Study of diamond film growth and properties

The objective was to study diamond film growth and its properties in order to enhance the laser damage threshold of substrate materials. Calculations were performed to evaluate laser induced thermal stress parameter, R(sub T) of diamond. It is found that diamond has several orders of magnitude higher in value for R(sub T) compared to other materials. Thus, the laser induced damage threshold (LIDT) of diamond is much higher. Diamond films were grown using a microwave plasma enhanced chemical vapor deposition (MPECVD) system at various conditions of gas composition, pressure, temperature, and substrate materials. A 0.5 percent CH4 in H2 at 20 torr were ideal conditions for growing of high quality diamond films on substrates maintained at 900 C. The diamond films were polycrystalline which were characterized by scanning electron microscopy (SEM) and Raman scattering spectroscopy. The top surface of the growing film is always rough due to the facets of polycrystalline film while the back surface of the film replicates the substrate surface. An analytical model based on two dimensional periodic heat flow was developed to calculate the effective in-plane (face parallel) diffusivity of a two layer system. The effective diffusivity of diamond/silicon samples was measured using a laser pulse technique. The thermal conductivity of the films was measured to be 13.5 W/cm K, which is better than that of a type Ia natural diamond. Laser induced damage experiments were performed on bare Si substrates, diamond film coated Si, and diamond film windows. Significant improvements in the LIDT were obtained for diamond film coated Si compared to the bare Si.

Albin, Sacharial↗

Ultra Wide Bandgap Laser Addressable Photoconductors

Wide Band Gap (WBG) and Ultra Wide Band Gap (UWBG) photoconductors have the potential to meet several critical mission needs for LLNL and the broader USG due to their exceptional characteristics related to large critical electric field. In particular, high energy laser systems such as the National Ignition Facility would benefit from the development of new materials for active optical devices such as the Optically Addressable Light Valve (OALV) used in the Programmable Spatial Shaper System. Missions in Global Security would benefit from higher performance Photoconductive Semiconductor Switches for pulsed power and radiofrequency amplifiers. This project examined the suitability of both commercially available and custom synthesized semi insulating WBG and UWBG materials for several of these applications. We developed high laser damage threshold OALVs for optical systems based on several of these materials as well as new RF, pulsed power, and power electronics devices based on the same. These devices show superior power handling in terms of laser damage threshold, electric field, and power output. A number of the technologies developed have been transitioned to both internal and external customers.

42 ENGINEERING↗

Laser-induced damage-growth threshold at 351 nm in the nanosecond regime in dielectric coatings employing different high-index materials

The laser-damage performance of HfO 2 /SiO 2 and Al 2 O 3 /SiO 2 mirrors was investigated at a laser wavelength of 351 nm with nanosecond pulse durations. A method was developed to quantify the laser-induced damage-growth threshold under conditions relevant to high-repetition-rate, large-aperture laser systems. The results suggest that the damage-growth performance cannot be inferred from the corresponding damage-initiation threshold that is commonly used to evaluate the performance of optical materials. Here, a systematic difference was also observed in the performance between these two groups of high-index materials, with the Al 2 O 3 /SiO 2 mirrors exhibiting about twofold improvement in the damage-growth threshold.

36 MATERIALS SCIENCE↗

Manufacturing-induced contamination in common multilayerdielectric gratings

Contamination of pulse compression gratings during the manufacturing process is known to give rise to reduced laser damage performance and represents an issue that has not yet been adequately resolved. The present work demonstrates that the currently used etching methods introduce carbon contamination inside the etched region extending to a 50- to 80-nm layer below the surface. This study was executed using custom samples prepared in both, a laboratory setting and by established commercial vendors, showing results that are very similar. The laser-induced-damage performance of the etched and unetched regions in the grating-like samples suggest that contaminants introduced by etching process are contributing to the reduction of the laser-induced damage threshold.

42 ENGINEERING↗

Diamond films for laser hardening

Laser-damage experiments were performed on free-standing polycrystalline diamond films prepared by plasma-enhanced CVD. The high laser-induced stress resistance found for this material makes it useful for thin-film coatings for laser optics. Results for diamond-coated silicon substrates demonstrate the enhanced damage threshold imparted by diamond thin-film coatings to materials susceptible to laser damage.

Albin, S.↗

Methods and apparatus for comprehensive characterization of performance attributes and damage thresholds of ultrafast laser optics

It is presently well understood that the operational performance limits of optics are determined by three fundamental attributes: the initiation of laser-induced damage, the growth of damage sites, and the transient (nondamaging) modification of optical parameters. The comprehensive characterization of the performance limitations of ultrafast optics requires consideration of all three fundamental attributes. Here, the vast majority of literature to date, however, has focused primarily on damage-initiation and testing systems that are largely focused on determining the damage-initiation threshold under single- and multipulse excitation. In this work, we discuss a testing apparatus that was designed to offer the capability to adequately characterize all three of these performance attributes under femtosecond, near-infrared laser irradiation. Key aspects of methodology are discussed, including high-dynamic-range energy control, variable beam size, wavelength tunability, B-integral management, and functional performance characterization to explore the true operational limits of the components. Example results for a metal-dielectric mirror demonstrate the test station’s operation.

