Search NASA⌕ Search

SEARCH · Search NASA

Results for “graphite strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Structure-to-property Relationships in Addition Cured Polymers 2: Resin Tg Composite Initial Mechanical Properties of Norbornenyl Cured Polyimide Resins

PRM (polymerization of monomeric reactants) methodology was used to prepare thirty different polyimide oligomeric resins. Monomeric composition as well as chain length between sites of crosslinks were varied to examine their effects on glass transition temperature (Tg) of the cured/postcured resins. An almost linear correlation of Tg versus molecular distance between the crosslinks was observed. An attempt was made to correlate Tg with initial mechanical properties (flexural strength and interlaminar shear strength) of unidirectional graphite fiber composites prepared with these resins. However, the scatter in mechanical strength data prevented obtaining as clear a correlation as was observed for the structural modification/crosslink distance versus Tg. Instead, only a range of composite mechanical properties was obtained at the test temperatures studied (room temperature, 288 and 316 C). Perhaps more importantly, what did become apparent during the attempted correlation study was: (1) that PMR methodology could be used to prepare composites from resins that contain a wide variety of monomer modifications, and (2) that these composites almost invariably provided satisfactory initial mechanical properties as long as the resins selected were melt processable.

Alston, W. B.↗

Structure-to-property relationships in addition cured polymers. II - Resin Tg and composite initial mechanical properties of norbornenyl cured polyimide resins

PRM (polymerization of monomeric reactants) methodology was used to prepare thirty different polyimide oligomeric resins. Monomeric composition as well as chain length between sites of crosslinks were varied to examine their effects on glass transition temperature (Tg) of the cured/postcured resins. An almost linear correlation of Tg versus molecular distance between the crosslinks was observed. An attempt was made to correlate Tg with initial mechanical properties (flexural strength and interlaminar shear strength) of unidirectional graphite fiber composites prepared with these resins. However, the scatter in mechanical strength data prevented obtaining as clear a correlation as was observed for the structural modification/crosslink distance versus Tg. Instead, only a range of composite mechanical properties was obtained at the test temperatures studied (room temperature, 288 and 316 C). Perhaps more importantly, what did become apparent during the attempted correlation study was: (1) that PMR methodology could be used to prepare composites from resins that contain a wide variety of monomer modifications, and (2) that these composites almost invariably provided satisfactory initial mechanical properties as long as the resins selected were melt processable.

Alston, William B.↗

Manufacture of fiber-epoxy test specimens: Including associated jigs and instrumentation

Experimental work on the manufacture and strength of graphite-epoxy composites is considered. The correct data and thus a true assessment of the strength properties based on a proper and scientifically modeled test specimen with engineered design, construction, and manufacture has led to claims of a very broad spread in optimized values. Such behavior is in the main due to inadequate control during manufacture of test specimen, improper curing, and uneven scatter in the fiber orientation. The graphite fibers are strong but brittle. Even with various epoxy matrices and volume fraction, the fracture toughness is still relatively low. Graphite-epoxy prepreg tape was investigated as a sandwich construction with intermittent interlaminar bonding between the laminates in order to produce high strength, high fracture toughness composites. The quality and control of manufacture of the multilaminate test specimen blanks was emphasized. The dimensions, orientation and cure must be meticulous in order to produce the desired mix.

Mathur, S. B.↗

Oxidation resistance of selected mechanical carbons at 650 deg C in dry flowing air

Oxidation experiments were conducted with several experimental mechanical carbons at 650 C in air flowing at 28 cu cm/sec (STP). Experiments indicate that boron carbide addition and zinc phosphate treatment definitely improved oxidation resistance. Impregnation with coal tar pitch before final graphitization had some beneficial effect on oxidation resistance and it markedly improved flexure strength and hardness. Graphitization temperature alone did not affect oxidation resistance, but with enough added boron carbide the oxidation resistance was increased although the hardness greatly decreased.

