Adversarial Ensemble Modeling of Multi-modal Mechanical Properties for Iron-Based Alloys

Mechanical properties of alloys are controlled by their microstructure; and microstructure evolution is controlled by internal and external stressors. Chemical complexity during the alloy processing may result in heterogeneity and observation of multimodal performance patterns. Thus, to ensure the desired performance of stressed components it is important to understand the origin and mechanisms of such behavior. Adversarial ensemble modeling was introduced here to explain multimodal mechanical properties of the iron-based alloys. The modeling results showed that the areas of a single mechanism predominance were contiguous across the alloy compositions clustered by similarity, with sharp and persistent boundaries separating the single-mechanism domains. The marginal compositions resulted in increased competition between the adversarial models but only led to the multimodal behavior when the competing models diverged. Transparency of the clustering method allowed explicit interpretation of the chemistries leading to such competition. The adversarial ensemble was interpreted through transition from ductile to brittle microstructure.

36 MATERIALS SCIENCE↗

Remanent magnetization and structural effects due to shock in natural and man-made iron-nickel alloys

Explosive shock or meteorite impact are significant remagnetization processes. The mechanisms of remagnetization associated with the dynamic processes depend on the peak shock pressure, the nature of the shocked materials, and the behavior of the shock in the material. Magnetic measurements can be used to classify products formed during a shock process, and magnetic measurements can be used to investigate the process itself because of the special characteristics of the remanent magnetization vectors. The magnetic coercive force increases more rapidly in quenched and annealed iron-nickel alloys as nickel is added than it does in the alloys which have been shocked.

Wasilewski, P. J.↗

Transformation enabled nitride magnets absent rare earths and a process of making the same

A process for producing an ordered martensitic iron nitride powder that is suitable for use as a permanent magnetic material is provided. The process includes fabricating an iron alloy powder having a desired composition and uniformity; nitriding the iron alloy powder by contacting the material with a nitrogen source in a fluidized bed reactor to produce a nitride iron powder; transforming the nitride iron powder to a disordered martensitic phase; annealing the disordered martensitic phase to an ordered martensitic phase; and separating the ordered martensitic phase from the iron nitride powder to yield an ordered martensitic iron nitride powder.

Matthiesen, David↗

Method and apparatus for mapping the distribution of chemical elements in an extended medium

Contaminants in an extended medium such as the wall of a building are mapped by locating neutron excitation source on one side of the wall and a gamma ray spectrometer, including a gamma ray detector on the opposite side of the wall facing the excitation source. The source and detector are moved in unison in discrete steps over opposing wall surfaces so as to determine the chemical composition of the elements in a hemispheric region of the wall adjacent the detector with the radius of the region being substantially that of the mean free path distance of gamma rays emitted from elements interacting with neutrons on the detector side of the wall. The source and detector are reversed for relatively thick walls for mapping the distribution of elements on the other side of the wall thickness. The output of the detector is fed to a multichannel pulse height analyzer where the intensity of the various gamma ray spectral lines are indicated relative to a dominant constituent element such as silicon. Resolution of anomalies such as the presence of voids and/or determining the bulk density of the medium is achieved by substituting a gamma ray source technique is also applied to metal alloys, such as iron alloys, in either the solid or molten state.

Evans, L. G.↗

Atomic-scale electronic inhomogeneity in single-layer iron chalcogenide alloys revealed by machine learning of STM/S data

Chemical pressure from the isovalent substitution of Se by a larger Te atom in the epitaxial film of iron chalcogenide FeSe can effectively tune its superconducting, topological, and magnetic properties. However, such substitution during epitaxial growth inherently leads to defects and structural inhomogeneity, making the determination of alloy composition and atomic sites for the substitutional Te atoms challenging. Here, we utilize machine learning to distinguish between Se and Te atoms in scanning tunneling microscopy images of single-layer FeSe1−xTex on SrTiO3(001) substrates. Defect locations are first identified by analyzing spatial-dependent dI/dV tunneling spectra using the K-means clustering method. After excluding the defect regions, the remaining dI/dV spectra are further analyzed using the singular value decomposition method to determine the Se/Te ratio. Our findings demonstrate an effective and reliable approach for determining alloy composition and atomic-scale electronic inhomogeneity in superconducting single-layer iron chalcogenide films.

