Editors’ Choice—Examining Performance and Durability of Anion Exchange Membrane Fuel Cells with Novel Spirocyclic Anion Exchange Membranes

A series of spirocyclic copolymer membranes with varying ion exchange capacities (IECs) were investigated to probe the impact of polymer properties on in situ fuel cell performance and stability. In-situ electrochemical tests and post-mortem electron microscopy analysis of cross-sectioned membrane electrode assemblies (MEAs) have been combined with voltage loss breakdown analysis to evaluate the performance and degradation of different MEAs, and to probe the catalyst morphology and electrode structure at different stages of operation. Voltage loss breakdown results show that membrane degradation and kinetic losses played only a minor role in observed performance degradation and that performance losses were primarily related to increasing mass transport losses. From microscopy studies, carbon corrosion and Pt nanoparticle growth were identified at both the cathode and anode although more pronounced on the cathode resulting in significant structural changes. The membrane with the lowest IEC (1.3 mmolg −1 ) demonstrated the lowest peak power density ~ 1.16 W cm −2 , however, it showed the most stable performance (constant 0.6 A cm −2 hold) with ~ 5% degradation over 540 h. Isolation of performance losses and microscopic analysis of electrodes for anion exchange membrane fuel cells has not been reported previously, and these results help identify critical performance degradation concerns.

25 ENERGY STORAGE↗

Investigating the Effects of Copper Impurity Deposition on the Structure and Electrochemical Behavior of Hydrogen Evolution Electrocatalyst Materials

Electrolysis of impure water (such as seawater) has recently garnered research interest as it may enable hydrogen production at reduced costs. However, the tendency of impurity ions and other species to degrade electrocatalysts and membranes within an electrolyzer is a serious challenge. Here, we investigate the effects of copper impurities of varying concentrations on the hydrogen evolution reaction (HER) using platinum electrocatalysts. A decrease of current density is observed with an increasing copper concentration. By comparing the effect of ionic impurities on current density at different concentrations, we gain insight into how impurities can interfere with the HER at different potentials. Surface characterization of the electrodes reveals differences in the morphology and extent of copper deposition on HER-active platinum vs inactive gold electrodes. This enables an improved understanding of how copper nucleates and grows on the two types of electrodes under different electrochemical conditions while also confirming deposition in low-concentration cases, as present in seawater. The results indicate that copper electrodeposition competes with the HER, and the nature of copper electrodeposition varies depending on the electrocatalytic activity of the electrode. This study provides insight toward catalyst design that can withstand the effects of impurity-induced degradation over extended use.

08 HYDROGEN↗

Cross-Linker Selection Controls Glass Transition Elevation or Reduction in Dynamic Covalently Bonded Polymer Networks

Introducing cross-links is a powerful approach to improve polymeric material performance relevant to controlling viscoelasticity, thermal and creep resistance, degradability, and efficient membrane separations. The chemically specific glass transition temperature T g is of fundamental importance in determining the time scales of key dynamical processes and physical state of the material in such applications. Here, we study experimentally how the introduction of relatively large cross-linking molecules in slowly exchanging dynamic bond-forming polymers (vitrimers) impacts vitrification for diverse polymer chemistries and a wide range of cross-link fractions. We find T g can increase, decrease, or even remain essentially unchanged, in qualitative contrast to the generic elevation of T g in traditional permanent polymer networks. We formulate an effective terpolymer network model to understand this rich behavior, which emerges as a consequence of a competition between pure cross-linking and generalized plasticization effects. The latter is associated with the tunable cross-linker size and intrinsic dynamic mobility that can offset slowing down due to traditional permanent cross-linking constraints. Here, a new strategy for functional polymer network design is suggested based on adjusting the relative importance of the two competing physical effects, which potentially can significantly enhance energy savings in applications while retaining other intrinsic properties germane to advanced materials performance.

Copolymers↗

Poly(norbornene) anion conductive membranes: homopolymer, block copolymer and random copolymer properties and performance