Allen, G. P.↗

Graphite Material Behavior: NRC Graphite Behavior Model

Introduction to graphite Fabrication of graphite Unique features of nuclear grade graphite Providing the properties As-fabricated material properties of interest Thermal diff, thermal stability, mechanical strength, etc. General graphite behavior and degradation Microstructure: key to behavior Crystallographic structure Basal plane (covalent) bonding Porosity and pore microstructure Degradation Irradiation behavior Oxidation behavior Molten salt issues

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Toughening of graphite-epoxy composites by interlaminar perforated Mylar films

Fracture and notch strength tests of graphite-epoxy composites showed that unidirectional lay-ups generally exhibit longitudinal cracking before failure, whereas multidirectional lay-ups fail transversely with little longitudinal cracking. A simple qualitative analysis suggested that the higher matrix shear stresses in unidirectional materials cause the longitudinal cracking, and that this cracking was responsible for the high toughness of unidirectional composites. In a series of comparative tests, the interlaminar strength of multi-directional composites was reduced by placing perforated Mylar films between laminae; tests on notched and slotted specimens showed that the interlaminar films promoted delamination and longitudinal cracking near the notches and that, as a result, toughness, notch strength, and impact strength were substantially increased.

Elber, W.↗

Residual-strength tests of L-1011 vertical fin components after 10 and 20 years of simulated flight service

Part of the NASA/ACEE Program was to determine the effect of long-term durability testing on the residual strength of graphite-epoxy cover panel and spar components of the Lockheed L-1011 aircraft vertical stabilizer. The results of these residual strength tests are presented herein. The structural behavior and failure mode of both cover panel and spar components were addressed, and the test results obtained were compared with the static test results generated by Lockheed. The effect of damage on one of the spar specimens was described.

Lopez, O. F.↗

Statistical Models of Fracture Relevant to Nuclear-Grade Graphite: Review and Recommendations

The nuclear-grade (low-impurity) graphite needed for the fuel element and moderator material for next-generation (Gen IV) reactors displays large scatter in strength and a nonlinear stress-strain response from damage accumulation. This response can be characterized as quasi-brittle. In this expanded review, relevant statistical failure models for various brittle and quasi-brittle material systems are discussed with regard to strength distribution, size effect, multiaxial strength, and damage accumulation. This includes descriptions of the Weibull, Batdorf, and Burchell models as well as models that describe the strength response of composite materials, which involves distributed damage. Results from lattice simulations are included for a physics-based description of material breakdown. Consideration is given to the predicted transition between brittle and quasi-brittle damage behavior versus the density of damage (level of disorder) within the material system. The literature indicates that weakest-link-based failure modeling approaches appear to be reasonably robust in that they can be applied to materials that display distributed damage, provided that the level of disorder in the material is not too large. The Weibull distribution is argued to be the most appropriate statistical distribution to model the stochastic-strength response of graphite.

Nemeth, Noel N.↗

Effect of impact damage and open holes on the compression strength of tough resin/high strain fiber laminates

Structural damage and design-based inclusions such as cutouts can reduce significantly the strength of graphite-epoxy laminates. One composite mechanics research activity at the Langley Research Center is to assess and improve the performance of composite structures in strength are common to both tension and compression loaded laminates; however, the problem associated with compression performance is the most illusive to solve. Compression failure involves both shear crippling and delamination modes. Several graphite-epoxy material systems proposed for improved damage-tolerance were studied. Material parameters included both tough resin formulations and high strain fibers.

Williams, J. G.↗

New bismaleimide matrix resins for graphite fiber composites

Two new bismaleimide resins based on the N,N'-m-phenylene-bis(m-amino-benzamide) structure have been synthesized and characterized. The mixtures of the two resins gave better handling, processing, mechanical, and thermal properties in graphite composites than did the individual resins. The mechanical strength of the cured graphite composites prepared from the 1:1 copolymer of the two bismaleimide resins was excellent at both ambient and elevated temperatures. The physical and mechanical properties of the composites from the new bismaleimide matrix resin systems are compared with conventional composites based on epoxy and other bismaleimide systems. The copolymer system provides another method for improving bismaleimide resins.

Hsu, M.-T. S.↗

New bismaleimide matrix resins for graphite fiber composites

Two new bismaleimide resins based on the N, N'-m-phenylene-bis(m-amino-benzamide) structure have been synthesized and characterized. The mixtures of the two resins gave better handling, processing, mechanical, and thermal properties in graphite composites than did the individual resins. The mechanical strength of the cured graphite composites prepared from the 1:1 copolymer of the two bismaleimide resins was excellent at both ambient and elevated temperatures. The physical and mechanical properties of the composites from the new bismaleimide matrix resin systems are compared with conventional composites based on epoxy and other bismaleimide systems. The copolymer system provides another method for improving bismaleimide resins.

