Search NASA⌕ Search

SEARCH · Search NASA

Results for “friction stir”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Indentation investigation of 304L stainless steel friction stir weld simulated crack repair

Simulated cracks were repaired in 304L stainless steel using low temperature friction stir welding. Indentation studies were carried out to understand the effect of microstructural features on the mechanical property variation across the weld and to measure the size of the weld zones with a quantitative technique. Microhardness and nanoindentation hardness profiles were constructed on a transverse section across the weld. The data obtained were correlated by extrapolating the nanoindentation hardness to greater depths which showed that the nanoindentation hardness closely reflects the microhardness values throughout the weld. Finally, grain size in the stir zone (SZ) was found to vary with the tool temperature which, in turn, alters the nanoindentation modulus variability and higher tool temperature resulted in widening of the SZ.

36 MATERIALS SCIENCE↗

Additive friction stir deposition of SS316: Effect of process parameters on microstructure evolution

Solid state nature of additive friction stir deposition (AFSD) additive manufacturing process is very advantageous in terms of defect formation and microstructural refinement in the material. Current study presents the process optimization, microstructural evolution and kinetics of recrystallization for AFSD deposited low stacking fault energy material - SS316. As deposited microstructure shows equiaxed ultra fine grains with an average grain size of ~5.0 ± 0.5 μm. Shear deformation at high temperature during processing leads to the operation of restoration mechanisms. Observation of necklace type microstructure in the as deposited SS316 is attributed to discontinuous dynamic recrystallization during processing. Recrystallization kinetics of the AFSD SS316 is characterized using Johnson-Mehl-Avarami-Kolmogorov (JMAK) model. Deformation – thermal cycling during AFSD process resulted in inconsistent recrystallization kinetics. Variation in strain, strain rate and temperature during processing with processing parameters result in varying microstructure and tool wear. Further, high strength-ductility combination and sustained work hardening in as deposited SS316 appear to arise from transformation and twinning during deformation, leading to the formation of hierarchical twins and martensitic phase after deformation.

36 MATERIALS SCIENCE↗

Manufacturing Oxide Dispersion Strengthened (ODS) steel plate via cold spray and friction stir processing

Oxide dispersion strengthened (ODS) steels, traditionally fabricated by ball milling and conventional powder metallurgy techniques to achieve bulk form, followed by intricate rolling and thermal treatment steps to achieve plate or sheet form. Here, we present a novel processing route that combines cold spray (CS) with friction stir processing (FSP) to manufacture ODS steel plate directly from gas atomization reaction synthesis (GARS)-prepared powder, thus no rolling steps involved. Microstructural and mechanical characterizations were performed to assess the quality and properties of the resulting ODS steel plate. Our findings demonstrate that the slightly porous CS deposited layer was fully consolidated after FSP, yielding a fully dense ODS steel plate that exhibited a favorable tradeoff between strength and ductility upon extraction from the substrate. Furthermore, through microstructural analysis, we revealed the presence of an appreciable density (∼10 22 /m 3 ) of nano-sized oxide particles, with the majority being smaller than 5 nm via the combined CS + FSP fabrication route. This work serves as a first proof-of-concept demonstration of the manufacturing approach described herein, offering a possible alternative route for producing ODS steel plates.

36 MATERIALS SCIENCE↗

On the solid-state-bonding mechanism in friction stir welding

This study is a critical assessment of various solid-state-bonding mechanisms is established for friction stir welding (FSW) processes of engineering alloys. The commonly assumed sintering-like diffusional-bonding hypothesis is criticized in this work as not the dominant mechanism. For the wide spectrum of material constitutive laws and FSW processing conditions examined and employed in realistic applications, the thermomechanical history on the workpiece–workpiece interface traverses in the creep-dominated regime for the growth/shrinkage of interfacial cavities. The evolution of the bonding fraction relies mainly on the creep strain rate in the adjourning workpieces, weakly on stress triaxiality, and negligibly on interfacial diffusion.