It has previously been shown that phase-separated block copolymers with non-ion conducting (hydrophobic) blocks and ion conducting (hydrophilic) blocks can form efficient ion conducting channels with high ionic mobility and conductivity. Block copolymers can provide a means for phase segregation and ion channel formation while homopolymers and random copolymers have been shown to have lower ion mobility. In this study, the properties of poly(norbornene) based anion exchange membranes (AEMs) comprising homopolymers, block copolymers, and random copolymers with high ion-exchange capacity (IEC) (3.48–4.55 meq. g -1 ) have been investigated and compared. The polymers were cross-linked with N,N,N',N'-tetramethyl-1,6-hexanediamine before casting the membranes to avoid excessive water swelling due to high water uptake. It was shown that high ionic conductivity can be achieved in both random copolymers and homopolymers even in the absence of microphase-separated structures. For example, the conductivity of a random copolymer was 194 mS cm -1 at 80 °C, which was comparable to the block copolymer, 201 mS cm -1 at 80 °C. The H 2 /O 2 fuel cell performance of random copolymer composite membranes showed a peak power density of 3.05 W cm -2 and peak current density of 7.85 A cm -2 at 80 °C compared to block copolymer membranes (peak power density of 3.21 W cm -2 and peak current density of 8.27 A cm -2 at 80 °C). It is more critical that high water transport be achieved in AEMs than achieving a phase-segregated morphology. Finally, the homopolymer, block copolymer, and random copolymer membranes showed <1.35% degradation after aging in 1 M NaOH at 80 °C for 1000 h.

08 HYDROGEN↗

The SEMA3F-NRP1/NRP2 axis is a key factor in the acquisition of invasive traits in in situ breast ductal carcinoma

A better understanding of ductal carcinoma in situ (DCIS) is urgently needed to identify these preinvasive lesions as distinct clinical entities. Semaphorin 3F (SEMA3F) is a soluble axonal guidance molecule, and its coreceptors Neuropilin 1 (NRP1) and NRP2 are strongly expressed in invasive epithelial BC cells. We utilized two cell line models to represent the progression from a healthy state to the mild-aggressive or ductal carcinoma in situ (DCIS) stage and, ultimately, to invasive cell lines. Additionally, we employed in vivo models and conducted analyses on patient databases to ensure the translational relevance of our results. We revealed SEMA3F as a promoter of invasion during the DCIS-to-invasive ductal carcinoma transition in breast cancer (BC) through the action of NRP1 and NRP2. In epithelial cells, SEMA3F activates epithelialmesenchymal transition, whereas it promotes extracellular matrix degradation and basal membrane and myoepithelial cell layer breakdown. Together with our patient database data, these proof-of-concept results reveal new SEMA3F-mediated mechanisms occurring in the most common preinvasive BC lesion, DCIS, and represent potent and direct activation of its transition to invasion. Moreover, and of clinical and therapeutic relevance, the effects of SEMA3F can be blocked directly through its coreceptors, thus preventing invasion and keeping DCIS lesions in the preinvasive state.

60 APPLIED LIFE SCIENCES↗

Relief Zones Enhance the Durability of Ultrathin Membranes in Electrochemical Conversion Devices

Premature failures in electrochemical conversion systems often result when membrane electrode assemblies (MEAs) use ultrathin (≤15 μm-thick) polymer electrolyte membranes, susceptible to mechanical degradation from stress concentrations arising from device-level integration. Herein, relief zones were developed to mitigate mechanical degradation by alleviating excess and nonuniform compression across active areas. Relief zones, created through ablation of carbonaceous diffusion media, enable seamless adaptation across MEA dimensions without need for hardware modifications. Demonstrated using fuel cells as a case study, accelerated stress tests revealed a 6-fold lifetime improvement (∼1500 h) compared to conventional edge-protected MEAs, decoupling device-level engineering effects from material limitations.

accelerated stress test↗

Assessing the Oxidative Stability of Anion Exchange Membranes in Oxygen Saturated Aqueous Alkaline Solutions

While anion exchange membrane water electrolyzers show promise as a source of green hydrogen using low-temperatures and non-platinum group metal catalysts, many concerns must be addressed. A primary challenge for the development of high-performance anion exchange membrane water electrolyzers is the fabrication of a stable membrane that will be able to survive long-term stability test while maintaining high anion conductivity, which is a necessity for a durable water electrolyzer. This method will present a standardized protocol that can be used by researchers to assess the quality of their AEM materials and be able to provide insight into how materials may be degrading and how to improve the quality of AEMs. Using Mohr or Volhard titration to measure ion-exchange capacity, EIS to determine the ionic conductivity, NMR and FTIR to understand the extent of membrane degradation over time, and mechanical analyzers to determine the strength of their AEMs, this standardized protocol will guide researchers to determining and improving upon the long-term durability and performance of their AEM materials.