Hsu, M.-T. S.↗

Residual strength of composite laminates subjected to tensile-compressive fatigue loading

Results are presented on the measurements of the residual strengths of T300/934 graphite epoxy laminates, in tension and in compression, after the samples were exposed to tension-compression fatigue loading (R = -1). Four laminate ocnfigurations were tested: unidirectional, cross-ply, angle-ply, and quasi-isotropic. It was found that the fatigue behavior of laminates was dependent on the quasi-static strengths and the specific structure of the laminate. No direct correlation was found between remaining residual strengths and the percentage of average fatigue life. However, a correlation scheme was developed for the individual specimen under test, based on a cumulative damage model and a stiffness change of the material.

Rotem, Assa↗

Effects of moisture on apparent flexure strength and on torsion and flexure fatigue properties of graphite-epoxy composites

The effects of moisture and temperature on unidirectional and multi-ply laminates of T300/934 and AS/3501 graphite-epoxy systems were investigated. Properties studied were static flexure strength and flexure and torsion fatigue strengths at room temperature and at 74 C. Specimens with increased moisture content showed a reduced static flexure strength; water as the test environment had only a negligible influence. In flexure fatigue and torsion fatigue, the water environment caused somewhat reduced fatigue strengths at room temperature and significantly greater degradation in 74 C water. The failure mode in all cases was interlaminar delamination.

Sumsion, H. T.↗

Improved oxidation-resistant carbon and graphite materials

A variety of silicon-carbide treated carbon and graphite products were prepared, and oxidation and strength properties determined. Carbon and graphite materials used in the preliminary study include fiber, tape, felt, foam, bulk, and laminar configurations. The silicon-carbide treatment used in preparing the oxidation resistant specimens employs either vacuum or ultrasonic impregnation of various silicone-silicon mixtures into the matrix material. The impregnation phase is followed by controlled thermal reaction at which time the silicon carbide is synthesized and takes the form of an integral protective boundary layer. Thickness of the layer ranges from a fraction of a mil to 10 mils, depending on the matrix material and processing parameters. Oxidation resistance of all the silicon-carbide-treated specimens investigated was found to be significantly improved. Mechanical strengths of the laminar composites were also found to be somewhat improved. At room temperature the specific strength of the silicon-carbide treated fibers and tapes was degraded to some extent; however, their relative strengths were significantly increased at elevated temperatures in oxidizing atmosphere.

Muir, H. M.↗

Computational modeling of graphite degradation in molten salt reactors: Role of infiltration

Molten salt reactors (MSRs) often employ graphite as a moderator and reflector. An important challenge for deploying graphite in these reactors is that, due to limited experimental data, our understanding of graphite’s structural integrity in molten salt environments remains incomplete. Here, this study addresses heat generation from fuel-bearing salt that has infiltrated open pores in the graphite, driven primarily by pressure differentials. This is one of multiple identified physical and chemical mechanisms through which molten salt could potentially degrade graphite. Thermally driven stresses are quantified using the Molten-Salt Reactor Experiment (MSRE) graphite moderator elements as a case study. Finite element simulations predict stress distributions at varying infiltration levels, indicating that thermal stresses increase with higher infiltration. Rare-event simulations using the parallel subset simulation framework identify the combinations and corresponding ranges of input parameters that lead to stresses above a specified threshold. In particular, combinations involving high infiltration amounts, high power density, and low thermal conductivity tend to induce the highest stresses. Under the inputs and assumptions considered in this work, the magnitudes of the thermally driven stresses are quite low, with a very low likelihood of causing failure due to exceeding the graphite’s tensile strength. Additionally, rare-event simulations were performed for two more scenarios: a scaled-up moderator geometry and a localized hotspot in the original geometry. Both cases resulted in increased susceptibility to failure, though not to a detrimental extent. Furthermore, the combined effects of irradiation and infiltration-induced thermal stresses were evaluated. The results showed that thermal stresses from infiltration were negligible compared to those caused by irradiation. The findings of such a study are inherently component-specific, but the methodology presented here could be used for similar assessments of salt-infiltration effects in other graphite components.

