Search NASA⌕ Search

SEARCH · Search NASA

Results for “helium irradiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Micromechanical properties of spherical and facetted He bubble loaded copper

Exploring new irradiation resistant materials requires understanding their mechanical responses to irradiation. Resistance to helium bubble formation and understanding bubble effects on the mechanical response of candidate materials are crucial factors to qualify materials as irradiation resistant. Here, in this paper, we explore the effect of spherical and facetted helium bubbles on the mechanical response of copper via in-situ micromechanical tensile testing at room temperature. Bubble formation and shape effects on strength and ductility, and their behavior on grain boundaries are discussed and compared to literature. Loading Cu with helium bubbles is shown here to increase strength but decrease ductility.

42 ENGINEERING↗

Additively manufactured refractory high-entropy alloys with superior radiation resistance

Refractory high-entropy alloys (RHEAs) are promising candidates for next-generation nuclear and high-temperature applications. Among many approaches to manufacture RHEAs, additive manufacturing (AM) represents the most recent and advanced metal manufacturing method which allows near-net-shape manufacturing to reduce material waste and post-processing time. However, performance of AM RHEAs under complex irradiation conditions remains largely unexplored. Here, in this study, we demonstrate for the first time the response of directed energy deposition (DED) AM quaternary RHEAs (HfTaVW, CrTaVW) subjected to sequential dual-beam ion irradiation, consisting of helium pre-implantation followed by high-dose heavy ion bombardment. Compositions of DED AM RHEAs were selected using Monte Carlo (MC) simulations based on a cluster expansion (CE) Hamiltonian parameterized by density functional theory (DFT). Post-irradiation microstructural characterization revealed that the AM RHEA maintained remarkable stability, with suppressed helium bubble growth and reduced defect accumulation compared to conventional alloys. Even at high doses (∼100 dpa), the alloy exhibited no void swelling, a low density of dislocation loops, and no evidence of severe degradation. These results highlight the intrinsic ability of AM-derived microstructures and multicomponent chemistry to synergistically mitigate irradiation effects. Our findings establish AM RHEAs as a class of materials with superior resistance to radiation damage under conditions relevant to advanced fusion and fission environments and demonstrate the importance of sequential ion beam studies in evaluating their long-term performance.

36 MATERIALS SCIENCE↗

Effects of transition metal carbide dispersoids on helium bubble formation in dispersion-strengthened tungsten

Abstract The formation of helium bubbles and subsequent property degradation poses a significant challenge to tungsten as a plasma-facing material in future long-pulse plasma-burning fusion reactors. In this study, we investigated helium bubble formation in dispersion-strengthened tungsten doped with transition metal carbides, including TaC, ZrC, and TiC. Of the three dispersoids, TaC exhibited the highest resistance to helium bubble formation, possibly due to the low vacancy mobility in the Group VB metal carbide and oxide phases. Under identical irradiation conditions, large helium bubbles formed at grain boundaries in tungsten, while no bubbles were observed at the interfaces between the carbide dispersoid and tungsten matrix. Moreover, our results showed the interfaces could suppress helium bubble formation in the nearby tungsten matrix, suggesting that the interfaces are more effective in trapping helium as tiny clusters. Our research provided new insights into optimizing the microstructure of dispersion-strengthened tungsten alloys to enhance their performance.

36 MATERIALS SCIENCE↗

Radiation damage in tungsten under high-energy He-ion irradiation

Tungsten (W) is a primary candidate for plasma-facing components (PFCs) in fusion reactors and hybrid fission-fusion reactors. However, W suffers from severe microstructural damage under Helium (He) ion irradiation in operation conditions. Key irradiation parameters, including incident ion energy, fluence, and irradiation temperature, are known to determine the formation of He bubbles and dislocation loops, which ultimately lead to the degradation of mechanical properties, such as radiation hardening and ductile-to-brittle transition temperature (DBTT) shifts. Various strategies, for instance, interface engineering and alloying, have been developed to enhance He irradiation tolerance in W to address these challenges. Studies in the recent two decades have enhanced the understanding of the underlying mechanisms that drive defect evolution and mechanical performance degradation, thereby offering more insights into the design of more resilient W-based materials for extreme environments.

