Search NASA⌕ Search

SEARCH · Search NASA

Results for “intermetallic alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

The cyclic oxidation resistance at 1200 C of beta-NiAl, FeAl, and CoAl alloys with selected third element additions

The intermetallic compounds Beta-NiAl, FeAl, and CoAl were tested in cyclic oxidation with selected third element alloy additions. Tests in static air for 200 1-hr cycles at 1200 C indicated by specific weight change/time data and x-ray diffraction analysis that the 5 at percent alloy additions did not significantly improve the oxidation resistance over the alumina forming baseline alloys without the additions. Many of the alloy additions were actually deleterious. Ta and Nb were the only alloy additions that actually altered the nature of the oxide(s) formed and still maintained the oxidation resistance of the protective alumina scale.

Barrett, C. A.↗

The Influence of C and Si on the Flow Behavior of NiAl Single Crystals

Alloys based on the intermetallic compound NiAl are considered potential replacements for Ni and Co-based superalloys in high temperature structural applications due to their excellent oxidation resistance, low densities, high thermal conductivities, and increased melting points. Unfortunately, NiAl exhibits low tensile ductility at room temperature and low strengths at elevated temperatures which have combined to hinder its development. Recent efforts, have revealed that NiAl in the presence of sufficient solute levels, is subject to the phenomenon of strain aging which manifests itself as: sharp yield points, abnormally low strain rate sensitivities (SRS), plateaus or peaks in yield stress and work hardening rate as a function of temperature, flow stress transients upon an upward change in strain rate, reduced tensile elongations at elevated temperatures, and serrated stress-strain curves. Though recent efforts via either alloying or the removal of interstitial impurities, have resulted in consistent room-temperature tensile elongations exceeding 5% and the elimination of serrated flow, the effects of particular substitutional and interstitial elements and the mechanisms by which they might enhance or hinder the mechanical properties remain unknown. Consequently, the purpose of the present paper is to provide a preliminary assessment of the influence of common substitutional and interstitial impurities on the deformation behavior of NiAl. To accomplish this goal a series of NiAl single crystal alloys containing various interstitial solutes were prepared and their mechanical properties were evaluated between 77 and 1100 K. Because Si is a common impurity in conventional purity single crystals grown by the Bridgman method, Si concentrations were also varied in order to determine the influence of this element.

Weaver, M. L.↗

Thermophysical Properties of 60-NITINOL for Mechanical Component Applications

The linear thermal expansion coefficient, specific heat capacity, electrical resistivity and thermal conductivity of 60- NITINOL were studied over a range of temperatures representing the operating environment of an oil-lubricated bearing. The behavior of this material appears to follow wellestablished theories applicable to either metal alloys, in general, or to intermetallic compounds, more specifically and the measured data were found to be comparable to those for conventional bearing alloys.

Stanford, Malcolm K.↗

Design and Manufacturing Considerations for Shockproof and Corrosion-Immune Superelastic Nickel-Titanium Bearings for a Space Station Application

An intermetallic nickel-titanium alloy, 60NiTi (60wt%Ni, 40wt%Ti), is a promising tribological material for space mechanisms. 60NiTi offers a broad combination of physical properties that make it unique among bearing materials. 60NiTi is hard, electrically conductive, highly corrosion resistant, readily machined prior to final heat treatment, easily lubricated and is non-magnetic. It also falls within the class of superelastic alloys and can elastically endure large strains (beyond 5 percent) making it highly resistant to excessive and unexpected (shock) loads. Key material properties and characteristics such as elastic modulus, tensile fracture sensitivity and residual stress behavior, however, differ from conventional alloys such as steel and this significantly affects bearing design and manufacturing. In this paper, the preliminary design and manufacture of ball bearings made from 60NiTi are considered for a highly corrosive, lightly loaded, low speed bearing application found inside the International Space Station s water recycling system. The information presented is expected to help guide more widespread commercialization of this new technology into space mechanism and other applications.