36 MATERIALS SCIENCE↗

Peak microhardness recovery via T6 heat treatment with extremely soft annealed Al7075 feedstock in additive friction stir deposition

With standard T6 heat treatments, precipitate-hardened alloys such as Al7075 and Al6061 fabricated using Additive Friction Stir Deposition (AFSD) method restore to noticeablely different peak mechanical properties. Previous research observed similar results but did not provide a viable solution. This study proposes a new processing strategy, namely enhanced plastic deformation by subjecting the Al7075 feedstock to annealed softening treatments. Specifically, by annealing the standard T651-Al7075 feedstock and deposition substrate (179 HV), their Microhardness were first degraded to its lowest state (80 HV), which is called a Soft-to-Soft system. For the Soft-to-Soft system subjected to AFSD, after undergoing appropriate T6 heat treatment, the microhardness of the AFSD 7075 alloy was restored to its peak value (183.1 ± 1.8 HV). The results indicate that this softening strategy can effectively reduce the non-strengthening phase in the AFSD matrix, thereby increasing the strengthening phase (η′ phase). This addresses the issue of traditional AFSD-prepared aluminum alloys being unable to achieve peak performance through T6 heat treatment.

36 MATERIALS SCIENCE↗

Computationally inexpensive part-scale thermal history of additive friction-stir deposition

This study presents an analytical model for steady-state power generation and tool heat loss in additive friction-stir deposition (AFSD), developed to enable part-scale thermal simulation while remaining computationally inexpensive. The model predicts total generated power, yielding 3.7–4.7 kW across deposition temperature setpoints of 400–460 °C for the deposition of AA6061 with a Be-Cu tool. This corresponds to 90–95% of the reported spindle power. Tool heat loss is experimentally determined by calibrating a steady-state energy balance between the generated power, the substrate-deposition thermal gradient, and a temperature dependent tool heat loss term: q tool (T) = a + b (T - 400°C) with a = 2.7 x 10 6 Wm -2 and b = 9.5 x 10 3 Wm -2 K -1 . The calibration indicates that about 69% of the generated heat is conducted into the tool for this configuration, which is much higher than previously reported. The calibrated heat-source is implemented in finite element software (Adamantine) to simulate the transient thermal history of a 100 cm 3 representative build in 8 min on a standard desktop (at 0.635 mm build-height resolution). For the first three layers, the substrate temperatures between simulation and experiment are within 10% mean absolute percentage error. Sensitivity analysis indicates that uncertainties in average deposition temperature and deformation localization (stir-zone geometry, depth, and spatial dependance of strain-rate and flow stress) dominate model variance, motivating additional experimental verification.

Additive Friction-Stir Deposition↗

Galvanic corrosion of AZ31B joined to dual-phase steel with and without Zn layer by ultrasonic and friction stir welding

Galvanic corrosion of AZ31B joined with bare or Zn-coated DP590 steel by ultrasonic spot welding or linear friction stir welding was quantitatively studied by pre-defining anode and cathode in the lap joint samples. Corrosion volume and depth from Mg anode surfaces exposed to 0.1 M sodium chloride solution was analyzed as functions of cathode surface type and welding method. Characterization of as-welded joints was performed to identify any microstructural feature of the bonding zone that could impact galvanic corrosion behavior. COMSOL modeling with modified user subroutine was conducted to simulate the progression of Mg corrosion in the same joint and electrode configurations used for the corrosion experiments. The experimental results indicated that Zn-coated cathode surface can reduce Mg galvanic corrosion significantly as galvanic polarization and cathodic current on Zn-coated surface remained relatively low for Mg in the weld joints. COMSOL modeling described the growth of Mg galvanic corrosion in a reasonable manner but showed limitation by underestimating the corrosion volume as it did not capture self-corrosion.

36 MATERIALS SCIENCE↗

A comparative analysis of residual stresses from friction stir processing of aluminum cast 380 and wrought 7075 alloy sheets: experimental characterization and modeling

Residual stresses are often overlooked in friction stir processing (FSP), but their significant impact on fatigue performance necessitates their consideration in optimizing processing parameters. The first step in this effort is understanding how process conditions influence residual stress distributions, especially across different alloys. This study focuses on determining and explaining the through-thickness residual stress variations and the effect of process temperature on the residual stress magnitude in wrought AA7075 and cast AA380.0 alloys. Additionally, for AA380.0, the impact of a second FSP pass was investigated. To achieve this, hole-drilling electronic speckle pattern interferometry (ESPI) and the thermal pseudo-mechanical (TPM) model within finite element analysis were employed to study the 3D distributions of in-plane residual stresses in processed samples under various conditions. A key finding was the varying impact of process temperatures on residual stress magnitudes. Higher process temperatures reduced stresses in AA380.0 but increased them in AA7075. Additionally, the through-thickness stress distributions differed between the two alloys. Further analysis revealed that yield stresses are crucial in explaining these phenomena and the effects of additional FSP passes. Further, this fundamental understanding will be vital in guiding the efforts to mitigate residual stresses and assess their impact on the performance of FSP aluminum alloys.

