SEARCH · Search NASA
Results for “graphite anodes”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Ab initio molecular dynamics simulations of the initial stages of solid–electrolyte interphase formation on lithium ion battery graphitic anodes
Explore the source record for details and available documents.
Assessment of Li-Inventory in Cycled Si-Graphite Anodes Using LiFePO 4 as a Diagnostic Cathode
Not Available
Understanding the Thermal Behavior and Safety of Silicon-Graphite Anodes
Explore the source record for details and available documents.
Materials Safety Studies of Practical Nano-Silicon + Graphite Anodes for Lithium-ion Batteries.
Abstract not provided.
High voltage aqueous electrolyte system for lithium metal or graphite anode
The present invention is directed to aqueous solid state electrolytes that comprise a fluoride additive to stabilize the interface between the anode and aqueous electrolyte. The present invention is also directed to methods of making the solid state electrolyte materials and methods of using the solid state electrolyte materials in batteries and other electrochemical technologies.
High efficiency electrolytes for high voltage battery systems
Disclosed herein are embodiments of an electrolyte that is stable and efficient at high voltages. The electrolyte can be used in combination with certain cathodes that exhibit poor activity at such high voltages with other types of electrolytes and can further be used in combination with a variety of anodes. In some embodiments, the electrolyte can be used in battery systems comprising a lithium cobalt oxide cathode and lithium metal anodes, silicon anodes, silicon/graphite composite anodes, graphite anodes, and the like.
Direct recycling of lithium-ion battery scraps for manufacturing a new anode
An improved method of recycling lithium-ion battery anode scraps is provided. The method involves isolating an anode scrap including a graphite anode film adhered to a current collector foil with a polyvinylidene fluoride binder. The anode scrap is combined with deionized water to form a first mixture. The graphite anode film is delaminated from the current collector foil to form a second mixture comprising a free collector foil and a free graphite anode film. The free graphite anode film is filtered and dried from the second mixture to recover the free graphite anode film. The free graphite anode film is combined with a solvent comprising N-methyl-2-pyrrolidone (NMP) to form an anode formation slurry. The slurry is coated onto a copper current collector to produce a new anode.
Minimizing Polysulfide Shuttle Effect in Lithium-Ion Sulfur Batteries by Anode Surface Passivation
Lithium-ion sulfur batteries use non-metal materials as the anode to address safety concerns associated with lithium metal anode. However, polysulfide shuttle reactions still occur on the non-metal anode (such as graphite and Si), and result in limited battery efficiency. In this work, we used Al2O3 layers coated by atomic layer deposition (ALD) technique to suppress the shuttle reactions. With the optimal thickness of 2 nm Al2O3 coated on graphite anode, the Coulombic efficiency of the sulfur cathode was improved from 84% to 96% in the first cycle, and from 94% to 97% in the subsequent cycles. As a result, the discharge capacity of the sulfur cathode was increased to 550 mAh g-1 in the 100th cycle, as compared with 440 mAh g-1 when the pristine graphite anode was used. The Al2O3 passivation layer minimizes the formation of insoluble polysulfide (Li2S2, Li2S) on the surface of graphite anode and improves the efficiency and capacity retention of the graphite-sulfur batteries. The surface passivation strategy could also be used in other Li sulfur battery systems (with Li, Si, and Sn anodes), to minimize side reactions and enable high-performance and safe sulfur batteries.
The Anode Challenge for Lithium‐Ion Batteries: A Mechanochemically Synthesized Sn–Fe–C Composite Anode Surpasses Graphitic Carbon
Carbon‐based anodes are the key limiting factor in increasing the volumetric capacity of lithium‐ion batteries. Tin‐based composites are one alternative approach. Nanosized Sn–Fe–C anode materials are mechanochemically synthesized by reducing SnO with Ti in the presence of carbon. The optimum synthesis conditions are found to be 1:0.25:10 for initial ratio of SnO, Ti, and graphite with a total grinding time of 8 h. This optimized composite shows excellent extended cycling at the C/10 rate, delivering a first charge capacity as high as 740 mAh g −1 and 60% of which still remained after 170 cycles. The calculated volumetric capacity significantly exceeds that of carbon. It also exhibits excellent rate capability, delivering volumetric capacity higher than 1.6 Ah cc −1 over 140 cycles at the 1 C rate.