Liu, Yinghang [Purdue University]↗

Comparative study of spermatogonial survival after X-ray exposure, high LET (HZE) irradiation or spaceflight

Spermatogonial cell loss has been observed in rats flown on Space Lab 3, Cosmos 1887, Cosmos 2044 and in mice following irradiation with X-ray or with HZE particle beams. Spermatogonial loss is determined by cell counting in maturation stage-6 seminferous tubules. With the exception of iron, laboratory irradiation experiments (with mice) revealed a similar pattern of spermatogonial loss proportional to the radiation dose at levels less than 0.1 Gy. Helium and argon irradiation resulted in a 5-percent loss of spermatogonia after only 0.01 Gy exposure. Significant spermatogonial loss (45 percent) occurred at this radiation level with iron particle beams. The loss of spermatogonia during each spaceflight was less than 10 percent when compared to control (nonflight) animals.

Sapp, W. J.↗

Investigation of the Anisotropy of Y-Ba-Cu-O Thin Films With Photoemission Electron Microscopy

Understanding the anisotropy in the electrical properties of YBa2Cu3O7-δ (YBCO) is important for understanding the fundamental mechanism of superconductivity in unconventional superconductors. Additionally it is also essential for achieving uniform and controllable critical currents and resistances in YBCO Josephson junctions. Here, this study correlates work function measurements of different intrinsic regions on YBCO thin films, obtained through PhotoEmission Electron Microscopy (PEEM), with in plane tunneling data and helium ion imaging. YBCO thin films, 40 nm in thickness, were selectively irradiated with 300 keV helium using a Pelletron to investigate the effects of irradiation compared to unirradiated regions. Post-irradiation PEEM images revealed distinct contrasts between irradiated and non-irradiated regions, suggesting a metal-to-insulator transition. In non-irradiated areas, a domain pattern was detected, showing a 25 meV difference in work function, attributed to CuO and BaO rich surface regions. A similar domain structure was observed using high-resolution helium ion imaging; however, the helium ion beam can damage the YBCO, making PEEM a valuable non-destructive alternative. This work highlights the correlation between PEEM measurements and in-plane tunneling properties of YBCO, providing insights into material orientation and its impact on Josephson junction performance. Furthermore, it offers a non-destructive approach to understanding the anisotropy of cuprate materials, its superconducting properties, and the factors affecting Josephson junction performance.

Qu, Rochelle Y. [Univ. of California, Riverside, C↗

The effect of helium on cavity swelling in dual-ion irradiated Fe and Fe-10Cr ferritic alloys

We report Ferritic-martensitic (FM) steels for in-vessel components in proposed fusion reactors are expected to suffer from high levels of displacement damage and helium (He) generation by neutron transmutation. However, a thorough understanding of the He synergistic effects on the cavity swelling in FM steels is still not well established. To gain fundamental insights into the He effect on cavity swelling, high purity Fe and Fe-10 wt.% Cr ferritic model alloys were irradiated with 8 MeV Ni ions and co-implanted He ions at 400 to 550 °C up to 30 displacements per atom (dpa) with He implantation rates of 0.1, 10 and 50 appm He/dpa. The current study focuses on the 50 appm He/dpa, 500 °C behavior vs. 0.1 and 10 appm He/dpa. Irradiation-induced defects, including cavities, dislocation loops, and dislocation networks were characterized using transmission electron microscopy (TEM). In the grain interior, a bimodal cavity size distribution was observed in the 10 and 50 appm He/dpa samples, but not for 0.1 appm He/dpa. Cavity swelling was maximized at intermediate He implantation rates of ~10 appm He/dpa for both ion-irradiated Fe and Fe-10Cr alloys. The cavity swelling behavior as a function of He implantation rate appears to be controlled by the He/dpa-dependent variation of cavity sink strengths. Treating small bubbles as biased sinks for interstitial absorption can significantly increase the ratio of biased to unbiased sink strengths (Q) and results in maximized cavity swelling for a Q ratio close to one.

