam epitaxy. The TD densities were determined by nondestructive x-ray diffraction rocking curve measurements in on-axis symmetric and off-axis skew symmetric geometries and calibrated by transmission electron microscopy measurements. TD densities were dominated by edge-type TDs with screw-component TDs accounting for less than 10% of the total TD density. A significant decrease in edge-type TD density was observed for In-face InN films grown at increasingly higher substrate temperatures. In-face InN films grown with excess In exhibited lower TD densities compared to films grown under N-rich conditions. The edge-type TD density of N-face InN films was independent of substrate temperature due to the higher allowable growth temperatures for N-face InN compared to In-face InN. TD densities in In-face InN also showed a strong dependence on film thickness. Films grown at a thickness of less than 1 {mu}m had higher TD densities compared with films grown thicker than 1 {mu}m. The lowest measured TD density for an In-face InN film was {approx}1.5x10{sup 10}/cm{sup 2} for 1 {mu}m thick films.

36 MATERIALS SCIENCE↗

Reduction of Crosshatch Roughness and Threading Dislocation Density in Metamorphic GaInP Buffers and GaInAs Solar Cells

Surface crosshatch roughness typically develops during the growth of lattice-mismatched compositionally graded buffers and can limit misfit dislocation glide. In this study, the crosshatch roughness during growth of a compressive GaInP/GaAs graded buffer is reduced by increasing the phosphine partial pressure throughout the metamorphic growth. Changes in the average misfit dislocation length are qualitatively determined by characterizing the threading defect density and residual strain. The decrease of crosshatch roughness leads to an increase in the average misfit dislocation glide length, indicating that the surface roughness is limiting dislocation glide. Growth rate is also analyzed as a method to reduce surface crosshatch roughness and increase glide length, but has a more complicated relationship with glide kinetics. Using knowledge gained from these experiments, high quality inverted GaInAs 1 eV solar cells are grown on a GaInP compositionally graded buffer with reduced roughness and threading dislocation density. The open circuit voltage is only 0.38 V lower than the bandgap potential at a short circuit current density of 15 mA/cm{sup 2}, suggesting that there is very little loss due to the lattice mismatch.

14 SOLAR ENERGY↗

Reduction in threading dislocation densities in AlN epilayer by introducing a pulsed atomic-layer epitaxial buffer layer

A method of reducing threading dislocation (TD) density in AlN epilayers grown on sapphire substrate is reported. By introducing an AlN buffer layer grown by a pulsed atomic-layer epitaxy method, TDs in epitaxial AlN films were greatly decreased. From transmission electron microscopic images, a clear subinterface was observed between the buffer layer and the subsequently continuous grown AlN epilayer. In the vicinity of the subinterface, the redirection, annihilation, and termination of TDs were observed. The increase in lateral growth rate accounted for TD redirection and annihilation in the AlN epilayer. Strain variation between the two regions resulted in the termination of TDs owing to the dislocation line energy minimization.

36 MATERIALS SCIENCE↗

Effect of loading path on grain misorientation and geometrically necessary dislocation density in polycrystalline aluminum under reciprocating shear

Solid phase processing (SPP) is a promising alloy fabrication technique to produce fine and homogeneous grain structures for high-performance alloys. However, there is very limited modeling capability to understand and predict the grain refinement during SPP. In this work, the crystal plasticity theory was used to study elastic-plastic deformation in polycrystalline aluminums under large shear deformation. Two approaches, kernel averaged misorientation (KAM) and grain reference orientation deviation (GROD), were used to assess the grain misorientations. The geometrically necessary dislocation (GND) density was computed with the plastic strain rate. The deformation simulations were carried out under two loading conditions to investigate the effect of loading paths on the evolutions of grain misorientation and GND density. The results show that the regions with high misorientation and GND density first appear near grain boundaries. These regions then extend toward interior grains. The loading path affects dislocation system activation and dislocation recovery, hence dislocation evolution and misorientation. In conclusion, both two- and three-dimensional simulations showed that the spatial and temporal evolutions of GROD, KAM, and GND density in are closely correlated, which indicates they all can be used as criteria of grain refinement or recrystallization.

36 MATERIALS SCIENCE↗

Quantification of grain boundary effects on the geometrically necessary dislocation density evolution and strain hardening of polycrystalline Mg 4Al using in situ tensile testing in scanning electron microscope and HR-EBSD

In situ tensile testing in a scanning electron microscope (SEM) in conjunction with high-resolution electron backscatter diffraction (HR-EBSD) under load was used to characterize the evolution of geometrically necessary dislocation (GND) densities at individual grain boundaries as a function of applied strain in a polycrystalline Mg—4Al alloy. The increase in GND density was investigated at plastic strains of 0 %, 0.6 %, 2.2 %, 3.3 % from the area including 76 grains and correlated with (i) geometric compatibility between slip systems across grain boundaries, and (ii) plastic incompatibility. We develop expressions for the grain boundary GND density evolution as a function of plastic strain and plastic incompatibility, from which uniaxial tensile stress-strain response of polycrystalline Mg—4Al are computed and compared with experimental measurement. The findings in this study contribute to understanding the mechanisms governing the strain hardening response of single-phase polycrystalline alloys and more reliable prediction of mechanical behaviors in diverse microstructures.

