At least 73 records · Page 4

Cooperative Atomically Dispersed Fe–N 4 and Sn–N x Moieties for Durable and More Active Oxygen Electroreduction in Fuel Cells

One grand challenge for deploying porous carbons with embedded metal–nitrogen–carbon (M–N–C) moieties as platinum group metal (PGM)-free electrocatalysts in proton-exchange membrane fuel cells is their fast degradation and inferior activity. Here, we report the modulation of the local environment at Fe–N 4 sites via the application of atomic Sn–N x sites for simultaneously improved durability and activity. We discovered that Sn–N x sites not only promote the formation of the more stable D2 FeN 4 C 10 sites but also invoke a unique D3 SnN x –Fe II N 4 site that is characterized by having atomically dispersed bridged Sn–N x and Fe–N 4 . This new D3 site exhibits significantly improved stability against demetalation and several times higher turnover frequency for the oxygen reduction reaction (ORR) due to the shift of the reaction pathway from a single-site associative mechanism to a dual-site dissociative mechanism with the adjacent Sn site facilitating a lower overpotential cleavage of the O–O bond. This mechanism bypasses the formation of the otherwise inevitable intermediate that is responsible for demetalation, where two hydroxyl intermediates bind to one Fe site. Lastly, a mesoporous Fe/Sn-PNC catalyst exhibits a positively shifted ORR half-wave potential and more than 50% lower peroxide formation. This, in combination with the stable D3 site and enriched D2 Fe sites, significantly enhanced the catalyst’s durability as demonstrated in membrane electrode assemblies using complementary accelerated durability testing protocols.

36 MATERIALS SCIENCE↗

Review—Development of Highly Active and Durable Hybrid Compressive Platinum Lattice Catalysts for Polymer Electrolyte Membrane Fuel Cells: Mathematical Modeling and Experimental Work

This review provides a comprehensive overview on the development of highly active and durable platinum catalysts with ultra-low Pt loadings for polymer electrolyte membrane fuel cells (PEMFCs) through a combined mathematical modeling and experimental work. First, simulation techniques were applied to evaluate the validity of the Tafel approximation for the calculation of the mass activity (MA) and specific activity (SA). A one-dimensional agglomeration model was developed and solved to understand the effects of exchange current density, porosity, agglomerate size, Nafion ® film thickness, and Pt loading on the MA and SA. High porosity (> 60%) and agglomerations at high Pt loadings cause the loss of the Tafel approximation and consequently the decrease in MA and SA. A new structure parameter was introduced to estimate the real porous structure using the fractal theory. The volumetric catalyst density was corrected by the fractal dimension (measured by Hg porosimetry), which gave a good agreement with the experimental values. The loading-dependent Tafel equation was then derived, which contains both the utilization and the non-linear scaling factor. Second, activated carbon composite support (ACCS) with optimized surface area, porosity, pore size, and pore size distribution was developed. The hydrophilic/hydrophobic ratio, structural properties (amorphous/crystalline ratio), and the number of active sites were optimized through metal-catalyzed pyrolysis. Stability of ACCS and Pt/ACCS were evaluated using an accelerated stress test (AST). The results indicated that Pt/ACCS showed no significant loss of MA and power density after 5,000 cycles at 1.0–1.5 V, while the commercial Pt/C catalysts showed drastic losses of MA and power density. Finally, monolayers of compressed Pt (core–shell-type Pt 3 Co 1 ) catalysts were structured by diffusing Co atoms (previously embedded in ACCS) into Pt. Compressive Pt lattice (Pt * ) catalysts were synthesized through an annealing procedure developed at the University of South Carolina (USC). The Pt * /ACCS catalyst showed high initial power density (rated) of 0.174 g Pt kW −1 and high stability (24 mV loss) at 0.8 A cm −2 after 30,000 cycles (0.6–1.0 V). The outstanding performance of Pt * /ACCS is due to the synergistic effect of ACCS and compressive Pt * lattice.

25 ENERGY STORAGE↗

Ordered CoPt oxygen reduction catalyst with high performance and durability

A high-performance and durable polymer electrolyte membrane fuel cell cathode catalyst composed of an ordered L10–CoPt core and a thin Pt shell was designed and prepared. Under practical fuel cell membrane electrode assembly testing conditions, the cathode catalyst showed an outstanding initial mass activity of 0.6 A/mgPt, which satisfies the U.S. Department of Energy performance target while also meeting the durability target of less than 40% loss in mass activity after 30,000 accelerated stress test voltage cycles. The high structural stability of the L10–CoPt@Pt-shell catalyst was confirmed by postmortem materials characterization, and the origin of this robustness was revealed by density functional theory calculations, where the barriers for diffusion of Co atoms were observed to be significantly increased in the ordered intermetallic core.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Durability testing at 5 atmospheres of advanced catalysts and catalyst supports for gas turbine engine combustors