DellaCorte, Christopher↗

Metal- and intermetallic-matrix composites for aerospace propulsion and power systems

The requirements for high specific strength refractory materials of prospective military, civil, and space propulsion systems are presently addressed in the context of emerging capabilities in metal- and intermetallic-matrix composites. The candidate systems encompass composite matrix compositions of superalloy, Nb-Zr refractory alloy, Cu-base, and Ti-base alloy types, as well as such intermetallics as TiAl, Ti3Al, NiAl, and MoSi2. The brittleness of intermetallic matrices remains a major consideration, as does their general difficulty of fabrication.

Doychak, J.↗

COSAM program overview

The COSAM program for reduction of the use of strategic alloying elements in nickel-based superalloys for gas turbine engines was reviewed. Sources, consumption, and pricing of cobalt, tantalum, columbium, and chromium are surveyed. Research projects in strategic element substitution, advanced processing concepts, and the development of alternate materials (intermetallics and iron-base alloys) are listed and research plans for FY 1983 and FY 1984 summarized.

Stephens, J. R.↗

Improving the low temperature ductility of NiAl

The intermetallic NiAl exhibits excellent potential as a structural material for application in air-breathing and single-stage-to-orbit engines. Unfortunately NiAl is brittle at ambient temperature, which is partly attributed to the lack of five independent slip systems as required by von Mises criterion for uniform, volume conserving deformation since the operative group of zone axes (100) slip offers only three independent slip systems. Isostructural FeAl, however, deforms by group of zone axes (111) slip at room temperature which provides five independent slip systems. Thus, it was decided to macroalloy NiAl with Fe to promote group of zone axes (111) slip thereby possibly improving the ductility. For Ni - 30 at. (percent) Al - 20 at. (percent) Fe having essentially bcc microstructure indicated up to 6 percent tensile elongation combined with high yield strength (about 800 MPa). The results compare favorably with those of stoichiometric Ni - 50 at. (percent) Al which, however, deforms by group of zone axes (100) slip at room temperature. The multi-phase alloy approach has proven even more successful for Ni - 20 at. (percent) Al - 30 at. (percent) Fe. The high temperature ductility of the multi-phase alloy was attributed to deformation transfer across interphase boundaries and the crack stopping action of the constituent gamma/gamma' phase. While the constituent phase became increasingly brittle, the beta' phase became more ductile at elevated temperatures. Thus the multi-phase alloy did not exhibit any elevated temperature embrittlement. Similarly, while the beta' phase became weak at high temperatures, the gamma/gamma' phase exhibited better strength retention leading to the improved elevated temperature strength of the multi-phase alloy. Thus, the multi-phase alloy benefits from both its constituent phases, with each phase alleviating the disadvantages associated with the other phase over any temperature range. The multi-phase alloy approach is suggested as a possible approach to designing intermetallic-based alloys.

Guha, Sumit↗

Microstructural development during directional solidification of peritectic alloys

Despite the widespread commercial use of peritectic alloys (e.g., steels, brass, bronze, intermetallic compounds, Co based superalloys and A3B type superconductors), the characterization of the microstructural development during directional solidification of peritectics has historically lagged behind similar efforts directed towards other types of binary invariant reactions such as eutectic or monotectic. A wide variety of possible microstructures has been shown to form in peritectics depending upon the imposed temperature gradient, G, the solidification velocity, V, as well as the presence or absence of convection in the melt. This has important technological implications since many commercially important alloys exhibit peritectics and processing methods such as casting and welding often involve widely changing conditions. It has been the aim of this project to examine, in a systematic fashion, both experimentally and theoretically, the influence of gravitationally driven convection on segregation and microstructural development during solidification in peritectic systems under terrestrial conditions. The scientific results of the project will be used to establish ground based data in support of a meaningful microgravity flight experiment.