36 MATERIALS SCIENCE↗

Friction stir processing: A thermomechanical processing tool for high pressure die cast Al-alloys for vehicle light-weighting

This study uses friction stir processing (FSP) for thermomechanical processing of high-pressure die-casting (HPDC) to modify microstructure and improve mechanical properties. FSP is carried out on two different HPDC aluminum alloys: (a) general-purpose, high-iron, HPDC A380 alloy and (b) premium quality, low-iron HPDC Aural-5 alloy in thin wall, flat plate geometry. Subsequent mechanical testing shows ~30 % and ~65 % enhancement in yield strength and tensile ductility. In addition, FSP leads to ~10 times improvement in fatigue life for A380 alloy and ~70 % improvement in fracture toughness for Aural-5 alloy. These findings emphasize the capability of FSP to modify the microstructure of HPDC Al-alloys-based structural components so that they can demonstrate a good combination of strength, ductility, fracture toughness, and high fatigue properties for long-term durability and reliability.

36 MATERIALS SCIENCE↗

Three-dimensional microstructure of a friction stir welded magnesium/steel interface characterized via high-energy synchrotron X-rays

Here, the three-dimensional (3D) microstructure of a friction stir assisted scribe technique (FaST) weld interface consisting of AZ31 magnesium (Mg) alloy and zinc (Zn)-coated DP590 steel was analyzed via synchrotron micro-computed tomography (μ-CT), correlated to synchrotron x-ray diffraction, and electron microscopy. Diffraction assessment of the AZ31/Zn-coated DP590 steel interface revealed the presence of several complex Mg–Zn intermetallic phases and differences in crystalline orientation of the Mg phase at the weld interface. The 3D characterization of the synchrotron μ-CT images of the weld interface revealed: (1) the presence of AZ31 weld nugget material with iron (Fe)-rich particles; (2) the presence of a weld layer at the joining interface with Fe-rich particles; (3) the formation of a thin non-uniform layer between the weld layer and the interface of the scribed DP590 material; and (4) the presence of an Fe–Al-rich intermetallic layer and Fe-rich particles at the interface of the scribed DP590 material. This study also performed a detailed analysis of lump-like features seen in the Zn coating layer at the weld interface. A detailed 3D particle analysis of the Fe-rich particles in the AZ31 weld nugget and the weld layer at the weld interface revealed the presence of several types of particle morphologies (i.e., spherical and irregular).

36 MATERIALS SCIENCE↗

Heterogenous activation of dynamic recrystallization and twinning during friction stir processing of a Cu-4Nb alloy

An interplay between high degree of shear deformation and deformation-induced heating occurs during friction stir processing (FSP) of metals. In medium-to-low stacking fault energy Cu alloys, this can lead to a complex spatially heterogenous activation of dynamic recrystallization (DRX) and twinning mechanisms. Within the Cu-Nb system, the presence of Nb is further expected to influence the DRX mechanism of the Cu matrix. However, the microstructural changes induced by the co-deformation of Nb during FSP are still not well understood. So, this study uses a combination of multimodal microstructural characterization, solution thermodynamics-based predictions, and computational crystal plasticity simulation to reveal the various microstructural evolution mechanisms that can occur during FSP of a Cu-4at.%Nb binary model alloy. The formation of softer DRX zones, and harder shear localization regions are revealed using electron backscatter diffraction, transmission electron microscopy, atom probe tomography, and crystal plasticity modeling.