Geometrically necessary dislocations↗

Quasi in-situ analysis of geometrically necessary dislocation density in α-fibre and γ-fibre during static recrystallization in cold-rolled low-carbon Ti-V bearing microalloyed steel

Highlights: • Average GND density is higher in gamma fibre than alpha fibre. • Higher drop in average GND density in un-recrystallized portion of gamma fibre • Fine precipitates pin the grain boundary at 700 °C 0 s. • Precipitates are coarse at 800 °C and present inside strain-free grains. - Abstract: In the present study, cold-rolled low-carbon steel is annealed at three different conditions: 700 °C for 0 s, 800 °C for 0 s and 800 °C for 2 min at the heating rate of ~10 °C/s. Recrystallization behaviour on sample surface is studied using a heated stage Scanning Electron Microscopy and Electron Backscattered Diffraction. For the lower annealing temperature of 700 °C with no dwell, almost no recrystallization is observed and microstructure resembles the as-received deformed material with the exception of occasional sub-micron sized nuclei. For the annealing conditions of 800 °C 0 s and 800 °C 2 min, onset and evolution of recrystallization is observed in-situ as a function of the initial as-cold rolled texture. Slower recovery rate of alpha fibre than gamma fibre is observed and confirmed by lower drop in average geometrically necessary dislocation (GND) density for un-recrystallized alpha fibres (1.1E+14 m{sup −2} for 700 °C 0 s, 1.4E+14 m{sup −2} for 800 °C 0 s and 4.5E+14 m{sup −2} for 800 °C 2 min) than for un-recrystallized gamma fibre grains (3.0E+14 m{sup −2} for 700 °C 0 s, 6.2E+14 m{sup −2} for 800 °C 0 s and 9.8E+14 m{sup −2} for 800 °C 2 min) during annealing. Strong gamma texture in recrystallized matrix is found for annealing conditions of 800 °C 0 s and 800 °C 2 min. From TEM characterisation it was shown that sub-grain boundaries are decorated with fine precipitates (diameter d < 15 nm) of titanium‑vanadium carbides (Ti,V)C for the annealing condition of 700 °C 0 s, which suggests that these precipitates play a major overall role in retardation of the recrystallization kinetics.

36 MATERIALS SCIENCE↗

Characterization of 100 mm diameter 4H-silicon carbide crystals with extremely low basal plane dislocation density

Synchrotron White Beam X-ray Topography (SWBXT) studies are presented of basal plane dislocation (BPD) configurations and behavior in a new generation of 100mm diameter, 4H-SiC wafers with extremely low BPD densities (3-4 x 10{sup 2} cm{sup -2}). The conversion of non-screw oriented, glissile BPDs into sessile threading edge dislocations (TEDs) is observed to provide pinning points for the operation of single ended Frank-Read sources. In some regions, once converted TEDs are observed to re-convert back into BPDs in a repetitive process which provides multiple BPD pinning points.

36 MATERIALS SCIENCE↗

Characterization of 100 mm Diameter 4H-Silicon Carbide CrystalsWith Extremely Low Basal Plane Dislocation Density

Synchrotron White Beam X-ray Topography (SWBXT) studies are presented of basal plane dislocation (BPD) configurations and behavior in a new generation of 100mm diameter, 4H-SiC wafers with extremely low BPD densities (3-4 x 10{sup 2} cm{sup -2}). The conversion of non-screw oriented, glissile BPDs into sessile threading edge dislocations (TEDs) is observed to provide pinning points for the operation of single ended Frank-Read sources. In some regions, once converted TEDs are observed to re-convert back into BPDs in a repetitive process which provides multiple BPD pinning points.

36 MATERIALS SCIENCE↗

Characterization of 100 mm Diameter 4H-Silicon Carbide CrystalsWith Extremely Low Basal Plane Dislocation Density

Synchrotron White Beam X-ray Topography (SWBXT) studies are presented of basal plane dislocation (BPD) configurations and behavior in a new generation of 100mm diameter, 4H-SiC wafers with extremely low BPD densities (3-4 x 10{sup 2} cm{sup -2}). The conversion of non-screw oriented, glissile BPDs into sessile threading edge dislocations (TEDs) is observed to provide pinning points for the operation of single ended Frank-Read sources. In some regions, once converted TEDs are observed to re-convert back into BPDs in a repetitive process which provides multiple BPD pinning points.

36 MATERIALS SCIENCE↗