Materials Science↗

Sound velocities of iron-nickel (Fe90Ni10) alloy up to 8 GPa and 773 K: The effect of nickel on the elastic properties of bcc-iron at high P-T

Sound velocities of iron and iron-based alloys at high pressure and high temperature are crucial for understanding the composition and structure of Earth’s and other telluric planetary cores. In this study, we performed ultrasonic interferometric measurements of both compressional (ν P ) and shear (ν S ) velocities on a polycrystalline body-centered-cubic (bcc)-Fe 90 Ni 10 up to 8 GPa and 773 K. The elastic moduli and their pressure and temperature derivatives are derived from least-square fits to third-order finite strain equations, yielding K S0 = 154.2(8) GPa, G 0 = 73.2(2) GPa, K' S0 = 4.6(2), G' 0 = 1.5(1), ∂K S /∂T = –0.028(1) GPa/K, and ∂G/∂T = –0.023(1) GPa/K. Furthermore, a comparison with literature data on bcc-Fe suggests that nickel not only decreases both P and S wave velocities but also weakens the temperature effects on the elastic moduli of Fe-Ni alloys.

36 MATERIALS SCIENCE↗

Apollo 14 very low titanium glasses - Melting experiments in iron-platinum alloy capsules

This paper describes two techniques that have been developed to produce Fe-Pt alloy capsules for hgh-pressure experiments, and reports liquidus-phase relations of the Apollo 14 very low titanium glasses determined using Fe-rich capsules (a/Fe/ approximately 0.6). The liquid is multiply saturated with olivine and clinopyroxene at equal to or greater than 22 kbar. The multiple saturation is at least 3 kbar higher than that determined using pure Fe capsules and corresponds to a source region at least 60 km deeper if olivine and clinopyroxene were the residual phases. However, independent data on iron activity or oxygen fugacity of the glasses are still needed in order to choose a container of optimum composition. Preliminary experiments in Fe-poor alloy capsules suggest that the valence state of iron and the crystallization sequence in the melt have changed, possibly as a result of oxidizing materials entrapped during the iron-plating processes. The FeO content of the charge decreases linearly with increasing run duration in experiments using pure Fe capsules. The observation that iron-rich globules grow with time suggests that the equilibrium Fe (bleb) + Fe2O3 (liq) = 3 FeO (liq) might be established in the liquid at high pressure. If this explanation is correct, an appreciable amount of 'FeO' in the liquid could actually be Fe2O3, and some natural lunar volcanic glasses may contain ferric iron as well.

Chen, H.-K.↗

Effect of Nuclear Radiation on Materials at Cryogenic Temperatures

The tensile properties for 33 polycrystalline structural materials including aluminum, titanium, nickel and iron alloys were obtained at -256.5 C (30 deg R) after irradiation exposure at this temperature to 10(exp 17) nvt (E greater than 0.5 Mev), at -256.5 C without previous irradiation, and at approximately 27 C (540 deg R) without previous irradiation. The data were evaluated statistically to permit identification of cryogenic effects and nuclear-cryogenic effects. A number of conclusions were drawn regarding suitability of certain of the materials for use in nuclear-cryogenic applications and regarding the need for further investigation.

NEUTRON BOMBARDMENT↗

The resistance to embrittlement by a hydrogen environment of selected high strength iron-manganese base alloys

Fe-16Mn and Fe-25Mn base alloys, which had been cold worked to yield strength levels of 201 and 178 KSI, were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature under the loading conditions employed in this investigation. Transmission electron microscopy established that bands of epsilon phase martensite and fcc mechanical twins were formed throughout the fcc matrix when these alloys were cold worked. In the cold worked alloys a high density of crystal defects were observed associated with both types of strain induced structures, which should contribute significantly to the strengthening of these alloys. High strength iron base alloys can be produced which appear to have some resistance to degradation of mechanical properties in a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

Influence of Chemical Composition on Rupture Properties at 1200 Degrees F. of Forged Chromium-Cobalt-Nickel-Iron Base Alloys in Solution-Treated and Aged Condition

The influence of systematic variations of chemical composition on rupture properties at 1200 degrees F. was determined for 62 modifications of a basic alloy containing 20 percent chromium, 20 percent nickel, 20 percent cobalt, 3 percent molybdenum, 2 percent tungsten, 1 percent columbium, 0.15 percent carbon, 1.7 percent manganese, 0.5 percent silicon, 0.12 percent nitrogen and the balance iron. These modifications included individual variations of each of 10 elements present and simultaneous variations of molybdenum, tungsten, and columbium. Laboratory induction furnace heats were hot-forged to round bar stock, solution-treated at 2200 degrees F., and aged at 1400 degrees F. The melting and fabrication conditions were carefully controlled in order to minimize all variable effects on properties except chemical composition. Information is presented which indicates that melting and hot-working conditions play an important role in high-temperature properties of alloys of the type investigated.