Lograsso, Thomas A.↗

Directional Solidification and Mechanical Properties of NiAl-NiAlTa Alloys

Directional solidification of eutectic alloys is a promising technique for producing in-situ composite materials exhibiting a balance of properties. Consequently, the microstructure, creep strength and fracture toughness of directionally solidified NiAl-NiAlTa alloys were investigated. Directional solidification was performed by containerless processing techniques to minimize alloy contamination. The eutectic composition was found to be NiAl-15.5 at% Ta and well-aligned microstructures were produced at this composition. A near-eutectic alloy of NiAl-14.5Ta was also investigated. Directional solidification of the near-eutectic composition resulted in microstructures consisting of NiAl dendrites surrounded by aligned eutectic regions. The off-eutectic alloy exhibited promising compressive creep strengths compared to other NiAl-based intermetallics, while preliminary testing indicated that the eutectic alloy was competitive with Ni-base single crystal superalloys. The room temperature toughness of these two-phase alloys was similar to that of polycrystalline NiAl even with the presence of the brittle Laves phase NiAlTa.

Johnson, D. R.↗

Effect of boron on tensile properties of B2 BeAl

Small additions of boron were shown to improve the room temperature ductility of the intermetallic compound Ni3Al. Boron is believed to segregate to the gain boundaries and strengthen them, allowing the inheret ductility of the grains to be achieved. The present study was undertaken to see if boron has a similar effect on the low temperature tensile properties of the equiatomic intermetallic compound FeAl. A binary alloy without boron is compared with an alloy containing 0.78 at % B (0.2 wt %) B, by tensile testing over the temperature range of 300 K to 640 K. Both alloys were processed by powder metallurgy. Results showed that 0.78 at % B addition to FeAl does indeed change the room temperature fracture mode from intergranular to transgranular, suggesting a strengthening of grain boundaries. The alloy containing boron is, however, still brittle at room temperature. A slight decrease in the ductile to brittle transition temperature is, nevertheless, observed. In addition a significant increase in strength of the alloy is observed with boron addition.

Crimp, M.↗

Reliability analysis of single crystal NiAl turbine blades

As part of a co-operative agreement with General Electric Aircraft Engines (GEAE), NASA LeRC is modifying and validating the Ceramic Analysis and Reliability Evaluation of Structures algorithm for use in design of components made of high strength NiAl based intermetallic materials. NiAl single crystal alloys are being actively investigated by GEAE as a replacement for Ni-based single crystal superalloys for use in high pressure turbine blades and vanes. The driving force for this research lies in the numerous property advantages offered by NiAl alloys over their superalloy counterparts. These include a reduction of density by as much as a third without significantly sacrificing strength, higher melting point, greater thermal conductivity, better oxidation resistance, and a better response to thermal barrier coatings. The current drawback to high strength NiAl single crystals is their limited ductility. Consequently, significant efforts including the work agreement with GEAE are underway to develop testing and design methodologies for these materials. The approach to validation and component analysis involves the following steps: determination of the statistical nature and source of fracture in a high strength, NiAl single crystal turbine blade material; measurement of the failure strength envelope of the material; coding of statistically based reliability models; verification of the code and model; and modeling of turbine blades and vanes for rig testing.

Salem, Jonathan↗

Undercooling, Rapid Solidification, and Relations to Processing in Low Earth Orbit (A Review of the Works of Bingbo Wei)