Chemical Evolution in Silicon–Graphite Composite Anodes Investigated by Vibrational Spectroscopy
Silicon–graphite composites are under development for the next generation of high-capacity lithium-ion anodes, and vibrational spectroscopy is a powerful tool to identify the different mechanisms that contribute to performance loss. With alloy anodes, the underlying causes of cell failure are significantly different in half-cells with lithium metal counter electrodes compared to full cells with standard cathodes. However, most studies which take advantage of vibrational spectroscopy have only examined half-cells. In this work, a combination of FTIR and Raman spectroscopy describes several factors that lead to degradation in full pouch cells with LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) cathodes. The spectroscopic signatures evolve after longer term cycling compared to the initial formation cycles. Several side-reactions that consume lithium ions have clear FTIR signatures, and comparison to a library of reference compounds facilitates identification. Raman microspectroscopy combined with mapping shows that the composite anodes are not homogeneous but segregate into graphite-rich and silicon-rich phases. Lithiation does not proceed uniformly either. A basis analysis of Raman maps identifies electrochemically inactive regions of the anodes. In conclusion, the spectroscopic results presented here emphasize the importance of improving electrode processing and SEI stability to enable practical composite anodes with high silicon loadings.
What makes lithium substituted polyacrylic acid a better binder than polyacrylic acid for silicon-graphite composite anodes?
Lithium substituted polyacrylic acid (LiPAA) has previously been demonstrated as a superior binder over polyacrylic acid (PAA) for Si anodes, but from where does this enhanced performance arise? In this paper, full cells are assembled with PAA and LiPAA based Si-graphite composite anodes that dried at temperatures from 100 °C to 200 °C. The performance of full cells containing PAA based Si-graphite anodes largely depend on the secondary drying temperature, as decomposition of the binder is correlated to increased electrode moisture and a rise in cell impedance. Full cells containing LiPAA based Si-graphite composite electrodes display better Coulombic efficiency than those with PAA, because of the electrochemical reduction of the PAA binder. This is identified by attenuated total reflectance Fourier transform infrared spectrometry and observed gassing during the electrochemical reaction. Finally, Coulombic losses from the PAA and Si SEI, along with depletion of the Si capacity in the anode results in progressive underutilization of the cathode and full cell capacity loss.
Superhydrophilic graphite surfaces and water-dispersible graphite colloids by electrochemical exfoliation
Superhydrophilic graphite surfaces and water-dispersible graphite colloids are obtained by electrochemical exfoliation with hydrophobic graphite electrodes. Such counterintuitive characteristics are caused by partial oxidation and investigated by examining both graphite electrodes and exfoliated particles after electrolysis. The extent of surface oxidation can be explored through contact angle measurement, scanning electron microscope, electrical sheet resistance, x-ray photoelectron spectroscopy, zeta-potential analyzer, thermogravimetric analysis, UV-visible, and Raman spectroscopy. The degree of wettability of the graphite anode can be altered by the electrolytic current and time. The water contact angle declines generally with increasing the electrolytic current or time. After a sufficient time, the graphite anode becomes superhydrophilic and its hydrophobicity can be recovered by peeling with adhesive tape. This consequence reveals that the anodic graphite is oxidized by oxygen bubbles but the oxidation just occurs at the outer layers of the graphite sheet. Moreover, the characteristics of oxidation revealed by UV peak shift, peak ratio between D and G bands, and negative zeta-potential indicate the presence of graphite oxide on the outer shell of the exfoliated colloids. However, thermogravimetric analysis for the extent of decomposition of oxygen functional groups verifies that the amount of oxygen groups is significantly less than that of graphite oxide prepared via Hummer method. The structure of this partially oxidized graphite may consist of a graphite core covered with an oxidized shell. The properties of the exfoliated colloids are also influenced by pH of the electrolytic solution. As pH is increased, the extent of oxidation descends and the thickness of oxidized shell decreases. Those results reveal that the degree of oxidation of exfoliated nanoparticles can be manipulated simply by controlling pH.
Superior long-term cycling of high-voltage lithium-ion batteries enabled by single-solvent electrolyte
A new single-solvent electrolyte system comprising lithium bis(fluorosuflonyl) imide (LiFSI) and beta-fluorinated sulfone (TFPMS) was designed to enable very stable long-term cycling of high-voltage lithium-ion batteries. Compared to other fluorinated solvents such as alpha-fluorinated sulfone (FMES) and fluorinated carbonate (FEMC), which are prone to reduction on the graphite anode, the LiFSI-TFPMS system displayed outstanding compatibility with graphite. While regular carbonate and sulfone from the LiFSI electrolyte system are compatible with the graphite anode, their high solvating power not only induces severe corrosion on the aluminum cathode current collector at high voltage, but also renders a low aggregation level at a normal salt concentration (about 1.0 M), resulting in the formation of an unstable solid-electrolyte interphase (SEI) on the graphite anode. Owing to the low solvating power of TFPMS, the aggregation level of the LiFSI-TFPMS system is relatively high even at normal salt concentration, which not only facilitates the formation of a robust SEI by the sacrificial decomposition of LiFSI, but also suppresses the aluminum corrosion of the LiFSI electrolyte system at high voltage. Together with the high intrinsic anodic stability of TFPMS, the superior cycling performance of graphite parallel to LiNi 0.6 Co 0.2 Mn 0.2 O 2 cells was achieved by employing the non-flammable LiFSI-TFPMS single-solvent electrolyte system.