The durability of CATCOM catalysts and catalyst supports was experimentally demonstrated in a combustion environment under simulated gas turbine engine combustor operating conditions. A test of 1000 hours duration was completed with one catalyst using no. 2 diesel fuel and operating at catalytically-supported thermal combustion conditions. The performance of the catalyst was determined by monitoring emissions throughout the test, and by examining the physical condition of the catalyst core at the conclusion of the test. Tests were performed periodically to determine changes in catalytic activity of the catalyst core. Detailed parametric studies were also run at the beginning and end of the durability test, using no. 2 fuel oil. Initial and final emissions for the 1000 hours test respectively were: unburned hydrocarbons (C3 vppm):0, 146, carbon monoxide (vppm):30, 2420; nitrogen oxides (vppm):5.7, 5.6.

Olson, B. A.↗

Constructing Highly Porous Low Iridium Anode Catalysts Via Dealloying for Proton Exchange Membrane Water Electrolyzers

Iridium (Ir) is the most active and durable anode catalyst for the oxygen evolution reaction (OER) for proton exchange membrane water electrolyzers (PEMWEs). However, their large-scale applications are hindered by high costs and scarcity of Ir. Lowering Ir loadings below 1.0 mgcm -2 causes significantly reduced PEMWE performance and durability. Therefore, developing efficient low Ir-based catalysts is critical to widely commercializing PEMWEs. Herein, an approach is presented for designing porous Ir metal aerogel (MA) catalysts via chemically dealloying IrCu alloys. In this study, the unique hierarchical pore structures and multiple channels of the Ir MA catalyst significantly increase electrochemical surface area (ECSA) and enhance OER activity compared to conventional Ir black catalysts, providing an effective solution to design low-Ir catalysts with improved Ir utilization and enhanced stability. An optimized membrane electrode assembly (MEA) with an Ir loading of 0.5 mg Ir cm -2 generated 2.0 A cm -2 at 1.79 V, higher than the Ir black at a loading of 2.0 mg Ir cm -2 (1.63 A cm -2 ). The low-Ir MEA demonstrated an acceptable decay rate of ≈40 µV h -1 during durability tests at 0.5 (>1200 h) and 2.0 A cm -2 (400 h), outperforming the commercial Ir-based MEA (175 µV h -1 at 2.0 mg Ir cm -2 ).

36 MATERIALS SCIENCE↗

Optimization of metal-supported solid oxide electrolysis cells with infiltrated catalysts

We report metal-supported solid oxide electrolysis cells (MS-SOECs) are being developed for steam-to-hydrogen electrolysis, especially for utilization of dynamic or intermittent electrical power from renewable sources. Various aspects of the electrocatalyst processing and composition, and metal support structure were explored. Catalyst materials, infiltration temperature and infiltration cycles were optimized for high performance and durability. Numerous catalyst materials were screened for both oxygen and steam electrodes. The oxygen catalyst had moderate impact on both initial cell performance and durability. Reducing Ni content in the steam electrode had little effect on durability, but reduced initial performance. Ex-situ XRD analysis and cell assessment of catalyst infiltration temperature revealed that the optimal range is 750–850 °C. The best cell performance and durability was achieved with LSCF-SDC oxygen electrocatalyst and SDC-Ni (60:40 vol%) steam electrocatalyst infiltrated 11 times at 800 °C and operated at 700 °C. At low steam content, a significant mass transport limitation on the steam side results in limiting current behavior. Thinner and more porous metal supports were implemented, and found to improve steam mass transport at low steam content, relevant for SOECs operating under high H 2 recycle rate or high steam utilization.

08 HYDROGEN↗

Investigation of methane and ethane pyrolysis with highly active and durable iron-alumina catalyst to produce hydrogen and valuable nano carbons: Continuous fluidized bed tests and reaction rate analysis