36 MATERIALS SCIENCE↗

Gradient process parameter optimization in additive friction stir deposition of aluminum alloys

As one of the most novel additive manufacturing methods, currently selection and optimization of processing parameters in additive friction stir deposition (AFSD) have mainly relied on experiments and subsequent characterization of microstructural and mechanical properties. Such approaches are both time- and resource-consuming. Therefore, an ultrasound elastography enhanced gradient process parameter optimization method was applied in the present work to obtain a window of optimized processing parameters for AFSD processing of aluminum alloy by varying both rotational and linear deposition speeds. Further, the quality of AFSD processed layer was investigated for physical nature of surface, dynamic elastic modulus, and microstructural aspects in cross-sections of the deposited layer. The efficiency in exploring process parameters was significantly enhanced by implementing a high-throughput screening experimental design based on application of gradient process parameters and continuous ultrasound elastographs. In addition, the applied ultrasonic elastography technique assisted in evaluating the homogeneity in microstructure and mechanical properties of AFSD sample over the entire gradients of the process parameters. The techniques adopted in current work can be further extended to identify suitable parameters for AFSD fabrication of components with desired mechanical properties such as hardness, fatigue, etc.

36 MATERIALS SCIENCE↗

Macroscale property assessment and indentation characteristics of thick section friction stir welded AA 5083

The spatial gradients in microstructure have been proven to be effective in optimizing the performance of components, and several techniques have been developed to achieve this microstructure. Nevertheless, the local microstructural modification methods inevitably result in the formation of gradient microstructure leading to a variation in the property. Herein this work systematically investigates the effect of gradient microstructure formed during thick section friction stir weld Al5083 alloy on its mechanical properties. A novel macro-indentation technique, profilometer-based indentation plastometry (PIP), is utilized to capture the variation in the mechanical properties in the feedstock (rolled plate) and weld region. The feedstock exhibited a gradient microstructure owing to different stress states during rolling. Additionally, the stirring of the tool resulted in a complex material flow pattern producing a microstructure gradient in the weld region. The aspect ratio of the grains was identified as the primary factor causing variation in indentation response in the feedstock. In contrast, variation in the grain size in the weld region resulted in property variation. Overall, the stir zone has a lower yield strength (158±4MPa) than the base material (173±3MPa). In addition, microstructure heterogeneity in the stir zone resulted in lower elongation than the base material.

36 MATERIALS SCIENCE↗

Real-time evolution of texture and temperature during friction stir processing of a magnesium alloy: An operando neutron diffraction study

The real-time development of texture and the evolution of temperature during friction stir processing (FSP) of a Mg alloy were investigated using an operando neutron diffraction measurement. A novel approach was applied in this study where the real-time, quasi-steady state measurements performed as a function of position during FSP are converted to a Lagrangian dataset that reveals the transient behavior as a function of time. The in-situ FSP was carried out under two different thermo-mechanical processing conditions represented by the Zener-Hollomon parameter, Z. Further, the results show that: (i) a shear texture develops from the initial strong basal texture with the peak temperature reaching about 774 K during a low-Z processing and (ii) a strong off-normal texture develops with a peak temperature of 616 K during a high-Z processing. Moreover, time-temperature-texture diagrams were established to reveal the real-time development of the texture during the processing for both the low Z and high Z processing conditions. The changes in texture will be discussed in terms of plastic deformation mechanisms active during various stages of the FSP under the two different processing conditions.

36 MATERIALS SCIENCE↗

Influencing mechanism of pre-existing nanoscale Al 5 Fe 2 phase on Mg–Fe interface in friction stir spot welded Al-free ZK60–Q235 joint

Al-free ZK60 magnesium (Mg) alloy sheet was selected as substrate material of Mg–steel pinless friction stir spot welding (FSSW), avoiding the effect of the Al element in the substrate on the alloying reaction of Mg-iron (Fe) interface. The sound FSSW joint of ZK60 Mg alloy and Q235 steel with a hot-dipped aluminum (Al)-containing zinc (Zn) coating was successfully realized. The detailed microstructural examinations proved that Al 5 Fe 2 phase at the Mg-Fe interface came from the pre-existing Al 5 Fe 2 phase in the coating and acted as the transition layer for promoting the metallurgical bonding of Mg and Fe. The interfaces with well-matched lattice sites among Fe, Al 5 Fe 2 and Mg were formed during FSSW. A low energy interface with good match of lattice sites ((002) Al5Fe2 //(110) Fe , [110] Al5Fe2 //[13] Fe ) between Al 5 Fe 2 and Fe was identified. For the interface between Al5Fe2 and Mg, an orientation relationship of ( 6 2 ¯ 2 ) A l 5 F e 2 / / ( 3 1 ¯ 1 ¯ 2 ¯ ) M g and [ 1 5 ¯ 8 ¯ ] A l 5 F e 2 / / [ 2 4 ¯ 23 ] M g was observed. The tensile–shear load of the ZK60–steel joint could reach 4.6 kN. Moreover, the joint fracture occurred at the interface between the Al5Fe2 layer and the Mg alloy substrate, suggesting the brittle fracture characteristic.