This is a survey of the published works of Prof. Bingbo Wei of the Department of Applied Physics at Northwestern Polytechnical University, Xian P.R. China. Transformations among solid - liquid - and vapor are fundamental to the foundations of life and culture on Earth. The development and understanding of materials has lead the evolution and advancement of the human race since antiquity. Materials and fluids research is continuing today, with us standing on the shoulders of those that have gone before us. Technological and scientific breakthroughs continue due to studies of greater and greater complexity, that include for example, research done at high pressures, in high magnetic fields, at temperatures near absolute zero, and in the low gravity environment of low Earth orbit. Of particular technological importance is the liquid to solid transformation of metals and alloys. Solidification processing is generally the most important factor in the final properties of objects made of metal; and undercooling is the fundamental driving force for all solidification. The interest and resources dedicated to the study of solidification and undercooling are great and World wide. For many years B. Wei and his coworkers have been studying undercooling and rapid solidification and have amassed a significant body of published research in this important field, contributing to the leading edge of the state-of-the-art. It is the goal of this memorandum to provide a review of the research of B. Wei et al.; publications in Chinese are included in the reference list but are not discussed. The bulk of Wei's work has been in the area of undercooling and rapid solidification [1-11, 13-16, 24-36] with papers dating back to 1989, the same year he earned his Ph.D. Below, discussions of Wei's undercooling and rapid solidification research have been grouped together mostly on the basis of alloy type, such as eutectic, intermetallic, or monotectic.

deGroh, Henry C., III↗

Investigation of Three-Dimensional Stress Fields and Slip Systems for FCC Single Crystal Superalloy Notched Specimens

Metals and their alloys, except for a few intermetallics, are inherently ductile, i.e. plastic deformation precedes fracture in these materials. Therefore, resistance to fracture is directly related to the development of the plastic zone at the crack tip. Recent studies indicate that the fracture toughness of single crystals depends on the crystallographic orientation of the notch as well as the loading direction. In general, the dependence of crack propagation resistance on crystallographic orientation arises from the anisotropy of (i) elastic constants, (ii) plastic deformation (or slip), and (iii) the weakest fracture planes (e.g. cleavage planes). Because of the triaxial stress state at the notch tips, many slip systems that otherwise would not be activated during uniaxial testing, become operational. The plastic zone formation in single crystals has been tackled theoretically by Rice and his co-workers and only limited experimental work has been conducted in this area. The study of the stresses and strains in the vicinity of a FCC single crystal notch tip is of relatively recent origin. We present experimental and numerical investigation of 3D stress fields and evolution of slip sector boundaries near notches in FCC single crystal tension test specimens, and demonstrate that a 3D linear elastic finite element model that includes the effect of material anisotropy is shown to predict active slip planes and sectors accurately. The slip sector boundaries are shown to have complex curved shapes with several slip systems active simultaneously near the notch. Results are presented for surface and mid-plane of the specimens. The results demonstrate that accounting for 3D elastic anisotropy is very important for accurate prediction of slip activation near FCC single crystal notches loaded in tension. Results from the study will help establish guidelines for fatigue damage near single crystal notches.

Arakere, Nagaraj K.↗

The effects of grain size on the flow and fracture of long-range ordered alloys

The effects of grain size on the mechanical properties of long-range ordered alloys are examined with reference to the short-term behavior of aluminide intermetallics. It is shown that in those L1(2) alloys which exhibit anomalous thermal strengthening, the grain size affects the magnitude of the strengthening. In some cases it also affects ductility, whereby the tensile elongation and the tensile strength increase as the grain size decreases below a critical point. It is also believed that grain size may affect the partitioning of microalloying elements, such as boron, in Ni3Al.

Schulson, E. M.↗

Non-ideality near the monotectic composition of a miscibility-gap type system - Succinonitrile-water

Differential scanning calorimetry (DSC) of near monotectic succinonitrile-water solutions, fast-quenched in hydrophilic and hydrophobic DSC pans, indicate, by degree of undercooling, thst there may be significant dependence of final ingot microstructure on the pre-quench equilibration temperature. Partial molal-volume determinations from density data, along with DSC data, suggest the nature of temperature dependent component associations from 20 to 55 C in homogeneous solutions. The undercooling profile in a hydrophilic container is explained in terms of solution-composition shifts arising from the Gibbs surface excess. The evidence shows that temperature-dependent preferred component aggregates may modulate surface-composition gradients. Similar effects may be present through intermetallic compound formation in metallic monotectic alloys.

Frazier, D. O.↗