A Fluorinated Ether Electrolyte Enabled High Performance Prelithiated Graphite/Sulfur Batteries
Lithium/sulfur (Li/S) batteries have attracted great attention as a promising energy storage technology, but so far their practical applications are greatly hindered by issues of polysulfide shuttling and unstable lithium/electrolyte interface. To address these issues, a feasible strategy is to construct a rechargeable prelithiated graphite/sulfur batteries. In this study, a fluorinated ether of bis(2,2,2-trifluoroethyl) ether (BTFE) was reported to blend with 1,3-dioxolane (DOL) for making a multifunctional electrolyte of 1.0 M LiTFSI DOL/BTFE (1:1, v/v) to enable high performance prelithiated graphite/S batteries. First, the electrolyte significantly reduces polysulfide solubility to suppress the deleterious polysulfide shuttling and thus improves capacity retention of sulfur cathodes. Second, thanks to the low viscosity and good wettability, the fluorinated electrolyte dramatically enhances the reaction kinetics and sulfur utilization of high-areal-loading sulfur cathodes. More importantly, this electrolyte forms a stable solid-electrolyte interphase (SEI) layer on graphite surface and thus enables remarkable cyclability of graphite anodes. Lastly, by coupling prelithiated graphite anodes with sulfur cathodes with high areal capacity of ~3 mAh cm -2 , we demonstrate prelithiated graphite/sulfur batteries that show high sulfur-specific capacity of ~1000 mAh g -1 and an excellent capacity retention of >65% after 450 cycles at C/10.
A Cobalt– and Manganese–Free High–Nickel Layered Oxide Cathode for Long–Life, Safer Lithium–Ion Batteries
High-nickel LiNi 1–x–y Mn x Co y O 2 and LiNi 1–x–y Co x Al y O 2 cathodes are receiving growing attention due to the burgeoning demands on high-energy-density lithium-ion batteries. The presence of both cobalt and manganese in them, however, triggers multiple issues, including high cost, high toxicity, rapid surface deterioration, and severe transition-metal dissolution. Herein, a Co- and Mn-free ultrahigh-nickel LiNi 0.93 Al 0.05 Ti 0.01 Mg 0.01 O 2 (NATM) cathode that exhibits 82% capacity retention over 800 deep cycles in full cells, outperforming two representative high-Ni cathodes LiNi 0.94 Co 0.06 O 2 (NC, 52%) and LiNi 0.90 Mn 0.05 Co 0.05 O 2 (NMC, 60%) is presented. It is demonstrated that a titanium-enriched surface along with aluminum and magnesium as the stabilizing ions in NATM not only ameliorates unwanted side reactions with the electrolyte and structural disintegrity, but also mitigates transition-metal dissolution and active lithium loss on the graphite anode. As a result, the graphite anode paired with NATM displays an ultrathin (≈8 nm), monolayer anode-electrolyte interphase architecture after extensive cycling. Furthermore, NATM displays considerably enhanced thermal stability with an elevated exothermic temperature (213 °C for NATM vs 180 and 190 °C for NC and NMC, respectively) and remarkably reduced heat release. This work sheds light on rational compositional design to adopt ultrahigh-Ni cathodes in lithium-based batteries with low cost, long service life, and improved thermal stability.
Effect of Si Content on Extreme Fast Charging Behavior in Silicon–Graphite Composite Anodes
Commercial Li-ion batteries typically incorporate a small amount of high-capacity silicon (Si)-based materials in the composite graphite-based anode to increase the energy density of the battery. However, very little is known about the effects of Si on the fast-charging behavior of composite anodes. Herein, we examine the effects of the Si/graphite ratio in the composite anode on the fast-charging behavior of full cells. We show that addition of Si increases the rate capability from 1C to 8C and improves the capacity retention in early cycles at 6C due to reduced overpotential in constant current charging cycles. The impacts of Si content on fast-charging aging were identified by Post-Test characterization. Despite realizing benefits of available capacity and reduced Li plating at 6C, silicon–electrolyte interactions lead the time-dependent cell performance to fade quickly in the long term. The Post-Test analysis also revealed the thickening of the electrode and nonuniform distribution of electrolyte decomposition products on the Si-containing anodes, as well as the organic-rich solid electrolyte interphase (SEI), which are the factors behind cell degradation. Our study sheds insight on the advantages and disadvantages of Si/graphite composite anodes when they are used in fast-charging applications and guides further research in the area by designing an optimized composition of Si incorporated in a mature graphite matrix.