42 ENGINEERING↗

Influence of Oxygen Flow and Stoichiometry on Optical Properties and Damage Resistance of Hafnium Oxide Thin Films

Hafnium oxide (HfO 2 ) is predominantly used as a high-index material in multi-layer dielectric coatings for high-peak- and high-average-power lasers, but laser damage often initiates within the HfO 2 layers despite their wide bandgap. Oxygen deficiency during deposition can introduce vacancy-related sub-bandgap states and absorptive defects, lowering damage resistance. This study investigates how oxygen flow during HfO 2 deposition with ion beam sputtering (IBS) affects its stoichiometry, defect formation, and nanosecond laser-induced damage threshold (LIDT) and whether single-layer trends predict multilayer performance. Single layers were deposited at varying oxygen flows, characterized for optical and structural properties, and tested for the LIDT at 1064 nm and 355 nm. Increasing oxygen flow drove the layer toward near-stoichiometric HfO 2 , reduced the refractive index, and altered the density of surface pinhole-like features. The single-layer LIDT at 355 nm increased with oxygen, whereas the 1064 nm LIDT was comparatively less sensitive to oxygen flow, consistent with the wavelength-dependent roles of absorptive precursors and microstructural defects. In contrast, a HfO 2 -based high-reflector (HR) showed a higher LIDT at lower oxygen flow, indicating that the family of damage precursors changes between single layers and multilayers; in stacks, structural properties such as stress, gas entrapment and thermal dissipation may outweigh the isolated absorptive defects found in single layers. These results demonstrate that the optimal oxygen flow condition depends on both LIDT wavelength and film architecture. We identified, for single layers, a 15–35 sccm window for maximizing the 1064 nm LIDT and a high-flow optimum (45 sccm) for the 355 nm LIDT and, for 355 nm HR stacks, a distinct lower-flow regime (~10 sccm).

Optics and optical instruments↗

Enhanced Damage-Resistant Optics for Spaceflight Laser Systems: Workshop findings and recommendations

NASA has defined a program to address critical laser-induced damage issues peculiar to its remote sensing systems. The Langley Research Center (LaRC), with input from the Goddard Space Flight Center (GSFC), has developed a program plan focusing on the certification of optical materials for spaceflight applications and the development of techniques to determine the reliability of such materials under extended laser exposures. This plan involves cooperative efforts between NASA and optics manufacturers to quantify the performance of optical materials for NASA systems and to ensure NASA's continued application of the highest quality optics possible for enhanced system reliability. A review panel was organized to assess NASA's optical damage concerns and to evaluate the effectiveness of the LaRC proposed program plan. This panel consisted of experts in the areas of laser-induced damage, optical coating manufacture, and the design and development of laser systems for space. The panel was presented information on NASA's current and planned laser remote sensing programs, laser-induced damage problems already encountered in NASA systems, and the proposed program plan to address these issues. Additionally, technical presentations were made on the state of the art in damage mechanisms, optical materials testing, and issues of coating manufacture germane to laser damage.

Schulze, Norman↗

Effect of THz-bandwidth incoherent laser radiation on bulk damage in potassium dihydrogen phosphate crystals

Abstract The laser-damage performance characteristics of potassium dihydrogen phosphate (KDP) samples under exposure to a distinctive broadband incoherent laser pulse are investigated. A laser system providing such pulses is intended to explore improved energy-coupling efficiency on the target in direct-drive inertial confinement fusion experiments and provides incoherent bandwidths as large as 10 THz in a nanosecond pulse. A consequence of this bandwidth is very rapid fluctuations in intensity capable of reaching maxima much larger than the average intensity within the pulse. A custom damage-test station has been built to perform measurements with broadband incoherent pulses in order to determine what effect these fast and high-intensity oscillations have on laser damage. A set of experiments under different bandwidth and beam configurations shows the effect to be minimal when probing bulk damage in KDP. Modeling indicates this behavior is supported by long electron-relaxation times compared to the source-field fluctuations, following excitation of individual electrons in the conduction band. The results help better understand the laser-induced–damage mechanisms in KDP, and its ability to operate in broadband temporally incoherent high-energy lasers that may be particularly suitable for future laser-fusion energy systems.