36 MATERIALS SCIENCE↗

Helium co-implantation effects on dislocation loop evolution during in situ ion irradiations of a novel additive-manufactured Fe-9Cr steel alloy

This study examines the impact of helium injection rate on dislocation loop evolution during ion irradiation of a novel, additively manufactured (AM) 9Cr reduced-activation ferritic/martensitic (RAFM) steel. Through in situ transmission electron microscopy ion irradiations and post-irradiation characterization, the effects of simultaneous 1 MeV Kr²⁺ and 12 keV He⁺ ion irradiation at 400°C to 5 dpa with varying helium levels were examined. The findings reveal that helium co-injection significantly increases dislocation loop density, primarily through the formation of small defect features exhibiting contrast and projected morphologies consistent with a⟨100⟩ loops (∼1 nm), while suppressing larger a/2⟨111⟩ loops. The findings underscore the complex interplay among continuously increasing helium content, temperature, and alloy composition in the evolution of dislocation loops under irradiation in RAFM steels. The study highlights the need for further investigation into helium-mediated mechanisms, such as proposed interactions between self-interstitial atoms and helium atoms, to enhance the performance of RAFM steels in advanced nuclear reactors.

ANA2↗

2024 Second Half Semi Annual Report: Modeling plasticity-mediated flow in metals with pressurized cavities

The objective is to better predict the bulk-scale mechanical behavior of porous metals that have over pressurized cavities (e.g., irradiated metals with helium bubbles) by quantifying the complex coupling among cavity aspects (e.g., size distribution, inhomogeneous overpressure values, spatial arrangement) and metal properties (e.g., rate-dependency, crystallographic lattice). This requires up-scaling local mechanical fields from the single crystal scale and will be accomplished using a homogenization approach that combines full-field numerical simulations, analytical formalisms, and physics-informed machine learning to produce symbolically-defined constitutive equations (e.g., gauge functions). These equations will satisfy the objective because they enable computationally efficient predictions that approach the accuracy of computationally expensive full-field numerical simulations, abide by theoretical requirements (e.g., conservation of energy, work conjugacy), and retain the transparency of analytical models.

36 MATERIALS SCIENCE↗

Behavior and properties of helium cavities in ductile-phase-toughened tungsten irradiated with He + ions at an elevated temperature

Ductile-phase toughened tungsten (DPT W) composites have demonstrated a great potential for plasma-facing components in fusion power systems. These materials can retain the outstanding thermomechanical properties of W while significantly enhancing the fracture toughness. The DPT W composite in this study consists of W particles (88 wt.%) embedded in a ductile NiFeW (12 wt.%) solution matrix. Irradiation of the composite was performed with 90 keV He + ions to 1.0 × 10 17 He + /cm 2 at 973 K. The He cavities formed in both W and NiFeW phases are examined using convergent-beam scanning transmission electron microscopy (CB-STEM) at an atomic-level resolution. Full-range depth profiles of the He cavity diameters and number densities are analyzed. The results show that the average cavity diameter in NiFeW is ~2.7 times that in W, while the number density is an order of magnitude lower. A quantitative analysis of the He density and pressure in the cavities is also achieved using STEM electron energy loss spectroscopy (STEM-EELS) mapping. The He atoms in the cavities in NiFeW are found to be under-pressurized, while those in similar-sized cavities in W are not detectable. Further, the He energy-loss shift exhibits a linear relationship with the He density in cavities in NiFeW, with the slope comparable to that for martensitic steel.