Reynolds, E E↗

Bosch Carbon Catalyst Regeneration in Water II: Analysis of Bosch Catalyst Beads Throughout the Initial Regeneration Process

Catalyst integrity is an important factor in reactor longevity since it changes the effectiveness of a reaction. A Carbon Formation Reactor (CFR), used within Series Bosch (S-Bosch), utilizes an iron alloy catalyst to convert carbon monoxide and hydrogen into water and solid carbon. The catalyst promotes the formation of carbon to such an extent that pressure-causing clogs form within the reactor and reaction sites on the catalyst become limited. To remove carbon from both the reactor and the surface of the iron alloy catalyst, a technique was developed that utilizes water, an In-Situ Resource Utilization (ISRU) Resource, and agitation to regenerate the reactor. To ascertain catalyst integrity throughout this regenerative process, sample catalyst beads were taken before and after the carbon formation reaction, and then after the regeneration process. Additionally, wastewater from the regeneration process was sampled. The sampled beads and wastewater were observed under a Scanning Electron Microscopy (SEM) microscope and the beads were chemically etched to determine if the catalyst had degraded at any point during this process, and if catalyst was lost. Minimal catalyst degradation was observed after carbon formation in the CFR.

regeneration↗

Bosch Carbon Catalyst Regeneration in Water II: Analysis of Bosch Catalyst Beads Throughout the Initial Regeneration Process

Catalyst integrity is an important factor in reactor longevity since it changes the effectiveness of a reaction. A Carbon Formation Reactor (CFR), used within Series Bosch (S-Bosch), utilizes an iron alloy catalyst to convert carbon monoxide and hydrogen into water and solid carbon. The catalyst promotes the formation of carbon to such an extent that pressure-causing clogs form within the reactor and reaction sites on the catalyst become limited. To remove carbon from both the reactor and the surface of the iron alloy catalyst, a technique was developed that utilizes water, an In-Situ Resource Utilization (ISRU) Resource, and agitation to regenerate the reactor. To ascertain catalyst integrity throughout this regenerative process, sample catalyst beads were taken before and after the carbon formation reaction, and then after the regeneration process. Additionally, wastewater from the regeneration process was sampled. The sampled beads and wastewater were observed under a Scanning Electron Microscopy (SEM) microscope and the beads were chemically etched to determine if the catalyst had degraded at any point during this process, and if catalyst was lost. Minimal catalyst degradation was observed after carbon formation in the CFR.

Series Bosch↗

Prediction of crystal structures and motifs in the Fe–Mg–O system at Earth’s core pressures

Abstract Fe, Mg, and O are among the most abundant elements in terrestrial planets. While the behavior of the Fe–O, Mg–O, and Fe–Mg binary systems under pressure have been investigated, there are still very few studies of the Fe–Mg–O ternary system at relevant Earth’s core and super-Earth’s mantle pressures. Here, we use the adaptive genetic algorithm (AGA) to study ternary Fe x Mg y O z phases in a wide range of stoichiometries at 200 GPa and 350 GPa. We discovered three dynamically stable phases with stoichiometries FeMg 2 O 4 , Fe 2 MgO 4, and FeMg 3 O 4 with lower enthalpy than any known combination of Fe–Mg–O high-pressure compounds at 350 GPa. With the discovery of these phases, we construct the Fe–Mg–O ternary convex hull. We further clarify the composition- and pressure-dependence of structural motifs with the analysis of the AGA-found stable and metastable structures. Analysis of binary and ternary stable phases suggest that O, Mg, or both could stabilize a BCC iron alloy at inner core pressures.

Wang, Renhai↗

Sound velocities and thermal equation of state of fcc -iron-nickel alloys at high pressure and high temperature: Implications for the cores of Moon and several planets

Fcc-Fe-Ni alloy is believed to be the most dominant solid constitute of moderate-sized terrestrial planetary cores. Investigating the physical properties, especially the density and sound velocity of Fe-Ni alloys and comparing them with seismic observations is an indispensable approach to constructing compositional models for planetary interiors. In this study, we conducted sound velocity measurements on Fe-Ni alloys with 10 wt.% and 20 wt.% Ni up to ∼13.5 GPa and 1073 K, using the ultrasonic interferometry technique in a multi-anvil apparatus in conjunction with synchrotron radiation. By fitting the experimental data to finite strain equations, the bulk and shear moduli and their pressure and temperature derivatives are derived, yielding K S0 =145.8(14) GPa, G 0 = 73.2(7) GPa, K S0 ’ = 5.89(24), G 0 ’ = 2.89(8), (∂K S /∂T) P = -0.0181(12) GPa/K and (∂G/∂T) P = -0.0393(10) GPa/K for fcc-Fe 80 Ni 20 . An examination of the density-velocity relationship shows that compressional wave velocity is insensitive to temperature within the current pressure and temperature range, while shear wave velocity exhibits a large reduction with increasing temperature. Here, extrapolation of the sound velocities following the finite strain theories suggests that much slower Vs should be expected at pressure and temperature conditions corresponding to those of the lunar core. Possible core density and velocity profiles for other moderate planets and satellites, such as Mars, Mercury, and Ganymede are also calculated.

Equation of state↗