36 MATERIALS SCIENCE↗

PERFORMANCE CHARACTERIZATION OF THE DIRECT CONTACT MEMBRANE DISTILLATION MODULE OPERATED WITH HIGHLY CONCENTRATED SOLUTION

The experimental study was conducted to characterize the performance of the flat sheet Direct Contact Membrane Distillation. The length degradation was studied in a short and long module with and without spacers. The experimental study is validated using the predicted flux for a wide range of operating conditions using deionized water. Three different membranes are used in the parametric study for feed Reynolds number varied between 500 and 2000, and inlet feed temperature varied between 45°C and 80°C. PTFE membrane was shown to be more effective than the PVDF due to its higher permeability coefficient and higher hydrophobicity. Fouling study was conducted on the selected PTFE membrane with various feed Reynolds numbers between 500 and 2000 and feed inlet temperature between 50°C and 80°C. Membranes used in the fouling study were characterized using scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS) for the morphology and chemical composition of the fouling layer. 36 hours of operation with 10 wt% NaCl (100,000 ppm) at feed inlet temperatures 80°C and 60°C and fixed Reynolds 2000 demonstrated a drop in flux by 31% and 27%, respectively. Low flow rate and high temperature are favorable conditions for fouling formation and reduced permeate flux for highly concentrated solutions. The spacers improved the flux by 30.8% and 27.6% at the operating Reynolds numbers 2000 the short and long channel modules. This study helps to design and optimize DCMD modules for industrial-size desalination and water treatment applications.

Kim, Deliya↗

Strong degradation of polycarbonate and polystyrene by the CO 2 capture solvent diethyl sebacate

Here, we report on observations of strong degradation of a polycarbonate vessel by a solvent being considered for a CO 2 capture process, diethyl sebacate. This degradation led to failure of a polymeric hollow fiber membrane unit. Additional tests showed rapid degradation of polycarbonate safety glasses and polystyrene-based petri dishes by exposure to diethyl sebacate at ambient conditions. We also report on safe operations with diethyl sebacate in extensive experiments studying the corrosion of steel in CO 2 -pressurized reactors lined with PTFE and using PTFE gaskets. Used diethyl sebacate was also stored for long time periods in bottles made from low-density polyethylene bottles without physical deterioration. These observations indicate that care must be taken in development of new contactors and processes for CO 2 capture with diethyl sebacate and related solvents and in the choice of material for storage.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidating the degradation mechanisms of Pt-free anode anion-exchange membrane fuel cells after durability testing

The development of anion-exchange membrane fuel cells (AEMFCs) has recently accelerated due to synergistic improvements yielding highly conductive membranes, stable ionomers, and enhanced alkaline electrocatalysts. However, cell durability, especially under realistic conditions, still poses a major challenge. Herein, we employ low-loadings of Pt-free Pd-based catalysts in the anode of AEMFCs and elucidate potential degradation mechanisms impacting long-term performance under conditions analogous to the real-world (high current density, H 2 –air (albeit CO 2 -free), and intermittent operation). Our high-performing AEMFCs achieve impressive performance with power densities approaching 1 W cm —2 and current densities up to 3.5 A cm —2 . Over a 200 h period of continuous operation in H 2 –air at a current density of 600 mA cm —2 , our model Pd/C–CeO 2 anode cell exhibits record stability (~30 μV h —1 degradation) compared to the literature and up to 6× better stability than our Pd/C and commercial Pt/C anode cells. Following an 8 h shutdown, the Pd/C–CeO 2 anode cell was restarted and continued for an additional 300 h with a higher degradation rate of ~600 μV h —1 . Thorough in situ evaluations and post-stability analyses provide insights into potential degradation mechanisms to be expected during extended operation under more realistic conditions and provide mitigation strategies to enable the widespread development of highly durable AEMFCs.

08 HYDROGEN↗

Drawing on Membrane Photocatalysis for Fouling Mitigation

Photocatalysis is an effective and environmentally friendly approach for degrading organic pollutants, particularly in scenarios where sunlight can be utilized as the energy source. Opportunities are emerging to apply materials and methods from photocatalytic pollutant degradation to address the challenge of fouling. Membrane fouling, attributed to organic foulants, is a prevalent problem for all membrane-based technologies and represents a major deleterious impact on membrane performance. Integration of tactics developed in photocatalysis more broadly to membranes reveals new strategies for membrane fouling control-an approach taken by an increasing number of researchers. Furthermore, this review summarizes key developments in photocatalytic materials and methods in water treatment and presents recent progress in the development of processes for photocatalytic alleviation of membrane fouling, including photocatalyst design and modification strategies aimed at enhancing photocatalytic efficiency, as well as different configurations of photocatalysis-membrane systems (PMS). Perspectives on future research and development opportunities for photocatalytic membrane fouling control are also provided.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical characterization of evolving ionomer/electrocatalyst interactions throughout accelerated stress tests