The goal of this research work was to evaluate a novel iron-alumina catalyst for methane and ethane pyrolysis with high conversion rates to H 2 with a long life time to address two major issues reported with previous catalysts. Fluidized bed tests demonstrated continuous hydrogen production while collecting carbon containing fines. During the 230 h fluid bed test the methane conversion rate to hydrogen at 700 °C remained above 80% for 160 h while creating valuable nano carbons. Similarly high catalyst lifetimes with high methane conversions have not been reported before. Ethane was more active than methane for pyrolysis with 100% conversion to H 2 . Transmission electron microscopy and Raman analysis of the carbon showed single and multiwall nanotubes and conglomerate nano-fibers. Ethane did not impact the allotrope of carbon formed. TGA was used to create a data array that was used for kinetic analysis and reaction model parametric regressions. Ethane had a higher rate of pyrolysis that was 2.3–2.8 times that of methane. Ethane pyrolysis was found to be more sensitive to temperature with a higher activation energy of 62 kJ/mol as compared to methane at 43 kJ/mol. The frequency factor, A i , was significantly higher for ethane at 0.73 [[kmol/m 3 -sec]/[N/m2] n ] compared to 0.03 for methane on the same basis. Both gases had a functional partial pressure order dependence of ~0.6 based on the regression analysis.

08 HYDROGEN↗

Highly durable platinum group metal-free catalyst fiber cathode MEAs for proton exchange membrane fuel cells

For this work, Fe-based platinum group metal (PGM)-free catalysts were incorporated into electrospun fiber mat or powder cathode membrane-electrode-assemblies (MEAs) with a Nafion 211 membrane and a Pt/C powder anode. Fabrication and characterization tests were performed on MEAs with: (1) a conventional powder cathode with a neat Nafion binder, (2) a fiber mat cathode with a Nafion/polyethylene oxide (PEO) binder, where PEO was extracted before MEA testing, (3) a powder cathode with a blended binder of Nafion and polyvinylidene fluoride (PVDF), and (4) a series of fiber mat cathodes with different Nafion/PVDF binder weight ratios. Cathode degradation occurred, with a loss in power output, in MEAs with a neat Nafion powder cathode or with a Nafion fiber cathode. In contrast, little or no power loss was observed for powder or fiber cathodes when the binder was a blend of Nafion and PVDF. The presence of hydrophobic PVDF drove water and electrogenerated peroxide out of the cathode, away from catalyst particles, which improved cathode durability, but PVDF also decreased the binder conductivity and slowed oxygen reduction kinetics, resulting in lower power densities. A 75:25 w:w Nafion:PVDF fiber cathode MEA was the best compromise for maximizing power and minimizing catalyst degradation. For such a cathode, with a PGM-free cathode catalyst loading of 3.0 mg cm –2 , a power density of 88 mW cm –2 at 0.5 V, 80 °C, and 200 kPa abs pressure was maintained for 80 h of continuous operation.

25 ENERGY STORAGE↗

Durability testing at one atmosphere of advanced catalysts and catalyst supports for automotive gas turbine engine combustors, part 1

The durability of catalysts and catalyst supports in a combustion environment was experimentally demonstrated. A test of 1000 hours duration was completed with two catalysts, using diesel fuel and operating at catalytically supported thermal combustion conditions. The performance of the catalysts was determined by monitoring emissions throughout the test, and by examining the physical condition of the catalyst core at the conclusion of the test. The test catalysts proved to be capable of low emissions operation after 1000 hours diesel aging, with no apparent physical degradation of the catalyst support.

Heck, R. M.↗

Atomically dispersed metal–nitrogen–carbon catalysts for fuel cells: advances in catalyst design, electrode performance, and durability improvement

The urgent need to address the high-cost issue of proton-exchange membrane fuel cell (PEMFC) technologies, particularly for transportation applications, drives the development of simultaneously highly active and durable platinum group metal-free (PGM-free) catalysts and electrodes. The past decade has witnessed remarkable progress in exploring PGM-free cathode catalysts for the oxygen reduction reaction (ORR) to overcome sluggish kinetics and catalyst instability in acids. Among others, scientists have identified the newly emerging atomically dispersed transition metal (M: Fe, Co, or/and Mn) and nitrogen co-doped carbon (M–N–C) catalysts as the most promising alternative to PGM catalysts. Here, we provide a comprehensive review of significant breakthroughs, remaining challenges, and perspectives regarding the M–N–C catalysts in terms of catalyst activity, stability, and membrane electrode assembly (MEA) performance. A variety of novel synthetic strategies demonstrated effectiveness in improving intrinsic activity, increasing active site density, and attaining optimal porous structures of catalysts. Rationally designing and engineering the coordination environment of single metal MN x sites and their local structures are crucial for enhancing intrinsic activity. Increasing the site density relies on the innovative strategies of restricting the migration and agglomeration of single metal sites into metallic clusters. Relevant understandings provide the correlations among the nature of active sites, nanostructures, and catalytic activity of M–N–C catalysts at the atomic scale through a combination of experimentation and theory. Current knowledge of the transferring catalytic properties of M–N–C catalysts to MEA performance is limited. Rationally designing morphologic features of M–N–C catalysts play a vital role in boosting electrode performance through exposing more accessible active sites, realizing uniform ionomer distribution, and facilitating mass/proton transports. We outline future research directions concerning the comprehensive evaluation of M–N–C catalysts in MEAs. The most considerable challenge of current M–N–C catalysts is the unsatisfied stability and rapid performance degradation in MEAs. Therefore, we further discuss practical methods and strategies to mitigate catalyst and electrode degradation, which is fundamentally essential to make M–N–C catalysts viable in PEMFC technologies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Durability of Highly Active PGM Catalyst MEA Tested Via Nitrogen and Air AST Cycling Under HDV Condition