36 - MATERIALS SCIENCE↗

ASME Design Code Rule Changes for Nuclear Graphite

The American Society of Mechanical Engineers Boiler Pressure and Vessel Code (ASME BPVC) Section III, Division 5, Article HHA-3000 outlines graphite core component and graphite core assembly design guidelines. Graphite core components are defined as ?components manufactured from graphite that are installed to form a graphite core assembly within the reactor pressure vessel of a high temperature, graphite moderated fission reactor.? (p. 413) Graphites? inherent defect distributions do not allow for deterministic material reliability. Rather, graphite has variable strength distributions which change by grade. Article HHA-3000 outlines two semi-probabilistic methods, the full and simplified assessments, which set design load limit targets for each of three component structural reliability classes. The Design Task Group was officially recognized as a specialized task group within ASME November of 2023, though we?ve been collaborating since 2022. The purpose of the Design Task Group is to correct, clarify, and make HHA-3000 function as intended. The Design Task Group will sunset once we?ve achieved our objectives. The Design Task Group was specifically told to not write new Code. While there may be more precise and more accurate methods to determine reliability targets, the current methods are conservative, relatively simple to implement, and have thus far been considered satisfactory for setting design reliability targets. Much of the ground-work to write proposal files and background documents for records to make the changes needed to achieve our objective have been completed. The Design Task Group has documented much of their work through papers, presentations, and memorandums. Three memorandums in which INL team members had substantial contributions are found in the Appendices: FEA Modeling for the Baseline Program, Evaluating the Effects on Margin of Updating the Threshold and Shape Parameters in the Full Assessment, and Interpretations of the Full and Simplified Assessments in ASME BPVC. Most of the on-going work to achieve the Design Task Group?s objective will be addressing comments on existing records and moving records through the balloting process. The Design Task Group met bi-weekly mostly through the end of FY2023. Since February 2024, the Design Task Group has mostly been completed with solving and documenting the technical issues associated with the assessments. Unless new tasks are identified, the remaining work of the Design Task Group will be political and editorial.

97 MATHEMATICS AND COMPUTING↗

Design of a pressurized lunar rover

A pressurized lunar rover is necessary for future long-term habitation of the moon. The rover must be able to safely perform many tasks, ranging from transportation and reconnaissance to exploration and rescue missions. Numerous designs were considered in an effort to maintain a low overall mass and good mobility characteristics. The configuration adopted consists of two cylindrical pressure hulls passively connected by a pressurized flexible passageway. The vehicle has an overall length of 11 meters and a total mass of seven metric tons. The rover is driven by eight independently powered two meter diameter wheels. The dual-cylinder concept allows a combination of articulated frame and double Ackermann steering for executing turns. In an emergency, the individual drive motors allow the option of skid steering as well. Two wheels are connected to either side of each cylinder through a pinned bar which allows constant ground contact. Together, these systems allow the rover to easily meet its mobility requirements. A dynamic isotope power system (DIPS), in conjunction with a closed Brayton cycle, supplied the rover with a continuous supply of 8.5 kW. The occupants are all protected from the DIPS system's radiation by a shield of tantalum. The large amount of heat produced by the DIPS and other rover systems is rejected by thermal radiators. The thermal radiators and solar collectors are located on the top of the rear cylinder. The solar collectors are used to recharge batteries for peak power periods. The rover's shell is made of graphite-epoxy coated with multi-layer insulation (MLI). The graphite-epoxy provides strength while the thermally resistant MLI gives protection from the lunar environment. An elastomer separates the two materials to compensate for the thermal mismatch. The communications system allows for communication with the lunar base with an option for direct communication with earth via a lunar satellite link. The various links are combined into one signal broadcast in the S-band at 2.3 GHz. The rover is fitted with a parabolic reflector disk for S-band transmission, and an omnidirectional antenna for local extravehicular activity (EVA) communication. The rover's guidance, navigation, and control subsystem consists of an inertial guidance system, an orbiting lunar satellite, and an obstacle avoidance system. In addition, the rover is equipped with a number of external fixtures including two telerobotic arms, lights, cameras, EVA storage, manlocks, a docking fixture, solar panels, thermal radiators, and a scientific airlock. In conclusion, this rover meets all of the design requirements and clearly surpasses them in the areas of mobility and maneuverability.

Bhardwaj, Manoj↗