36 MATERIALS SCIENCE↗

A fusion relevant data-driven engineering void swelling model for 9Cr tempered martensitic steels

The UCSB database on cavity evolution in 9-12Cr tempered martensitic steels (TMS), includes the results for both dual heavy and helium ion (DII), and High Flux Isotope Reactor (HFIR) in situ helium injection (ISHI) neutron irradiations at 500°C. These results were combined with literature single ion and fission neutron irradiation data to derive a model for the void volume fraction, f v , as a function of displacements per atom (dpa) and transmutant helium concentrations in atomic parts per million (appm). The scientific foundation for the paper is described in a companion paper entitled “Cavity Evolution and Void Swelling in Dual Ion Irradiated Tempered Martensitic Steels”. Here, in this study, we show that f v (dpa, He/dpa) is described by the incubation dose, dpa i , for the onset of void growth, and the post-incubation growth rate, f v ’(%/dpa). Both dpa i and f v ’ decrease with increasing He/dpa at > ~ 5. The dpa i is also lower for the ISHI neutron irradiations at the same He/dpa. Single heavy ion and fission reactor neutron irradiations, with low He/dpa ratios, have a much larger dpa i . Based on a combined analysis of DII, single ion, ISHI and fission neutron data, we further show that the post-incubation f v data analyzed here have a common empirical curve shape, with f v ’ reaching up to ~ 0.2%/dpa at very high dpa. We also show that f v ’ can be predicted based on a physical model of defect partitioning between evolving sinks. At 500°C and fusion relevant He/dpa ≈ 10, the best-fit model predicts nominal swelling, S = f v /(1-f v ), of ~ 1.1, 4.9 and 16% at 50, 100 and 200 dpa, respectively. The physically motivated, data-driven model includes estimated uncertainties for both dpa i and f v ’.

36 MATERIALS SCIENCE↗

Weldability of irradiated Stainless Steel 304 materials harvested from the National Research Universal (NRU) reactor

In this work, the weldability of the neutron-irradiated Stainless Steel 304 (SS 304) materials containing estimated helium levels of 12 to 44 appm has been studied through a Collaborative Research and Development Agreement between the Canadian Nuclear Laboratories and Oak Ridge National Laboratory. The work utilizes a SS 304 component harvested from the National Research Universal reactor. Laser beam welding was used to explore suitable welding conditions and associated parameters, to determine helium concentration limits for successful welding of irradiated stainless-steels. The experimental results show that maximum fusion zone void sizes, fusion zone void quantity and total heat affected zone helium-induced crack length generally increased with increasing He levels and effective weld heat input. A proper combination of welding parameters with low effective heat input, such as, laser power, weld travel speed and wire feed speed, were shown to improve the welding quality, and potentially reduce the length and probability of the formation of grain boundary helium-induced cracking and voids of irradiated SS 304 even with He concentrations as high as about 44 appm.

36 MATERIALS SCIENCE↗

Probing the Damage Recovery Mechanism in Irradiated Stainless Steels Using In-Situ Microcantilever Bending Test

Single crystalline microcantilevers are fabricated from the base metal and heat-affected zone (HAZ) of a laser welded, neutron irradiated austenitic stainless steel, for scanning electron microscope (SEM) in-situ bending. In the HAZ, cantilevers exhibit higher yield point and lower crack tip blunting displacement than in the base metal and unirradiated archive specimen. These results suggest that radiation-induced defects harden the base metal, whereas the HAZ exhibits annealing of defects leading to mechanical softening. Dislocation nucleation ahead of the crack tip is responsible for ductile blunting behavior and provides a pathway to mitigating helium-induced cracking during weld repairs of irradiated materials.

36 MATERIALS SCIENCE↗

Estimating the Contribution of the Nickel to Protium Loading of Full-Length Getters