PEMFCs are widely considered as the most promising power sources, particularly for heavy-duty vehicles (HDVs). Unfortunately, the degradation of MEAs under HDV condition remains insufficiently studied. In this work, we systematically investigated two MEAs with catalysts of Pt nanoparticles (NPs) supported over high surface area carbon black. These MEAs were tested for durability under HDV condition in nitrogen using a DOE AST protocol for 180,000 cycles, which is equivalent to 30,000 hours or 1 million miles of operation. The commercial Catalyst MEA also underwent 6,000 AST cycles in air under M2FCT condition. We comprehensively investigated the degradation of catalysts. Our results indicate that both MEAs undergo continuous performance degradation in H 2 /air and H 2 /O 2 during the AST cycling in nitrogen, where analysis employing scanning transmission electron microscopy (STEM) and inductively coupled plasma mass spectrometry (ICP-MS) reveal significant degradation behavior for Pt catalysts. The MEA exhibits more significant degradation, especially within mass transfer region, during the AST process in air. In conclusion, this study describes the long-term degradation behavior and mechanism with AST cycling in nitrogen or air governing highly efficient and durable PGM-catalyst MEA design under HDV conditions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Review—Meeting Fuel Cell Catalyst Requirements for Heavy-Duty Vehicle Applications

Catalyst requirements for proton exchange membrane (PEM) fuel cells differ by applications. Commercial heavy-duty vehicle (HDV) applications consume more H 2 fuel and demand higher durability than many others and the total cost of ownership (TCO) of the vehicle is largely related to the performance and durability of catalysts. This article is written to bridge the gap between the industrial requirements and academic activity for advanced cathode catalysts with an emphasis on durability. From a materials perspective, the underlying nature of the carbon support, Pt-alloy crystal structure, stability of the alloying element, cathode ionomer volume fraction, and catalyst-ionomer interface play a critical role in improving performance and durability. We provide our perspective on four major approaches, namely, mesoporous carbon supports, ordered PtCo intermetallic alloys, thrifting ionomer volume fraction, and shell-protection strategies that are currently being pursued. While each approach has its merits and demerits, their key developmental needs for future are highlighted.

Ramaswamy, Nagappan (ORCID:0000000234302758)↗

The Impact of Membrane Inactive Area on the Durability of Pt-Co Catalyst

Platinum (Pt) is the most active catalyst for oxygen reduction reaction; however, its activity still requires a significant increase to meet the demands of practical applications. To enhance the catalytic activity, alloy catalysts like platinum-cobalt (Pt-Co), are being extensively investigated. However, Co leaching from the Pt-Co alloy remains a significant concern. Evaluating the durability of Pt-Co alloy catalyst is further complicated by variations in Co leaching, which affects both the observed performance and durability. This variability often arises from an overlooked factor: choice of the inactive area of the membrane electrode assembly (MEA) used during the evaluation. This study examines the critical role of membrane inactive area on the performance loss observed during durability testing of Pt-Co alloys. Our findings indicate that a large membrane inactive area reduces the impact of Co leaching on performance and durability, up to 200 mA cm −2 difference in performance is observed between large and small inactive area MEA at 0.7 V for dry conditions, and more Co is retained in the active area of MEA for smaller inactive areas which is responsible for larger performance losses.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Biphasic Janus Particles Explain Self-Healing in Pt–Pd Diesel Oxidation Catalysts