36 MATERIALS SCIENCE↗

Evaluation of the interfacial bonding strength between hafnia and silica layers deposited by electron-beam evaporation

Factors contributing to the mechanical strength of multilayer optical coatings involving alternating layers of electron-beam evaporated hafnia and silica is investigated. It is observed that upon rupture resulting from nanosecond laser damage, fragments consisting of layer pairs are produced. These pairs are formed as a result of a strong asymmetry in adhesion strength between interfaces, leading to preferential delamination at interfaces where silica is deposited on hafnia, and not the reverse, despite the fact that both interface types consist of the same pair of materials. The observed disparity in adhesion strength was further studied using nanomechanical scratch tests, revealing loads at which fracture occurs, and fracture morphology, both of which are highly dependent on deposition order. Based on these measurements, along with the morphological analysis of the nanostructure of the coatings, we conclude that the surface microstructure in each coating layer affects its adhesion strength with the succeeding layer. The findings outlined here are particularly relevant to the production of large aperture, high-performance optics designed for use in next-generation lasers.

adhesion strength↗

Improving the laser performance of ion beam sputtered dielectric thin films through the suppression of nanoscale defects by employing a xenon sputtering gas

Laser damage-prone precursors in high index materials such as hafnia are believed to be the primary limiter in the performance of dielectric multilayer films to advance ultra-high power and energy laser applications. Removing or suppressing these precursors is the key to fabricating laser damage resistant thin films for the enabling technologies. Early work has revealed that nanobubbles formed by entrapped argon (Ar) working gas in ion beam sputtering (IBS) produced hafnia films are primarily responsible for the onset of laser damage upon exposure to UV, ns-laser pulses. In this study, we demonstrate that the UV ns-laser damage onset of IBS produced hafnia films can be improved to 3.1 +/- 0.2 J/cm 2 by substituting the conventional Ar working gas with xenon (Xe), a nearly 1 J/cm 2 increase from that of the Ar produced hafnia films. In addition to the suppression of the overall point-defect density of the hafnia films, the reduction of the Xe entrapment eliminates the nanobubbles and the generation of plasmas that initiates the laser damage. The defect suppression and its correlation to the increase in laser damage threshold is revealed by the combined analysis of Rutherford backscattering spectroscopy, electron paramagnetic resonance spectroscopy, transmission electron microscopy, and laser damage testing. Monte Carlo simulations suggest a much smaller entrapment of Xe gas by comparison to Ar, which is attributed to the significant difference in the energy of the reflected neutrals (3X) which are likely to be implanted. These results provide an effective process route with a fundamental understanding for producing high laser damage resistant dielectric films for high power and high energy laser applications.

36 MATERIALS SCIENCE↗

Novel Co:MgF2 lidar for aerosol profiler

Lidars are of great interest because of their unique capabilities in remote sensing applications in sounding of the atmosphere, meteorology, and climatology. In this small business innovative research (SBIR) phase II program, laser sources including Co:MgF2, CTH:YAG, CTH:YSGG, CT:YAG, and Er:Glass were evaluated. Modulator of fused silica and TeO2 materials with Brewster's angle end faces were used with these lasers as acousto-optical (AO) Q-switches. A higher hold-off energy and hence a higher Q-switched energy was obtained by using a high power RF driver. The report provides performance characteristics of these lasers. The tunable (1.75-2.50 microns) Co:MgF2 laser damaged the TeO2 Q-switch cell. However, the CTH:YAG laser operating at 2.09 microns provided output energy of over 300 mJ/p in 50 ns pulse width using the fused silica Q-switch. This Q-switched CTH:YAG laser was used in a breadboard vertical aerosol profiler. A 40 cm diameter telescope, InSb and InGaAs detectors were used in the receiver. The data obtained using this lidar is provided in the report. The data shows that the eye safe lidar using CTH:YAG laser for the vertical aerosol density and range measurements is the viable approach.

Acharekar, M. A.↗

Polyvinyl acetate-based polymer host for optical and far-infrared spectroscopy of individualized nanoparticles

Preparation techniques for producing films of individualized solution-dispersed nanoparticles (NPs) for optical spectroscopy are frequently technically challenging and tailored for a specific NP system. In this work, we present a rapid, easy, and economical technique for producing polyvinyl acetate (PVAc)-based NP-polymer films on the order of 100’s of micrometers thick that exhibit high uniformity, low aggregation, excellent optical transparency, and low terahertz absorption. In addition, we find that these films are robust at cryogenic temperatures and have a high laser damage threshold of 0.3 TW cm –2 , which make them suitable for pulsed laser measurements. We show that free-standing, flexible, PVAc films can incorporate both one-dimensional single-wall carbon nanotubes (SWCNTs) and zero-dimensional Au NPs. Using absorbance, Raman scattering, and photoluminescence excitation spectroscopy, we observe that SWCNT individualization is maintained, and minimized polymer strain imposed, when the nanotubes are transitioned from the solution to the polymer host. This PVAc-based polymer host presents researchers with a straightforward method for producing free-standing and flexible NP films with low aggregation.

36 MATERIALS SCIENCE↗