The full-length getter (FLG) is a critical component of the tritium producing burnable absorber rod (TPBAR), designed to capture tritium produced within the lithium aluminate pellets. However, due to the chemical similarity between protium (¹H) and tritium (³H), the FLG readily absorbs protium, reducing its capacity to absorb tritium and increasing the risk of tritium permeation into the reactor coolant. This study evaluates protium produced from neutron irradiation of nickel plating on the FLG through 5?Ni(n,p) reactions, quantifies its contribution to the total protium observed, and informs models of tritium and hydrogen transport within TPBARs. During irradiation, neutron capture by 58Ni results in the formation of 5?Ni, which undergoes neutron bombardment to produce 4He via 5?Ni(n,a) reactions and protium via 5?Ni(n,p) reactions. The measured helium content post-irradiation provides insight into the neutron capture processes within the getter. The 4He measured within the getter may be useful in determining hydrogen produced by the nickel plating on FLG because 59Ni also produces protium in a 59Ni(n, p) reaction. The contribution of 1H from the nickel in FLG contributed less than 1% of the measured H2 gas in PIE, ranging from 0.005% to 0.614%. These findings refine current knowledge of the protium-tritium interplay in TPBARs and support the development of improved transport models for tritium and hydrogen, ultimately aiding in the optimization of TPBAR design and reactor operations.

Arbova, Dana L.↗

In-situ re-crystallization of heavily-irradiated Gd 2 Ti 2 O 7

Gadolinium titanate (Gd 2 Ti 2 O 7 , or GTO) and other lanthanide pyrochlores are interesting candidates for actinide waste disposal and fast ion conduction because the relevant material properties are intimately dependent on local cation structure. Therefore, a deep understanding of the kinetics associated with cation ordering and disordering is required if such material properties are to be tuned for specific device designs. To this end, single crystals of GTO were irradiated with 190 keV helium ions to a total fluence of 1 × 10 17 ions/cm 2 , amorphizing the sample surface to a depth of ~1 μm and resulting in significant He bubble accumulation. FIB lamellae lifted out from the irradiated sections were examined during heat treatment in the (scanning) transmission electron microscope. Two distinct stages of the re-crystallization of the amorphized material were observed. The material near the end of the ions’ range transformed first and with the same orientation as the pristine material. This was due to the close proximity of the pristine material and the presence of small defect fluorite seeds, but the propagation of this growth front was frustrated by the large pores (formerly bubbles) in the He accumulation layer. This was followed by heterogeneous nucleation of new crystallites at random orientations at the top of the He accumulation layer, which is attributed to the high surface area associated with the many small He bubbles in that region. Finally, it is inferred that the kinetics of grain growth in this material are significantly faster than the kinetics of grain nucleation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Helium interaction with solutes and impurities in neutron-irradiated nanostructured ferritic alloys: A first principles study

Density functional theory calculations are performed to explore the binding between He and alloying solutes, impurities, and transmutation products expected in neutron irradiated nanostructured ferritic alloys (NFAs), here 14YWT is taken as an example. Elements that exhibit significant binding (attraction) with an interstitial He are Y (binding energy = 0.46 eV), Mg (0.32), O (0.33), Ti (0.16), and C (0.15). Those that provide significant binding to a substitutional He are O (1.44), Y (1.24), N (0.73), H (0.56), Mg (0.52), Ti (0.34), Si (0.34), C (0.33), Al (0.32), Ni (0.26), Ta (0.23), and Mn (0.16). The presence of these elements in Fe matrix could reduce the transport of He towards oxide particles, dislocations, and internal boundaries, and could promote He bubble nucleation in the matrix. For convenience, we compile existing binding energy data of He with He n and He n V (He-vacancy) clusters. Dissociation pathway analysis reveals that, in general, the most likely dissociation of a He n V cluster is by a sequential emission of individual He atoms. Furthermore, larger bubbles are more prone to dissociation than smaller ones. In addition, we estimate the binding energy (segregation energy) of He in bulk Y 2 Ti 2 O 7 (YTO) single crystal, YTO/Fe interface, and YTO particle embedded in Fe, with respect to interstitial He in Fe, from existing formation energies of He in these structures. We also compile available data of He binding with Fe self-interstitial atom (SIA), SIA clusters, and edge and screw dislocations. Note that given the absence of DFT data, the binding with SIA clusters and dislocations are gathered from simulations with empirical potentials. Finally, the data presented in this paper is important to inform multiscale simulations of He bubble accumulation.

36 MATERIALS SCIENCE↗