The addition of Pd to Pt-based diesel oxidation catalysts is known to enhance performance and restrict the anomalous growth of Pt nanoparticles when subjected to aging at high temperatures in oxidative environments. To gain a mechanistic understanding, we studied the transport of the mobile Pt and Pd species to the vapor phase, since vapor phase transport is the primary route for sintering in these catalysts. The results are surprising: there is a 30-fold drop in the effective vapor pressure of Pt in the Pt-Pd catalysts compared to monometallic Pt. At the same time, there is a significant enhancement in the vapor pressure of Pd, compared to PdO, which otherwise has a negligible vapor pressure at the aging temperature. Such behavior cannot be explained simply by alloying Pt and Pd in the metallic phase, or a core-shell morphology where a PdO shell covers a Pt core. Transmission electron microscopic examination of catalysts aged up to 50 h in air at 800 °C shows that the particles exhibit a biphasic “Janus”-like structure. The metal and oxide phases are conjoined, exposing a metal and an oxide face to the gas phase. The high mobility of the Pt and Pd allows them to be partitioned into the metal and oxide phases, in apparent thermodynamic equilibrium. The PdO helps to trap mobile PtO2 and as a result contains high concentrations of Pt oxide, consistent with its role in mitigating the transport of Pt to the vapor phase and preventing the growth of anomalously large particles. In turn, Pt allows Pd to remain metallic, allowing the catalyst to retain both metal and oxide functionality for catalysis. The regeneration of deactivated catalysts typically requires an external input, such as a change in the working environment from reducing to oxidizing or vice-versa. Here, we show that the mobile species, which are primary contributors to catalyst sintering are effectively returned to the active site, hence our use of the term “selfhealing”. The detailed insights into the inner workings of the Pt-Pd diesel oxidation catalysts can help provide clues to the design of robust and durable heterogeneous catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Durability of Pt-Alloy Catalyst for Heavy-Duty Polymer Electrolyte Fuel Cell Applications under Realistic Conditions

As an emerging technology, polymer electrolyte fuel cells (PEFCs) powered by clean hydrogen can be a great source of renewable power generation with flexible utilization because of high gravimetric energy density of hydrogen. To be used in real-life applications, PEFCs need to maintain their performance for long-term use under a wide range of conditions. Therefore, it's important to understand the degradation of the PEFC under protocols that are closely related to the catalyst lifetime. Alloying Pt with transitional metal improves catalyst activity. It is also crucial to understand Pt alloys degradation mechanisms to improve their durability. To study durability of Pt alloys, accelerated stress tests (ASTs) are performed on Pt-Co catalyst supported on two types of carbon. Two different AST protocols were being studied: Membrane Electrolyte Assembly (MEA) AST based on the protocol introduced by the Million Mile Fuel Cell Truck consortium in 2023 and Catalyst AST, adopted from the U.S. Department of Energy (DoE).

25 ENERGY STORAGE↗

Characterization of a Sulfonated Poly(Ionic Liquid) Block Copolymer as an Ionomer for Proton Exchange Membrane Fuel Cells using Rotating Disk Electrode

Ionic liquid (IL) additives to both traditional and advanced oxygen reduction reaction (ORR) electrocatalysts have yielded remarkable improvements in catalyst performance and durability. However, incorporating ILs or IL-modified catalysts into the electrodes of a proton exchange membrane fuel cell (PEMFC) membrane electrode assembly (MEA) has proven to be challenging. Sulfonated poly(ionic liquid) block copolymers (S-PILBCP) present an opportunity to incorporate IL functionality directly into the ionomer, orthogonal to protonic conductivity. Here, we use a rotating disc electrode (RDE) to characterize the interface between a S-PILBCP and Pt catalyst in comparison to Nafion. Catalyst thin films prepared with S-PILBCP show an 80% improvement in the ORR activity over those containing Nafion. Thin films of S-PILBCP also show a significantly reduced degree of poisoning sulfonate adsorption on a Pt(111) surface in comparison to Nafion. Furthermore, these half-cell results provide useful insights that help to highlight the source of the impact of the S-PILBCP on PEMFC MEA performance.

25 ENERGY STORAGE↗

Electrochemical Degradation of Pt 3 Co Nanoparticles Investigated by Off-Lattice Kinetic Monte Carlo Simulations with Machine-Learned Potentials

In fuel cell applications, the durability of catalysts is critical for large-scale industrial implementation. However, limited synthesis controllability and spectroscopic resolution impede a comprehensive understanding of degradation mechanisms at the atomic level. In this study, we develop a machine-learned potential (MLP) to simulate the degradation processes for Pt3Co nanoparticles. The precision of MLP is determined to be comparable to that of density functional theory calculations. Using off-lattice kinetic Monte Carlo simulations with MLP, we successfully replicate established experimental trends and offer a logical resolution to ongoing debates regarding atomic orderings. Based on the simulation results, we suggest design principles for Pt3Co nanoparticles that combine high activity and durability. Finally, we validate the wide applicability of our method by successfully applying it to Pt3Ni and Pt3Co0.5Ni0.5 nanoparticles. The research serves as a guideline for developing MLPs for alloy electrochemical catalysts and lays the foundation for designing more durable and active fuel-cell catalysts.

36 MATERIALS SCIENCE↗