36 MATERIALS SCIENCE↗

Texture and precipitation behavior of friction stir welded Inconel 825 alloy

The microstructure, texture pattern, and precipitation behavior of friction stir butt welded Inconel 825 alloy are highlighted here. The microstructure of bright regions and black-banded regions in the stir zone (SZ) is characterized by SEM, EBSD, and TEM with EDS. EBSD analysis justifies that the SZ exhibits a dynamic recrystallized structure. Grain boundary mapping corroborates the insignificant difference in the low- and high-angle grain boundaries fraction between the SZ, the thermo-mechanically affected zone, and the base metal. TEM analysis confirms the formation of nano twins and dispersion of nano-size precipitations in the grains, and at the grain boundaries as well. Grain refinement and nano-size precipitation formation in the SZ significantly enhanced both microhardness and tensile strength.

Das, Hrishikesh↗

Microstructure and texture evolution of friction stir lap welded dissimilar multi-aluminum stack

Here this work investigates the microstructural evolution of a dissimilar multiple-aluminum alloy stack (AA7055, AA7055, AA6022) produced by friction stir lap welding (FSLW). A through-thickness analyses of grain orientation map, grain size and distribution, strain distribution, and texture evolution by electron backscattered diffraction-based characterization technique were performed. Two different welding parameters (combination of tool rotation and traverse speed) were used to study the effects of the welding parameters on these microstructural characteristics. The study shows that higher welding speed and higher rotation speed of the FSLW tool yield finer grains. FSLW resulted in shear texture formation in the weld regions due to high welding speeds. This texture development in the nugget zone is consistent with shear deformation, and (111) pole figures show ideal shear texture components. The Stir Zone (SZ) exhibits shear texture (A/A ̅ and B/B ̅ components), consistent with other shear-assisted processes. Recrystallization mechanisms observed are CDRX in SZ and DDRX in TMAZ (Thermo-Mechanically Affected Zone). Interface analysis reveals the presence of oxide layers between different aluminum sheets, affecting joint mechanical performance. The mechanical property of the lap welded joints was presented in terms of microhardness distribution across the weld cross section. Slightly higher hardness in higher speed welding setup was observed throughout the SZ and AA6022 layer, indicating greater grain refinement and uniform grain structure distribution.

36 MATERIALS SCIENCE↗

Understanding the effect of friction stir processing on electrical steel: Microstructural changes and mechanical transformations

Raising Si beyond 3.5 wt% reduces core loss but embrittles electrical steels, constraining processing and application. Here we assess friction stir processing (FSP) as a solid‑state route to enable Fe–4.0 wt% Si with improved mechanical performance. Temperature‑controlled FSP with a PcBN tool produced a defect‑free processed zone. SEM/EBSD revealed dynamic recrystallization and grain refinement from an average 110 μm in the base material to ∼20 μm in the processed region, with ∼ 80% of grains < 40 μm and a reduction in high‑angle boundary fraction to ∼65% (vs >85% in the base). Comparative mechanical property analysis shows a moderate increase in yield strength in FSP samples relative to the base material, with a significant improvement in ductility (∼35–50%). Post‑fracture EBSD identified 60° twin boundaries in the base while sub-grain formation with elevated KAM in the FSP sample. Fractography revealed a shift from quasi‑cleavage in the Base-faceted planes with river patterns, steps, and occasional secondary cracks—to ductile micro void coalescence after FSP. Following FSP, the material retains soft‑magnetic behavior, with modest shifts in saturation magnetization consistent with grain refinement and stored strain, accompanied by a clear gain in formability. These results indicate that FSP provides a viable route to deploy higher‑Si electrical steels with concurrent gains in strength and ductility.

Electrical steel↗