Here, the degradation of polymer electrolyte membrane fuel cells (PEMFCs) catalyst layers used for heavy-duty vehicles was examined using a catalyst-specific accelerated stress test (AST). High surface area carbon supported dispersed Pt (Pt/HSC), annealed Pt (a-Pt/HSC) and PtCo (PtCo/HSC) alloy catalysts were examined over the course of 90,000 cycles by measuring changes in mass activity, O 2 transport resistance, electrochemical active surface area (ECSA), catalyst accessibility and ionomer-electrocatalyst interactions. Compared to a-Pt/HSC and Pt/HSC catalyst, the PtCo/HSC showed better initial mass activity, a larger initial mass transport loss, and faster degradation after the first 30k AST cycles, as a large portion of Co leached out during potential cycling. Pt/HSC showed higher initial performance relative to a-Pt/HSC but had faster degradation. STEM characterizations show that the ECSA losses are largely related to Pt dissolution resulting in either catalyst particle growth via the Ostwald ripening mechanism or redeposition in the membrane. Catalyst accessibility measurements showed decreased RH sensitivity for all three samples, while CO impedance measurements revealed a decrease in both Pt-water and carbon-water interactions. This implies that, Pt is either preferentially redepositing on the exterior of the carbon support, or that the ionomer is undergoing morphological changes enabling the enhanced intrusion of mesopores.

25 ENERGY STORAGE↗

Sulfonated Diels–Alder Poly(Phenylene)s in Membrane Electrode Assemblies for Fuel Cells

The transition to environmentally sustainable materials in fuel cells requires alternatives to persistent polyfluoroalkyl substances (PFAS) like Nafion. This study investigates the performance-limiting factors of membrane electrode assemblies (MEAs) utilizing sulfonated Diels–Alder poly(phenylene)s (sDAPPs) as PFAS-free polymer electrolytes. Among the configurations evaluated, the greatest performance loss occurred when sDAPP is used as the cathode binder, primarily due to phenyl group adsorption on catalyst surfaces, which reduces oxygen reduction reaction activity and impedes oxygen transport. Additional performance degradation arises from membrane-electrode interfacial incompatibility and insufficient ionomer hydrophobicity. By addressing ionomer adsorption and improving interfacial contact, an sDAPP-based cathode achieved a current density of 1.57 A cm −2 at 0.6 V under fully humidified H 2 /air conditions at 80 °C and 150 kPa abs . These results offer key insights for advancing high-performance, PFAS-free fuel cell technologies.

08 HYDROGEN↗

Harnessing autocatalytic reactions in polymerization and depolymerization

Abstract Autocatalysis and its relevance to various polymeric systems are discussed by taking inspiration from biology. A number of research directions related to synthesis, characterization, and multi-scale modeling are discussed in order to harness autocatalytic reactions in a useful manner for different applications ranging from chemical upcycling of polymers (depolymerization and reconstruction after depolymerization), self-generating micelles and vesicles, and polymer membranes. Overall, a concerted effort involving in situ experiments, multi-scale modeling, and machine learning algorithms is proposed to understand the mechanisms of physical and chemical autocatalysis. It is argued that a control of the autocatalytic behavior in polymeric systems can revolutionize areas such as kinetic control of the self-assembly of polymeric materials, synthesis of self-healing and self-immolative polymers, as next generation of materials for a sustainable circular economy. Graphic Abstract

36 MATERIALS SCIENCE↗

Pseudomonas aeruginosa C-Terminal Processing Protease CtpA Assembles into a Hexameric Structure That Requires Activation by a Spiral-Shaped Lipoprotein-Binding Partner

Pseudomonas aeruginosa CtpA is a carboxyl-terminal processing protease that partners with the outer membrane lipoprotein LbcA to degrade at least five cell wall-associated proteins, four of which are cell wall hydrolases. This activity plays an important role in supporting P. aeruginosa virulence in a mouse model of acute pneumonia. However, almost nothing is known about the molecular mechanisms underlying CtpA and LbcA function. Here, we used structural analysis to show that CtpA alone assembles into an inactive hexamer comprising a trimer of dimers, which limits its substrate access and prevents nonspecific degradation. The adaptor protein LbcA is a right-handed open spiral with 11 tetratricopeptide repeats, which might wrap around a substrate to deliver it to CtpA for degradation. By structure-guided mutagenesis and functional assays, we also showed that the interfaces of the CtpA trimer of dimers and an N-terminal helix of LbcA are important for LbcA-mediated substrate degradation by CtpA both in vitro and in vivo. This work improves our understanding of the molecular mechanism of the LbcA-CtpA proteolytic system and reveals some striking differences from the arrangements found in some other bacterial CTPs.

structural biology↗